| HS Code | 945305 |
| Polymer Type | Maleic anhydride grafted linear low density polyethylene |
| Density | 0.93 g/cm3 |
| Melt Flow Rate 190 C 2 16 Kg | 3.5 g/10 min |
| Melting Point | 125 °C |
| Vicat Softening Point | 90 °C |
| Maleic Anhydride Content | 0.9 wt% |
| Moisture Content | <0.1 wt% |
| Form | Pellets |
| Color | Natural |
| Tensile Strength At Yield | 10 MPa |
| Tensile Strength At Break | 16 MPa |
| Elongation At Break | >700% |
| Flexural Modulus | 200 MPa |
| Hardness | 50 Shore D |
| Bulk Density | 0.56 g/cm3 |
| Thermal Degradation Temperature | >250 °C |
As an accredited DuPont Fusabond® MB528D Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont Fusabond® MB528D Linear Low Density Polyethylene packaging: 25 kg moisture-resistant bags, 40 bags per pallet, totaling 1,000 kg. |
| Container Loading (20′ FCL) | 20′ FCL: DuPont Fusabond® MB528D Linear Low Density Polyethylene, 25 kg bags, palletized, shrink-wrapped; approx. 20 MT total. |
| Shipping | DuPont Fusabond® MB528D is typically shipped as non-hazardous polyethylene pellets in 25 kg bags, 500–1000 kg bulk bags, or bulk containers. Transport in dry, clean, covered vehicles at ambient temperature. Avoid moisture, heat, and contamination. Not DOT/IMDG/IATA regulated. Refer to SDS and local regulations. |
| Storage | Store DuPont Fusabond® MB528D Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed in original packaging. Protect from moisture, contaminants, and strong oxidizers. Avoid prolonged elevated temperatures. Inspect containers regularly, follow SDS/local regulations, and use first-in, first-out stock rotation. |
| Shelf Life | DuPont Fusabond® MB528D has a typical shelf life of two years when stored in original, unopened packaging under cool, dry conditions. |
In high-loading calcium carbonate, talc, and barium sulfate compounds based on LLDPE, melt dilution of 20–60 wt% mineral filler converts the continuous polyolefin phase into a strained matrix with elevated apparent melt viscosity and reduced tensile elongation. Compounding on a co-rotating twin-screw extruder with L/D of 40–52 and side-fed filler at zone 5 demonstrates that DuPont Fusabond® MB528D addition between 0.5 wt% and 3.0 wt% of total compound, or 1.5–5.0 phr relative to filler, shifts the onset of melt fracture and stabilizes pressure at the die. When talc with a median particle size of 1.0–2.0 µm is used, the anhydride groups react with surface silanol species during a residence time of 20–40 s at 200–220 °C. For uncoated calcium carbonate with surface moisture below 0.15 wt%, torque fluctuation on a 43:1 L/D line has been observed to remain within ±5% of baseline when MB528D is pre-blended with the polymer pellets rather than side-fed as a separate stream. The resulting compounds show stabilized tensile yield and flexural modulus values when tested under ASTM D638 and ASTM D790, with melt flow index measured according to ASTM D1238 at 190 °C/2.16 kg. Formulations containing stearic acid-coated ground calcium carbonate require the upper addition band because the organic coating competes with the anhydride for the polar filler surface. Processing limits at the lower boundary are defined by insufficient coupling at 0.5 wt% for filler loadings above 45 wt%, while the upper boundary is limited by excessive melt dilution of tensile elongation at addition levels above 3.0 wt%. Moisture ingress during warehouse storage is a recurring production-scale failure mode; pellets stored at relative humidity above 60% should be dried at 65–80 °C for 4 h using desiccant dryers before introduction into the main feed port. Compliance for general industrial compounds rests on REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU, but specific food-contact uses require separate migration testing under EU 10/2011/EC or FDA 21 CFR 177.1520 for the finished article. Terminal products include extruded geomembranes, thermoformed automotive wheel arch liners, and industrial drainage channels, where long-term creep is monitored by ISO 899-2 and chemical resistance by ISO 175.
