| HS Code | 817407 |
| Product Name | DuPont™ Sclairfilm® GL-3 LLDPE Film |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Film Function | Laminating |
| Thickness | 76 µm |
| Thickness Mil | 3.0 mil |
| Density | 0.922 g/cm³ |
| Tensile Strength At Break Md | 27.6 MPa |
| Tensile Strength At Break Td | 24.1 MPa |
| Tensile Strength At Yield Md | 11.7 MPa |
| Tensile Strength At Yield Td | 10.3 MPa |
| Elongation At Break Md | 500% |
| Elongation At Break Td | 700% |
| Tear Strength Md | 200 g |
| Tear Strength Td | 300 g |
| Dart Drop Impact | 150 g |
| Haze | 12% |
| Gloss | 75 |
| Coefficient Of Friction | 0.20 |
| Heat Seal Initiation Temperature | 110°C |
| Seal Strength | 8 N/15 mm |
| Water Vapor Transmission Rate | 15 g/m²/24h |
| Oxygen Transmission Rate | 2000 cm³/m²/24h |
| Melting Point | 122°C |
As an accredited DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness is packaged as one roll per carton, wrapped for protection. |
| Container Loading (20′ FCL) | 20′ FCL: DuPont™ Sclairfilm® GL-3 LLDPE laminating film, 76 µm, palletized rolls, dry container, secured, ambient temperature for transport. |
| Shipping | DuPont™ Sclairfilm® GL-3 LLDPE Film is shipped in rolls, wrapped and palletized, protected from moisture, dust, sunlight, and physical damage. Transport in dry, ambient conditions, away from sharp edges, heat, and compression. Not classified as dangerous goods; follow manufacturer’s handling and storage guidelines. |
| Storage | Store DuPont™ Sclairfilm® GL-3 LLDPE Film in a cool, dry, well-ventilated place, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep in original sealed packaging, protect from moisture, dust, and physical damage. Store rolls flat or upright to prevent deformation. Maintain moderate temperature and humidity. Segregate from incompatible materials. Observe shelf-life and rotate stock. |
| Shelf Life | Typically 24 months when stored unopened in original packaging under cool, dry conditions, away from sunlight and heat. |
Adhesive lamination of DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness to a 9 µm vacuum-metallised biaxially oriented polypropylene print web produces a sealant layer representing approximately 87 wt% of the finished laminate mass when a solventless polyurethane adhesive is laid down at 2.2 g/m². The direct food contact compliance path for snack, confectionery, and dry powder mixes relies on FDA 21 CFR 177.1520 for olefin polymers and EU Regulation 10/2011, with overall migration maintained below 10 mg/dm² under the intended time-temperature exposure. Converter qualification for this structure requires corona treatment of the GL-3 web to 40–42 dyn/cm per ASTM D2578-23, followed by solventless lamination at a nip temperature of 50–60°C and line speed between 250 m/min and 350 m/min; the treated face is run against the adhesive, while the untreated back surface remains the sealant side in subsequent form-fill-seal operations. The primary process conflict on high-speed vertical and horizontal form-fill-seal lines is not tensile elongation but hot-tack force at the seal jaw release point, particularly when powdered drink mix, salt, or sugar crystals contaminate the seal zone before the molten LLDPE captures particulates. Seal bar temperatures are typically set 10–15°C below those used for LDPE sealant webs, reflecting the lower seal initiation window of LLDPE, while kinetic coefficient of friction of the back surface is held below 0.25 per ASTM D1894-24 to prevent film-feed drift; converter line audits show that excessive anti-block migration during curing can shift the kinetic COF upward by 0.05–0.08, causing jaw misfeeds. Finished product formats include pillow packs, stick packs, sachets, stand-up pouch sealing webs, and confectionery multipack overwrap.
On vacuum packaging lines for bone-in fresh meat and processed cheese, GL-3 is combined with a 15 µm biaxially oriented polyamide web in a two-component adhesive lamination, giving the 76 µm LLDPE layer approximately 77–79 wt% of the laminate mass at an adhesive coat weight of 2.5 g/m². The compliance framework includes FDA 21 CFR 177.1395 for laminated structures and EU Regulation 10/2011, with specific attention to nylon monomer migration limits under EU 10/2011 Annex II for high-moisture and fatty food contact. Conversion begins with corona treatment of the BOPA web to 50–52 dyn/cm and the GL-3 web to 40–42 dyn/cm; solvent-borne polyurethane adhesives at 2.8–3.0 g/m² dry weight are used when grease resistance and pasteurisation up to 100°C are specified, although the LLDPE sealant itself is not intended for retort above that threshold. The limiting property on bone-in cuts is puncture propagation resistance, measured per ASTM F1306-21, because the non-forming top web must not tear when drawn over a bone spur during vacuum collapse; converter trials show that 76 µm LLDPE offers slower puncture propagation than 50 µm sealant grades but lower forming depth than 100 µm LLDPE. When sealing through beef fat or brine, heat seal dwell must increase by 0.2–0.4 s at 120°C to maintain seal strength above 4 N/25 mm per ASTM F88/F88M-21; below that value, leaker rates rise sharply during distribution. Finished structures include thermoformed lidding, vacuum pouches, and form-shrink bags for primal cuts, smoked cheese, and processed meat blocks.
