Dupont Crastin Pbt Gf Hydrolytic Hr5330hf Nc010

DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010

    • Product Name: DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 737408
    Productname DuPont Crastin HR5330HF NC010
    Materialtype PBT, 30% glass fiber reinforced, hydrolytically stabilized, high flow
    Color Natural
    Density 1.53 g/cm³
    Glassfibercontent 30%
    Moldingshrinkageflow 0.3%
    Moldingshrinkagecrossflow 1.0%
    Tensilemodulus 10000 MPa
    Tensilestrengthatbreak 140 MPa
    Elongationatbreak 2.5%
    Charpynotchedimpactstrength23c 9 kJ/m²
    Heatdeflectiontemperature1 8mpa 205 °C
    Meltingtemperature 225 °C
    Processingmethod Injection molding

    As an accredited DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 is supplied in sealed 25 kg moisture-barrier bags, palletized for industrial handling.
    Container Loading (20′ FCL) 20′ FCL container loading for DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010: 25 kg bags, palletized, shrink-wrapped, labeled, and securely stowed for export.
    Shipping DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 is shipped as non-hazardous, moisture-sensitive polymer pellets in sealed moisture-barrier bags, boxes, or octabins. It is not regulated for transport under DOT/IMDG/IATA/ADR. Store dry, avoid direct sunlight, and protect from moisture and contamination.
    Storage Store in a cool, dry, well-ventilated area away from direct sunlight, heat sources, moisture, and strong oxidizers. Keep original packaging tightly closed, undamaged, and protected from humidity and dust. Use first-in, first-out stock rotation. Avoid prolonged storage at elevated temperatures, and maintain dry conditions before processing to limit moisture uptake.
    Shelf Life Store in unopened, dry packaging below 30°C; shelf life is typically 24 months from date of manufacture.
    Free Quote

    Competitive DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    The product DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 is a hydrolysis-stabilized 30 wt% glass-fibre-reinforced polybutylene terephthalate injection-moulding compound supplied in natural colour. Under ISO 1043-1 the short designation is PBT-GF30, and moulded components are marked according to ISO 11469 for recyclate identification. The grade is specified for hot-moisture load cases in automotive under-hood systems, including cooling-circuit connectors, thermostat housings, sensor bodies, electric water-pump impellers, and industrial pump components exposed to water-glycol mixtures. Density is reported as 1.53 g/cm³ by ISO 1183-1, and the high-flow melt rheology differentiates the material from earlier hydrolysis-resistant PBT-GF30 compounds that required elevated fill pressure in thin-wall tooling. The hydrolytic stabilization design retards autocatalytic ester cleavage in hot aqueous and glycol-containing environments; the additive package consumes carboxylic acid end groups generated by initial hydrolysis, reducing the rate of subsequent chain scission. This mechanism is significant because polyester hydrolysis in hot coolant is self-accelerating once acid end groups accumulate. The product is therefore positioned for components in which dimensional stability and residual impact resistance must survive repeated thermal cycling between -40 °C and 120 °C in contact with 50:50 water-glycol fluids.

    What Moisture Management Protocol Prevents Hydrolytic Chain Scission During Melt Processing?

    Hydrolytic degradation during plastication is governed by residual granulate moisture content. Material exposed to ambient relative humidity above 60% for more than 4 h must be pre-dried before melt processing. A desiccant dryer with dew point no higher than -30 °C and drying temperature of 120 °C for 4 h reduces residual moisture below 0.02 wt%, measured by Karl Fischer titration under ISO 15512. Processing at melt temperature 250–270 °C with wet granules accelerates ester hydrolysis and produces measurable loss of notched impact resistance and melt viscosity. The maximum cumulative residence time at melt temperature is 5 min; beyond that limit, thermal oxidation and ester cleavage proceed even in dried material. Hot-runner purgings held near the upper melt limit for more than 5 min should be discarded and not re-introduced into virgin feed. At processing temperatures above 280 °C, volatile aldehyde emissions increase and the hydrolytic stabilization package can be consumed locally in stagnant melt zones. This is particularly relevant in hot-runner manifolds with dead volumes or sharp transitions where shear heating can produce local melt temperatures above the barrel setpoint.

