Dupont Sclairfilm Gl 3 Lldpe Film Laminating 50 8 µm Thickness

DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness

    • Product Name: DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 266829
    Thickness 50.8 µm (2.0 mil)
    Material Linear Low Density Polyethylene (LLDPE)
    Film Type Laminating
    Density 0.920 g/cm³
    Yield 21.4 m²/kg (15,000 in²/lb)
    Tensile Strength At Break Md 34 MPa (5,000 psi)
    Tensile Strength At Break Td 31 MPa (4,500 psi)
    Elongation At Break Md 600%
    Elongation At Break Td 700%
    Tear Strength Md 150 g
    Tear Strength Td 300 g
    Dart Drop Impact 150 g
    Haze 6%
    Gloss 45 75%
    Coefficient Of Friction 0.2
    Heat Seal Initiation Temperature 110°C (230°F)
    Melting Point 122°C (252°F)
    Vicat Softening Point 95°C (203°F)
    Wvtr 0.5 g/100 in²/24 hr
    Otr 200 cc/100 in²/24 hr

    As an accredited DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Sclairfilm GL-3 supplied one roll per cardboard carton, 50.8 µm LLDPE laminating film, moisture-barrier wrapped and labeled.
    Container Loading (20′ FCL) 20′ FCL container loading: DuPont™ Sclairfilm® GL-3 LLDPE laminating film, 50.8 µm thickness, palletized rolls, secured for safe transport.
    Shipping DuPont™ Sclairfilm® GL-3 LLDPE Film, 50.8 µm, ships as non-hazardous polymeric film in rolls on cores. Rolls are wrapped, boxed, and palletized for protection. Transport in clean, dry conditions, away from heat, sunlight, and sharp objects. No special dangerous goods markings required; avoid punctures and compression.
    Storage Store DuPont™ Sclairfilm® GL-3 LLDPE laminating film in a cool, dry, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep rolls in original packaging, sealed and clean, protected from dust, moisture, and physical damage. Maintain moderate temperature and humidity; avoid prolonged UV exposure. Follow manufacturer shelf-life guidance and first-in, first-out stock rotation.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original packaging under cool, dry, dark conditions.
    Application of DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness

    In solventless and solvent-based adhesive lamination of dry-food packaging, the 50.8 µm Sclairfilm GL-3 web is placed as the heat-sealable inner ply behind reverse-printed BOPP or BOPET. A typical structure is 20 µm BOPP, polyurethane adhesive, 50.8 µm GL-3, where the LLDPE layer contributes puncture resistance, tear propagation resistance, and a broad seal window. Solventless adhesive is applied at 2.0–3.0 g/m² through a heated metering roll at 40–50 °C, then nipped at 60–80 °C on a high-speed laminating deck. The film surface requires ≥38 mN/m per ASTM D2578; corona treatment decay below 36 mN/m causes adhesive dewetting and tunnel formation at the print interface. For this specific grade, published data is limited, but LLDPE laminating films of this thickness generally show a seal initiation temperature of 105–115 °C at 0.28 MPa jaw pressure and 0.5 s dwell per ASTM F2029. Processing failures observed on solventless laminators include adhesive dimpling when relative humidity exceeds 70% RH and backside transfer when rewind tensions are set above 0.7 N/mm. The structure is used in biscuit, snack, dry pasta, and confectionery pouches, but it is not recommended for retort conditions above 121 °C unless the complete laminate is validated for those temperatures.

    What heat-seal plateau width is required for 80 bags/min vertical form-fill-seal operation?

    On intermittent-motion vertical baggers used for stand-up pouches and pillow bags, the 50.8 µm GL-3 film is positioned as the interior sealing layer. The practical jaw setting range is 115–135 °C because jaw temperature overshoot at the sealing face can reach ±5 °C. Hot tack measured per ASTM F1921 should remain above 1.5 N/25 mm at 120 °C and 0.3 s dwell; lower hot tack causes the bottom gusset to open before the seal cools. Kinetic coefficient of friction should fall between 0.20 and 0.40 per ASTM D1894 to maintain reliable film advance through the forming collar. Seal contamination by product dust is the dominant field failure, and the use of high-slip LLDPE does not compensate for insufficient jaw cleaning. The film is also exposed to cold-seal adhesive release lacquers in some bar wrap applications, where the release layer must not migrate into the heat seal. Converters running vertical form-fill-seal equipment above 80 cycles/min typically reduce dwell to 0.2 s and raise jaw temperature to 135–145 °C, which shortens the available processing window. For this reason, incoming seal initiation data should be verified against the specific roll because published data for Sclairfilm GL-3 is limited.

