Dupont Crastin Pbt Gf Sk605 Nc010

DuPont Crastin® PBT+GF SK605-NC010

    • Product Name: DuPont Crastin® PBT+GF SK605-NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 273586
    Density 1.53 g/cm³
    Glass Fiber Content 30%
    Color Natural
    Melt Volume Rate 250c 2 16kg 10 cm³/10 min
    Mold Shrinkage Flow 0.3%
    Mold Shrinkage Transverse 1.1%
    Tensile Modulus 9500 MPa
    Tensile Stress At Break 135 MPa
    Tensile Strain At Break 2.5%
    Flexural Modulus 9000 MPa
    Charpy Notched Impact Strength 23c 8 kJ/m²
    Charpy Unnotched Impact Strength 23c 45 kJ/m²
    Hdt 0 45mpa 220 °C
    Hdt 1 8mpa 205 °C
    Melting Temperature 225 °C
    Vicat Softening Temperature 210 °C
    Water Absorption 24h 0.3%

    As an accredited DuPont Crastin® PBT+GF SK605-NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Crastin® PBT+GF SK605-NC010 is packaged in 25 kg moisture-barrier bags, supplied palletized with identification labels.
    Container Loading (20′ FCL) 20′ FCL container loaded with DuPont Crastin® PBT+GF SK605-NC010 in moisture-proof bags on pallets, securely stowed for export shipment.
    Shipping DuPont Crastin® PBT+GF SK605-NC010 is shipped as non-hazardous, moisture-sensitive thermoplastic pellets in sealed 25 kg bags or octabins, palletized and shrink-wrapped. Keep dry, cool, and protected from sunlight, physical damage, open flames, and excessive heat during transport and storage.
    Storage Store DuPont Crastin® PBT+GF SK605-NC010 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep in tightly closed original packaging and prevent exposure to humid air. Avoid contact with strong oxidizers. Use first-in-first-out; if packaging is opened or moisture pickup is suspected, dry the resin according to supplier recommendations before processing.
    Shelf Life DuPont Crastin® PBT+GF SK605-NC010 has a typical shelf life of two years when stored dry in original unopened packaging below 30°C, away from moisture and sunlight.
    Free Quote

    Competitive DuPont Crastin® PBT+GF SK605-NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Crastin® PBT+GF SK605-NC010 is a 30% glass-fiber-reinforced polybutylene terephthalate injection-molding grade supplied in natural color under the NC010 designation. The ISO 1043-1 material designation is PBT-GF30. The grade is based on a medium-viscosity PBT matrix and is positioned between high-flow unreinforced PBT grades and heavily glass-filled PBT formulations where stiffness, dimensional stability, and short-term thermal resistance are required. Data cited below are typical published DuPont values, not specification limits or batch guarantees.

    The density is 1.52 g/cm³ under ISO 1183-1. Tensile modulus per ISO 527-1/-2 is approximately 9,500 MPa, tensile stress at break is approximately 130 MPa, and tensile strain at break is in the range of 2.3% to 2.8%. Flexural modulus per ISO 178 is approximately 8,700 MPa. Notched Charpy impact at 23 °C is approximately 7.0 kJ/m² under ISO 179/1eA. Heat deflection temperature at 1.8 MPa is approximately 205 °C under ISO 75-1/-2. Melt volume-flow rate per ISO 1133-1 at 250 °C and 2.16 kg is approximately 12 cm³/10 min. These values differentiate SK605-NC010 from unreinforced PBT, which typically has tensile modulus below 2,700 MPa and higher notched impact but lower dimensional stability under load.

    PropertyTest methodTypical value
    DensityISO 1183-11.52 g/cm³
    Tensile modulusISO 527-1/-29,500 MPa
    Tensile stress at breakISO 527-1/-2130 MPa
    Tensile strain at breakISO 527-1/-22.3–2.8%
    Flexural modulusISO 1788,700 MPa
    Charpy notched impact, 23 °CISO 179/1eA7.0 kJ/m²
    Heat deflection temperature, 1.8 MPaISO 75-1/-2205 °C
    Melting temperatureISO 11357-1/-3225 °C
    Melt volume-flow rate, 250 °C/2.16 kgISO 1133-112 cm³/10 min
    Molding shrinkage, parallelISO 294-40.2%
    Molding shrinkage, normalISO 294-40.8%

    Does Melt Viscosity Constrain Thin-Wall Filling in SK605-NC010?

    The 12 cm³/10 min melt volume-flow rate under ISO 1133-1 is not alone a sufficient predictor of thin-wall pressure drop because the 30% glass fibers orient and rotate during flow. At wall thickness below 1.2 mm, the pressure required to move the melt front is strongly influenced by fiber concentration, fiber length retention, and gate geometry. Valve-gated hot-runner systems with orifice diameters below 1.5 mm can generate shear heating, causing the melt to exit the gate above the barrel setpoint even when the nozzle setpoint is 250 °C. Published data for this specific configuration is limited, but direct melt-temperature probes at the nozzle are recommended during process validation.

    For thin-wall connector bodies, the practical lower wall thickness is typically 0.8 mm to 1.0 mm when adequate venting and short flow lengths are available. Below 0.8 mm, the risk of short shots and excessive fiber orientation increases sharply. At knit lines, glass fiber orientation parallel to the flow front reduces weld-line strength; the weld factor of 30% glass-filled PBT is lower than that of unfilled PBT. Mold-filling simulations should use fiber orientation tensors rather than isotropic generalized Newtonian viscosity because an isotropic viscosity model can underpredict injection pressure in thin sections. In production tools with more than 8 cavities, cavity-to-cavity filling imbalance is often larger than in unfilled PBT because the glass-fiber mass imposes varying shear history across runner branches. Short-shot mapping is used to balance runner sprues; the imbalance should not be attributed to material lot variation alone.

