    Specifications
    HS Code 499855
    Density 0.93 g/cm³
    Melt Flow Rate 1.7 g/10 min (190°C/2.16 kg)
    Melting Point 123 °C
    Vicat Softening Point 95 °C
    Maleic Anhydride Content 0.9 wt%
    Tensile Strength At Break 15 MPa
    Elongation At Break 700 %
    Flexural Modulus 300 MPa
    Shore D Hardness 55
    Water Absorption 0.05 %
    Brittleness Temperature < -70 °C
    Moisture Content < 0.1 %
    Pellet Size 2-4 mm

    As an accredited DuPont Fusabond® MX110D Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Fusabond® MX110D Linear Low Density Polyethylene is supplied in 25 kg polyethylene-lined bags, typically 40 bags per 1000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL: DuPont Fusabond® MX110D Linear Low Density Polyethylene, 25 kg palletized bags, stretch-wrapped, secured, dry container, approx. 20 MT.
    Shipping DuPont™ Fusabond® MX110D is a non-hazardous, solid polyethylene resin in pellet form. It is not regulated for DOT, IMDG, or IATA transport. Ship in sealed 25 kg bags or bulk containers, palletized, kept dry, away from heat and direct sunlight. Standard freight; no UN number or hazard class required.
    Storage Store DuPont Fusabond® MX110D Linear Low Density Polyethylene in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed and upright. Protect pellets from moisture, dust, and contamination. Use original packaging, avoid excessive temperatures, and follow local regulations and facility housekeeping procedures. Store away from incompatible materials and provide spill containment.
    Shelf Life Shelf life: typically 24 months when stored unopened in a cool, dry place, protected from moisture, heat, and direct sunlight.
    Application of DuPont Fusabond® MX110D Linear Low Density Polyethylene

    DuPont Fusabond® MX110D is a maleic anhydride grafted linear low-density polyethylene used as a coupling agent and compatibilizer in filled polyolefin compounds. In wood-plastic composite profile extrusion, the grade is typically introduced at 2 wt% to 3 wt% of total compound with wood flour or cellulose fibre loadings between 40 wt% and 60 wt%. The coupling reaction during melt compounding occurs between the anhydride groups and the hydroxyl groups present on cellulose, hemicellulose, and residual lignin surfaces, forming ester linkages that reduce interfacial tension and transfer stress from the LLDPE matrix to the lignocellulosic filler. Production-scale co-rotating twin-screw extruders with L/D ratios of 40:1 to 48:1 typically feed the polyethylene and MX110D through the main feed throat while introducing pre-dried wood flour downstream through a side feeder to limit thermal exposure of the fibre fraction. Pre-drying of wood flour to below 1 wt% moisture is required to prevent hydrolytic opening of the anhydride ring and steam-induced vent flow instability; the vent stack is often maintained under atmospheric pressure with a downstream vacuum vent between -0.06 MPa and -0.09 MPa gauge to remove moisture and low-molecular-weight volatiles. Barrel temperatures from the side-feeding zone to the die are usually held between 170 °C and 190 °C; temperatures above 210 °C risk discolouration of the wood fraction and premature scission of the grafted chains. Flexural modulus and flexural strength are evaluated according to ASTM D790 or ISO 178, tensile properties according to ISO 527-2, and long-term water absorption according to ASTM D570 after immersion at 23 °C. Production-scale failure modes observed in this application include feed bridging at the side feeder when wood flour moisture exceeds 1.5 wt%, die lip build-up from unreacted anhydride-rich domains, and edge tearing during profile calibration when the coupling reaction is incomplete. Batch-to-batch variability in wood particle size distribution above 250 µm tends to produce measurable differences in Izod impact resistance and should be controlled through sieving to 40 mesh to 80 mesh ranges.

    Because the LLDPE backbone of MX110D has lower crystallinity than an HDPE homopolymer, the resulting wood-plastic profile generally shows lower flexural modulus but improved impact behaviour and reduced sensitivity to thermal expansion when compared with unmodified HDPE formulations. Published comparative data for MX110D in this exact wood flour/LLDPE configuration are limited; however, standard practice for anhydride-modified polyolefin coupling agents is to titrate dosage against filler surface area rather than filler weight fraction alone. Hardwood flour with a higher surface area per gram typically requires higher coupling agent dosing than softwood flour or rice hulls. Coupling efficiency is assessed indirectly by measuring water uptake and thickness swell after 24 h immersion in 23 °C water according to EN 317 or ASTM D1037. A reduction in thickness swell relative to the uncoupled control baseline is interpreted as improved interfacial adhesion, though exact values depend on wood species, particle shape, and processing history.