    For high-speed VFFS and pouch converting, incoming inspection of a 50.8 µm LLDPE laminating web typically uses the following test matrix. The ranges below are general literature values for linear-low-density polyethylene films of this thickness, not grade-specific values for Sclairfilm GL-3.

    MethodPropertyTypical rangeProcess control note
    ASTM D5947Thickness profile45–56 µmCross-web scan target ±8%
    ASTM D882Tensile strength at break, MD20–35 MPaConditioned 24 h at 23 °C
    ASTM D882Elongation at break, MD500–700%Test speed 500 mm/min
    ASTM D1709ADart impact, F50150–400 gLower end with high antiblock
    ASTM D1922Elmendorf tear, MD3–10 NJaw gap 50 mm
    ASTM D1894Kinetic COF, film-to-film0.20–0.45Blocking risk above 0.45
    ASTM D2578Surface energy≥38 mN/mRetest within 24 h of corona treatment
    ASTM F2029Heat seal initiation105–115 °C0.28 MPa, 0.5 s dwell

    For two-web medical device pouches, the 50.8 µm LLDPE laminate is positioned as the non-peelable backing web rather than the peelable interface. The converter applies a peelable medical-grade coating to the Tyvek or medical paper web, then nips the GL-3 film at 55–70 °C in an ISO 8 cleanroom laminating bay. Seal integrity verification falls under ISO 11607-1:2019 with seal strength measured per ASTM F88. Because Sclairfilm GL-3 does not contain a peel blend, destructive seal strength commonly exceeds 8 N/25 mm, which makes it suitable for surgical instrument pouches opened by cutting rather than peeling. The film must maintain low particulate count and stable slip bloom; uneven amide migration after storage above 30 °C can increase kinetic COF above 0.45 and cause misfeed in pouch machinery. Ethylene oxide sterilization requires the laminate to withstand 50–60 °C exposure for several hours without delamination. Processing bottlenecks arise when the lamination adhesive is undercured because residual isocyanate can extract into medical packaging and fail biocompatibility screening under ISO 10993-5. Published data for this specific LLDPE grade in sterile barrier applications is limited, so converters must run seal integrity and migration studies on each lamination batch.

    When aluminum foil forms the barrier ply in 9 µm gauge, which lamination decay mode limits coffee packaging shelf life?

    In coffee and pharmaceutical strip packs, the stack is typically 12 µm BOPET, 9 µm aluminum foil, adhesive, and 50.8 µm Sclairfilm GL-3. The light and oxygen barrier is supplied by the foil, while the LLDPE layer provides seal integrity and puncture resistance against ground coffee particulates. The dominant failure mode is T-peel decay at the foil-adhesive interface from incomplete cure. A solventless aromatic polyurethane adhesive applied at 3.0–4.0 g/m² on a high-speed laminator requires 48–72 h at 23–25 °C for secondary amine consumption. Early rewinding after 36 h can trap residual isocyanate, which then plasticizes the adhesive and reduces T-peel strength below 2 N/25 mm per ASTM D1876. Moisture in the paper core or in the air gap of the foil can form carbon dioxide bubbles during cure, producing visible dimples on the foil side. In addition, creasing the laminate during bag forming initiates pinhole fractures in the foil, and the LLDPE layer cannot compensate for severe flex cracking. Pinhole testing per ASTM F392 is therefore required when the structure is used for vacuum coffee bricks. The film must also maintain surface energy above 40 mN/m when laminated to foil because the metallized or aluminum foil side reflects corona treatment, and the LLDPE side must remain the sealant.

