Dupont Sclairfilm Lx 1 Lldpe Film Laminating 50 8 µm Thickness

DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness

    • Product Name: DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 821272
    Thickness 50.8 µm
    Density 0.920 g/cm³
    Tensile Strength At Break 24.1 MPa
    Tensile Strength At Yield 10.3 MPa
    Elongation At Break 600%
    Tensile Modulus 172 MPa
    Elmendorf Tear Strength 350 g
    Dart Drop Impact 120 g
    Haze 6%
    Gloss 80%
    Coefficient Of Friction 0.20
    Water Vapor Transmission 15.5 g/m²/24h
    Oxygen Transmission 1550 cm³/m²/24h
    Melting Point 122°C
    Vicat Softening Point 95°C

    As an accredited DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied as one roll per protective, moisture-resistant carton of 50.8 µm DuPont™ Sclairfilm® LX-1 LLDPE laminating film.
    Container Loading (20′ FCL) 20′ FCL container loading of palletized DuPont Sclairfilm LX-1 LLDPE laminating film rolls, 50.8 µm, secured for ocean shipment.
    Shipping DuPont™ Sclairfilm® LX-1 LLDPE laminating film (50.8 µm) ships as a non-hazardous, non-DG plastic film. Rolls are wrapped, boxed, and palletized to protect against moisture, dust, heat, sunlight, and puncture. Store upright/secure in a cool, dry area, handling carefully to avoid creasing or damage.
    Storage Store DuPont™ Sclairfilm® LX-1 LLDPE Film in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep rolls in original packaging, supported upright or horizontal as supplied, to prevent crushing, dust, moisture, and physical damage. Maintain moderate temperature and humidity; avoid prolonged UV exposure. Follow local regulations and manufacturer’s guidelines.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original packaging at temperatures below 30°C, away from sunlight and moisture.
    Application of DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness

    Dry-laminated flexible food packaging uses 50.8 µm DuPont™ Sclairfilm® LX-1 as the inner sealant web rather than as a monolayer surface-print film. Converter verification of corona treatment at 38–42 dyn/cm is required before adhesive application; the web is laminated to a reverse-printed barrier substrate—typically 12–18 µm BOPET or 20 µm BOPP—with a food-contact polyurethane adhesive applied at 2.0–3.5 g/m² dry coating weight. In this construction, the 50.8 µm LLDPE layer usually represents 25–35% of the finished laminate thickness and acts as the heat-seal layer; lowering the LLDPE fraction below 20% reduces puncture resistance at frozen distribution temperatures, while raising it above 40% induces curl and web-tracking instability on multi-lane slitting. Food-contact compliance is assessed under FDA 21 CFR 177.1520(c) 3.2a, 21 CFR 175.105, and Regulation (EU) No 10/2011 with migration testing using 3% acetic acid and 10% ethanol simulants. The lamination process comprises gravure application of solvent or solventless adhesive, two-zone oven drying at 75–95°C, nip lamination of the printed web to the LLDPE at 60–80°C, and room-temperature curing for 24–48 h. Terminal products include frozen seafood pouches, dry mix pouches, and sugar confectionery pillow packs, where low-temperature sealability and high hot tack maintain seal integrity on high-speed fillers.

    Application corePrimary standardAssessment parameter
    Food-contact sealant webFDA 21 CFR 177.1520(c) 3.2aOlefin polymer extractives
    Adhesive lamination21 CFR 175.105Indirect additive migration
    Sterile barrier packagingISO 11607-1:2019Seal strength and package integrity
    Print overlaminateASTM D3330/D3330MPeel adhesion
    Pharmaceutical liddingPh. Eur. 3.1.3Polyolefin packaging monograph
    Bag-in-box linersRegulation (EU) No 10/2011Overall migration

    What Seal Initiation Window Applies to 50.8 µm LX-1 on Vertical Pouching Lines?