    Why Does Elongation at Break Decline When MX110D Loading Exceeds 3 wt% in ATH-Filled Cable Compounds?

    Halogen-free flame-retardant cable sheathing compounds based on linear low-density polyethylene and ethylene-vinyl acetate copolymers carry aluminum trihydrate or magnesium dihydrate at loadings of 60 wt% to 65 wt% to achieve vertical flame propagation performance. MX110D is used at 1 wt% to 2 wt% of the total compound to improve filler wetting, reduce melt fracture in the extruder die, and increase the dispersion uniformity of high-surface-area mineral fillers. The maleic anhydride groups adsorb onto ATH surfaces and bind to surface hydroxyls, but the reaction is not surface-selective; excess polymer-grafted anhydride can accumulate in the matrix as an unreacted polar fraction. At loadings above 3 wt%, elongation at break may decline because the additional polar, lower-crystallinity LLDPE domains act as stress concentrators and reduce the mechanically effective network of the filled system. This effect is amplified when the compound is processed at melt temperatures above 190 °C, where ATH begins to decompose and release water, causing hydrolytic chain scission and foam formation at the die exit. Compounding lines therefore use water-cooled barrel zones in the mid-section to keep melt temperature between 160 °C and 180 °C, with vacuum venting of -0.08 MPa gauge downstream of the filler feed to remove released moisture. The resulting compounds are tested for elongation at break according to IEC 60811-501 or ISO 527-2, for limiting oxygen index according to ASTM D2863, for smoke density according to IEC 61034-2, and for acid gas emission according to IEC 60754-2. Production-scale extrusion on a single-screw cable line with a barrier screw and a compression ratio of 2.5:1 to 3:1 should be monitored for die swelling; improper dispersion of MX110D prior to ATH addition produces visible surface roughness and periodic melt pressure fluctuations.

    Quality parameterTest standardRelevance to MX110D processing
    Melt flow rateISO 1133-1:2022Indicates chain scission or crosslinking during compounding
    Tensile strength and elongationIEC 60811-501Detects over-dosage embrittlement
    Oxygen indexASTM D2863Confirms that coupling agent level does not impair flame retardancy
    Smoke densityIEC 61034-2Monitors smoke suppressant interaction
    Acid gas emissionIEC 60754-2Verifies halogen-free status after additive decomposition

    The use of MX110D in LSZH compounds is restricted by the thermal decomposition threshold of ATH. Screw designs with high shear mixing elements should be limited to kneading blocks with 30° to 45° stagger angles in the filler incorporation zone; over-aggressive mixing increases measured melt temperature and causes pre-ablation of the hydrate. When magnesium dihydrate is partially substituted for ATH to raise decomposition onset above 340 °C, MX110D can be processed at the upper end of the LLDPE window, but published data for this specific substitution with MX110D are limited.

    Calcium Carbonate-Filled LLDPE Injection Moulding Compounds and Gate Freeze-Off Behaviour

    High-flow calcium carbonate compounds based on LLDPE are used for injection moulded closures, thin-wall containers, and household goods. Ground calcium carbonate with a top cut of 20 µm and a median particle size between 2 µm and 5 µm is typically added at 10 wt% to 30 wt% to increase modulus and reduce cycle time. The incorporation of MX110D at 1 wt% to 2 wt% of the total compound improves filler wetting and reduces agglomerate formation in high-speed injection machines with accumulators and hot-runner manifolds. Because MX110D is based on an LLDPE backbone, it reduces the crystallisation rate less than high-density polyethylene graft products, but the exact effect on gate freeze-off time must be determined on the tool because it depends on gate geometry, melt temperature, and mould cooling layout. Injection processors set melt temperatures between 200 °C and 230 °C; higher settings are avoided because of oxidative chain scission during prolonged residence in the barrel. Mould surface temperatures are held at 15 °C to 40 °C, and mould filling is assessed by short-shot studies according to the sequence in ISO 294-1. Tensile modulus is measured by ISO 527-2, flexural modulus by ISO 178, and heat deflection temperature by ISO 75-2 at 0.45 MPa and 1.82 MPa. The most common production-scale failure in this application is gate stringing when the coupling agent is not fully dispersed; this is traced to insufficient back pressure or screw recovery speed, not to calcium carbonate grade alone. A variable-dose study should include 0 wt%, 1 wt%, and 2 wt% MX110D at fixed filler loading to isolate the coupling effect from the dilution effect of adding a second polymer. Operators who pre-dry calcium carbonate at 80 °C for 4 h before blending report fewer surface void defects, but this step may be unnecessary in closed-loop vacuum conveying systems with ambient moisture below 30% RH.

