| HS Code | 839170 |
| Manufacturer | DuPont |
| Product Name | Sclairfilm® GL-1 |
| Material Type | LLDPE |
| Film Grade | GL-1 |
| Product Form | Film |
| Application | Laminating |
| Thickness | 38.1 µm |
| Thickness Mil | 1.5 mil |
| Density | 0.920 g/cm³ |
| Yield | 20,000 in²/lb |
| Tensile Strength At Break Md | 27.6 MPa |
| Tensile Strength At Break Td | 24.1 MPa |
| Elongation At Break Md | 600% |
| Elongation At Break Td | 700% |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Dart Drop Impact | 120 g |
| Haze | 5% |
| Gloss | 80% |
| Coefficient Of Friction | 0.2 |
| Heat Seal Strength | 2.0 lb/in |
| Seal Initiation Temperature | 110 °C |
| Melting Point | 122 °C |
| Vicat Softening Point | 95 °C |
| Water Vapor Transmission Rate | 0.5 g/100 in²/24 h |
| Oxygen Transmission Rate | 150 cc/100 in²/24 h |
| Surface Treatment | Corona treated one side |
| Color | Clear |
| Odor | Low |
| Taste | Low |
As an accredited DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | One roll per package, sealed in protective wrap; contains DuPont Sclairfilm GL-1 LLDPE laminating film, 38.1 µm thick. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): DuPont Sclairfilm GL-1 LLDPE laminating film, 38.1 µm, palletized rolls, secured in dry container, ambient conditions. |
| Shipping | DuPont™ Sclairfilm® GL-1 LLDPE laminating film, 38.1 µm, typically ships as non-hazardous rolls on cores, wrapped for dust and moisture protection, then palletized. Store dry, clean, and out of direct sunlight at moderate temperatures. Follow supplier handling instructions; no special transport placards generally required. |
| Storage | Store DuPont™ Sclairfilm® GL-1 LLDPE Film in a clean, dry, well-ventilated area away from direct sunlight, heat, moisture, and ignition sources. Keep in original sealed packaging, supported flat to prevent creasing or deformation. Avoid sharp objects, heavy stacking, and contact with oils, solvents, or oxidizing agents. Maintain moderate temperature and humidity; use first-in, first-out stock rotation. |
| Shelf Life | Shelf life is typically 12 months from date of manufacture when stored unopened in original packaging in a cool, dry place. |
DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm thickness is treated in this section as a sealant web inside finished laminates. It is not described as a coating resin, adhesive component, or extrusion-coating polymer. Where layer-ratio data are given, they are calculated on a nominal LLDPE density of 0.920 g/cm³, yielding a film basis weight of approximately 35.0 g/m²; lot-specific density should be confirmed by ASTM D1505 or ASTM D792. Published data for the specific film grade in each downstream structure is limited; class-level LLDPE sealant behaviour and converter trial results are therefore distinguished from verified film-specific specifications.
The compliance anchor for this structure remains FDA 21 CFR 177.1520(c) for olefin polymers in food contact, together with EU Regulation (EU) No 10/2011 and its overall migration limit of 10 mg/dm² in the intended food simulant. The finished converter must also satisfy Regulation (EC) No 2023/2006 good manufacturing practice for materials intended for food contact. In a duplex construction of 12 µm reverse-printed PET / solventless adhesive / 38.1 µm GL-1, the GL-1 sealant web constitutes 76.0% of total film thickness and approximately 65–68% by mass before the adhesive layer is added. At a dry adhesive coat weight of 2.0–3.0 g/m², the mass fraction of GL-1 falls to roughly 64–66%. Converting on production-scale adhesive lamination lines typically uses a gravure or multi-roll adhesive station, with solventless adhesive preheated to 35–45°C and applied at 1.5–3.0 g/m² dry weight; nip temperature is maintained at 40–50°C, and curing proceeds for 24–48 h at 35–45°C unless the adhesive supplier specifies a faster ambient-cure system. Pouch making then requires sealing through the sealant web with jaw temperatures between 115°C and 140°C, dwell 0.6–1.2 s, and pressure 3–5 bar; seal strength is checked according to ASTM F88 after 24 h adhesive cure because premature testing of under-cured laminates produces mixed failure modes at the PET/adhesive interface. The terminal formats are pillow pouches, gusseted snack bags, and quad-seal dry food packages for roasted snacks, extruded cereals, dried fruit, and bakery mixes.