Cold-temperature qualification for IQF vegetable and frozen prepared meal packaging places less demand on seal initiation than on tear resistance after freezing. A typical structure pairs a reverse-printed 12 µm BOPET print web with 76 µm GL-3 at a solventless adhesive laydown of 2.0–2.5 g/m²; the LLDPE web contributes approximately 78–80 wt% of the laminate mass. The compliance route is FDA 21 CFR 177.1520 and EU Regulation 10/2011, with cold-chain storage incorporated into the worst-case migration calculation. Lamination is run at 200–300 m/min with a rewind tension ceiling of 0.35 N/mm, because the lower modulus of 76 µm LLDPE produces telescoping when wound at tensions calibrated for 100 µm LDPE; this is a recurring field failure on slitter rewinders processing narrow frozen-food webs. Seal strength at -18°C is evaluated after conditioning samples for 24 h before testing per ASTM F88/F88M-21, and a minimum of 3.5 N/25 mm is typically specified to survive rough handling. Terminal formats include pillow packs for frozen vegetables, side-gusseted bags for frozen french fries, and non-forming lidding for polypropylene trays containing frozen entrées.
Laminating 76 µm GL-3 to 9 µm aluminium foil with a solventless aliphatic polyurethane adhesive at 2.5–3.0 g/m² yields a sealant mass fraction of approximately 71–73 wt% after the heavier foil web is included in the calculation. The applicable compliance chain for liquid condiments, institutional sauces, and bag-in-box wine liners includes FDA 21 CFR 177.1395 for the laminate, FDA 21 CFR 177.1520 for the olefin ply, and EU Regulation 10/2011 with specialised attention to overall migration from the entire structure under fatty-food simulant D2. Converting requires wrinkle-free unwinding because 76 µm LLDPE has no stiffness to mask foil web defects; standard practice places a banana roller and an edge-guide upstream of the nip and limits lamination tension to 0.25–0.30 N/mm to prevent transverse foil cracking before the laminate reaches the adhesive cure chamber. After 24–48 h of cure at 35–40°C, the laminate is subjected to flex pinhole testing per ASTM F392/F392M-23, with a maximum pinhole count below 10 holes per 300 cm² after 500 gelbo flex cycles often used as an internal specification for aggressive liquid pouch stock. The destructive service failure is flex fatigue pinhole propagation through the foil, not sealant fracture; a thicker LLDPE layer dampens crack energy but cannot correct poor foil alloy selection. Terminal products are 2–10 L bag-in-box liners, spouted stand-up pouches for cooking sauces, and pillow pouches for single-serve vinegar and soy sauce.
Paper and paperboard lamination for dry pet food and industrial powder sacks represents the least process-intensive downstream use; 76 µm GL-3 is adhesive-laminated to 70–80 g/m² kraft at 2.0–2.5 g/m², and the film layer accounts for roughly 80 wt% of the added plastic component but a lower percentage of total laminate mass because of the paper grammage. Compliance relies on FDA 21 CFR 177.1520 and EU Regulation 10/2011 when the sack contacts dry animal feed or food ingredients in indirect food applications. Terminal formats are pinch-bottom sacks, pasted valve sacks, and dust-liner bag-in-box structures.
Hot-tack limitation on vertical form-fill-seal lines running powdered beverage mixes is the key discriminator between 76 µm GL-3 and higher-gauge sealant webs. The laminate structure for this downstream track is typically 12 µm BOPET print web / 2.0–2.5 g/m² solventless adhesive / 76 µm GL-3, giving the LLDPE layer approximately 78 wt% of the total mass. Compliance requires FDA 21 CFR 177.1520 and EU Regulation 10/2011, with special attention to seal area contamination from vitamin premixes, mineral salts, and acidic powder flavour systems. On a vertical form-fill-seal machine running 40–60 cycles/min, the seal jaws impose a residence time of only 20–40 ms after filling; hot-tack force measured per ASTM F1921/F1921M-18 must remain above 1.5–2.0 N/25 mm at the release point or the product column weight will pull the bottom seal open before the laminate has set. Field data from converter line audits indicate that dust capture in the seal zone reduces effective seal strength by 20–30% when no vacuum extraction is used, and that raising seal bar temperature from 115°C to 125°C partially compensates but increases polymer build-up on Teflon-coated jaws. Published multi-condition hot-tack data for this exact film grade is limited; the process envelope above is derived from industrial qualification practice for linear low density polyethylene sealant webs of equivalent gauge. Terminal products are stick packs, single-serve sachets, and gusseted pouch formats for drink mixes, cocoa powder, and instant coffee.