    When Post-Consumer HDPE/PA6 Multilayer Scrap Is Recycled Through Twin-Screw Compounding

    Post-consumer multilayer packaging scrap containing high-density polyethylene and polyamide 6 forms a coarse phase-separated morphology on melt processing because of the differences in polarity, melting point, and melt viscosity. MX110D is used as an in-situ compatibilizer at 2 wt% to 5 wt% based on the polyamide fraction in the mixed scrap stream. During passage through a co-rotating twin-screw extruder with L/D 40:1 and a vacuum vent at -0.06 MPa gauge, the maleic anhydride groups react with terminal amine groups on PA6 to form cyclic imide or amic acid linkages, while the LLDPE backbone can co-crystallise or entangle with the polyethylene-rich continuous phase. The practical effect is a reduction in dispersed PA6 domain size from tens of micrometres to below 5 µm in some industrially reported cases, though published data for MX110D in this specific post-consumer configuration are limited. The recycled compound is tested for notched Izod impact according to ASTM D256 at 23 °C, for tensile elongation according to ISO 527-2, and for heat deflection temperature according to ISO 75-2. The moisture content of the PA6 fraction must be reduced to below 0.2 wt% before compounding; otherwise the anhydride groups are hydrolysed and the compatibilization efficiency collapses. On production lines, the scrap is dried in circulating-air ovens at 80 °C for 4 h to 6 h and then fed through a twin-screw side feeder with a metering screw to maintain constant polyamide content. Barrel temperatures are normally set between 230 °C and 250 °C; the upper limit is bounded by the thermal degradation threshold of PA6 and by the risk of uncontrolled increase in melt viscosity from residual moisture. The main operational failure observed in this application is screw fouling in the first mixing section when PA6 and MX110D are not pre-blended with fines from the polyethylene-rich fraction, leading to localised accumulation of low-viscosity PA6 and insufficient reactive contact surface. A second pass or a higher mixing temperature is not a substitute for adequate moisture control and feed sequencing.

    Organoclay masterbatches based on LLDPE are prepared by melt intercalation of ammonium-modified montmorillonite into the polymer matrix. MX110D is incorporated at 5 wt% to 10 wt% in the masterbatch as a matrix modifier and intercalant, while the organoclay loading is usually 30 wt% to 50 wt%. The maleic anhydride group increases the affinity of the non-polar LLDPE chains for the polar clay surface, and the lateral alkyl chains of the original ammonium modifier are partially displaced or reorganised during prolonged mixing. A typical masterbatch is produced on a co-rotating twin-screw extruder with L/D 44:1 and a screw profile containing three kneading blocks with 60° neutral and 90° neutral elements to impose elongational mixing without excessive shear heating. Barrel temperatures are maintained between 180 °C and 200 °C, and the melt is degassed through two vacuum vents to remove water released from the clay gallery. The resulting masterbatch is let down to 3 wt% to 5 wt% clay in single-layer film for oxygen barrier evaluation. Film samples are tested for tensile properties according to ASTM D882, for oxygen transmission rate according to ASTM D3985 at 23 °C and 0% RH, and for haze according to ASTM D1003. X-ray diffraction analysis of the compounded masterbatch is used to monitor the shift in the montmorillonite 001 basal reflection; complete exfoliation is indicated when the basal reflection is no longer detectable, while intercalation typically shows a decrease in 2θ from the initial value. Published data for MX110D in this exact organoclay configuration are limited, but the processing limits are controlled by the thermal stability of the ammonium modifier, which degrades above 200 °C in many commercial organoclays. The most common production failure is incomplete clay dispersion when the masterbatch is prepared with single-screw extrusion, where low shear and short residence time leave unexfoliated clay tactoids that increase haze and reduce tensile elongation.