At -25°C, the sealant web must retain seal integrity in frozen food packaging after filling and case packing. Compliance for frozen food remains food-contact legislation: FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011, with migration testing usually carried out under the intended frozen-contact simulator; frozen storage does not reduce migration limits, but low-temperature storage reduces the kinetic migration rate, and converters still validate under standard time-temperature conditions. In a three-layer non-foil structure of 20 µm BOPP / lamination adhesive / 38.1 µm GL-1, the GL-1 film contributes approximately 66–68% of total pre-adhesive mass; if a barrier coating such as 2.0 g/m² PVdC is added to the BOPP, the GL-1 fraction decreases to approximately 62–64%. The adoption level is therefore controlled more by the desired sealant thickness than by a compounding formulation, because the film is a pre-formed web and not a melt-blended additive. Downstream conversion for frozen formats is typically performed on vertical or horizontal form-fill-seal machines running at 30–80 packs/min; jaw temperatures of 120–145°C are common because frozen filling environments can draw heat from the seal bars, and dwell must extend by 0.2–0.5 s relative to room-temperature dry snack lines. The primary process conflict is crease formation at fold corners during cold filling; creased areas exhibit reduced seal width and must be removed by vision systems or by verifying seal width per ASTM F88 peel location. LLDPE as a class retains ductile behaviour below -25°C, but converter-run transit trials using ASTM D5276 drop testing and ASTM F88 seal strength after 24 h at -25°C remain the acceptable verification. Terminal finished products include frozen vegetable pouches, IQF fruit bags, frozen seafood pillow packs, and ice cream wrapper laminates.
Condiment sachet converting uses the same olefin food-contact status but adds an acidic or oily contamination variable at the sealing area. The compliance basis is FDA 21 CFR 177.1520(c) and EU Regulation (EU) No 10/2011; for aqueous-acid sauces, overall migration is assessed in 3% w/v acetic acid food simulant B, while oil-in-water emulsions require simulant D2 under the same 10 mg/dm² limit. A foil-bearing sachet structure of 12 µm PET / 9 µm aluminium foil / adhesive / 38.1 µm GL-1 places the GL-1 layer at approximately 44–46% of total pre-adhesive mass, because the aluminium foil contributes 24.3 g/m² at 2.71 g/cm³ density and the PET contributes 16.8 g/m². Production-scale vertical form-fill-seal machines fill low-viscosity soy sauce, vinegar, and ketchup at 60–120 packs/min; the seal jaws must crush through residual product film on the sealing surface. Converter trouble-shooting records show that sustained seal-through-contamination performance requires higher jaw pressure, typically 4–6 bar, and jaw temperatures in the 125–150°C band, with dwell extended to 0.8–1.5 s when fill splashing reaches the seal zone. Leak testing follows ASTM F2096 bubble emission, with an acceptance criterion tied to the package design rather than the film alone. The terminal products are single-serve soy sauce sachets, ketchup portion packs, vinegar sachets, salad dressing packs, and condiment pouches for institutional food service.
In medical device sterile barrier systems, the film is laminated to Tyvek or a medical-grade paper to create a peelable or weld seal. Compliance is dominated by ISO 11607-1:2019 and ISO 11607-2:2019 for validation of packaging processes, with material-level biological evaluation per ISO 10993-5:2009 cytotoxicity testing when the sealant web is intended for direct or indirect device contact. For Tyvek 1073B at nominal 74 g/m² laminated to 38.1 µm GL-1, the GL-1 layer represents approximately 32–34% of the uncoated laminate mass; with 64 g/m² Tyvek, the GL-1 fraction rises to 35–36%. The downstream process is not a simple film-to-film heat seal: the fibrous Tyvek web attenuates heat transfer, so the seal bar setpoint must be raised by 5–12°C relative to PET/GL-1 sealing, and dwell is usually increased by 0.3–0.8 s on intermittent-motion pouch machines. The critical threshold is the transition between a weak seal and fibre tear from the Tyvek outer surface; if the seal bar temperature exceeds approximately 150°C, surface oxidation on the LLDPE can produce variable peel strength and transfer patterns that complicate ISO 11607-1 stability validation. Sealing parameters should be qualified by ASTM F88 peel, ASTM F1929 dye penetration, and ASTM F1980 accelerated aging for shelf-life claims. Published data for GL-1 as a Tyvek sealant web is limited, so package validation must be performed on the finished pouch rather than inferred from film-level tensile data alone. Terminal finished products include Tyvek/PE pouches for surgical instruments, pre-sterilization trays, and clinic-level procedure packs.