    On vertical form-fill-seal machines running intermittent sealing jaws, the seal initiation window of the 50.8 µm LX-1 web is generally quoted between 95°C and 115°C for a 0.4–0.8 s dwell at 40–60 N/cm² jaw pressure, but confirmation runs on a specific line are required because jaw temperature uniformity varies by ±8°C on older reciprocating machines. Published Sclairfilm LX-1-specific seal initiation data are limited; the figures below are derived from industrial LLDPE laminating webs of identical thickness and should be confirmed on the target pouch machine. In the adhesive-laminated structure, the LLDPE sealant layer remains 100% of the sealant-side formulation; if an anti-block masterbatch is introduced downstream, the addition ratio is kept below 1500 ppm to avoid hot tack loss. Conformance of seal strength is tested according to ASTM F88/F88M-21 at 200–300 mm/min jaw separation speed; typical sealed seam strengths for 50.8 µm LLDPE on unprinted BOPET are 12–18 N/25 mm once the seal plateau is reached, depending on sealant gauge and adhesive cure. The food contact and package integrity standards are FDA 21 CFR 177.1520(c) 3.2a, Regulation (EU) No 10/2011, and ASTM F392 for Gelbo flex pinhole detection after 50 flexes. Terminal products are frozen vegetable pouches, snack packs, and powder sachets.

    Preformed sterile barrier pouches for ethylene oxide and gamma sterilization impose peelability requirements that differ from those of retail food pouches. In Tyvek-film constructions, 50.8 µm Sclairfilm LX-1 is laminated to a porous web—typically uncoated Tyvek 1073B or 60–70 gsm medical-grade paper—and functions as the transparent non-porous side of the pouch. The lamination adhesive is applied at 2.0–3.0 g/m², with the LX-1 web accounting for 30–35% of the finished pouch mass; adhesion is controlled below the seal-peel transition so that the film-fibre peel remains the intended opening mechanism. Sterile barrier conformance is evaluated under ISO 11607-1:2019 for design, ISO 11607-2:2019 for forming and sealing processes, and ISO 10993-1:2018 for biological evaluation, with ethylene oxide residual verification under ISO 10993-7:2008. Production consists of roll-fed pouch-making machines with heated seal bars set at 120–150°C, dwell times of 0.5–1.0 s, and platen pressures of 3–5 bar; post-seal inspection includes dye penetration per ASTM F1929 and burst testing per ASTM F1140. Terminal products are flat sterile pouches for surgical instruments, anesthesia kits, and pre-cut procedural trays, with gamma doses up to 50 kGy causing measurable but acceptable reduction in elongation at break.

    When Solventless Adhesives Replace Solvent-Based Systems in Dry Lamination

    Two-component solventless adhesives impose a narrower operating window on 50.8 µm Sclairfilm LX-1 than solvent-borne systems because the thin web has no solvent-absorbing capacity to mask uneven adhesive deposition. Solventless adhesive is metered at 1.2–2.0 g/m² using multi-roll coating with nip temperatures of 40–60°C; this is significantly lower than the 2.5–3.5 g/m² dry weight used in solvent systems, so the LLDPE sealant web should remain at 25–38% of the final laminate thickness. The converting process is governed by REACH (EC) No 1907/2006 for chemical handling, FDA 21 CFR 175.105 and Regulation (EU) No 10/2011 for food-contact adhesive migration, and ISO 11607-1:2019 for medical pouch constructions when output is converted into sterile devices. Curing rooms are held at 30–40°C for 24–48 h; primary aromatic amine migration is checked against the applicable EU limit before slitting. Terminal products include high-barrier stand-up pouches, quad-seal coffee and snack pouches, and liquid detergent spouted pouches where the LLDPE sealant layer withstands stress-cracking agents in the filled product.

    Thermal Lamination Nip Parameters and Print Protection

    Thermal lamination of printed paper and paperboard with 50.8 µm Sclairfilm LX-1 uses the film as a protective print-face web rather than a sealant web. The film is bonded with a pre-applied EVA or rubber-based hot-melt adhesive whose add-on is maintained at 3–6 g/m²; at that level, the 50.8 µm LLDPE film represents 70–85% of the total caliper of the overlaminate layer. Nip pressure is set between 2–4 bar and roll temperature between 85–100°C; below 80°C the EVA adhesive does not flow sufficiently into the paper-pore structure, while above 110°C the film develops curl due to differential thermal shrinkage. Peel adhesion is assessed by ASTM D3330/D3330M with a 180° peel geometry, and optical clarity after lamination is verified by ASTM D1003 haze measurement on a BYK haze-gard instrument. For document and food-contact packaging applications, the polyolefin layer is measured against FDA 21 CFR 177.1520(c) 3.2a and Regulation (EU) No 10/2011, while the hot-melt adhesive must meet FDA 21 CFR 175.105. Terminal products include book covers, laboratory notebook covers, and point-of-sale tags exposed to repeated handling.