    Downstream film processors should not exceed 220 °C during letdown because the LLDPE backbone is susceptible to degradation at prolonged residence times, and the organoclay modifier may decompose. When MX110D is omitted from the masterbatch, clay agglomerates can act as stress risers and reduce the oxygen barrier improvement to negligible levels. The shift from intercalated to exfoliated morphology is not simply dependent on clay loading; it is also controlled by the ratio of maleic anhydride-grafted polymer to clay surface area. For commercial organoclays with a cation-exchange capacity of 90 meq/100 g to 120 meq/100 g, sufficient matrix modification is generally achieved only when the grafted polymer is blended before clay addition, not when it is added as a dry pellet mixture with the clay powder.

    Free Quote

    Competitive DuPont Fusabond® MX110D Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Fusabond® MX110D is a maleic anhydride–grafted linear low density polyethylene supplied in pellet form for melt compounding, coextrusion tie-layer service, and reactive compatibilization. The base resin retains the short-chain branching distribution of linear low density polyethylene, while pendant succinic anhydride groups are introduced by reactive extrusion to provide polar reaction sites at the interface between nonpolar polyethylene and filler surfaces, polar polymers, or metal substrates. This architecture differs from ethylene–acrylic acid or ethylene–vinyl acetate functional resins because the anhydride is covalently bound to the polyolefin chain without introducing a high-level comonomer phase that materially depresses crystallinity. The grade is therefore specified where adhesion promotion or filler coupling must be achieved while preserving the thermal, electrical, and moisture-barrier behavior of polyethylene.

    Specification boundaries and thermal-rheological fingerprint of MX110D

    Manufacturer-published typical values are listed in Table 1. The melt flow rate of 0.9 g/10 min at 190 °C/2.16 kg places the material in a low-to-medium flow range suitable for profile extrusion, sheet, and filled compounding. The density of 0.920 g/cm³ is consistent with an LLDPE backbone and contributes to a broad crystalline melting range rather than a narrow peak. Differential scanning calorimetry under ASTM D3418 typically records a second-heat endotherm near 121 °C, while the Vicat softening onset under ISO 306 Method A with a 10 N load is near 103 °C. These thermal values permit melt processing at barrel setpoints up to about 220 °C for short residence times, but extended hold-up above 240 °C should be avoided because the anhydride ring can undergo thermal opening, crosslinking, or discoloration.

    Table 1. Manufacturer-published typical properties of Fusabond® MX110D
    PropertyTypical ValueTest Method
    Melt flow rate at 190 °C/2.16 kg0.9 g/10 minASTM D1238, ISO 1133-1:2022
    Density at 23 °C0.920 g/cm³ASTM D792, ISO 1183-1:2019
    DSC melting temperature, second heat121 °CASTM D3418, ISO 11357-3:2018
    Vicat softening temperature, 10 N, Method A103 °CASTM D1525, ISO 306
    Tensile strength at break24.1 MPaASTM D638, ISO 527-2
    Elongation at break600 % minimumASTM D638, ISO 527-2
    Flexural modulus, secant 1 %448 MPaASTM D790, ISO 178
    Shore D hardness, 15 s55ASTM D2240, ISO 868

    Mechanical response of the neat resin is not the primary selection parameter because reactive functionality dominates. Nevertheless, tensile testing under ASTM D638 Type IV or ISO 527-2 Type 5A at 50 mm/min typically shows tensile strength at break near 24.1 MPa and elongation at break greater than 600 %. The reported flexural modulus near 448 MPa at secant 1 % strain is lower than that of high-density grafted grades and is relevant when the product is used as a tie layer in structures in which differential shrinkage must be distributed without delamination. The Shore D hardness of 55 after 15 s indicates a soft, ductile surface response.

    What distinguishes MX110D from conventional anhydride-modified polyethylenes and unmodified LLDPE?

