| HS Code | 823019 |
| Material Type | LLDPE |
| Thickness | 38.1 µm |
| Density | 0.920 g/cm³ |
| Tensile Strength Ultimate | 24.1 MPa |
| Tensile Strength Yield | 10.3 MPa |
| Elongation At Break | 500% |
| Tensile Modulus | 0.207 GPa |
| Tear Strength | 3.5 kN/m |
| Dart Drop Impact | 120 g |
| Melting Point | 122 °C |
| Vicat Softening Point | 100 °C |
| Haze | 6% |
| Gloss | 80% |
| Coefficient Of Friction | 0.20 |
| Water Vapor Transmission Rate | 0.5 g/100 in²/24h |
| Oxygen Transmission Rate | 150 cc/100 in²/24h |
As an accredited DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | One roll of 38.1 µm DuPont™ Sclairfilm® LX-1 LLDPE laminating film, wound on a core, sealed in moisture-resistant packaging. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Palletized rolls of DuPont™ Sclairfilm® LX-1 LLDPE laminating film, 38.1 µm thickness, secured for transport. |
| Shipping | DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness, is shipped as non-hazardous, non-regulated goods. Rolls are wound on cores, protected with polyethylene wrap, and packed in cartons or on pallets. Store/transport in a clean, dry, moderate-temperature environment, away from direct sunlight, heat, moisture, and sharp objects. |
| Storage | Store in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, sparks, flames, and strong oxidizing agents. Keep in original sealed packaging, clean, flat, and supported to prevent wrinkles, punctures, or compression. Protect from moisture, dust, and UV light. Maintain moderate temperatures with low humidity, avoid heavy stacking, rotate stock, and follow supplier guidance. |
| Shelf Life | Shelf life is typically 24 months when stored in original packaging under cool, dry conditions, away from direct sunlight. |
DuPont™ Sclairfilm® LX-1 LLDPE film at 38.1 µm nominal thickness is specified as a laminating web for multi-layer flexible structures. The five downstream positions below cover the web as a sealant, barrier, or protective ply. Each position identifies the regulatory standard, construction ratio, production route, and finished article categories without extrapolating beyond established LLDPE laminating practice.
For dry-food and snack rollstock, the 38.1 µm Sclairfilm® LX-1 web is positioned as the inner sealant layer in a reverse-printed laminate. The industry compliance standard is FDA 21 CFR 177.1520(c) for olefin polymers in food-contact use, with EU Regulation (EU) No 10/2011 overall migration below 10 mg/dm²; converters typically test the finished laminate under EN 1186 migration protocols for dry snack simulants. The lamination ratio places the 38.1 µm LLDPE web at 60–73% of total caliper in a typical 12 µm PET / 2.0–2.5 g/m² adhesive / 38.1 µm LLDPE stack, depending on print primer weight. The downstream process is adhesive lamination on a solventless or solvent-based laminator, with corona treatment of the film to a surface tension of 38–42 mN/m, nip temperature 45–60°C, line speed 120–180 m/min, and a 24–48 h ambient cure at 25–35°C before slitting. Pouch making uses heat seal jaws at 115–150°C, dwell 0.3–0.6 s, and pressure 2–4 bar. The low seal-initiation temperature of the LLDPE layer reduces thermal load on the outer printed BOPP or PET web. Terminal finished product types include pillow pouches, gusseted snack packs, and cold-seal release register side-gusset formats. This structure is not intended for high-acid liquid hot-fill above 90°C; for those conditions the laminate must be re-qualified for seal creep and delamination resistance.
In terminally sterilized medical device packaging, a 38.1 µm LLDPE laminating web forms the continuous sealable face of a sterile barrier pouch, joined to a porous microbial barrier material or a PET/foil upper web. The governing compliance standards are ISO 11607-1:2019 clause 5.2.6 for seal integrity and ISO 11607-2:2019 for process validation, with ASTM F88/F88M-23 used for seal strength and ASTM F1929-15 for dye penetration after sterilization. The construction ratio in a formed pouch is typically 12 µm PET / 38.1 µm LLDPE or 60–70 g/m² medical-grade paper / 38.1 µm LLDPE, so the sealant web comprises 73–80% of the polymeric thickness in the film-based structure. The downstream production process uses pouch-making machines running at 60–120 cycles/min, with heated knife or rotary sealing at 120–150°C, dwell 0.4–1.0 s, and 3–5 bar jaw pressure; the formed pouches are then sterilized by ethylene oxide, gamma, or electron beam depending on device compatibility. Terminal finished product types include header bags, vented sterilization pouches, and double-sided clear pouches for pre-filled syringes and surgical kits. Validation requires worst-case seal parameter studies and post-sterilization integrity testing because the LLDPE seal interface is sensitive to dwell time and jaw contamination.