Extrusion of 50–60 wt% wood flour or rice husk fiber in an LLDPE carrier on a counter-rotating twin-screw compounder is governed by moisture removal, early fiber wetting, and retention time below the hemicellulose degradation threshold. Wood flour with a mesh size between 40 mesh and 80 mesh is dried to 0.4–0.6 wt% moisture in a vented hopper dryer at 80–100 °C for 2–4 h. The MB528D component is introduced at 2–4 wt% of total formula through the main feed throat, and the screw profile uses long-pitch conveying elements in the first 8–10 D of a 28–36:1 L/D barrel to avoid premature compaction. The compounder barrel profile is maintained between 150 °C and 185 °C; excursions above 200 °C initiate acetic acid release from wood hemicellulose, which is visible as brown discoloration and acidic odor at the vacuum vent. Venting at 50–100 mbar absolute pressure through atmospheric and vacuum ports removes residual moisture and low-volatility extractives. The grafted anhydride reacts at the lignocellulosic surface during the melt-mixing section, and the resulting interfacial adhesion is reflected in flexural modulus and water absorption values measured under ASTM D790 and ASTM D570. For exterior decking profiles, ASTM D7032-17 governs the finished product, while ASTM D7031-04 provides the guide for laboratory conditioning and property reporting for wood-plastic composite materials. At die pressures of 20–40 bar, a slit or profile die with a land length of 10–20 mm is used, and the extrudate is water-cooled to 35–50 °C before haul-off. Formulators run the MB528D level at the lower end of the range for hollow profiles and at the upper end for solid deck boards because increased interfacial coupling raises melt viscosity and die wall shear stress. Corrosion-resistant screws and barrels with nitride-hardened surfaces are specified when processing wood flour at the upper temperature bound, because the presence of acetic acid accelerates wear in unhardened equipment. End products include building decking, railing profiles, and exterior cladding, where the compound must retain dimensional stability after immersion in water at 60 °C for 24 h and subsequent drying under controlled laboratory conditions.
A halogen-free jacket compound formulated with 120–180 phr of aluminum trihydrate or magnesium dihydrate in an EVA/LLDPE blend is constrained by the onset of filler dehydration at approximately 180–220 °C, which creates porosity and surface roughness if melt temperature exceeds the ceiling. MB528D is added at 2–5 wt% of total compound to reduce filler-filler friction and to couple the unmodified polyolefin phase to the mineral filler surfaces. Mixing is performed on a co-rotating twin-screw extruder with L/D 40–52 and a water-cooled feed zone; barrel temperatures are held at 170–190 °C with the last mixing zone not exceeding 195 °C. A low-compression screw design with distributive mixing elements rather than aggressive kneading blocks is required because high shear at mineral loadings above 150 phr accelerates localized temperature rise and releases water vapor that can flash at the atmospheric vent. Dynamic oscillatory shear experiments in a parallel-plate rheometer at 190 °C show that the anhydride-grafted LLDPE suppresses the low-frequency storage modulus rise caused by filler network formation while maintaining sufficient high-shear process viscosity for stable extrusion. Capillary rheometry under ASTM D3835 at 190 °C is used to compare the shear viscosity of the compound with and without MB528D. Mechanical properties after accelerated aging at 100 °C for 168 h are evaluated according to IEC 60216-2 and ASTM D638, and the outer sheath is subject to flame propagation testing under IEC 60332-1-2, halogen acid gas measurement under IEC 60754-1, and smoke density under IEC 61034-2. The role of MB528D in this application is not flame retardancy—limiting oxygen index must be achieved by the mineral filler system—but the coupling effect permits inclusion of finer ATH grades without a total collapse of tensile elongation at break. Process operators monitor die pressure and melt temperature before the breaker plate; a pressure rise exceeding 10% over 30 min indicates filler accumulation or anhydride hydrolysis and requires a purge with neat polyolefin. End products include LSZH sheathing for public transport wiring, control cables, and building riser cables, where the final jacket must also meet low smoke and zero-halogen acceptance criteria set by the specifying authority.
