Dupont Crastin Pbt Gf Sk605 Bk851

DuPont Crastin® PBT+GF SK605 BK851

    • Product Name: DuPont Crastin® PBT+GF SK605 BK851
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 478334
    Density 1.53 g/cm³
    Molding Shrinkage Flow 0.2–0.4%
    Molding Shrinkage Transverse 1.0–1.2%
    Tensile Modulus 10000 MPa
    Tensile Stress At Break 140 MPa
    Tensile Strain At Break 2.5%
    Flexural Modulus 9500 MPa
    Charpy Notched Impact Strength 8 kJ/m²
    Charpy Unnotched Impact Strength 60 kJ/m²
    Heat Deflection Temperature 1 8 Mpa 205 °C
    Melting Temperature 225 °C
    Water Absorption 0.4%
    Flammability UL94 HB
    Volume Resistivity >1E15 Ω·cm
    Dielectric Strength 30 kV/mm
    Coefficient Of Thermal Expansion 3E-5 /K

    As an accredited DuPont Crastin® PBT+GF SK605 BK851 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg moisture-resistant bags, DuPont Crastin® PBT+GF SK605 BK851 is supplied as black glass-fiber-reinforced PBT pellets.
    Container Loading (20′ FCL) 20′ FCL container loaded with DuPont Crastin® PBT+GF SK605 BK851 in 25 kg bags on pallets, sealed for shipment.
    Shipping Shipping description: DuPont Crastin® PBT+GF SK605 BK851, glass-fiber-reinforced PBT black pellets; non-hazardous and not regulated for transport. Packed in moisture-barrier bags or octabins. Keep dry, avoid direct sunlight, and store at ambient temperature. No special dangerous-goods documentation required.
    Storage Store DuPont Crastin® PBT+GF SK605 BK851 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers tightly closed, labeled, and protected from damage or contamination. Avoid dust generation and static accumulation. Follow the SDS and local regulations, use oldest stock first, and maintain supplier-recommended storage temperatures. Store only in designated chemical storage areas.
    Shelf Life Shelf life is typically 2 years from date of manufacture when stored unopened in a dry, cool place, protected from moisture and sunlight.
    Free Quote

    Competitive DuPont Crastin® PBT+GF SK605 BK851 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Crastin® PBT+GF SK605 BK851 is a 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding grade classified in ISO 1043 as PBT-GF30 and supplied in a black colour designated by the BK851 suffix. The compound is specified for electrical connectors, sensor housings, relay bobbins, automotive underbonnet brackets and appliance structural parts where dimensional stability at elevated temperature is required. The glass reinforcement raises density to approximately 1.53 g/cm³ when measured to ISO 1183-1 and increases tensile modulus to approximately 10,500 MPa when tested to ISO 527-2/1A. The material exhibits a melting point near 225 °C by differential scanning calorimetry according to ISO 11357-3 and a melt volume-flow rate of approximately 15 cm³/10 min under 250 °C and 5 kg loading using ISO 1133-1:2022. These values are representative rather than contractual minima; grade-specific published data should be confirmed against the current manufacturer technical bulletin because black pigmentation and production lot variation can shift individual results.

    What processing window applies to SK605 BK851 in multi-cavity injection moulding?

    The first processing constraint is moisture control. Polybutylene terephthalate hydrolyses at melt processing temperatures, and glass-filled grades containing 30 wt% fibre exhibit rapid molecular weight loss when moisture exceeds 0.02 wt%. Pre-drying in a desiccant dryer at 120 °C for 4 h is required for material that has been exposed to ambient humidity. Dew point of the drying air should remain below -30 °C. If moisture levels exceed 0.05 wt%, drying time should be extended or vacuum drying at 100 °C applied until the return-air dew point stabilises. In production, surface splay, silver streaks and reduced tensile impact strength near gate regions are commonly observed failure modes when hopper residence time is too short or when saturated material is reintroduced after a weekend shutdown.

    The melt is processed on reciprocating screw injection moulding machines with clamp force typically selected between 3.5 kN/cm² and 6.0 kN/cm² of projected part area. A general-purpose screw with L/D ratio of 20:1 to 22:1 and compression ratio near 2.2:1 is adequate; high-shear mixing sections are not required and can cause additional glass-fibre attrition. Barrel settings from rear to nozzle are commonly 240 °C, 255 °C, 265 °C and 270 °C; actual melt temperature measured by a needle pyrometer should not exceed 270 °C. Screw recovery should be set so that total melt residence time remains below 5 min in the barrel. Back pressure near 0.3–0.7 MPa and screw surface speed below 0.25 m/s limit fibre breakage, which would otherwise reduce tensile modulus and create anisotropic filler distribution. Batch-to-batch variation in glass fibre length can alter MVR by approximately ±2 cm³/10 min; when pack pressure is controlled by machine load cell only, a lot change may require hold-pressure adjustment of 5–10 % to maintain gate seal on multi-cavity connector tools.

    Mould temperature is normally maintained at 80 °C to 100 °C. This range promotes crystallisation and improves heat distortion performance. Mould temperatures below 60 °C shorten cycle time but produce unfinished surfaces, lower crystallinity and larger post-moulding shrinkage gradients; above 110 °C cycle time increases and demoulding may require additional draft or mould release in unstructured cavities. Hot-runner systems should use balanced manifolds with individually controlled drops. When the hot-runner manifold volume is large and total shot weight is small, melt residence time in the manifold can exceed 5 min; pre-purge cycles or a smaller manifold should be used to avoid discoloration and black speck formation.

