| HS Code | 219088 |
| Material | Linear Low Density Polyethylene (LLDPE) |
| Film Type | Laminating Film |
| Thickness | 38.1 µm |
| Thickness Mil | 1.5 mil |
| Density | 0.920 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Tensile Strength At Break Md | 26.2 MPa |
| Tensile Strength At Break Td | 24.1 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Elmendorf Tear Strength Md | 200 g |
| Elmendorf Tear Strength Td | 300 g |
| Dart Drop Impact | 150 g |
| Haze | 5% |
| Gloss | 80% |
| Coefficient Of Friction | 0.2 |
| Melting Point | 122°C |
| Heat Seal Initiation Temperature | 110°C |
| Water Vapor Transmission Rate | 0.5 g/100 in²/24 hr |
| Oxygen Transmission Rate | 200 cc/100 in²/24 hr |
| Yield | 28.5 m²/kg |
As an accredited DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Each carton contains one roll of DuPont™ Sclairfilm® GL-3 LLDPE laminating film, 38.1 µm thick, sealed in protective wrap. |
| Container Loading (20′ FCL) | 20′ FCL container loading of DuPont™ Sclairfilm® GL-3 LLDPE laminating film, 38.1 µm thickness; palletized rolls secured for dry transport. |
| Shipping | DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness is shipped as non-hazardous, non-regulated film rolls. Rolls are wrapped, boxed, and palletized for protection. Store and transport dry, at ambient temperature, away from direct sunlight, heat, and sharp objects. Handle carefully to avoid punctures or crushing. No special shipping labels required. |
| Storage | Store DuPont™ Sclairfilm® GL-3 LLDPE Film in its original packaging in a clean, dry, well-ventilated area. Keep away from direct sunlight, heat, ignition sources, moisture, and chemicals. Maintain moderate temperatures and humidity. Store flat or on a core to prevent wrinkling, crushing, or edge damage. Avoid excessive stacking and rough handling. Ensure good housekeeping and use first-in, first-out inventory rotation. |
| Shelf Life | Shelf life is 12 months from date of manufacture when stored in original packaging at 23°C and 50% relative humidity. |
In commercial print lamination lines, DuPont Sclairfilm GL-3, a 38.1 µm LLDPE laminating film, is processed as a continuous overlay on 90–120 g/m² offset, aqueous inkjet, and electrophotographic stocks. The web does not enter a solvent blend or coating formulation; its formulation contribution in a two-ply paper/film laminate is expressed as layer mass fraction. At an areal mass of 34.8–36.3 g/m² calculated from a density band of 0.913–0.953 g/cm³, the film adds 25–30% of final dry grammage when dry adhesive coat weight is controlled between 2.8 g/m² and 4.2 g/m² on a 100 g/m² coated cover stock. If the paper input is heavier, the film fraction falls accordingly; the percentage should not be fixed without weighing the coated sheet and cured adhesive. Compliance for this downstream is evaluated under EU REACH Regulation (EC) No 1907/2006 Annex XVII restricted substance limits, RoHS Directive 2011/65/EU where laminated print enters electrical equipment, and EN 71-3:2019+A1:2021 for heavy-metal migration where the finished print is intended for children. Optical uniformity of the laminate is checked with ASTM D1003-21 haze and ISO 14782:1999 clarity methods; film thickness distribution is verified by ISO 4593:1993. Tension control is critical because this film will elongate more than PET or nylon overlays at equivalent load.
Thermal roll laminators should be set at 90–115°C surface temperature, 60–100 kPa nip pressure, and 8–15 m/min line speed. The unwind tension is maintained at 12–18 N/m to limit machine-direction draw; backheated rollers or preheated stock at 30–40°C reduce differential curl. Field failure on lay-flat book covers appears as edge curl within 4–6 h of ambient conditioning when roll temperature exceeds 115°C or when film shrinkage exceeds 2% in the machine direction. Finished output includes menus, book covers, instruction manuals, folded maps, display cards, and trade-show graphics.
Dry food and detergent refill pouch converting requires the film to perform as an inner sealant web in PET 12 µm / Al 8 µm / LLDPE 38.1 µm laminated structures. Its formulation role is defined by layer weight fraction in the finished stack, not by admixture into adhesive or ink. The LLDPE layer contributes 34.5–36.5 g/m², while the PET and foil layers contribute approximately 16.6 g/m² and 21.6 g/m² respectively; with two solventless adhesive interfaces at 2.0–3.0 g/m² each, the LLDPE sealant represents 42–46% of total laminate mass. This fraction matters because the sealant layer dominates heat-seal initiation and puncture behaviour, but it does not control oxygen or moisture barrier. Published oxygen transmission data for 38 µm LLDPE place the layer above 1000 cm³/(m²·day·atm) at 23°C, 0% RH; aluminium foil or metallized polyester must supply the barrier.