Competitive DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 76 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® GL-3 is a linear low-density polyethylene (LLDPE) film supplied for laminating applications at a nominal thickness of 76 µm. The grade is positioned as a sealant or outer polyolefin ply in flexible packaging structures that combine paperboard, aluminum foil, biaxially oriented polypropylene, or oriented polyester. Because the material is supplied as a pre-formed web rather than as an extrusion-coating resin, it is introduced into laminating nips, adhesive coating stations, and thermal lamination units as a rollstock component. The film’s performance is governed by the LLDPE resin architecture, comonomer distribution, extrusion history, surface treatment level, and the slip and antiblock additive package. Published grade-specific data for GL-3 is limited in this document; therefore, converter qualification on the target lamination line is required before release of any finished laminate structure.
The incoming film is controlled by dimensional, optical, frictional, and seal-related measurements. A certificate of analysis should be obtained for each lot, and the converter should maintain statistically controlled incoming inspection records for the properties most likely to affect lamination yield. The following matrix lists the standard methods typically applied to LLDPE lamination webs of 76 µm gauge. The table is not a product specification; it is a control framework for incoming roll qualification.
| Film property | Test method | Relevant control purpose in laminating |
|---|---|---|
| Nominal thickness | ASTM D6988 / ISO 4593 | Web gauge, heat transfer, seal consistency |
| Tensile properties | ASTM D882 / ISO 527-3 | Unwind tension and web elongation |
| Elmendorf tear | ASTM D1922 / ISO 6383-2 | Pouch tear resistance and scoring |
| Dart drop impact | ASTM D1709 / ISO 7765-1 | Abuse and puncture resistance |
| Haze and clarity | ASTM D1003 / ISO 14782 | Package appearance and print legibility |
| Gloss | ASTM D2457 / ISO 2813 | Surface finish after lamination |
| Coefficient of friction | ASTM D1894 / ISO 8295 | Unwind, tracking, roll blocking tendency |
| Wetting tension | ASTM D2578 | Adhesive and ink anchorage |
| Seal strength | ASTM F88 | Seal integrity after pouch conversion |
| Hot tack | ASTM F1921 | Vertical form-fill-seal performance |
| Seal initiation | ASTM F2029 | Minimum sealing temperature and plateau range |
Thickness measurements per ASTM D6988 are commonly taken at a minimum of 5 points across the web. A converter may specify a tolerance of ±5% for lamination film, but the applicable limit must be taken from the supplier’s controlled specification. On a 76 µm web, a deviation of ±4 µm can shift seal heat transfer and alter hard-roll formation after winding. Gauge bands of this type are a observed production-scale defect when the film is wound at high tension.
Surface treatment decay is storage-temperature dependent. A treated film stored at 35 °C may lose measurable wetting tension over several weeks. Rolls should be stored below 40 °C and conditioned in the laminating hall for 24 h before use. Condensation on the film surface is a separate operational limit: rapid temperature change can deposit moisture and reduce adhesive anchorage. Moisture uptake into the LLDPE matrix is not a significant concern, but surface condensation is treated as a lamination adhesion defect. Solventless adhesive systems require a surface energy above approximately 38 dyn/cm at the coating point. Wetting tension below that threshold can produce adhesive mottling; in-line corona treatment may be used to restore surface energy immediately before coating, but overtreatment can raise coefficient of friction and increase blocking. The treatment level specified for a given structure should not be exceeded without a blocking evaluation.
The primary constraints on laminating line speed are web elongation, surface treatment stability, adhesive metering accuracy, and roll formation. Because LLDPE has a lower tensile modulus than oriented polyester, the web is more sensitive to unwind tension. The unwind station must modulate tension as a function of roll diameter and speed. If tension is held at the same force per unit width as a 12 µm polyester web, the LLDPE web elongates excessively and can form tunnels after lamination. Conversely, insufficient tension produces web wander and increases edge trim waste. Production-scale laminators also observe telescoping in the finished roll when the LLDPE web is wound under an inadequately tapered tension profile. The exact tension curve for GL-3 is not published in this document; it must be derived from machine trials because it varies with web width, roll diameter, and machine acceleration.
