| HS Code | 133918 |
| Density | 1.53 g/cm3 |
| Glass Fiber Content | 30 % |
| Tensile Modulus | 9500 MPa |
| Tensile Stress At Break | 135 MPa |
| Strain At Break | 2.5 % |
| Charpy Notched Impact Strength | 8 kJ/m2 |
| Hdt At 1 8 Mpa | 200 °C |
| Hdt At 0 45 Mpa | 220 °C |
| Melting Temperature | 225 °C |
| Vicat Softening Temperature | 210 °C |
| Molding Shrinkage Flow | 0.3 % |
| Molding Shrinkage Cross Flow | 0.9 % |
| Water Absorption Saturation | 0.4 % |
| Volume Resistivity | >1E14 ohm·cm |
| Dielectric Strength | 30 kV/mm |
| Flammability Rating | HB |
As an accredited DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 is supplied in 25 kg moisture-resistant bags, palletized, stretch-wrapped, and labeled for safe storage and transport. |
| Container Loading (20′ FCL) | Standard 20′ FCL dry container loaded with DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503, palletized, secured, sealed, and ready for export shipment. |
| Shipping | DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 is shipped as pelletized black thermoplastic resin in moisture-barrier bags or liners, palletized and secured for transport. Keep dry and avoid heat or moisture exposure. It is typically not regulated as dangerous goods; verify the current SDS and local regulations before shipment. |
| Storage | Store DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 in a cool, dry, well-ventilated area in original sealed containers. Protect from moisture, humidity, direct sunlight, heat sources, flames, and oxidizing materials. Keep containers closed, prevent dust generation, and avoid prolonged storage above recommended temperatures. Store away from food, drink, and animal feed. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is two years from manufacture when stored dry in original unopened packaging below 30°C, protected from sunlight. |
Competitive DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont Crastin® PBT+GF-Hydrolytic HR5330HF BK503 is a 30% glass-fibre-reinforced, hydrolysis-stabilised polybutylene terephthalate injection-moulding compound supplied as black pellets. The material conforms to the ISO 1043 designatory structure PBT-GF30 HR and is differentiated from non-hydrolysis-stabilised GF30 PBT grades by a stabiliser system intended to retard ester-chain scission during hot-water or water-glycol exposure. Selected dry-as-moulded datasheet values are presented in the specification matrix below; these are typical values, not batch-release specifications, and should be confirmed against the current supplier certificate of analysis for production validation.
| Property | Test method | Typical value |
|---|---|---|
| Density | ISO 1183-1 | 1.53 g/cm³ |
| Tensile stress at break | ISO 527-1/-2 | 135 MPa |
| Tensile modulus | ISO 527-1/-2 | 10,500 MPa |
| Tensile strain at break | ISO 527-1/-2 | 2.6% |
| Flexural modulus | ISO 178 | 9,800 MPa |
| Charpy notched impact strength, 23 °C | ISO 179/1eA | 9.0 kJ/m² |
| Charpy notched impact strength, -30 °C | ISO 179/1eA | 7.0 kJ/m² |
| Melt volume-flow rate, 250 °C/2.16 kg | ISO 1133-1 | 25 cm³/10 min |
| Melting temperature | ISO 11357-1/-3 | 225 °C |
| Deflection temperature under load, 1.8 MPa | ISO 75-1/-2 | 205 °C |
| Comparative tracking index | IEC 60112 | 275 V |
| Dielectric strength | IEC 60243-1 | 32 kV/mm |
| Volume resistivity | IEC 62631-3-1 | 1 × 1015 ohm·cm |
| Flammability classification | UL 94 | HB |
The 30% glass-fibre reinforcement reduces the coefficient of linear thermal expansion relative to unfilled PBT and raises tensile modulus to a level suitable for rigid housings and connector bodies. The high-flow designation is expressed in the melt volume-flow rate of 25 cm³/10 min to ISO 1133-1, which permits filling of thin-wall geometries with lower injection-pressure demand than standard-flow hydrolysis-stabilised GF30 PBT grades. Because the material is a semi-crystalline thermoplastic, the final crystallinity, shrinkage, and hydrolysis resistance are strongly influenced by mould temperature and cooling rate, not merely by barrel set-point.
Hydrolytic degradation of PBT proceeds through cleavage of ester linkages along the terephthalate backbone. The carboxylic acid end-groups released during chain scission catalyse further hydrolysis, producing autocatalytic molecular-weight loss, embrittlement, and a corresponding decline in tensile stress at break. In an unstabilised 30% glass-filled PBT, this degradation is accelerated along the fibre-matrix interface because coolant or condensed water can wick along glass fibres and attack the sizing and surrounding polymer. The HR5330HF BK503 grade is formulated with a hydrolysis-stabiliser package and is intended to delay this autocatalytic sequence in intermittent hot-water and water-glycol service. Published multi-lot data for the exact retention of tensile properties after 1,000 h in 50:50 water/ethylene glycol at 125 °C is limited from public sources; therefore application-specific validation should be performed by tensile testing to ISO 527-1/-2 after fluid immersion under the intended service temperature. Industrial comparative screening of hydrolysis-stabilised and unstabilised GF30 PBT compounds under similar coolant-ageing conditions frequently shows the HR grades retaining above 80% of original tensile strength while non-HR grades fall below 50%, but this is grade-dependent and cannot be assumed without confirming the specific batch formulation and ageing medium.