Compliance assessment for food contact proceeds under EU 10/2011 overall and specific migration limits and FDA 21 CFR 177.1520(c) olefin polymer provisions, with good manufacturing practice under EC 2023/2006. Converters must verify that slip and antiblock additives from the film do not exceed specific migration limits under the intended food simulant, processing time, and temperature. For detergent and non-food pouches, REACH Regulation (EC) No 1907/2006 and the CLP Regulation (EC) No 1272/2008 govern packaging-level classification and communication.
On solventless laminating lines, the first pass applies adhesive to the aluminium sheet, and the second pass laminates the film at 45–60°C with nip pressure 0.4–0.6 MPa. Curing proceeds for 24–48 h at 20–25°C before slitting. Unwind tension is held at 10–16 N/m because the soft LLDPE web can form baggy edges that misregister in subsequent form-fill-seal operations. Heat sealing is conducted at 120–135°C, 0.35–0.50 MPa, and 0.5–1.0 s dwell, with seal samples pulled per ASTM F88/F88M-21. A decline in seal force after 48 h at 40°C ageing can indicate slip additive migration to the seal surface; corona treatment below 38 mN/m on the adhesive-receiving side is a separate source of delamination. End products include dry powder sachets, frozen vegetable pouches, detergent refill packs, and non-food lidding films where foil or metallized barrier is present.
Sterile barrier package converting for Tyvek and polyester lidding pouches imposes a narrower operating window than commercial print lamination because seal force, fibre tear, and microbial barrier continuity must be validated after lamination, ageing, and sterilisation. The 38.1 µm olefin web is introduced as a peelable heat-seal inner layer on multilayer lidding, with solventless or solvent-based adhesive coat weight of 3–6 g/m². In a PET 12 µm / Tyvek 1073B / LLDPE 38.1 µm construction, the LLDPE layer contributes 34.8–36.3 g/m², approximately 22–28% of total structure mass depending on Tyvek grade and adhesive type. Published third-party validation data for this specific Sclairfilm grade in ISO 11607-validated configurations is limited; the converter therefore generates package-specific seal windows and barrier test data instead of relying on a generic film datasheet.
| Standard / method | Role in sterile barrier converting | Measured endpoint on this structure |
|---|---|---|
| ISO 11607-1:2019 | Packaging system design and risk assessment | Seal integrity, material compatibility, microbial barrier |
| ISO 11607-2:2019 | Process validation for forming and sealing | Installation, operational, and performance qualification |
| ASTM F88/F88M-21 | Destructive seal strength testing | Peel force in N/25 mm |
| ASTM F1929-15 | Dye penetration testing | Absence of channel contact across seal |
| ISO 10993-5:2009 | Cytotoxicity evaluation | Cell viability threshold per standard |
| ISO 10993-7:2008 | Ethylene oxide residue assessment | Residual limits by exposure category |
Compliance references further include ISO 10993-10:2013 for sensitisation and 21 CFR Part 820 quality system requirements. Gamma sterilisation at 25 kGy or 40 kGy may oxidise the polyolefin and shift seal initiation; requalification must be performed on sterilised specimens after the maximum intended dose. Ethylene oxide validation includes residual gas analysis on the finished laminate according to ISO 10993-7:2008.
Production lamination to Tyvek is run with drying tunnel temperatures of 60–80°C; pouch sealing jaws are set at 120–140°C with 0.3–0.5 MPa pressure and 0.5–1.0 s dwell. Destructive seal tests are performed at intervals no greater than 30 min during the seal run. Seal temperature above the upper edge produces loose fibre transfer and visual peel inconsistency; temperature below the lower edge yields channel leak failures in ASTM F1929-15. Finished goods include Tyvek lidding films for catheter trays, syringe pouches, dressing kits, and single-use surgical instrument packs.
For printed pressure-sensitive labels destined for steel and HDPE drums carrying solvents, cleaning agents, and lithium-ion battery precursors, the 38.1 µm clear LLDPE overlaminate is applied as a continuous web over printed PET or BOPP facestocks. It is not formulated into the ink or adhesive; its formulation contribution is the grammage share of the finished label. At an overlaminate adhesive coat weight of 16–22 g/m² and a final label grammage of 150–200 g/m², the film adds 34.5–36.5 g/m², representing 15–25% of total product mass. The overlaminate cannot compensate for poor ink-to-face adhesion or unprimed digital ink; a cross-cut or tape-pull adhesion test on the printed surface is required before full web lamination.