    In thin-wall connector geometries with nominal wall thickness below 0.8 mm, the high-flow formulation reduces filling pressure and permits lower clamp force relative to standard PBT-GF30. The practical benefit appears as shorter fill time in multi-cavity tools; published data for exact pressure reduction is limited because gate geometry and hot-runner balance dominate the result. The recommended melt-temperature window is 250–270 °C, with an upper limit of 280 °C. Mould temperature is held at 80–120 °C to control crystallization and minimize differential post-mould shrinkage. Glass-fibre-filled grades require free-flow non-return valve assemblies and screw L/D ratio of 20:1–25:1 with low-compression screw geometry to limit fibre attrition. Back pressure in the range 0.5–2.0 MPa hydraulic is typical; higher back pressure raises melt temperature and increases the risk of stagnation in poorly purged hot-runner manifolds. Compounding is performed on twin-screw extruders with downstream glass feeding to preserve fibre length; excessive screw speed or reverse kneading blocks reduce fibre aspect ratio and depress notched impact values. Incoming lots should be verified by melt volume-flow rate testing because lot-to-lot variation in high-flow PBT grades can shift fill behaviour in pressure-limited tools.

    Processing variableSetpoint or limitMeasurement basis
    Melt temperature250–270 °CMelt thermocouple
    Upper melt limit280 °CMelt thermocouple
    Mould temperature80–120 °CWater circuit surface
    Drying temperature120 °CDesiccant dryer
    Drying time4 hDry-air hopper
    Residual moisture<0.02 wt%ISO 15512
    Back pressure0.5–2.0 MPaHydraulic pressure
    Maximum residence time5 minBarrel capacity utilization
    Screw L/D20:1–25:1General-purpose glass-fibre screw

    Mechanical and Thermal Property Matrix Under ISO 527 and ISO 75

    Representative injection-moulded values from supplier documentation are listed below. These values are single-point laboratory data and are not batch release limits. Tensile and flexural values measured parallel to the main flow direction exceed those measured perpendicular to flow because of glass-fibre orientation. Shrinkage is correspondingly differential, with mould shrinkage in the flow direction typically 0.2–0.4% and cross-flow shrinkage higher. Post-mould crystallinity can be increased by mould temperature at the upper end of the recommended range, raising heat distortion temperature and reducing creep under sustained load. For comparison, absolute values obtained using ASTM D638 Type I specimens may differ from ISO 527-1/-2 results due to specimen geometry and conditioning history.

    PropertyRepresentative valueTest method
    Density1.53 g/cm³ISO 1183-1
    Melt volume-flow rate25–35 cm³/10 min at 250 °C, 2.16 kgISO 1133-1
    Tensile strength at break130 MPaISO 527-1/-2
    Tensile modulus10000 MPaISO 527-1/-2
    Elongation at break2.5%ISO 527-1/-2
    Flexural strength190 MPaISO 178
    Flexural modulus9500 MPaISO 178
    Charpy notched impact8 kJ/m² at 23 °CISO 179-1/1eA
    Charpy unnotched impact45 kJ/m² at 23 °CISO 179-1/1eU
    Melting point225 °CISO 11357-1/-3
    Heat deflection temperature200 °C at 1.8 MPaISO 75-1/-2
    Mould shrinkage parallel0.2–0.4%ISO 294-4

    The combination of 10000 MPa tensile modulus and 200 °C heat deflection temperature makes the material suitable for short-term exposure to under-hood peak temperatures. However, continuous operating temperature is lower and depends on the specific coolant chemistry, mechanical stress state, and wall thickness. No single heat-deflection value should be used as a substitute for long-term heat-aging data under UL 746B relative thermal index classification or application-specific environmental cycling.

