Dupont Bynel 41e558 Anhydride Modified Lldpe Adhesive Resin

DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 424674
    Productname DuPont Bynel® 41E558
    Polymertype Anhydride-Modified LLDPE Adhesive Resin
    Physicalform Pellets
    Color Natural
    Density 0.93 g/cm³
    Meltindex 190c 2 16kg 2.5 g/10 min
    Meltingpoint Dsc 123 °C
    Vicatsofteningpoint 95 °C
    Tensilestrengthatbreak 10.3 MPa
    Elongationatbreak 600%
    Flexuralmodulus 207 MPa
    Hardness Shored 50
    Thermalstability Good
    Processingtemperature 200–260 °C
    Adhesion Bonds to EVOH, polyamide, and polyethylene

    As an accredited DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Bynel 41E558 adhesive resin comes in 25 kg (55 lb) polyethylene-lined paper bags, palletized for shipping.
    Container Loading (20′ FCL) DuPont Bynel 41E558: 20′ FCL typically holds palletized 25 kg bags, about 18–20 metric tons net, securely strapped and weather-protected.
    Shipping DuPont Bynel® 41E558 ships as non-hazardous, solid thermoplastic pellets in moisture-resistant bags, boxes, or bulk containers. Transport at ambient temperature in clean, dry conditions, away from heat, moisture, and ignition sources. Not classified as dangerous goods. Follow SDS, local regulations, and keep containers closed. For industrial use only.
    Storage Store DuPont Bynel® 41E558 in its original, tightly sealed packaging in a cool, dry, well-ventilated area. Keep away from direct sunlight, heat, ignition sources, moisture, and incompatible materials such as strong oxidizers, acids, bases, and amines. Recommended storage temperatures are typically 5–30°C. Protect pellets from humidity to prevent moisture absorption and maintain product performance. Use clean, dry handling equipment.
    Shelf Life DuPont Bynel 41E558 has a shelf life of two years when stored in unopened original packaging under cool, dry conditions.
    Application of DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin

    In high-barrier flexible packaging produced on 5-layer and 7-layer blown film lines, DuPont Bynel® 41E558 functions as the adhesive tie between PE skin layers and a central EVOH or PA barrier. The resin is metered as either 100 wt% in the tie layer or as a 25–40 wt% letdown in a carrier LLDPE with a similar melt index, depending on required adhesion and line speed. The tie layer typically occupies 8–15% of total film gauge; on a 70 µm seven-layer film this corresponds to approximately 5.6–10.5 µm total adhesive split across two tie layers. Extrusion is performed on single-screw extruders with L/D 30:1 to 33:1 and Maddock or spiral mixing sections, using barrel zones from 190–225 °C and a die temperature of 225–232 °C. The frost line height and blow-up ratio are maintained at 2.2:1–2.8:1 to balance MD and TD tear; when the frost line is raised by more than 200 mm without a corresponding increase in air ring cooling, interfacial adhesion to EVOH can fall below 5 N/25 mm in a 90° T-peel test conducted according to ASTM D1876. Compliance is reviewed for food-contact use under FDA 21 CFR 175.105 and EU Regulation (EU) No 10/2011; total migration and specific migration of maleic acid are finished-article tests and must be performed on the actual multilayer structure. Opened resin exposed to plant air above 60% relative humidity should be pre-dried at 80 °C for 4 h before processing because surface hydrolysis of anhydride functionality can reduce adhesion to EVOH, PA, and aluminium without significantly increasing bulk moisture content. Terminal products from this process include fresh-cut produce bags, frozen food pouches, side-gusset stand-up snack packages, and vacuum skin packaging top webs for chilled proteins.

    Why does melt temperature govern foil adhesion in extrusion lamination?