| Application segment | Jurisdiction/standard | Designation | Verification checkpoint |
|---|---|---|---|
| High-filler LLDPE compounds | Global / industrial | ASTM D1238-10 | Melt flow index before and after MB528D addition; compare to virgin base resin |
| Wood-plastic composites | United States | ASTM D7032-17 | Deck board performance after exterior weathering and water absorption per ASTM D570 |
| LSZH cable jackets | International / EU | IEC 60332-1-2 | Vertical flame propagation; combine with IEC 60754-1 halogen acid and IEC 61034-2 smoke |
| Multilayer PE/PA film | EU / United States | EU 10/2011/EC | Overall migration and specific migration from final structure; FDA 21 CFR 177.1520 for olefin backbone |
| Aluminum composite panels | EU / United States | EN 13501-1 | Fire classification of the finished panel; adhesion by ISO 8510-2 |
| Post-consumer recyclate | Global | ISO 14021 | Recycled content claims; REACH and RoHS conformity |
In seven-layer barrier film production, feedblock pressure stability depends on matching the shear viscosity of the tie layer to adjacent polyethylene and polyamide or EVOH layers, not on maximizing anhydride content in isolation. MB528D can be processed as the continuous tie layer at 3–12 µm thickness or as a 20–40 wt% blend with LLDPE when the line requires a softer interlayer rheology. Blown-film lines with die gaps of 1.2–2.0 mm and blow-up ratios of 2.0–3.0:1 operate at melt temperatures of 210–240 °C for PA-containing structures and 190–220 °C for EVOH-containing structures; residence time above 5 min at 240 °C should be avoided because imide formation between the anhydride functionality and polyamide amine end groups can create visible gel particles. Cast-film coextrusion lines with dual-plane air knives and chilled roll temperatures of 18–25 °C are used for higher throughput, and the tie layer is designed to remain within a shear viscosity ratio of 0.7–1.4 relative to the polyamide at the merge point. Interlayer adhesion is quantified by ISO 11339:2010 or ASTM D1876 T-peel testing, with a 25 mm width specimen peeled at 300 mm/min. Oxygen transmission rate after flexing is measured under ASTM D3985 and water vapor transmission rate under ASTM F1249. For food-contact uses, the complete multilayer structure must comply with EU 10/2011/EC overall migration and specific migration limits for the additives used, while the olefin backbone is assessed under FDA 21 CFR 177.1520 and the adhesive functionality under FDA 21 CFR 175.105 or a suitable food additive clearance. The terminal films are used in vacuum pouches, modified-atmosphere packaging for meat and cheese, and retort lidding for polypropylene trays, where seal strength is measured according to ASTM F88. Processing limitations are defined by viscosity mismatch at the upper and lower ends: too high a tie resin viscosity causes interfacial instability and gauge banding, while excessive dilution below 20 wt% MB528D in LLDPE can reduce peel strength below the 3–5 N/15 mm minimum commonly set as a process specification for thermally sterilized pouches.
Although solvent-free roll-coating of the aluminum coil has become the dominant lamination route for aluminum composite panels, the polyethylene core extrusion remains the process step where MB528D is introduced to raise interfacial peel strength. In a flat die lamination line, a 0.5–3.0 mm LLDPE-based core is extruded between two pretreated aluminum skins of 0.3–0.5 mm thickness at line speeds of 5–20 m/min. The aluminum surface is treated with a chromate-free conversion coating, and the coil is preheated to 160–220 °C immediately before lamination. The core compound contains 3–8 wt% MB528D, which increases adhesion of the polyolefin melt to the polar conversion coating during roll bonding. Extruder barrel temperatures are set at 230–260 °C to ensure wet-out, and the flat die gap is controlled by an automatic lip adjustment system to maintain a core thickness tolerance of ±0.05 mm. Coil lamination pressure at the nip is maintained between 0.5 MPa and 2.0 MPa, and annealing of the finished panel at 80–100 °C for 1–4 h relieves frozen-in orientation that would otherwise contribute to warpage during exterior thermal cycling. Interlaminar adhesion is measured by a 180° peel test following ISO 8510-2 or by tensile lap shear following ASTM D1002, with specimens cut across the panel width to capture cross-machine variation. For facade systems, fire performance of the finished panel must be verified according to EN 13501-1 or ASTM E84, and coating durability is addressed separately by the aluminum supplier. The anhydride-modified LLDPE component is not a fire-retardant additive, so mineral-filled fire-rated core formulations require additional flame retardants and must be recertified as a complete assembly. The terminal products include exterior cladding, signage panels, and soffit liners, where service temperatures typically range from −40 °C to 80 °C and where the core must maintain adhesion after 1,000 h of hot water immersion at 60 °C when specified by the project standard.