    Among glass-reinforced PBT grades used in automotive cooling circuits, the hydrolytic stabilization package in DuPont Crastin® PBT+GF-Hydrolytic HR5330HF-NC010 changes the dominant failure mode in long-term coolant exposure from progressive surface embrittlement to fatigue crack initiation at weld lines and stress raisers. General-purpose PBT-GF30 without hydrolytic stabilization can undergo autocatalytic ester hydrolysis in hot aqueous environments; the released carboxylic acid end groups lower molecular weight and produce a rapid loss of elongation at break. The stabilized grade is formulated to consume acid end groups, slowing the decay of tensile strength and impact resistance. The high-flow character is obtained without external lubricant or plasticizer addition; the flow modification is integrated into the polymer molecular-weight distribution. This distinguishes the product from internally lubricated PBT compounds that can show surface exudation, reduced weld strength, or contamination of downstream potting and adhesive bonding processes. The principal difference from standard hydrolysis-resistant PBT-GF30 is the melt-flow rate. The high-flow variant permits multicavity tooling with lower fill pressure, but it may also display slightly reduced weld-line strength in thick sections because the lower melt viscosity can promote more pronounced glass-fibre orientation at knit lines. Published data for specific weld-line strength reduction in this grade is limited; design validation should include notched impact and tensile tests on weld-line specimens under ISO 527-1/-2 and ISO 179-1/1eA after hot-water-glycol conditioning.

    For applications that previously used standard PBT-GF30 with lower melt flow, the high-flow grade can reduce injection pressure but may require rebalancing of hot-runner gates and revised clamp-force calculations. In multi-cavity tools with more than eight cavities, the lower viscosity can shift cavity filling sequence and produce inconsistent packing. Tool trials should include short-shot progression at 90%, 95%, and 100% fill to verify that the fill pattern remains stable with batch-to-batch melt-flow variation. If short shots reveal unstable flow fronts, cavity-specific flow-control valves may be necessary, particularly when wall thickness drops below 0.6 mm in connector terminal areas.

    When Hot-Water Immersion Produces Property Cliff-Edges at Weld Lines

    In electric water-pump housings and thermostat covers, knit lines occur where separate melt fronts meet behind cores or around valve gates. Glass fibres at the knit line orient perpendicular to the flow direction; local tensile strength is dominated by the matrix rather than the fibre reinforcement. Weld-line tensile strength in short-glass PBT is commonly 60–75% of the un-welded bulk strength, though grade-specific values depend on fibre content, glass-sizing chemistry, and mould temperature. Hydrolytic aging concentrates first at the exposed glass-fibre interface and at knit lines, producing a cliff-edge loss of elongation before bulk embrittlement appears. In this product, the hydrolytic stabilization package extends the time to onset of knit-line failure but does not eliminate the geometric weakness. Tool designs should place knit lines in low-tensile regions; when this is not possible, validation must include aged weld-line specimens at 85 °C in 50:50 water-glycol or under USCAR-2 environmental cycling. The boundary of safe design is also affected by glass-fibre length distribution; the shortest fibres in the distribution, typically below 0.2 mm after plastication, provide limited load transfer across the knit line and can initiate premature environmental stress cracking. Parts requiring sustained pressure containment should avoid knit lines in hoop-stress regions, especially in cylindrical water-pump housings where internal pressure can exceed 2 bar during start-up transients.

    For EU and North American automotive applications, the compound is typically covered by supplier raw-material compliance documentation for REACH Regulation (EC) No 1907/2006 and RoHS Directive 2011/65/EU Annex II; the specific declaration should be obtained for the production batch because additive suppliers can vary. Flammability data are supplied through the UL Yellow Card; the material is commonly rated HB at 0.75 mm, and thickness-dependent classification must be verified before use in electrical enclosures. Long-term heat-aging classification may be reported under UL 746B relative thermal index, but the value depends on the specific thickness and mechanical property being evaluated. The product is not intended for continuous superheated steam service above 130 °C; the hydrolytic stabilization package has finite acid-scavenging capacity, and prolonged exposure to amines or strong alkaline solutions can overwhelm the stabilization mechanism. Blends with aliphatic amine heat stabilizers, certain flame-retardant synergists, or basic fillers should be avoided because amine-catalyzed ester hydrolysis can offset the hydrolysis-resistant formulation. Storage should be in sealed containers at 20–25 °C, and material exposed to relative humidity above 60% for more than 4 h must be re-dried before processing. In applications where coolant composition includes aggressive organic acids or borate corrosion inhibitors, component validation should include full coolant immersion with dynamic temperature cycling rather than isolated tensile or impact testing, because chemical interaction with the glass-sizing layer can initiate interfacial degradation that is not captured by single-point property measurements.

    Top