| Validation standard | Test method | Measured attribute | Typical acceptance basis |
|---|---|---|---|
| ISO 11607-1:2019 5.2.6 | ASTM F1929-15 | Dye penetration through seal | No channel formation after sterilisation |
| ISO 11607-2:2019 | Process validation | Seal parameter reproducibility | IQ/OQ/PQ with lower and upper control limits |
| ASTM F88/F88M-23 | Seal strength testing | Peel force of bonded webs | Package-design-specific minimum before and after sterilisation |
| ASTM F1608-21 | Porous material microbial ranking | Microbial barrier of porous web | Pass/fail per device manufacturer |
For liquid agricultural chemical single-dose sachets, the 38.1 µm Sclairfilm® LX-1 web is used as the innermost heat-seal layer in a foil-containing laminate that must resist the packaged liquid and prevent pinhole corrosion. The applicable compliance framework includes 49 CFR 173.154 for non-bulk packagings of hazardous materials and the UN Model Regulations packaging instructions for limited quantities, plus chemical compatibility testing per ASTM D543-21. The lamination ratio is commonly 12 µm PET / 9 µm aluminum foil / 38.1 µm LLDPE, and the 38.1 µm web represents 60–65% of total laminate thickness by caliper, with adhesive layers at 2.5–3.5 g/m² on each side of the foil. The downstream production process involves a two-pass adhesive lamination line: the foil is first bonded to the PET at 2.5–3.0 g/m², then the LLDPE sealant web is bonded to the foil at 2.5–3.5 g/m², followed by 48–72 h cure at 30–40°C. Sachet forming on vertical or horizontal form-fill-seal machines uses seal jaw temperatures of 130–160°C, dwell 0.5–1.0 s, and pressures of 3–5 bar. Terminal finished product types include single-dose liquid herbicide sachets, liquid fertilizer pouches, and chemical reagent portion packs. When the packaged liquid contains more than 30% aromatic hydrocarbon, published data for this specific film configuration is limited, and qualification must include long-term sachet storage at 40°C and 75% relative humidity with periodic seal strength evaluation.
In rigid polyisocyanurate and mineral wool board facer lamination, a 38.1 µm LLDPE web is adhesive-laminated to a 12–25 µm aluminum foil or metallized PET facing to create the vapor and puncture side of the insulation panel. The compliance standard is ASTM C1289-23 for faced rigid cellular polyisocyanurate thermal insulation board, with facer water vapor transmission measured under ASTM E96/E96M-22 and facer tensile properties under ASTM D882-18. The lamination ratio in a foil/LLDPE facer typically places the 38.1 µm LLDPE web at 50–65% of the facer thickness; when metallized PET is used, the LLDPE may exceed 70% of total facer caliper. The downstream production process uses a high-speed adhesive laminator with corona treatment of the LLDPE to 40–44 mN/m, nip pressure 4–6 bar, and rewinding tension below 100 N/m to avoid blocking or telescoping. The laminated facer is then fed into a continuous foam lamination line where the foam exotherm and adhesive cure occur at board surface temperatures up to 60°C. Terminal finished product types include faced polyisocyanurate roofing boards, wall sheathing panels, and cold storage insulation boards. Rolls stored at ambient temperatures above 35°C may develop blocking; unwind tension and roll diameter must be controlled to prevent film distortion before the nip.