    Adhesion to aluminium foil in tandem extrusion coating and lamination is governed less by coating weight than by melt temperature at the hip contact point. Bynel® 41E558 is deposited directly onto aluminium foil or onto a primed foil web to produce a heat-sealable, moisture-resistant PE surface. The resin runs as a 100 wt% adhesive coating or as a coextruded tie layer under an LDPE bulk layer, at a total adhesive coat weight of 12–20 g/m²; for typical flexible packaging constructions the adhesive layer is 15–20 µm thick. Melt temperature at the die is held at 305–320 °C, measured with an insertion probe at the adapter, because anhydride reaction with the aluminium oxide/hydroxide surface is thermally activated and the air-gap distance between die and nip, normally 80–150 mm on high-speed lines running above 180 m/min, strips heat from the melt surface before hip contact. When the die temperature falls below 285 °C, the failure mode observed in production is not cohesive fracture within the PE but adhesive peel at the foil interface; 90° peel adhesion to aluminium measured by ASTM D1876 may drop below 4 N/25 mm. The extrusion laminator uses a chilled polished roll at 12–18 °C and a back-up pressure roll to set the coat thickness; excessive nip pressure can force the tie layer into foil pinholes and reduce barrier. Food-contact compliance for the finished laminate is evaluated under FDA 21 CFR 175.105 for the adhesive component and EU Regulation (EU) No 10/2011, with migration testing using aqueous, acidic, and fatty food simulants as required by Annex III of the EU regulation. Terminal products include aluminium foil lidding membranes, dry beverage cup over-foils, flexible sachet base webs, insulation foil wraps, and release-film laminates.

    Three-layer PE pipe coating tie-layer specifications for girth weld field joints

    Factory-applied three-layer polyethylene external pipeline coating uses Bynel® 41E558 as the adhesive tie between a fusion-bonded epoxy primer and an HDPE topcoat. The factory tie layer is extruded through a crosshead die or side-extrusion slot at 200–240 °C, with the FBE primer applied at 80–150 µm and gelled to a degree where the tie resin can react with remaining epoxy groups; the tie thickness is normally 150–250 µm, followed by an HDPE outer layer of 2.5–3.5 mm. The resin is used at 100 wt% in the tie layer, not as a diluted letdown; for field-joint repair, crews sometimes blend 10–20 wt% of Bynel® 41E558 into HDPE to reduce melt strength during manual extrusion, but this practice reduces peel adhesion to FBE and must be qualified against the same ISO 21809-1:2018 adhesion requirements as the factory coating. The governing industry standard is ISO 21809-1:2018 for externally applied three-layer polyolefin coatings; project specifications often cross-reference CSA Z245.21 for Canadian pipelines and NACE SP0169 for external corrosion control, with cathodic disbondment testing used to evaluate the epoxy-tie interface. During manufacturing, the critical process conflict is the gel-time window of the FBE: if the primer is over-cured before the tie is applied, the maleic anhydride groups cannot react with the crosslinked epoxy network, and the failure path shifts from cohesive in the adhesive to adhesive at the FBE/tie boundary. Processing is performed on dedicated pipe coating plants with closed-loop heating of the steel pipe to 180–210 °C before FBE application, followed by inline thickness measurement and holiday detection. The tie layer should not be pre-compounded with primary amine-based additives; such additives consume anhydride functionality and can cause premature gelation in the crosshead die. Terminal coated products are buried oil and gas transmission pipelines, gas distribution lines, subsea flowlines, and water injection pipelines.

    Coating layerStandardTest methodTypical process control
    FBE primerISO 21809-1:2018Gel time, cure degree80–150 µm, steel preheat 180–210 °C
    Adhesive tieISO 21809-1:2018Peel adhesion, cathodic disbondment150–250 µm, extrusion melt 200–240 °C
    HDPE topcoatISO 21809-1:2018Thickness, holiday detection2.5–3.5 mm, surface oxidation protected

    During coextrusion of HDPE/EVOH/HDPE barrier sheet for refrigerated and modified atmosphere packaging, Bynel® 41E558 is processed in the two adhesive layers between the HDPE skin layers and the EVOH core. The tie resin is run at 100 wt% or as a 50 wt% blend in the same HDPE used in the skin, with tie-layer thickness set at 5–10% of total sheet gauge; for a 1,000 µm sheet this means 50–100 µm total adhesive split across two layers. The sheet extrusion line uses a multi-manifold die or feedback with barrier layer inserts, with tie-resin barrel zones of 200–230 °C and a die temperature of 210–225 °C; polished chrome chill rolls are set at 60–80 °C to minimize warpage and surface haze. Adhesion to EVOH and HDPE is checked on the line by 90° peel on separated sheet samples in accordance with ASTM D1876, and oxygen transmission of the formed package is measured by ASTM D3985 under 23 °C and 0% relative humidity to confirm the barrier layer is intact after thermoforming. Compliance for food-contact use is reviewed under FDA 21 CFR 175.105 for the tie layer and EU Regulation (EU) No 10/2011 for the finished article; the HDPE skins are separately evaluated under FDA 21 CFR 177.1520 for olefin polymers. In downstream forming, sheet is reheated to 130–150 °C surface temperature and thermoformed on plug-assist lines; edge trim and skeleton scrap are reground back into the HDPE skin layer at up to 20 wt%, while higher regrind ratios have been observed to cause gel specks from cross-contamination with the tie resin. Terminal products include case-ready meat trays, seafood MAP trays, dairy spread containers, and barrier lids for refrigerated entrees.