Conformity for marine dangerous goods labels is assessed under BS 5609:1986 Section 2 and Section 3, the latter requiring printed label performance after immersion in seawater for 3 months and subsequent abrasion testing. REACH Regulation (EC) No 1907/2006 Annex XVII and RoHS Directive 2011/65/EU apply where the label is used on equipment or packaging with restricted substance limits. For labels applied to lithium-ion cell packaging, the finish must be evaluated against UN GHS labelling durability expectations; published data for this specific film in BS 5609-certified constructions is limited, and certification belongs to the completed label, not to the film alone.
Flexographic and digital label lines laminate cold at 20–35°C with nip pressure 0.2–0.4 MPa and run speeds of 20–40 m/min. No heat assist is required because the overlaminate adhesive is pressure-activated. The laminated web is then rotary die-cut, stripped, and slit; excessive film unwind tension above 12 N/m can cause overlaminate elongation and misregistration between die-cut edge and print edge. Finished products include GHS drum labels, IBC tank labels, hazardous-material package labels, and maintenance instruction plates for corrosive chemical service.
Competitive DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® GL-3 LLDPE Film, Laminating, 38.1 µm Thickness is a linear low-density polyethylene web supplied for use as a laminating ply or sealant web in flexible packaging. The product designation identifies the film as an LLDPE laminating grade rather than a high-pressure low-density polyethylene or ethylene-vinyl acetate sealant. At the nominal thickness of 38.1 µm (0.0381 mm, 1.5 mil), the web occupies the mid-gauge range used where seal integrity, puncture resistance, and controlled stiffness are required without high-temperature retort exposure. Published supplier documentation for this specific configuration is limited; therefore, application-specific property values must be taken from lot-specific certificates or converter qualification trials.
The base material is classified as linear low-density polyethylene, with solid-state density typically falling between 0.915 g/cm³ and 0.925 g/cm³ depending on comonomer type and molar level. At the nominal thickness of 38.1 µm and an assumed density of 0.920 g/cm³, the calculated basis weight is approximately 35 g/m². The corresponding area yield is approximately 28.5 m²/kg. These values are dimensional calculations rather than certified film properties. Thickness is verified on incoming reels according to ASTM D6988-21 or ISO 4593. Measurements should be taken after conditioning at 23 ± 2 °C and 50 ± 5 % RH because polyethylene dimensions respond to ambient temperature. On slitting and rewinding operations, gauge variation in a 38.1 µm web becomes magnified as roll diameter increases. A local deviation of ±2 µm can produce visible hard bands or gauge bands in the finished reel, which later feed as web flutter into the laminating nip.
In production converting environments, the web is typically unwound into an adhesive laminating station after surface treatment is verified. If the film is supplied with one-sided corona treatment, the treated surface is identified with dyne solutions according to ASTM D2578. A wetting tension of 38–42 mN/m is commonly specified for solventless and waterborne lamination, while some solvent-based systems may tolerate 36–40 mN/m depending on coating rheology. Production failure records show that corona-treated polyethylene can lose wetting tension during warehouse storage. Reels retained for 6–12 months in warm conditions may fall below 36 mN/m, producing adhesive dewetting, tunneling, or delamination after the laminate is cured. The coating nip is typically run with a rubber-covered backup roll of 70–80 Shore A hardness and a hardened steel coating roll. For a web of this gauge, nip pressure should be set to avoid transverse stretching and should be validated by monitoring web width before and after the coating station. Web tension must remain below the yield point of LLDPE. At a basis weight near 35 g/m², tension loss can fold the film at the lay-on roll or cause blocking when adhesive is applied to the corona-treated side. Solventless adhesive coat weights are commonly controlled between 1.5 g/m² and 2.5 g/m² for flat lamination. Because the film itself is thin, a 0.5 g/m² adhesive deviation can produce visible lay-flat defects even when it represents a small fraction of the total finished structure.
Compared with high-pressure LDPE laminating film of equal nominal gauge, an LLDPE class web typically exhibits higher dart impact and Elmendorf tear values. The comparison is made under ASTM D1709 Method A for dart impact and ASTM D1922 for tear propagation. Published class data for general-purpose LLDPE films near 38 µm often report dart impact values from 150 g to 400 g, while LDPE webs of similar gauge may fall below 100 g. These ranges are not GL-3 certified values and are included only as class-level orientation. The trade-off occurs in optics: LLDPE films may exhibit haze from 2 % to 8 % under ASTM D1003, whereas cast LDPE sealant webs frequently produce haze below 5 %. The product selection therefore depends on whether the laminate is specified for clarity or for puncture and tear resistance.