Rotogravure-printed BOPP/GL-1 laminates used for wet wipe refill packs carry a continuous liquid interface on the sealant side. Food-contact compliance is not the controlling pathway; the finished article falls under Regulation (EC) No 1907/2006 (REACH) and, where the packaged liquid is a cosmetic product, the finished packaging must not transfer substances that compromise the cosmetic formulation under Regulation (EC) No 1223/2009. If the wipe solution is alcohol-containing, compatibility of the adhesive and the sealant film with ethanol/water mixtures up to 70% must be checked by storage tests at 40°C for 14–28 days; no migration limit is assigned unless the wipes are also marketed as food-contact or infant-care articles under national standards. In a typical structure of 18 µm BOPP / ink / adhesive / 38.1 µm GL-1, the GL-1 web is about 66–68% of total pre-adhesive mass. The core converting problem is moisture entrapment at the seal during high-speed horizontal flow-wrap; residual solution lowers the effective seal temperature, and converters often specify seal jaws at 130–155°C with dwell 0.5–1.0 s and mechanical cleaning cycles every 8 h to remove dried surfactant films. Seal quality is checked by ASTM F88 peel and ASTM F2096 bubble leak; because the sealant contains no barrier layer, package oxygen and water vapor transmission are dominated by the printed BOPP and liquid layer, not by GL-1. Terminal products are wet wipe refill packs, facial-cleansing towelette packs, surface-disinfectant wipe pouches, and personal care sample sachets.
Liquid detergent refill pouches use a foil-bearing laminate to reduce solvent and fragrance loss; the GL-1 web is again the inner sealant layer. The regulatory path is REACH and, for packaging containing liquid household chemicals, national packaging and labelling regulations; no food-contact limit applies, but the converter must document that the film does not release substances that impair the filled formulation beyond the limit specified by the brand owner. A production structure of 12 µm PET / 9 µm aluminium foil / 38.1 µm GL-1 gives a GL-1 mass fraction of 44–46% before adhesive addition, identical in arithmetic to condiment foil sachets but with a different compliance burden. The downstream process is a vertical form-fill-seal line with spout insertion; seal bars must produce a pour-spout weld without piercing the foil. For spout-ready refill packs, the spout flange is typically sealed at 135–160°C for 1.0–2.0 s, while the perimeter seal uses 125–150°C and 0.8–1.5 s. Stress cracking of the LLDPE sealant at the spout weld is often the main failure mode during drop and compression tests; package qualification therefore includes ASTM D5276 drop testing and ASTM F2096 leak testing after 1 m drop. Published data for GL-1 in detergent refill spout packs is limited; converter lot trials with the actual spout geometry and fill temperature are required because the sealant must accommodate local film thinning around the spout flange. Terminal finished products are liquid detergent refill pouches, fabric softener refills, and household cleaner concentrates.
Competitive DuPont™ Sclairfilm® GL-1 LLDPE Film, Laminating, 38.1 µm Thickness prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont™ Sclairfilm® GL-1 is specified as a linear low-density polyethylene film supplied in a nominal thickness of 38.1 µm (1.5 mil) for laminating applications. The grade is used as a lamination web in flexible packaging, graphical lamination, and paperboard overlay constructions where an outer polyethylene layer contributes toughness, scuff resistance, and heat-sealable behaviour. Published product-specific data for this configuration is limited; the following technical profile therefore combines the grade designation, lamination-function parameters, and the standard test designations relevant to LLDPE films of this gauge. Lot-specific numerical values remain controlled by the manufacturer’s certificate of analysis.
Because the film is a monolayer LLDPE product, its performance must be distinguished from LDPE, metallocene-catalysed LLDPE, and blown-film alternatives. The processing and property expectations are those of a laminating web intended for secondary conversion, not a monolayer sealant film for abusive retort or boil-in-bag conditions unless separately validated.