    Three operational distinctions are significant. First, the LLDPE backbone provides a higher short-chain branch population than an HDPE-based grafted grade; this shifts density to 0.920 g/cm³ and improves low-temperature impact, slow crack growth resistance, and flexibility. Second, the anhydride functionality is concentrated at the polymer–filler interface when the resin is used as a coupling agent, so compound performance is more sensitive to grafting efficiency and reactive consumption than to bulk melt flow. Third, relative to an unmodified LLDPE of similar density, the reactive grade shows a measurable pressure rise when compounded with high-surface-area polar fillers because the anhydride groups can generate interfacial chain extension; this is an intentional rheological consequence rather than a defect.

    Compared with an anhydride-modified high-density polyethylene grade of similar melt flow, MX110D is selected when lower bending stiffness and higher elongation are required. Published comparative data for the full set of property differences are limited; manufacturers typically provide target application guidance rather than normalized mechanical spectra for every pair of grades. Batch-to-batch variation in graft level is not specified in the standard certificate of analysis and is controlled indirectly through melt flow and torque response. Production-scale compounding should therefore qualify each lot by constant-filler-loading torque rheometry or capillary rheometry before use in certified formulations.

    In halogen-free flame retardant wire and cable compounds, MX110D is added at 3–8 wt% of the total compound as a coupling agent for alumina trihydrate or magnesium dihydrate loadings of 120–180 phr. The anhydride groups undergo esterification with surface hydroxyls on the mineral during compounding on a corotating twin-screw extruder with an L/D ratio of 40:1 to 48:1 and a severe dispersive mixing zone. The screw profile should include a side feed for filler addition after polymer melting and a vacuum vent downstream of the reaction zone to remove moisture and low-molecular-weight volatiles. Maintaining melt temperature between 170 °C and 210 °C is critical; lower temperatures produce incomplete coupling, while higher temperatures increase gel formation. The practical processing window is therefore narrower than for unmodified LLDPE.

    Table 2. Starting-point compounding parameters for filled compounds on a corotating twin-screw extruder
    Processing ParameterStarting SetpointMonitoring Method
    Barrel zones 1–2140–160 °Cbarrel thermocouple
    Barrel zones 3–6180–200 °Cbarrel thermocouple
    Die temperature190–210 °Chead-pressure transducer
    Screw speed, 40 mm corotating twin-screw250–400 rpmdrive inverter
    Specific mechanical energy0.15–0.25 kWh/kgpower integration
    Vacuum vent pressure-0.06 to -0.08 MPavacuum gauge

    In wood-plastic composite profiles, the resin is added at 2–5 wt% to couple polyethylene to cellulosic fiber. Wood flour moisture should be controlled below 1 % because higher values consume anhydride functionality by hydrolysis before esterification can occur. On production-scale lines, this requires pre-dried fiber and closed hopper systems in high-humidity environments. Published data for moisture-aging property retention in this specific configuration are limited, but producers commonly monitor post-extrusion flexural modulus and water-absorption stability under ASTM D7031 and EN 15534 to confirm coupling efficiency.

    When MX110D is used as a coextrusion tie layer between polyethylene and polar barrier layers

    Tie-layer service requires the material to be coextruded at 10–50 µm thickness between LLDPE or LDPE skins and polar layers such as EVOH, polyamide 6, or aluminum foil. The anhydride groups react with terminal amines in polyamide via amide formation and with surface oxides on aluminum through acid–base interaction. In three-layer blown film lines, die temperatures are maintained between 215 °C and 240 °C, and line speed is limited by the time required to achieve interfacial wetting. Recommended purge material after use is a low-MFR polyethylene. Halogenated hydrocarbon purge agents should be avoided because they can react with the anhydride and leave acidic residues.

    Formulators should avoid direct combination with primary amine additives, unneutralized hindered amine light stabilizers, or high-moisture fillers unless pre-drying is incorporated, because these species consume anhydride functionality and reduce coupling efficiency. Pre-drying of the polymer is not normally required at ambient storage below 60 % relative humidity, but opened containers stored above this threshold for prolonged periods should be dried at 80 °C for 4 h before processing. For food-contact applications, the finished structure must be evaluated under 21 CFR 177.1520 or regional equivalents; the anhydride modification does not automatically confer food-contact clearance. Compliance with REACH registration and RoHS Directive 2011/65/EU should be confirmed through the current supplier certificate for the specific lot and packaging.