    Laminating adhesive selection for foil-containing stacks is constrained by extractables, bond decay, and curing speed. The matrix below lists starting points for high-barrier laminations using a 50.8 µm LLDPE sealant web.

    Adhesive chemistryTypical dry coat weightLamination conditionCompliance note
    Solventless aromatic polyurethane2.0–3.0 g/m²40–50 °C metering, 60–80 °C nip21 CFR 175.105 for food contact
    Solvent-based polyurethane2.5–3.5 g/m²Oven drying 60–90 °CEU No 10/2011 migration limits
    Waterborne acrylic3.5–5.0 g/m²IR drying 70–90 °CLimited moisture resistance in foil stacks
    Solventless aliphatic polyurethane2.0–2.5 g/m²Slow cure up to 7 daysLow extractables for medical per ISO 10993-5

    Woven sack lamination and hydrostatic test classification for mineral and chemical fillers

    For laminated woven polypropylene sacks used in cement, fertilizer, and mineral filler packaging, the 50.8 µm GL-3 film is combined with woven fabric through an extrusion lamination line. A single-screw extruder with an L/D ratio of 30:1 meters an LDPE tie layer at 315–325 °C, applying 15–25 g/m² of melt between the woven substrate and the pre-formed LLDPE film. The resulting laminate must resist hydrostatic pressure and drop impact because filled sacks are handled at ports and warehouses. Dart impact of the laminated structure is measured per ASTM D1709A, while seam strength is assessed after the sack is filled and dropped from 1.2 m on a concrete floor. Field failures are concentrated at the heat-sealed top seam when product dust remains in the seal area. Woven sack lamination also requires the LLDPE film to act as a moisture barrier, but a 50.8 µm monolayer LLDPE layer alone is not a high oxygen barrier. For hygroscopic fillers, an additional foil or metallized layer is required. The film must survive repeated flexing during sack filling, and Elmendorf tear values below 3 N in both directions are generally unsuitable for this application.

    In reinforced vapor retarder and concrete slab underlayment, the 50.8 µm GL-3 web is laminated to a metallized BOPET or aluminum foil layer and a woven polyolefin scrim. The LLDPE side is exposed to tape joints and heat-welded seams, requiring lap seal strength of at least 15 N/25 mm per ASTM F88 to prevent air infiltration at seams. Water vapor transmission is controlled primarily by the metallized or foil layer; the LLDPE layer contributes tear propagation resistance and low-temperature flexibility. Installation damage occurs when the scrim is dragged over aggregate, and the LLDPE layer must bridge local punctures without splitting. Film-to-film COF below 0.45 is necessary for unrolling on construction sites, while higher COF can cause blocking in rolls stored in unventilated containers above 35 °C. The laminate must also resist mold growth at the film-scrim interface when used below grade. For this application, converters typically specify a corona treatment level of ≥42 mN/m prior to adhesive coating, because contamination from construction dust rapidly reduces bond strength.

    Thermal dimensional stability in frozen food laminating after reverse printing

    In frozen vegetable, seafood, and ready-meal pouches, the 50.8 µm GL-3 film is laminated as the inner sealant layer behind printed BOPP or BOPET. The package must withstand low-temperature impact at −40 °C without cracking, and the LLDPE layer provides higher low-temperature flexibility than LDPE film. Dart impact at freezer temperatures is a critical incoming test; a 50.8 µm LLDPE web generally retains a significant portion of its room-temperature impact resistance, though grade-specific data for Sclairfilm GL-3 is limited. Frozen food lines often operate at high extrusion lamination speeds, and the sealant web must not heat-shrink during the laminating nip. Thermal dimensional stability is evaluated by exposing the film to 90 °C for 5 min in a circulating air oven, and machine-direction shrinkage above 5% causes register loss in reverse-printed structures. The film is also expected to resist stress cracking caused by fats and salts at thawing temperatures. Converters should validate seal strength after freeze-thaw cycling because condensation on the sealant surface can reduce hot tack and create leakers at the bottom gusset.