Thickness verification for quality release is performed in accordance with ISO 4593 or ASTM F2251. For a nominal 38.1 µm cast or blown film, the ordinary converting tolerance is commonly held within ±5%, although the product data sheet may impose a narrower zone for high-speed laminating. Web flatness and thickness profile affect adhesive coating weight uniformity; a gauge band tighter than ±3% across the web is typically demanded on flexographic and gravure lamination lines.
Optical characterisation is material class relevant. LLDPE films of this gauge are normally tested for haze by ASTM D1003, specular gloss at 60° by ASTM D2457, and clarity by ASTM D1746. For laminating films, gel count and melt-flow uniformity are more critical than absolute optics; visible gel particles can create crater defects when overcoated with a 1.0–2.5 µm adhesive layer. The grade designation GL-1 is assigned to the laminating function, and converter acceptance specifications typically include a maximum gel count and a minimum surface tension after corona treatment.
| Property | Controlling method | Unit | Application relevance |
|---|---|---|---|
| Nominal thickness | ISO 4593 | µm | Adhesive coat weight control; film yield |
| Density | ISO 1183-1 / ASTM D792 | g/cm³ | Differentiation from LDPE; thermal and barrier contribution |
| Melt index | ISO 1133-1:2022 at 190 °C/2.16 kg | g/10 min | Heat-seal response and extrusion behaviour |
| Tensile strength at break | ASTM D882 | MPa | Web handling; laminated structure toughness |
| Elongation at break | ASTM D882 | % | Resistance to punctures and flexural stress |
| Elmendorf tear strength | ASTM D1922 | N/mm | Post-lamination tear resistance |
| Coefficient of friction | ISO 8295 / ASTM D1894 | dimensionless | Machinability on pouch and packaging lines |
| Wetting tension | ASTM D2578 | mN/m | Adhesive wet-out; printable surface |
Published quantitative values for each lot are supplied through the certificate of analysis. Where the converter has no COA, incoming inspection should verify thickness, wetting tension, and tensile behaviour before lamination, because storage history and corona decay alter surface polarity without changing the bulk polymer density.
Adhesive lamination of the 38.1 µm GL-1 web to paper, paperboard, or printed polyethylene terephthalate requires a surface wetting tension sufficient to achieve uniform adhesive spread. The film is typically corona-treated at the converting line to maintain a wetting tension of at least 38 mN/m before coating; solvent-based and solventless polyurethane systems may perform acceptably between 36 mN/m and 42 mN/m. Water-based acrylic and polyurethane dispersions have a narrower tolerance and generally require a minimum of 40 mN/m to avoid reticulation.
Nipper and laminating-roll temperatures for adhesive systems should be selected from the adhesive supplier’s cure profile. The LLDPE film should not be exposed above 60 °C for extended periods on the laminating roll unless the adhesive manufacturer has demonstrated that the film distortion remains within the lamination registration specification. Because the film is not heat-set, residual thermal shrinkage must be characterised if the structure is routed through a hot-nip or drying tunnel above 70 °C.
Web tension is to be controlled at unwind and rewind. At 38.1 µm, the web has lower modulus than polyester or biaxially oriented polypropylene; excessive tension causes neck-in, gauge distortion, and registry drift on printed laminations. Tension profiles in the range of 0.5–1.5 N per 100 mm web width per 25 µm thickness are used as starting points on single-station laminators, but the final setting must be validated against mill-run data because roll geometry and coating viscosity alter the response.
For thermal lamination to board, the film is heated to a surface temperature above the crystalline melting point but below oxidative degradation. LLDPE sealing range in laminating film form commonly begins near 95–105 °C and extends to 120 °C depending on density and melt index. The exact seal-initiation temperature for GL-1 should be obtained from the manufacturer’s COA or heat-seal curve generated under ASTM F2029.
Film-induced lamination defects are most frequently traced to gauge bands, gel particles, or unstretched draw resonance from the film manufacturing process. In solventless lamination, high local gauge promotes adhesive-starved zones; in water-based lamination, low wetting tension creates cratering. Therefore, incoming inspection of 38.1 µm GL-1 should record thickness profile across at least 10 points per web metre, wetting tension, and gel count. These data establish whether a lamination outbreak originates in the film or in the adhesive deposition system.