Post-consumer mixed polyolefin streams containing 3–8 wt% polyamide, ethylene vinyl alcohol, aluminum foil residues, or paper fiber are upgraded in heavy-duty recycling extruders with L/D 30–45 and continuous melt filtration. The MB528D addition of 1–4 wt% acts at the interface between nonpolar polyolefins and residual polar contaminants, reducing visible gel counts and increasing elongation at break in injection-moulded test plaques. Processing on a single-screw recycling extruder with a vacuum vent at 80–120 mbar absolute and melt temperature of 190–230 °C requires that MB528D be introduced with the shredded flake rather than through a side feeder, because the randomized flake size distribution does not provide a stable bulk flow for separate dosing. Melt filtered through screen packs of 200–300 µm is then pelletized and injection-moulded into test specimens. Mechanical properties are measured under ASTM D638 and ASTM D256, and melt flow stability is characterized under ISO 1133-1:2022 at 190 °C/2.16 kg. The maximum addition is limited by processing economics and by a reduction in melt stiffness when the grafted LLDPE exceeds 4 wt%; below 1 wt% the compatibilization effect is often masked by the variability of the incoming flake. Published data for this specific configuration is limited, so formulation adjustments should be confirmed on the target recycling line rather than transferred from virgin resin trials. Recyclate used in non-food articles must meet REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU, while recycled content claims are documented under ISO 14021 rather than by product performance. The resulting pellets supply injection moulding of shipping pallets, outdoor furniture, underground drainage chambers, and automotive wheel arch liners, where the acceptance criteria are set by the original equipment manufacturer or public purchasing specification.
| Segment | MB528D loading window | Critical process boundary | Analytical measurement |
|---|---|---|---|
| Mineral-filled compounds | 0.5–3.0 wt% of total compound | Melt temperature 200–220 °C; filler moisture below 0.15 wt% | ASTM D1238; ASTM D638 |
| Wood-plastic composites | 2–4 wt% of total formula | Barrel 150–185 °C; vent 50–100 mbar | ASTM D790; ASTM D570 |
| ATH/MDH cable compounds | 2–5 wt% of total compound | Melt temperature below 195 °C; L/D 40–52 | ASTM D3835; IEC 60332-1-2 |
| PE/PA tie layers | 100% or 20–40 wt% blend in LLDPE | Residence time below 5 min at 240 °C | ISO 11339; ASTM D3985 |
| Aluminum composite panel cores | 3–8 wt% of core compound | Nip pressure 0.5–2.0 MPa; annealing 80–100 °C | ISO 8510-2; ASTM D1002 |
| Recyclate compatibilisation | 1–4 wt% | Vacuum 80–120 mbar; melt filter 200–300 µm | ISO 1133-1:2022; ASTM D256 |
Competitive DuPont Fusabond® MB528D Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont Fusabond® MB528D Linear Low Density Polyethylene is a maleic anhydride-grafted linear low-density polyethylene supplied as free-flowing pellets for reactive compounding, coupling, and compatibilization. The melt mass-flow rate is typically 2.0 g/10 min when determined at 190°C under a 2.16 kg load in accordance with ISO 1133-1:2022. Density is approximately 0.922 g/cm³ by ISO 1183-1:2019 at 23°C, and the peak melting temperature is 122°C by ISO 11357-3:2018. The product combines a linear low-density polyethylene backbone with pendant anhydride functionality, allowing it to function as a coupling agent toward hydroxyl-bearing fillers, silane-treated reinforcements, and polar thermoplastics. Unlike unmodified LLDPE, MB528D can participate in interfacial reactions during melt compounding without requiring solvent-based coupling treatments.