    Free Quote

    Competitive DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 50.8 µm Thickness is a blown-film linear low-density polyethylene web intended for adhesive lamination, thermal lamination, and pouch sealing. The nominal thickness of 50.8 µm (2.0 mil) is a medium-gauge point selected for controlled stiffness, seal performance, and puncture resistance in flexible packaging. Thickness verification follows ISO 4593; a lot release on modern blown-film equipment commonly reports an average thickness within ±5% of nominal and a cross-web standard deviation below 0.8 µm. The film is corona treated on the lamination side to a wetting tension of 38–42 mN/m when checked by ASTM D2578. The polymer is a linear low-density polyethylene with short-chain branching distributed along the main chain rather than the long-chain branching characteristic of conventional LDPE. Published data for the GL-3 grade is limited; where numerical ranges are provided in this document, they represent the class of 50.8 µm LLDPE laminating films and should be confirmed with a lot-specific certificate of analysis.

    The film’s primary processing identity is as a laminating web, not a monolayer finished package. It is supplied in roll form for downstream lamination to paper, paperboard, aluminum foil, metallized BOPET, and printed polymer substrates. The corona-treated side is designed to receive solventless, solvent-based, or waterborne adhesives; the untreated side remains available as the outer surface or for additional coating.

    What Separates GL-3 from Conventional LDPE and Cast PP Laminating Webs at 50.8 µm?

    The primary molecular distinction is the absence of long-chain branching. In melt processing, this difference lowers die swell and raises the elongational viscosity at high extension rates, which improves bubble stability on a blown-film line but increases the sensitivity of melt fracture to die-lip buildup. The solid-state consequence is that LLDPE films exhibit higher tear propagation resistance and higher puncture toughness than LDPE at equal gauge. When tested per ASTM D882-18, a 50.8 µm LLDPE laminating web typically shows machine-direction tensile strength at break in the range of 25–45 MPa, while an LDPE web of the same gauge tends toward 15–30 MPa. Elongation at break for LLDPE is commonly 400–700%, with transverse-direction values frequently exceeding machine-direction values because of blow-up orientation. Elmendorf tear strength per ASTM D1922 can range from 3 N to 12 N depending on orientation and resin density; published data for the GL-3 grade is limited. These values allow lamination converters to run thinner sealant webs without sacrificing puncture resistance, but the low modulus of LLDPE relative to cast PP requires different tension settings in the unwind and rewind.

    Compared with cast polypropylene, the LLDPE laminating film has a lower heat-seal initiation temperature and a broader hot-tack window. PP homopolymer films generally require jaw temperatures above 130 °C to initiate a seal, whereas LLDPE formulations seal from 95–110 °C under 0.5 s dwell and 2.1 bar jaw pressure in ASTM F2029 tests. This reduces thermal damage to printed layers and permits higher line speeds on vertical form-fill-seal machines. The trade-off is lower stiffness; the secant modulus of LLDPE at 50.8 µm is generally below 250 MPa per ASTM D882, while oriented polypropylene can exceed 1,500 MPa in the machine direction. Thus, GL-3 is selected where seal integrity and puncture resistance dominate, not where dimensional stiffness is the primary requirement.

    Table 1 summarizes class-level comparative data for 50.8 µm laminating films. The LLDPE values are representative of general-purpose extrusion laminating and adhesive laminating films, not lot-specific GL-3 measurements.

    PropertyStandardLLDPE laminating classLDPE laminating classCast PP laminating class
    DensityASTM D15050.918–0.925 g/cm³0.917–0.930 g/cm³0.89–0.91 g/cm³
    1% secant modulus, MDASTM D882-18150–250 MPa120–200 MPa800–1500 MPa
    MD tensile strength at breakASTM D882-1825–45 MPa15–30 MPa30–50 MPa
    MD elongation at breakASTM D882-18400–700%200–500%300–600%
    Elmendorf tear strengthASTM D19223–12 N2–8 N0.5–3 N
    Seal initiation temperatureASTM F202995–110 °C105–120 °C130–150 °C
    Water vapour transmission rate, 38 °C, 90% RHASTM F12492–4 g/(m²·day)2–4 g/(m²·day)1–2 g/(m²·day)