Compared with ethylene-vinyl acetate sealant films, GL-3 as an LLDPE web offers a different heat-seal profile and a lower volatile profile because vinyl acetate monomer and acetic acid are absent. Heat seal strength is measured according to ASTM F88/F88M-21. EVA copolymers generally initiate seal formation at lower temperatures, but LLDPE class materials can provide a stable plateau above 20 N/25 mm when sealed against properly treated aluminum foil or polyester at 140–160 °C. The absence of EVA also reduces the possibility of acid-catalyzed corrosion in aluminum foil laminates; packaging quality audits should verify laminate pH after curing when acrylic or polyurethane adhesives are used.
Metallocene LLDPE grades are often specified for lower seal initiation and improved puncture at equivalent gauge. GL-3 is identified as an LLDPE lamination grade, but the supplier does not publish a metallocene or Ziegler-Natta designation in the available product listing. Converters should not interchange GL-3 with metallocene LLDPE sealant webs without running a comparative hot-tack profile under ASTM F1921/F1921M-12, because hot-tack behavior, not final seal strength, frequently controls throughput on vertical form-fill-seal lines. Similarly, replacement of a cast polypropylene sealant with a 38.1 µm LLDPE web requires re-validation of seal jaw temperature, dwell, and cooling time because polypropylene and polyethylene differ in crystalline melting range and thermal conductivity.
Compliance is assessed at two levels: the polyolefin base film and the finished laminate. For food-contact use in the United States, the olefin polymer may be covered under 21 CFR 177.1520. For the European Union, the finished article is evaluated under EU Regulation No 10/2011 for overall migration and, where applicable, specific migration limits. The converter is responsible for end-use compliance because adhesive, printing ink, coating, and substrate layers modify the migration profile. A supplier certificate for the film is necessary but not sufficient for finished-packaging compliance.
| Standard or regulation | Designation or scope | Relevance to GL-3 lamination film |
|---|---|---|
| 21 CFR 177.1520 | Olefin polymers | US food-contact status of the base polyolefin resin class |
| EU No 10/2011 | Plastics in food contact | Overall migration and specific migration limits |
| ASTM D6988-21 | Film thickness | Verification of the nominal 38.1 µm gauge |
| ASTM D882-18 | Tensile properties | Modulus and elongation of unsupported film |
| ASTM D1709 | Dart impact | Puncture resistance of free film |
| ASTM D1922 | Elmendorf tear | Tear propagation in machine and transverse directions |
| ASTM D1003 | Haze | Optical clarity after lamination |
| ASTM F88/F88M-21 | Seal strength | Sealant web performance after heat sealing |
| ASTM F1921/F1921M-12 | Hot tack | Seal integrity at elevated packaging speeds |
| ASTM D2578 | Wetting tension | Corona treatment level for adhesion |
Migration testing must include the adhesive and the food-contact surface, not the film alone. The analytical laboratory should measure overall migration in appropriate food simulants under EU No 10/2011; aqueous, acidic, and fatty-food simulants may include 10 % ethanol, 3 % acetic acid, and 95 % ethanol or isooctane. Published data for this specific GL-3 formulation is limited, and a control laminate containing the same adhesive and substrate must be submitted with any production qualification.
GL-3 is an LLDPE lamination web and should not be assigned to high-temperature retort or boil-in-bag cycles approaching the crystalline melting region of polyethylene. The peak melting temperature of LLDPE class materials is typically 120–127 °C by differential scanning calorimetry according to ISO 11357-3. A 121 °C retort cycle therefore approaches this range, creating a risk of seal creep, web distortion, and film shrinkage. For retort applications, oriented polyester or cast polypropylene sealant webs are normally specified instead.
For non-retort laminating, the film should be stored below 40 °C and away from ozone-generating equipment because polyethylene degrades by chain scission under corona discharge and high-ozone atmospheres. It should not be exposed to aromatic solvents or chlorinated solvents because these substances migrate into polyethylene and may swell the web. The product is not intended for use with amine-based adhesion promoters without a controlled trial; amine species can interact with oxidized polyethylene and disrupt interfacial bond strength. On lamination lines with hot-air ovens, web temperature must be limited below the onset of film shrinkage. If drying tunnel air temperature is maintained above 70–80 °C for prolonged dwell, a 38.1 µm LLDPE web may undergo transverse relaxation, especially under high winding tension. The resulting dimensional change appears as tunneling or baggy edges in the finished laminate. When converting lines switch from a 50 µm LDPE sealant to this 38.1 µm LLDPE web, unwind tension and rewind taper must be reduced; otherwise, the thinner film stretches and neck-in increases at the coating station.