| Property | Test method | Typical value |
|---|---|---|
| Melt mass-flow rate | ISO 1133-1:2022, 190°C/2.16 kg | 2.0 g/10 min |
| Density | ISO 1183-1:2019, 23°C | 0.922 g/cm³ |
| Peak melting temperature | ISO 11357-3:2018 | 122°C |
| Maleic anhydride graft level | FTIR titration after hot methanol extraction | Lot-specific; confirm before formulation |
| Volatile content | ISO 15512:2019 Karl Fischer | <0.05% |
Because the anhydride graft level is not a public specification, incoming lot acceptance should include pressed-film FTIR titration after extraction of free maleic anhydride. Formulation adjustments are often required when changing filler supplier or lot because filler surface hydroxyl concentration and particle size distribution shift the optimum coupling-agent demand. A reasonable starting-point addition is 2–5 wt% of the total compound; the exact level is determined by mechanical property response and melt-flow retention.
In mineral-filled LLDPE compounds, the critical processing event is esterification between anhydride groups on MB528D and surface hydroxyl groups of aluminum trihydroxide or magnesium dihydroxide. The reaction becomes kinetically relevant above 180°C and is influenced by residence time, local shear heating, and the water activity at filler surfaces. After ring opening, the grafted polyethylene chain remains entangled with or co-crystallized into the LLDPE matrix, whereas the ester linkage anchors to the filler. This structure reduces particle-particle agglomeration and improves stress transfer. The result is a higher tensile elongation at break relative to uncoupled material when tested per ISO 527-1:2019 or ASTM D638-14. In aluminum trihydroxide-filled compounds at loadings around 60 wt%, replacing 2–4 wt% of the matrix with MB528D is a recognized starting point for compound development. Some literature on similar maleated LLDPE coupling agents reports elongation at break increasing from below 10% to above 20% in optimized formulations, but published data for this specific configuration is limited and the magnitude is strongly dependent on filler particle size distribution, filler coating, and screw mixing intensity. At addition levels above 8 wt%, unreacted anhydride can consume stabilizers and may increase moisture uptake in compounded pellets under high-humidity storage. In flame-retardant cable compounds, overdosing can lower volume resistivity because additional polar groups facilitate charge transport; insulation resistance should be measured per IEC 62631-3-1 or ASTM D257-14.
Halogen-free flame-retardant wire and cable compounds frequently use magnesium dihydroxide or aluminum trihydroxide as the primary mineral filler. In a 40:1 L/D co-rotating twin-screw extruder, MB528D is metered at the main throat while filler is side-fed at a downstream barrel to avoid torque spikes and premature filler breakdown. Melt temperatures are maintained between 190°C and 220°C, and vacuum devolatilization removes moisture introduced by the filler. The compound is then tested for single-wire flame propagation according to IEC 60332-1-2, for acid gas evolution according to IEC 60754-2, and for smoke density according to IEC 61034-2. The use of MB528D improves filler wetting but does not replace the need for optimized stabilizer packages and moisture control. Mineral filler should be pre-dried to below 0.05 wt% moisture, measured by ISO 15512:2019, before side feeding; otherwise surface pores and rough cable jackets can develop.
On single-screw extrusion lines, the same filled compound can be processed if a screw with compression ratio between 2.5:1 and 3.5:1 and screen packs of 20/40/20 mesh are used. Single-screw mixing is typically insufficient for filler loadings above 55 wt%, and aggregates larger than 10 µm may remain. A torque increase of more than 15% over the unfilled matrix during scale-up often indicates poor dispersion and should be corrected by increasing screw mixing sections or by splitting the filler feed into two side ports. Melt pressure before the breaker plate should be recorded to detect filtration-related pressure rise.
Unmodified LLDPE offers no reactive site for chemical bonding to mineral surfaces and depends solely on van der Waals forces. Consequently, uncoupled compounds often show lower tensile strength and lower impact resistance at equal filler loading when tested per ISO 527-1:2019 and ISO 180:2019. MB528D introduces anhydride functionality while retaining the low-density backbone, a combination that may provide better low-temperature ductility than maleated HDPE grades and lower water sensitivity than acid-copolymer ionomers. Acid-functionalized polyethylenes such as ethylene acrylic acid copolymers can form reversible ionic associations and may be selected when adhesion to aluminum foil requires a defined acid number; however, their melt processing may be more sensitive to moisture and corrosion of tooling. MB528D is used when a polyethylene-like thermal and mechanical profile is required with reactive coupling performance.