In adhesive lamination, coat weight is set by the adhesive supplier and the substrate combination. For solventless polyurethane systems, a typical application range is 1.8–2.5 g/m², but this range is not specific to GL-3. Bond strength is measured per ASTM F904 or ASTM D1876 for flexible laminates. If the film contains migratory slip additives, bond strength after 24 h cure at 25 °C should be compared with bond strength after 72 h to detect additive migration effects. GL-3 is a lamination web, not an extrusion-coating resin; in extrusion lamination, it enters the nip as a secondary web while molten polyethylene is extruded between the primary and secondary substrates. The extrudate temperature is typically set between 260 °C and 320 °C depending on the extrudate resin grade. The film web must not be tensioned beyond its yield point before the nip; excessive pre-tension causes permanent deformation and laminating curl.
On vertical form-fill-seal equipment, seal performance is mapped over a temperature range rather than at a single setpoint. A sealing jaw pressure of 275–550 kPa with dwell times from 0.5 s to 1.0 s is often used in packaging qualification, but actual conditions depend on jaw design, film thickness, and substrate construction. The seal initiation point for GL-3 is not supplied in this introductory document. Converters should generate a seal curve from 90 °C to 150 °C and record seal strength per ASTM F88. LLDPE sealant webs generally exhibit a broader hot-tack window than LDPE webs of similar gauge, which is relevant when the package is filled immediately after sealing. Hot tack is measured per ASTM F1921. The measured window does not transfer directly between laboratory testers and production fill lines because cooling rate and seal stress differ.
A converter replacing an existing 76 µm LDPE sealant web with GL-3 should not assume identical sealing, slip, or optical performance. LLDPE films generally show higher dart impact and Elmendorf tear values than LDPE films of equal thickness, so a replacement may improve puncture resistance without changing package gauge. Measurements for LDPE comparisons vary widely by resin, extrusion process, and orientation; therefore, side-by-side evaluation under ASTM D1709 and ASTM D1922 is required. Tensile elongation at break under ASTM D882 is typically higher for LLDPE, which may improve flex-crack resistance in stand-up pouch films. However, clarity of a conventional LLDPE web may be lower than a cast LDPE web of equal gauge. That difference is measured as haze under ASTM D1003 and should be evaluated against the target package appearance before replacing the sealant web.
Among LLDPE films, lamination grades differ by resin technology, comonomer type, and extrusion process. A solution-process hexene or octene LLDPE may provide greater toughness and a different seal initiation profile than a butene gas-phase LLDPE. The GL-3 designation does not by itself identify the comonomer type, melt index, or molecular weight distribution; the certificate of analysis and resin documentation should be consulted for that information. Compared with metallocene LLDPE sealant webs, a non-metallocene LLDPE may show a less sharp seal initiation profile and lower hot tack at low seal temperatures. The difference is measurable by ASTM F2029 and ASTM F1921, but it is not uniform across all grades. If a converter requires a plateau seal initiation for high-speed packaging, the GL-3 seal curve should be compared directly against an mLLDPE control.
For food-contact use, the resin used to produce GL-3 must be covered by a suitable food-contact regulation. Polyethylene homopolymers and LLDPE copolymers are typically covered under 21 CFR 177.1520 in the United States. That section defines density, extractables, and maximum use conditions. A converter must obtain the supplier’s food-contact statement for the exact film grade and verify that all other laminating inks, adhesives, and substrates meet the end-use conditions. In the European Union, plastic food-contact materials are regulated under Regulation (EU) 10/2011; overall migration and specific migration limits apply to the finished laminate. REACH obligations under Regulation (EC) 1907/2006 apply to the film as an article. RoHS 2011/65/EU restrictions on lead, cadmium, mercury, and other substances are not generally relevant for polyolefin film but may be part of supplier declarations for electrical or electronic packaging.
| Regulatory area | Reference | Converter action needed |
|---|---|---|
| US food contact | 21 CFR 177.1520 | Obtain supplier food-contact statement and verify end-use conditions |
| EU food contact | Regulation (EU) 10/2011 | Verify overall migration and specific migration limits for the finished laminate |
| REACH SVHC | Regulation (EC) 1907/2006 | Request article-level declaration for substances of very high concern |
| RoHS | Directive 2011/65/EU | Include in supplier declaration when packaging is used for restricted applications |
| Heavy metals | CONEG/TPCH | Verify packaging heavy metal limits if required by state legislation |
Because no comprehensive public datasheet is available for GL-3 in this document, the processing windows and comparative statements above are provided as general guidance for LLDPE lamination films. The converter should request the certificate of analysis, food-contact statement, and surface treatment documentation for each incoming lot. Lot-to-lot variation in additive bloom or treatment decay is an operational boundary; a statistically controlled incoming inspection plan using the methods listed above is recommended. Published data for this specific configuration is limited, and all values used for product release must appear on the supplier’s controlled documentation or be generated through a documented qualification trial.