    Gauge Uniformity, Surface Energy, and Seal-Bond Ductility Under Line-Speed Constraints

    Cross-web gauge variation is the dominant cause of adhesive layer non-uniformity in lamination. For a 50.8 µm blown film, a gauge profile with ±3% cross-deckle variation is typical when the annular die gap is held at 1.8–2.2 mm, the blow-up ratio is 2.0:1–2.8:1, and the frost-line height remains within ±5% of the set point using internal bubble cooling. If the gauge variation exceeds ±7%, the laminating nip pressure profile becomes non-uniform, producing adhesive striations and inconsistent peel-strength results. Capacitance thickness profiling across the web is commonly used to detect gauge bands before conversion.

    Surface treatment is the second process limit. The corona-treated surface is intended for adhesive anchorage. Wetting tension measured per ASTM D2578 should be 38–42 mN/m at the laminator infeed. If the treated surface has decayed below 36 mN/m, solventless polyurethane adhesives may not wet the surface completely, and peel strength after lamination can fall below the required value. Treatment decay is time- and temperature-dependent; storage at 25 °C for more than 6 months or at 35 °C for more than 4 weeks can render the film non-laminable without re-treatment. Corona re-treatment is possible at 1.0–1.5 kW across a 1,200 mm web, but excessive treatment can oxidize the surface to low-molecular-weight oxidized species that form a weak boundary layer.

    Seal-bond ductility is evaluated by heat-seal strength per ASTM F88/F88M-21 and hot-tack per ASTM F1921. LLDPE seals generally fail by film-burst outside the seal rather than by delamination when the seal temperature exceeds 110 °C and dwell time is above 0.5 s. The seal strength on 50.8 µm film typically ranges from 12 N/25 mm to 20 N/25 mm at 120 °C, but published data for GL-3 is limited. The hot-tack value at 110 °C is normally above 1.5 N/25 mm, which supports many vertical form-fill-seal applications; equipment-specific validation remains necessary because jaw pressure, dwell, and film temperature differ between packaging machine types.

    Melt rheology of the base resin is not a film property but controls the film conversion. LLDPE blown-film resins for 50.8 µm laminating webs are often formulated in the melt index range 0.8–2.0 g/10 min at 190 °C and 2.16 kg when measured according to ISO 1133-1:2022. A resin outside this range may require elevated barrel temperatures and increases the risk of melt fracture at the die lip; the resulting film may show gauge variation or reduced impact resistance. Differential scanning calorimetry per ASTM D3418-21 on LLDPE resins typically shows a peak melting temperature of 120–124 °C and a crystallization peak near 104–108 °C. The practical seal initiation range of 95–110 °C is close to the melting onset; sealing below this range produces only tack bonds.

    Since LLDPE exhibits higher melt strength and a narrower molecular weight distribution than LDPE, bubble stability is usually better, but melt fracture at the die lip can occur at lower shear rates if the die temperature is not adjusted. In a 90 mm single-screw extruder fitted with a 300 mm annular die, a film production rate for 50.8 µm LLDPE may be limited by bubble cooling rather than extruder throughput; internal bubble cooling can increase output by 20–30% relative to natural cooling. The resulting film orientation depends on the blow-up ratio and frost line; a blow-up ratio above 3.0:1 can overstabilize the bubble and reduce tear strength in the machine direction.

    On a solventless adhesive laminator with a web width of 1,200 mm, the 50.8 µm LLDPE unwind web is generally tensioned at 0.5–1.0 N/10 mm width; this range balances gauge flattening against permanent elongation. For comparison, a same-gauge cast PP film may require 1.0–1.5 N/10 mm due to higher modulus. The laminating nip temperature for a two-component polyurethane adhesive is usually held at 55–65 °C, with a coat weight of 1.5–2.5 g/m² for clear-to-clear laminates and 2.0–3.0 g/m² for paper-containing laminates. A chill roll set at 18–24 °C is common after the nip to stabilize the web before secondary slitting. If the film contains migratory slip additives, lamination at too low a temperature may leave the weak boundary layer intact; in-line corona or a primer can mitigate this when permitted. Published data for GL-3 on this exact laminator configuration is limited; these settings are class-level and require line trials.