    Pharmaceutical blister lidding converts 50.8 µm Sclairfilm LX-1 into the peelable heat-seal layer that is adhesive-laminated to 20–30 µm hard aluminium foil and die-cut for sealing against PVC/PVDC or Aclar blister webs. The LLDPE layer constitutes 55–70% of the lidding foil mass after adhesive coating at 2.0–3.0 g/m²; a thinner sealant layer of 38 µm is sometimes substituted, but 50.8 µm is retained where puncture resistance and child-resistant formulations are required. The film must satisfy FDA 21 CFR 177.1520(c) 3.2a, the European Pharmacopoeia monograph 3.1.3 for polyolefins for pharmaceutical packaging, and ICH Q3D elemental impurity guidelines where requested by the marketing authorisation holder. Blister sealing lines operate at 160–200°C with 0.5–1.0 s dwell and 3–5 bar pressure; seal integrity is tested using vacuum decay per ASTM F2338 and T-peel per ASTM F88/F88M. Terminal products are child-resistant foil lidding stocks for tablet and capsule blister packs, including peel-push configurations for oral solid dose products.

    Bag-in-box liner conversion for high-water-activity liquid foods places 50.8 µm Sclairfilm LX-1 as the innermost sealant and product-contact ply in a multi-layer laminate that includes an EVOH oxygen barrier and a coextruded tie layer. The LLDPE web typically accounts for 25–35% of the liner film mass, with the EVOH layer at 5–7% and the adhesive or tie layer at 1–2 g/m² dry add-on. Food-contact conformance is evaluated under FDA 21 CFR 177.1520(c) 3.2a, Regulation (EU) No 10/2011, and 21 CFR 175.105 for laminating adhesives; hygienic design and traceability for dairy concentrates and wine transport must also meet Regulation (EC) No 178/2002. The web is processed by extrusion lamination or adhesive lamination to the barrier film, then heat-sealed into bag-in-box liners at 120–160°C, 0.5–1.0 s dwell, and 3–5 bar; filling follows cold-sterile injection with headspace oxygen below 2%. Terminal products are bag-in-box liners for milk concentrates, post-mix syrups, and wine transport bladders.

    Free Quote

    Competitive DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 50.8 µm Thickness

    Supplier documentation classifies DuPont™ Sclairfilm® LX-1 as a linear low-density polyethylene web supplied at 50.8 µm nominal thickness for adhesive lamination. The product is normally converted as an inside sealant web or as a surface ply in flexible packaging, where the treated side is bonded to a structural substrate such as oriented polyester, biaxially oriented polypropylene, or paper. The resin is an ethylene/α-olefin copolymer; comonomer type, density, additive package, and lot-specific melt flow rate are not fixed by the film designation and must be taken from the certificate of analysis. At 50.8 µm, the gauge corresponds to 2.0 mil and provides a measurable balance between abuse resistance and laminate flexibility. The technical boundary conditions below separate material properties from machine-dependent processing behaviour; no single setpoint is authoritative without a specific laminator and adhesive system.

    Lot-to-lot variation in α-olefin length, molecular weight distribution, and antiblock loading changes the conversion response. For that reason, this document uses industrial property envelopes for 50.8 µm LLDPE laminating film when grade-specific published data is limited. The product is not a high-barrier material, a retort-grade sealant, or a dimensionally stable substrate; it is a low-modulus polyolefin web whose function is sealability, toughness, and moisture resistance in the finished laminate.

    What Distinguishes a 50.8 µm LLDPE Laminating Web from an LDPE Sealant Film?

    Linear low-density polyethylene differs from low-density polyethylene in molecular architecture. LDPE produced in autoclave or tubular reactors contains long-chain branches; LLDPE has a linear backbone with short-chain branches introduced by butene, hexene, or octene comonomer. This structure raises tensile properties, puncture resistance, and dart impact when measured under ASTM D882 and ASTM D1709. A 50.8 µm LLDPE web can often replace a 60–70 µm LDPE sealant web without loss of package integrity, but the melt rheology is different: at equivalent melt index, LLDPE exhibits lower shear thinning and higher extensional viscosity, which may require higher extruder torque in any reprocessing or sealing operation. The exact comparison for Sclairfilm LX-1 is grade-dependent; Table 1 therefore reports a typical property envelope for 50.8 µm LLDPE lamination film rather than a product certificate.