The stabiliser package does not eliminate hydrolysis. It reduces the concentration of active acid end-groups and slows chain scission until the stabiliser is consumed or extracted. At continuous coolant temperatures above 135 °C, in strong alkaline media above pH 12, or under saturated steam above 150 °C, the hydrolytic attack becomes severe enough to embrittle the material even with HR stabilization. The grade is therefore positioned for underhood components with intermittent or moderate coolant exposure, not for continuous high-pressure steam environments.
Prior to melt processing, the pellet moisture concentration should be reduced to 0.02 wt% or lower by Karl Fischer titration to ISO 15512. The material is normally dried at 120 °C for 4 h in a dehumidifying dryer with a dew point of -40 °C or lower. Insufficient drying is a production-scale failure mode because residual moisture hydrolyses the melt during residence time in the barrel, producing splay, gas burn marks, viscosity drift, and reduced weld-line strength. Pellets exposed to ambient air above 60% relative humidity for more than 30 min should be re-dried before moulding. Injection-moulding machines with 25:1 L/D general-purpose PBT screws are adequate for this grade. Melt temperature should be held between 250 °C and 260 °C, and total residence time at melt temperature should not exceed 8 min. Extended residence time in hot-runner drops or oversized barrels can produce black specks and surface delamination at the gate. A back pressure of 0.3 MPa to 0.5 MPa is typical for dosing consistency without excessive fibre attrition.
The high-flow melt behaviour reduces injection-pressure demand in thin-wall tooling, but shear sensitivity remains. Filling velocities above approximately 500 m/s at the gate can cause glass-fibre breakage and local weld-line tensile-strength loss greater than 20% relative to the nominal bulk value. Gate diameters below 0.8 mm are not recommended for structural bosses or snap-fit features because fibre-packed weld lines may crack under insertion repeated load. Hot-runner systems should be free of dead spots and should maintain uniform melt-channel diameters; stagnation zones permit hydrolytic degradation to initiate from a single overheated shot and then propagate as intermittent defects in downstream parts.
PBT crystallises rapidly from the melt, but quench cooling against a cold mould surface produces an amorphous or low-crystallinity skin. In sections below 1.5 mm, mould temperatures below 80 °C can suppress the formation of the crystalline phase at the surface and reduce the effective deflection temperature under load, even if the core remains semi-crystalline. The result is post-mould shrinkage, warpage after thermal exposure, and reduced hydrolytic stability because amorphous PBT regions are more susceptible to moisture ingress and chain scission. A mould temperature of 100 °C to 120 °C is recommended for this grade when dimensional stability is required after hot-fluid exposure. The higher mould temperature increases cooling time but improves part flatness and retention of snap-fit engagement force. Shrinkage compensation for the tool cut should be established by moulding plaques or representative parts and measuring to ISO 294-4, because the effective shrinkage depends on wall thickness, gate location, glass-fibre orientation, and mould temperature. Typical mould shrinkage for the grade is approximately 0.3% in the flow direction and 1.0% transverse to flow, but these values are geometry-dependent and not acceptable as tool design constants without validation.
In underhood electrical-connector carriers and sensor housings exposed to 50:50 water-glycol coolant at temperatures up to 120 °C, HR5330HF BK503 is selected over standard GF30 PBT where terminal retention force, dimensional stability, and resistance to coolant-induced embrittlement are required after 1,000 h of ageing. The coefficient of linear thermal expansion parallel to flow is approximately 2.5 × 10−5 K−1 and transverse to flow is approximately 9.0 × 10−5 K−1 when measured to ISO 11359-2. These anisotropic values must be accommodated in connector pitch and terminal alignment tolerances. The published comparative tracking index of 275 V to IEC 60112 is suitable for many low-voltage connector applications, but creepage and clearance requirements in final equipment depend on pollution degree, overvoltage category, and enclosure design under IEC 60664-1.
The grade is not a direct substitute for flame-retardant Crastin PBT grades where UL 94 V-0 classification is required. HR5330HF BK503 is classified UL 94 HB and will propagate flame unless protected by enclosure geometry or adjacent flame barriers. Processing equipment should be purged of polycarbonate, PVC, acetal, or flame-retardant halogenated compounds before moulding, because residual acidic or halogenated degradation products accelerate PBT hydrolysis and can reduce molecular weight during barrel residence. Amine-based heat stabilisers, certain silane additives, and strongly alkaline mould-release agents are incompatible with the polymer backbone and should be avoided unless validated by melt-viscosity stability studies. For applications involving continuous steam, chlorinated solvents, strong acids, or strong alkaline cleaning media, the material should be qualified by environmental stress-cracking or mechanical property retention tests appropriate to the specific fluid mixture before production release.