    Unlike unfilled Crastin PBT grades, SK605 BK851 exchanges ductility for stiffness and lower mould shrinkage. Unfilled PBT typically shows tensile strain at break above 30 % and flexural modulus below 3,000 MPa, whereas the 30 wt% glass-reinforced product displays nominal strain at break near 2.5 % and flexural modulus between 9,000 MPa and 10,500 MPa depending on test orientation. Shrinkage is anisotropic: flow-direction shrinkage is approximately 0.3–0.5 %, while transverse shrinkage is approximately 0.8–1.0 %. This anisotropy creates flatness risk in large parts; unfilled PBT exhibits more isotropic shrinkage around 1.8–2.0 % but lower warpage potential. Compared with mineral-reinforced PBT grades, the glass-filled SK605 BK851 grade generally provides higher tensile strength and notched impact at ambient temperature, but can show higher warpage due to fibre orientation. Compared with higher glass loadings of 40 wt% or 50 wt%, SK605 BK851 retains better surface appearance and lower melt viscosity, although published data for the specific BK851 black variant is limited.

    PropertyTest methodSK605 BK851 typicalUnfilled PBT typical
    DensityISO 1183-11.53 g/cm³1.31 g/cm³
    Tensile modulusISO 527-2/1A10,500 MPa2,600 MPa
    Tensile stress at breakISO 527-2/1A135 MPa55 MPa yield
    Nominal strain at breakISO 527-2/1A2.5 %>30 %
    Flexural modulusISO 1789,200 MPa2,500 MPa
    Notched Izod impact at 23 °CISO 180/1A8.0 kJ/m²4.0 kJ/m²
    Heat deflection temperature at 1.80 MPaISO 75-2/A200 °C60 °C
    Melt volume-flow rate at 250 °C/5 kgISO 1133-1:202215 cm³/10 min18–25 cm³/10 min

    The comparative table should be interpreted as engineering guidance, not as a basis for procurement specification. For critical load-bearing features, the design should use the ISO 527-2 specimen geometry and the actual gate location because glass-fibre orientation can shift tensile modulus by approximately ±15 %.

    Design constraints imposed by fibre orientation and weld lines

    The glass fibres align predominantly along the flow direction during cavity filling. Tensile modulus and strength are therefore higher in the flow direction than in the transverse direction, while transverse shrinkage is higher than flow-direction shrinkage. A flat rectangular housing gated at one end can exhibit concave warpage because flow-direction shrinkage is lower than transverse shrinkage. Gate location should be selected using mould-fill simulation and verified by short-shot studies on the production tool, not by nominal wall thickness alone. If the part requires flatness to 0.10 mm, a single edge gate on a part larger than 150 mm is generally inadequate; multiple gates or a melt-conveying hot-runner gate with sequential valve pins should be used.

    Weld lines in glass-reinforced PBT are inherently weaker because glass fibres do not bridge the weld plane. The retained tensile strength in a weld region is commonly 40–60 % of the parent material strength, and notched impact retention is lower. In connector housings, weld lines should be positioned away from snap-fit arms, latch interfaces and terminal retention features. Sharp corners should be radiused to at least 0.5 mm because the glass-filled grade is notch-sensitive. Chemical exposure to strong alkaline solutions and hot water above 80 °C can attack PBT through hydrolysis; unfilled PBT and PBT copolymers can differ in their resistance, and published data for this specific BK851 black variant under continuous hot-water immersion is limited.

    For electrical and electronic applications, comparative tracking index and dielectric strength are not governed solely by glass content; wall thickness, filler distribution and moisture conditioning shift results. The grade should be evaluated to IEC 60112 and IEC 60243-1 on moulded plaques from the production tool. Surface carbon-black pigmentation in BK851 can alter surface resistivity and UV exposure response compared with natural NC010 grades, but published data for this specific difference is limited.

    If high-humidity storage or hot-runner dwell alters moulding consistency

    The following operational boundaries are imposed by the matrix and filler system. Unopened bags should be kept in a dry area below 40 °C. Opened containers should be re-sealed and returned to a desiccant dryer; exposure at relative humidity above 60 % for more than 1 h can raise surface moisture above 0.02 wt%. Do not blend SK605 BK851 with acetal or PVC in granulate form; cross-contamination produces gas evolution during melt processing. Avoid amine-based mould-release additives or flame-retardant masterbatches that may interact with the PBT ester groups. When regrind is used, it should not exceed 25 wt% of the feed and should be dry and free of fines; higher regrind ratios can reduce tensile elongation and produce black specks in the black surface.

    Compliance areaDesignation or clauseTypical assessment for SK605 BK851
    ISO 1043 classificationISO 1043-1:2011PBT-GF30
    FlammabilityIEC 60695-11-10; UL 94HB at 1.5 mm
    RoHS recastDirective 2011/65/EU Annex IICompliant per supplier declaration
    REACH SVHCRegulation EC 1907/2006 Article 33No SVHC above 0.1 wt% per supplier statement

    For components operating outside these boundaries, grade selection should be re-evaluated against the specific environmental and mechanical load case.

    Top