    Corona Treatment Retention and the Risk of Adhesive Dewetting

    Adhesive lamination requires a wettable surface. Corona discharge oxidation generates polar functional groups on the polyethylene surface; wetting tension is determined under ASTM D2578 using mixed formamide/ethyl cellosolve fluids. For solventless polyurethane systems, converters commonly specify 38–42 mN/m on the treated side. Values below this interval produce adhesive dewetting, uneven coating, and tunnel formation after curing. The treatment decays with storage because low-molecular-weight oxidation products migrate into the bulk; high ambient temperature accelerates decay. Incoming rolls should be re-tested before splicing. The reverse side is normally left untreated or treated at a lower level to control blocking and coefficient of friction under ASTM D1894. Roll identification should clearly distinguish treated side from untreated side; lamination with the untreated side facing the adhesive is a common start-up failure on production lines.

    On a laminating line, the web is unwound with closed-loop tension control. For 50.8 µm LLDPE, tension is typically set between 0.5 N/cm and 1.5 N/cm of web width. Higher tensions cause width loss and gauge-band deformation before coating. The unsupported span between the unwind and coating station should be minimized, because polyethylene has lower modulus than polyester or polyamide and can flutter or accumulate static. Static dissipators are required above 150 m/min line speed. Nip temperature for a solventless polyurethane adhesive is set from the adhesive supplier’s technical data sheet; typical starting conditions are 60–80 °C and 0.3–0.5 MPa nip pressure. These values are not universally valid and must be adjusted for the specific laminator roll diameter, sleeve hardness, and adhesive grade.

    If the Film Is Run on High-Speed Solventless Laminating Equipment

    When Sclairfilm LX-1 is used as the secondary web in a two-component solventless adhesive lamination, the adhesive’s pot life and the film’s surface treatment must be matched to line speed. Solventless polyurethane systems are applied at 1.5–2.5 g/m² coat weight; excessive coat weight increases the chance of edge oozing and creates stiff laminates. The 50.8 µm LLDPE web is not dimensionally stable under high heat, so lamination nip temperatures above 80 °C should be avoided unless supported by the adhesive supplier. Web temperature at the nip should be monitored with an infrared sensor to prevent thermal expansion differences from generating curl. Because the polyethylene surface is nonpolar, a primer may be required if the adhesive system has poor wetting on low-energy films. Converters must verify wetting tension after corona because post-treatment decay can occur within weeks under warm storage.

    Hot Tack and Seal Initiation Are Controlled by Comonomer Length and Dwell Time

    Seal performance is evaluated by ASTM F1921 for hot tack and ASTM F88/F88M for seal strength. In form-fill-seal operation, the sealant layer must maintain crease-holding strength before the web cools. Longer α-olefin comonomers, such as hexene or octene, generally produce lower seal initiation temperatures and broader hot-tack windows than butene copolymers. The grade-specific seal initiation threshold may be defined as the temperature at which seal strength reaches 1.0 N/15 mm under 0.5 s dwell and 0.3 MPa jaw pressure. Published data for this specific Sclairfilm LX-1 configuration is limited, so end-users should request a seal-temperature curve from the supplier. The film is not suitable for retort or hot-fill use; the crystalline melting range of polyethylene is approximately 105–125 °C, and seal creep increases above 70 °C. Packages requiring boil-in-bag or steam sterilization should be validated with a different sealant chemistry.

    Storing, Slitting, and Converting the Treated Web

    Rolls should be kept in original vapour-barrier packaging at 10–27 °C and 40–60% RH. Cold storage below 5 °C requires a 24 h equilibration period before unwinding to prevent condensation. Direct sunlight and UV exposure accelerate surface treatment decay and oxidative embrittlement; storage in high-ozone environments is not recommended. Slitting of laminated or monolayer LLDPE films requires sharp shear blades. Elevated blade temperature above 60 °C can produce edge stringing and resin dust. Winding tension after slitting should be lower than that used for polyester or BOPP to prevent blocking of the low-softening sealant surface. Stacking rolls horizontally may increase interlayer pressure and blocking; vertical storage on edge is preferred for rolls wider than 1,000 mm.

    Antiblock particles such as silica or synthetic zeolite are incorporated to reduce blocking and adjust coefficient of friction. These additives slightly increase haze and can affect adhesive wetting. Measurement of coefficient of friction is performed under ASTM D1894 on treated and untreated sides. Kinetic coefficient of friction for lamination films is typically specified between 0.20 and 0.45, depending on downstream filling machinery. Too low coefficient of friction causes web tracking problems; too high coefficient of friction causes drag and jam in form-fill-seal tunnels.