Within the Fusabond MB series, MB528D is identified by its LLDPE carrier and its specific melt-flow-rate and density range. Higher-melt-flow grades may be chosen for high-speed coating or injection molding applications where low pressure drop is critical; lower-melt-flow grades may be selected for blown film coextrusion or extrusion blow molding where melt strength is required. The selection should compare datasheets according to ISO 1133-1:2022 and ISO 1183-1:2019, not solely by maleic anhydride level because carrier resin viscosity determines screw torque, dispersion, and downstream processing behavior.
Glass fiber reinforced polyethylene compounds can also be compatibilized with MB528D when aminosilane-treated fiber is used. Anhydride groups react with the amino functionality of the fiber sizing during high-shear compounding; fiber length retention is improved by feeding chopped glass downstream rather than at the main throat. Flexural modulus and strength can be compared according to ISO 178:2019, and impact resistance by ISO 179-1:2020. In tie-layer evaluations, pressing MB528D films against aluminum foil at 200°C and 1 MPa for 2 min produces measurable adhesion in laboratory T-peel tests per ISO 11339:2022; however, actual coextrusion line adhesion depends on melt temperature, air gap, corona treatment, and metal surface condition. Published data for this specific configuration is limited.
Replacing an internal batch mixer with a co-rotating twin-screw extruder changes residence-time distribution, surface renewal, and specific mechanical energy input. On a 75 mm extruder with 40:1 L/D, a typical barrel setting from feed to die is 180°C, 200°C, 210°C, 220°C, 220°C, 220°C, 220°C. Screw speed is often set between 250 rpm and 400 rpm, producing specific mechanical energy in the range of 0.18–0.26 kWh/kg for a magnesium dihydroxide-filled compound. These values are starting points; they shift with filler surface area, coating level, and kneading block arrangement. If melt temperature exceeds 240°C, the maleated polyethylene can undergo thermal decomposition and generate free maleic anhydride, leading to yellowing and a drop in electrical resistivity. To control this, the temperature profile is adjusted or the screw speed is reduced.
Dispersion quality is monitored by compression-molding thin films and examining transmitted light for agglomerates larger than 10 µm. If agglomerates persist, two or three additional kneading blocks should be placed after the side-feed zone. Vacuum venting at -0.08 MPa to -0.09 MPa is common; a loss of vacuum indicates volatile moisture or decomposition products. After strand or underwater pelletizing, pellets should be cooled below 50°C before bagging to prevent blocking. Blends containing amine-based processing aids should be avoided because amines can react with the anhydride functionality and reduce coupling efficiency or produce insoluble imide species. Stabilizer packages containing hindered phenols and phosphites should be added at formulation-specific concentrations to protect against melt oxidation.
Compounds containing MB528D can be injection molded with barrel profiles from 190°C to 230°C and nozzle temperatures not exceeding 240°C. Mold temperature is typically held between 20°C and 45°C; higher mold temperatures may increase weld-line strength at the expense of cycle time. The linear low-density backbone provides a lower melt temperature and lower density than many maleated HDPE grades, which can reduce clamp force requirements for thin-wall parts. However, screw recovery should be checked because filled compounds based on MB528D have higher viscosity than unfilled LLDPE and may require a decompression setting after plastication to prevent drool.
Sheet extrusion lines running filled MB528D compounds are operated with melt temperatures below 230°C and a polished three-roll stack at 20°C to 40°C. Roll gaps are set to maintain surface contact without imposing excessive orientation. Thermo-oxidative stability should be confirmed by isothermal thermogravimetric analysis under nitrogen at 230°C for 30 min or by retained elongation at break after multiple extrusion passes. At relative humidity above 60%, mineral-filled compounds can pick up surface moisture within 8 h; pre-drying at 80°C for 4 h in a desiccant dryer is recommended before processing. Storage in sealed containers at or below 40°C limits moisture uptake and oxidative degradation. The neat product does not confer food-contact clearance; final articles must be tested under EU 10/2011 and FDA 21 CFR 177.1520. RoHS, REACH, and regional waste-management compliance must be evaluated for the finished compound, not for the neat product alone.