For dry bulk and chemical packaging, the 38.1 µm Sclairfilm® LX-1 web is adhesive-laminated to woven polypropylene fabric to provide a moisture barrier and sealable inner surface. The industry compliance standard for non-dangerous goods FIBC and sack construction is ISO 21898:2004; for regulated materials, additional 49 CFR 173.24 packaging compatibility and ASTM D543-21 chemical exposure data are used during qualification. The lamination ratio is defined by the woven PP fabric mass of 65–85 g/m² and the film mass of approximately 35 g/m², meaning the 38.1 µm LLDPE layer contributes 29–35% of the total laminate mass, while providing the complete impermeable inner ply. The downstream production process applies a polyurethane adhesive at 2.5–4.0 g/m² to the woven PP, nips the corona-treated LLDPE web at 60–80°C roll temperature and 3–5 bar pressure, then cures the roll for 24–48 h at 30–35°C. Sack conversion uses bottom gusset formation, seam sewing, and heat-sealed valve strips. Terminal finished product types include laminated woven sacks for minerals, dry chemicals, animal feed, and seed packaging, as well as FIBC liner tubes. If the woven PP fabric has surface contamination or corona treatment below 38 mN/m, adhesive transfer to the LLDPE web becomes uneven and seam leakage may occur in hygroscopic powder applications.
Competitive DuPont™ Sclairfilm® LX-1 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® LX-1 is a linear low-density polyethylene (LLDPE) cast film supplied as a laminating web at a nominal thickness of 38.1 µm (1.50 mil). At a typical LLDPE density of 0.920 g/cm³, the area factor is approximately 28.5 m²/kg. Roll formats for converting lines are generally slit from master rolls to widths between 300 mm and 1,800 mm, with a thickness tolerance of ±5% on the nominal gauge; the controlling document for batch-level dimensions remains the supplier certificate of analysis. The film is intended for web-to-web lamination to paper, paperboard, nonwovens, or other polymer films where a polyolefin surface is required, not as a stand-alone sealant or high-barrier layer. A 1,000 kg master roll at this thickness and density contains approximately 28,500 m² of film, which serves as a basis for splice-count estimation on high-speed laminators.
Relative to high-pressure LDPE, the linear backbone of LX-1 contains short-chain branches introduced through alpha-olefin comonomer incorporation and fewer long-chain branches. This molecular architecture alters the response of the film in solid-state orientation and in melt drawing. On cast-film lines, LLDPE grades of this gauge are typically extruded at die temperatures between 205 °C and 240 °C, with chill roll temperatures between 15 °C and 30 °C. Published data for this specific DuPont Sclairfilm LX-1 configuration is limited; therefore the numerical ranges that follow are compiled from a typical LLDPE cast laminating web envelope and should be verified against the certificate of analysis for each lot.
On a production cast-film line, the resin is normally melted in a single-screw extruder with a barrier screw and an L/D ratio between 30:1 and 33:1. The melt exits a slot die with lip gap between 0.4 mm and 0.8 mm and is pinned to a polished or matte chill roll. The draw ratio between die lip and chill roll is typically 2:1 to 3:1 for polyolefin cast film; exceeding 4:1 can create transverse thickness variation, edge curl, and elevated internal stress. A beta or X-ray thickness gauge scans the web and drives die-bolt adjustments to hold total thickness variation within ±5%. For a nominal 38.1 µm film, local thin bands below 33 µm can create adhesive strike-through and flex-crack initiation in the finished laminate.
The conversion of LX-1 in a laminating line is governed by thickness uniformity, surface energetics, and the additive package rather than by polymer melt flow alone. Melt index measured according to ISO 1133-1:2022 at 190 °C with 2.16 kg is typically in the 0.5–2.0 g/10 min range for laminating grades, but LX-1 lot-specific values are not controlled solely by this parameter. A lower melt index tends to increase melt strength and reduce neck-in on a chill-roll line, while a higher melt index improves drawdown at high line speed but can increase edge weave. Table 1 lists a representative property envelope for a 38.1 µm LLDPE cast laminating web.