    Processing Limits, Drying Requirements, and Screw Geometries

    Moisture control is a critical boundary condition. PBT undergoes hydrolytic cleavage at melt temperature when moisture is present. For SK605-NC010, final moisture content should be maintained below 0.04% by weight. A desiccant dryer at 110 °C to 120 °C for 4 h is typical for freshly opened containers. Material exposed to relative humidity above 60% for several hours may require 6 h to 8 h of drying, particularly in humid production environments. The dry-air feed should have a dew point below −30 °C. Inadequate drying first manifests as loss of molecular weight, followed by reduced tensile strength and notched impact before visible splay occurs.

    Barrel temperature programming from rear to nozzle is typically 230 °C, 240 °C, 250 °C, and 250 °C. Melt temperature should not exceed 270 °C; residence time at melt temperature should be kept below 10 min. At temperatures above 270 °C, the polymer can liberate tetrahydrofuran and degrade, causing yellowing, splay, and loss of mechanical strength. A general-purpose three-zone screw with L/D ratio from 18:1 to 22:1 and compression ratio of 2.0:1 to 3.0:1 is suitable. A deep-flight screw or reverse-taper nozzle may require a lower barrel setting because of shear heating.

    Mold temperature should be maintained between 60 °C and 100 °C. The lower end shortens cycle time but increases differential shrinkage; the upper end favors crystallinity and dimensional stability. For parts requiring tight post-mold tolerances, mold temperature should be measured at multiple cavity positions with an infrared pyrometer or thermocouple array. Hold pressure is set by gate-seal study; actual cavity pressure should be measured with piezoelectric sensors rather than inferred from hydraulic pressure.

    In injection molding of large automotive housings, the 0.2% parallel and 0.8% normal mold shrinkage values under ISO 294-4 produce anisotropic post-mold shrinkage. This anisotropy is lower than that of a 45% glass-filled PBT but greater than that of a 20% glass-filled grade. When a part transfers from a mold temperature of 80 °C to ambient 23 °C, differential shrinkage can generate warpage unless gate position and rib design are optimized. Clamp force calculations based on projected area alone are insufficient; the cavity pressure at end of fill in PBT-GF30 is typically higher than in unfilled PBT because glass fiber increases viscosity. Published data for specific clamp force requirements in SK605-NC010 is limited; process validation should use short-shot studies and cavity-pressure sensors.

    Crastin SK605-NC010 Against Other PBT Formulations

    The NC010 suffix denotes a natural, unpigmented formulation. Compared with black or colored grades, the natural color allows self-coloring or masterbatch addition but exhibits lower ultraviolet resistance. Outdoor components should not rely on natural PBT unless UV stabilization is supplied by the final compound or coating. The natural grade also shows different near-infrared transmission than carbon-black-loaded grades because carbon black absorbs near-infrared radiation in laser-welding operations.

    Against an unfilled PBT, the 30% glass-fiber reinforcement raises heat deflection temperature from approximately 50–60 °C to 205 °C at 1.8 MPa under ISO 75-1/-2 and raises tensile modulus from roughly 2,600 MPa to 9,500 MPa. The trade-off is a reduction in notched impact and weld-line strength. Against a 45% glass-filled PBT, SK605-NC010 offers lower tensile modulus and HDT but better flow, lower barrel wear, and generally better weld-line integrity. Against a 20% glass-filled PBT, SK605-NC010 provides higher stiffness and lower isotropic shrinkage tendency, but melt flow is more limited and surface gloss may be lower. The medium-viscosity matrix of SK605-NC010 is best matched to housings with wall sections from 1.5 mm to 4.0 mm; very thin walls may require a high-flow PBT grade, whereas very thick sections may require a higher-glass-content or low-warpage material.

    For powertrain-adjacent underhood housings, the combination of 205 °C HDT at 1.8 MPa and resistance to automotive oils and glycols supports use in sensor brackets, connector shells, and relay bases. However, continuous hot-oil exposure at 150 °C should be assessed with environmental stress-cracking protocols such as ISO 22088-2, because PBT-GF30 can crack under constrained exposure to aggressive engine fluids. In electrical connectors, the comparative tracking index of 350 V under IEC 60112 and volume resistivity of approximately 1 × 1014 Ω·m under IEC 60093 provide adequate insulation for low-voltage applications, but the UL 94 HB rating means the material is not suitable for applications requiring V-0 self-extinguishing performance without an additional flame-retardant system.

    For power tool housings, SK605-NC010 may be selected for motor mounts and gear cases where glass-reinforced PBT offers impact tolerance and thermal resistance under intermittent heating. The material should be considered only after direct comparison with a 30% glass-reinforced polyamide 6/6 in the same geometry, because moisture-conditioned strength retention and chemical exposure differ. Published data for SK605-NC010 and PA66-GF30 in identical component geometries is limited.

    RequirementStandard or regulationTypical status
    Material designationISO 1043-1PBT-GF30
    Flammability classificationUL 94HB at thickness listed on DuPont Yellow Card
    Hazardous substancesRoHS Directive 2011/65/EUConforms as supplied
    SVHC declarationREACH Regulation (EC) No 1907/2006No SVHC above 0.1% w/w as supplied
    Comparative tracking indexIEC 60112350 V