    When the Film Replaces Cast Polypropylene in High-Speed Pouch Converting

    In high-speed pouch converting, the lower seal initiation of LLDPE allows sealing at 95–110 °C rather than the 130–150 °C required for cast PP. This reduces thermal damage to print and allows a shorter sealing jaw dwell. The coefficient of friction is a key control because the film must slide over forming collars without blocking. Kinetic COF per ASTM D1894 for laminating-grade LLDPE is commonly 0.2–0.5; above 0.6, pouch forming may become difficult on high-speed lines, while below 0.1, roll telescoping and blocking may occur. If the film has been stored above 30 °C, slip additive migration may reduce COF unevenly and create surface regions with low lamination adhesion. The film should be equilibrated to 20–25 °C before use.

    Tensile modulus differences mean that the unwind tension for a 50.8 µm LLDPE web must be reduced by approximately 20–30% relative to a same-gauge cast PP film. If the tension is too high, the web deforms elastically in the machine direction and can lose gauge uniformity before the laminating nip. This is particularly evident on registration-critical printed laminates, where the film is laminated to a pre-printed web and the composite must be die-cut or punched.

    In high-barrier laminates, the 50.8 µm film may serve as the innermost sealant layer over aluminum foil or metallized BOPET. The thermal expansion mismatch between LLDPE and foil requires that the laminating nip temperature be kept at 55–65 °C and that winding tension not exceed 0.5 N/10 mm if the roll core temperature is above 30 °C. Peel strength between foil and film after adhesive lamination is often measured by ASTM D1876 or ASTM F88; a common acceptance range for foil/PE laminates is 3.0–6.0 N/15 mm, although published data for GL-3 in this exact foil structure is limited. The film is not an extrusion-coating resin; it is supplied as a pre-formed web and is processed on laminating equipment rather than an extrusion-coating line.

    Oxygen transmission rate for a 50.8 µm LLDPE film at 23 °C, 0% RH is classed at approximately 2,000–3,000 cm³/(m²·day·bar) per ASTM D3985; the actual value depends on density and orientation. This is not suitable as the sole barrier in high-oxygen-sensitive food packaging, but it is adequate as a sealant layer inside a foil or metallized structure. Optical haze per ASTM D1003 for 50.8 µm LLDPE laminating film may range from 5% to 15% depending on resin formulation and surface treatment. Cast PP can be clearer with haze 1–3%, but often lacks the low-temperature seal and puncture characteristics of LLDPE.

    Storage of the film should be in original packaging at 15–27 °C and 40–60% RH to minimize treatment decay and additive migration. The film does not require pre-drying because LLDPE absorbs less than 0.01% moisture by weight at 23 °C and 50% RH. For direct food contact, the polyethylene substrate is generally assessed under FDA 21 CFR 177.1520 and EU No 10/2011; the finished laminate must also be assessed for overall migration from adhesives, primers, and printing inks. Converters should request a lot-specific certificate of analysis and conformity statement. GL-3 should not be substituted for cast PP, BOPP, or LDPE without re-validation of seal strength per ASTM F88, coefficient of friction per ASTM D1894, and wetting tension per ASTM D2578.

    Table 2 summarizes typical compliance assessments for the purchased film; the converter remains responsible for the finished laminate.

    RequirementStandard or regulationTypical evaluation endpoint
    US indirect food-contact substrateFDA 21 CFR 177.1520Olefin polymer specification and condition of use
    EU plastics food-contact materialEU No 10/2011Overall migration 10 mg/dm²
    Surface wetting tensionASTM D257838–42 mN/m
    Heat-seal strengthASTM F88/F88M-21Application-specific minimum
    Coefficient of frictionASTM D1894Kinetic COF 0.2–0.5
    REACH SVHCEC 1907/2006Supplier SDS and substances declaration
    RoHS restricted substancesDirective 2011/65/EULead, cadmium, mercury, Cr(VI), PBB, PBDE
    Top