| Property | Test standard | Typical range |
|---|---|---|
| Nominal thickness | ASTM D6988 | 36.2–40.0 µm (±5%) |
| Density | ASTM D1505 | 0.918–0.922 g/cm³ |
| Tensile strength at break, MD | ASTM D882 | 30–45 MPa |
| Tensile strength at break, TD | ASTM D882 | 25–40 MPa |
| Elongation at break, MD/TD | ASTM D882 | 350–700 % |
| Elmendorf tear, MD | ASTM D1922 | 2.0–6.0 N |
| Kinetic coefficient of friction | ASTM D1894 | 0.25–0.60 |
| Haze | ASTM D1003 | 1.5–5.0 % |
| Gloss at 60° | ASTM D2457 | 70–90 |
| Wetting tension after corona | ASTM D2578 | 38–42 mN/m |
| Melting peak | ASTM D3418 | 120–126 °C |
| Water vapor transmission rate | ASTM F1249 at 38 °C, 90% RH | 12–18 g/m²/day |
The ranges in Table 1 are not specification limits unless stated on the supplier certificate. Slip and antiblock loadings shift coefficient of friction and haze; corona treatment history alters wetting tension; optical values are influenced by chill roll surface and polymer crystallization rate. If the chill roll is maintained above 30 °C, spherulitic growth increases haze and reduces gloss. The mechanical anisotropy between MD and TD is controlled by draw ratio and quench rate; at high draw ratio, MD tensile strength rises but MD elongation falls, and the film becomes more prone to splitting along the machine direction.
Thermal lamination of 38.1 µm LLDPE to paperboard requires roll-surface temperature above the polymer melting onset. Typical hot-roll settings are 120–150 °C, with nip line pressure between 30 N/mm and 80 N/mm face and line speeds of 20–80 m/min on a three-roll stack. If surface temperature is below 120 °C, the film may not flow into the paper surface and peel-strength values measured by ASTM F88 remain below target. Above 150 °C, board moisture can flash and cause blistering. For adhesive lamination, two-component solventless polyurethane adhesives are applied to the film after corona treatment; coating weight of 1.0–2.0 g/m² is common, and lamination nip temperature is set to 40–60 °C to reduce adhesive viscosity without overheating the film.
Untreated polyethylene film typically exhibits a wetting tension of 30–32 mN/m as measured by ASTM D2578. Adhesive lamination with solventless polyurethane systems generally requires a wetting tension of at least 38 mN/m; water-based primers may require 40 mN/m or higher. Corona discharge treatment at power levels between 1.5 kW/m and 3.0 kW/m of web width is used to oxidize the surface and produce carbonyl, hydroxyl, and carboxyl species. After treatment, wetting tension decays because of migration of slip additives such as erucamide or oleamide from the bulk to the surface; this migration is temperature-dependent and becomes rapid above 30 °C. If surface energy declines below 34 mN/m, adhesive spread becomes discontinuous and delamination can occur under Gelbo flex testing performed according to ASTM F392.
Treaters should be placed after the film has cooled below 40 °C, with air gap between 0.5 mm and 1.5 mm. Uniform treatment to 38 mN/m requires clean electrodes and controlled ozone extraction. Wetting tension test fluids should be applied along the web width at intervals no greater than 300 mm to detect treatment decay at edges. For rolls stored longer than 6 months or stored above 25 °C, re-treatment immediately before lamination is required. In-line treatment between the unwind and coating station is preferred, using a ceramic electrode with a bare-roll treater; exact watt density should be adjusted to avoid backside treatment and pinholing at 38.1 µm gauge.
Slip and antiblock additives are used in polyolefin films to control coefficient of friction and prevent blocking. Kinetic coefficient of friction measured by ASTM D1894 for a 38.1 µm LLDPE laminating web typically ranges from 0.25 to 0.60 after additive bloom. Erucamide migrates to the surface over 3–7 days after extrusion; kinetic coefficient of friction measured immediately after slitting may be above 0.60 and then decrease. This temporal drift matters for laminating operations that use corona treatment after aging: the slip bloom competes with corona-induced oxidation, and treatment may need to be repeated. Antiblock particles such as silica or talc at 1,000–3,000 mg/kg create surface micro-roughness; excessive antiblock can increase haze and reduce adhesion.
The film should be wound below 40 °C to avoid blocking at the core. Storage at 15–30 °C and 40–60% relative humidity reduces dimensional change and surface bloom variability. No predrying is required because polyethylene absorbs less than 0.01% moisture at 23 °C; if rolls are moved from cold storage into a warm humid room, condensation on cold roll edges can cause local blocking when introduced to a laminator. Unwind tension at 38.1 µm webs is normally set between 10 N/m and 25 N/m of web width on high-speed laminators to prevent stretching and gauge loss. Slitting is best performed with shear knives set at a side-force between 20 N and 40 N and an overlap of 0.02–0.08 mm; dull blades create hairy edges and filament transfer. Tangential speed between top and bottom knife should be held within 0.5–1.0% to avoid web marking.