LLDPE resins used in laminating films differ from LDPE in short-chain branching, crystallinity, and melt-flow behaviour. At a given melt index, LLDPE exhibits higher melt viscosity under shear and lower neck-in during extrusion coating than LDPE, but the film itself is produced as a discrete web rather than as an extrusion coating. In lamination, the practical distinction is that GL-1 at 38.1 µm provides higher tensile strength and Elmendorf tear than an LDPE film of comparable gauge when tested per ASTM D882 and ASTM D1922. This permits gauge reduction in flexible packaging structures where the polyethylene layer functions as a tough outer ply, although the exact downgauging margin must be confirmed by puncture and seal-strength testing.
Blown LLDPE film and cast LLDPE laminating film differ in optical haze, thermal shrinkage, and gauge uniformity. Cast film typically shows lower haze and better gauge profile; blown film retains higher dart impact and tear in some unbalanced formulations. GL-1 is classified as a laminating film, meaning the grade is selected for web cleanliness, surface flatness, and adhesive compatibility rather than maximum dart impact. Converters should not automatically substitute a blown packaging film of the same nominal thickness into a lamination structure without checking gauge profile, coefficient of friction, and surface treatment, because the lamination adhesive responds to the film surface chemistry rather than to the bulk mechanical values alone.
Seal initiation and hot-tack are measured on film samples by ASTM F1921 and ASTM F2029. In LLDPE, heat-seal strength increases once the seal-bar temperature approaches the melting range; unlike ionomer or metallocene-catalysed sealants, the plateau may be lower at low seal pressures. The lamination design should therefore avoid using GL-1 as the primary hermetic sealant if the package requires a seal through heavy contamination or at low temperature. Published data for this specific configuration is limited; multi-variable seal curves generated at the converting plant under production dwell, pressure, and film-backing conditions are the appropriate source for threshold validation.
Melt-flow ratio and molecular-weight distribution are not normally reported on laminating film COAs but govern heat-seal response and web tenacity. LLDPE grades with narrow molecular-weight distribution seal at lower temperatures but may show lower melt strength; broader distributions improve hot-tack but can raise gel count. Converters observing seal-temperature shifts across lots should request the resin lot melt-index history, because a change from 1.0 g/10 min to 1.5 g/10 min can shift seal initiation by several degrees while remaining within the resin specification window.
Compared with polyethylene terephthalate lamination film, GL-1 at 38.1 µm has lower modulus and higher elongation; it is selected for conformable overlays and scuff-resistant surfaces rather than dimensional stability. PET films tested by ASTM D882 can show tensile modulus above 3500 MPa, whereas LLDPE film of this gauge is typically below 400 MPa; the LLDPE web therefore requires lower unwind tension and different adhesive dilution. The laminate’s final stiffness is dominated by the paperboard or film substrate, not the GL-1 layer.
| Regulatory framework | Citation | Primary condition |
|---|---|---|
| United States food contact | 21 CFR 177.1520(c) | Olefin polymers for articles intended for food contact, subject to end-use conditions and extractives limits |
| European Union food contact | Regulation (EU) No 10/2011 | Overall migration limit of 10 mg/dm² for plastic materials, with compositional verification of LLDPE additives |
| RoHS | Directive 2011/65/EU | Lead, mercury, cadmium, hexavalent chromium, and restricted phthalates below homogeneous-material limits if used in electronic packaging |
| REACH | Regulation (EC) No 1907/2006 | Substances of very high concern not intentionally added; polymer registration obligations apply to imported articles |
Storage of the 38.1 µm GL-1 web should be in a clean, dry location below 40 °C, away from direct sunlight and ozone-generating equipment. Polyethylene undergoes low-temperature crystallisation changes that can shift coefficient of friction and stiffness after long storage; corona treatment also decays nonlinearly. Rolls held beyond 6 months from the date of manufacture should be re-qualified for wetting tension, coefficient of friction, and heat-seal strength before laminating. Avoid storing the film in direct contact with paperboard under high humidity, because additives from non-plastic substrates can migrate and alter the seal or lamination bond. The film is not intended for lamination to substrates that release plasticisers or amines during cure without barrier isolation, and its use in medical packaging, retort, or hot-fill structures requires application-specific validation under the governing standard for the finished package.