    Property Envelope Compared with LDPE Sealant Webs

    Typical property envelope for 50.8 µm LLDPE lamination films; values are not lot-specific
    PropertyTest methodLLDPE lamination rangeLDPE sealant range
    Nominal thicknessASTM D374 Method C50.8 µm50.8 µm equivalent
    DensityASTM D15050.918–0.925 g/cm³0.920–0.930 g/cm³
    Tensile strength at break MDASTM D88225–45 MPa15–25 MPa
    Elongation at break MDASTM D882500–750%300–600%
    Dart impactASTM D1709 Method A250–600 g100–250 g
    HazeASTM D10032–6%5–12%
    Water vapor transmission rateASTM F1249 at 38 °C, 90% RH5–8 g/m²·day6–10 g/m²·day
    Seal initiation to 1.0 N/15 mmASTM F192195–115 °C105–125 °C

    The ranges in Table 1 are drawn from general LLDPE and LDPE laminating film literature, not from a specific Sclairfilm LX-1 certificate. Grade-specific values may differ; procurement documentation must be referenced before setting acceptance limits.

    Regulatory and Test Method Cross-Reference

    Test methods and regulatory references invoked during incoming inspection
    AttributeReferenceApplication
    ThicknessASTM D374-16Gauge verification
    Wetting tensionASTM D2578-09Corona treatment
    Seal strengthASTM F88/F88M-21Heat seal quality
    Hot tackASTM F1921-20Form-fill-seal leaker resistance
    Tensile and elongationASTM D882-18Mechanical strength
    Dart impactASTM D1709-16aAbuse resistance
    HazeASTM D1003-13Optical quality
    Coefficient of frictionASTM D1894-14Machinability
    Water vapor transmissionASTM F1249-20Barrier calculation
    Food contactFDA 21 CFR 177.1520; EU No 10/2011Compliance verification

    Food-contact compliance is not automatic; it requires supplier documentation for the specific grade and lot. The converter must verify the final laminate under the applicable regulatory framework, including overall migration testing where required.

    Compared with ethylene-vinyl acetate sealant films, the 50.8 µm LLDPE web generally has lower blocking tendency, better moisture resistance, and higher melt temperature, but EVA sealants may seal through powdered or liquid contamination at lower temperatures. Compared with metallocene LLDPE, conventional LLDPE may show wider molecular weight distribution and lower hot tack; the Sclairfilm LX-1 datasheet should be consulted to determine whether the product is metallocene-catalyzed or Ziegler-Natta-catalyzed. Compared with ionomer sealants, LLDPE has lower cost and lower seal-through-contamination performance. Published data for this specific product is limited; therefore, converter trials are required for final structure approval.

    During lamination, optical defects such as gels, fisheyes, and die lines are classified under supplier specifications and are not necessarily lot reject criteria. Gel counts are reported as number per square meter; typical specifications for high-clarity lamination LLDPE are below 10 defects larger than 0.5 mm². Fisheyes larger than 1.0 mm² can cause adhesive discontinuity and visible spots after lamination. Because the film is 50.8 µm thick, a gel particle of 30–50 µm in height may not be visible in the monolayer web but can bridge the adhesive layer and create a pinhole or tunnel. Inspection should include transmitted light and bright-field microscopy under 10×–40× magnification. The allowed defect level depends on final packaging print coverage and fill content; clear beverage pouches require stricter limits than opaque dry-food pouches.

    Thickness uniformity across the web should be checked with a capacitance or optical gauge. A tolerance band of ±10% of nominal is common for 50.8 µm cast polyethylene film, but specific grade limits may be tighter. Variation in thickness changes seal dwell and local barrier, producing uneven seal strength. In production, thickness data are recorded across the web width and compared with the laminator’s coat weight profile; mismatched profiles produce hard and soft lanes in the finished laminate.

    Laminate structures using this 50.8 µm LLDPE web as the sealant layer are assessed for bond strength under ASTM F904-16 or an equivalent in-house method. Because the LLDPE sealant stretches during peel, the measured bond strength includes tensile energy absorbed by the substrate; a high numerical value may not indicate high interfacial adhesion if the failure mode is elongation rather than clean separation. In production, peel values after 24 h and 48 h of solventless adhesive cure are compared to detect incomplete crosslinking. If bond strength does not increase with time, the adhesive mix ratio, surface treatment level, or nip temperature is reviewed. The film’s low modulus also means that curl and tunnel defects are not solely material properties; they arise from tension imbalance and adhesive shrinkage. Process adjustments to unwind, rewind, and nip pressure are therefore as important as the film’s surface quality.

    Top