At equal thickness, LLDPE film generally has a higher dart drop impact than high-pressure LDPE; typical dart impact values for 38.1 µm LLDPE cast film measured by ASTM D1709 are between 150 g and 350 g, whereas LDPE of the same gauge is often 80–180 g. The improvement originates from the ability of linear chains to form oriented tie molecules during impact loading; long-chain branching in LDPE reduces this post-yield load distribution. Elmendorf tear by ASTM D1922 follows a similar trend, although the effect is direction-dependent and is influenced by extrusion draw ratio. The trade-off in LX-1 is lower melt strength during high-speed draw; neck-in on a cast line may increase if the die-to-chill-roll gap exceeds 25 mm, so converter settings commonly use a gap of 15–25 mm and an air knife to pin the melt curtain.
Compared with ethylene-vinyl acetate (EVA) laminating film of equal gauge, LX-1 does not emit acetic acid during extrusion or thermal lamination, which reduces corrosion risk on engraved steel rolls and downstream idlers. EVA may offer lower thermal lamination initiation temperature and higher polar surface energy, but it can absorb moisture and may require predrying at high relative humidity. For LX-1, predrying is unnecessary, but adhesion to polar inks and water-based adhesives requires corona treatment or a primer. Sclairfilm LX-1 is therefore selected where a nonpolar polyolefin surface is acceptable and where the laminate will not experience retort or aggressive solvent contact.
A gauge comparison is also relevant. Increasing from 25 µm to 38.1 µm raises bending stiffness approximately as the cube of thickness; at equal modulus, the 38.1 µm web is about 3.5 times stiffer than a 25 µm web. This reduces sheet-fed creasing and handling damage but increases roll diameter for a given length. Compared with 50 µm LLDPE film, LX-1 at 38.1 µm provides lower stiffness and cost per square meter but less puncture resistance; the choice depends on downstream die-cutting, fold geometry, and comparative puncture work measured by methods such as ASTM D5748.
Food-contact and electrical/electronic applications require documentation beyond physical property data. Table 2 provides a typical compliance matrix for LLDPE laminating films; it is not a substitute for the supplier declaration for LX-1.
| Regulatory reference | Scope | Limit or condition |
|---|---|---|
| FDA 21 CFR 177.1520 | Olefin polymers for food contact | Density 0.85–1.00 g/cm³; extraction limits per §177.1520(c) |
| EU No 10/2011 | Plastic materials and articles for food contact | Overall migration < 10 mg/dm²; monomer-specific SML |
| EU 1907/2006 REACH | SVHC presence in articles | Candidate List substance < 0.1% w/w per article |
| Directive 2011/65/EU RoHS | Homogeneous material heavy metal limits | Pb < 1000 mg/kg; Hg < 1000 mg/kg; Cd < 100 mg/kg; Cr(VI) < 1000 mg/kg; PBB/PBDE < 1000 mg/kg |
Specific migration of additives and monomers must be assessed under the actual food simulant and temperature/time conditions of the finished laminate. The presence of adhesive, ink, or primer on the non-food side does not relieve the surface layer from compliance; multilayer migration modeling under EU No 10/2011 uses layer-specific diffusion coefficients. Published data for this specific Sclairfilm LX-1 multilayer configuration is limited.
Operational boundaries include limited resistance to aromatic and chlorinated hydrocarbons; toluene, xylene, and methylene chloride swell polyethylene and increase permeation. The film is not an oxygen barrier; oxygen transmission rate for a 38.1 µm LLDPE web measured by ASTM D3985 at 23 °C, 0% RH is typically 3,500–5,000 cm³/m²/day. Direct UV or outdoor exposure without carbon black or hindered amine stabilizer causes embrittlement within months. Continuous service temperature in unlaminated form should remain below the crystalline melting onset; thermal lamination above 150 °C for extended dwell can cause gauge distortion and polymer degradation. On laminators running above 200 m/min, static charge accumulation requires active ionization and grounded backing rolls to prevent adhesive misting and spark defects.