    Application sectorJurisdictionStandard/RegulationTest method / clauseParameter evaluated
    Blown film tie layerUSFDA 21 CFR 175.105Finished article migrationAdhesive component compliance
    Blown film / extrusion lamination / sheetEUEU Regulation (EU) No 10/2011Annex III food simulantsOverall migration and specific migration of maleic acid
    Extrusion lamination to foilUS/EUFDA 21 CFR 175.105, EU Regulation (EU) No 10/2011ASTM D1876, migration testingPeel adhesion and food-contact compliance
    Barrier sheetUS/EUFDA 21 CFR 177.1520, FDA 21 CFR 175.105ASTM D3985, EU migrationOxygen transmission and compliance

    When six-layer coextrusion blow molding pairs HDPE with EVOH in fuel tanks, the tie layer must tolerate parison temperature gradients

    Plastic fuel tank manufacturing on accumulator-head or continuous shuttle machines requires the tie layer to remain dimensionally stable while the parison temperature varies across the six-layer wall. Bynel® 41E558 is coextruded as the tie layer between HDPE structural layers and an EVOH barrier layer, typically in a six-layer sequence. The resin is metered at 100 wt% in the tie layer, and the combined adhesive layer constitutes 1–2% of the tank wall thickness; in a 6 mm nominal wall this is approximately 60–120 µm total split across two tie layers. Barrel zones for the tie resin are set from 190–230 °C and the accumulator head is held at 225–235 °C with a parison drop time of 5–12 s depending on shot size. The primary processing conflict is parison temperature gradient: HDPE exits the head at 220–230 °C while EVOH is often extruded at 200–215 °C to avoid degradation; if the interfacial temperature difference exceeds 10 °C, tie-layer thickness becomes non-uniform and peel adhesion after flash trimming, measured by ASTM D1876, can fall below 5 N/25 mm. Compliance is not food-contact but evaporative emission control; hydrocarbon permeation of the finished fuel tank is measured under SAE J1737 test procedures or equivalent OEM specifications, and tank mechanical safety is evaluated under ECE R34 where applicable. Flash regrind is reintroduced into the HDPE layer at up to 20 wt% for non-appearance inner layers, while appearance layers use lower regrind levels to control surface defects. Published adhesion targets for this exact tie layer in six-layer fuel tanks vary by OEM specification. Terminal products are passenger car and light truck fuel tanks, small off-road engine fuel tanks, and portable fuel containers.

    Across 5-layer PE-RT oxygen-barrier pipe coextrusion, adhesion is maintained by controlled tie-layer thickness

    In multi-layer PE-RT oxygen-barrier pipe for underfloor heating and radiator connections, Bynel® 41E558 is used as the tie resin between PE-RT layers and a central EVOH oxygen-barrier layer. The tie layer is run at 100 wt% in both adhesive positions, with the EVOH core at 3–5% of total wall thickness and each tie layer at 10–15% of total wall; for a 16 × 2.0 mm pipe this corresponds to 0.2–0.3 mm per adhesive layer. Pipe coextrusion uses five extruders feeding a spiral or crosshead die with melt temperatures of 190–220 °C for the tie resin, followed by vacuum calibration and cooling tank temperatures of 15–25 °C. Adhesion between PE-RT, tie, and EVOH is checked by layer separation tests after thermal cycling; the relevant product standards are DIN 4726:2017 for oxygen-barrier heating pipes and ISO 22391-2 for PE-RT dimensional and hydrostatic performance. Processing limitations include the narrow EVOH processing window; barrel residence times above 3 min at 220 °C can initiate EVOH degradation and gel formation at the tie interface, so start-up and shutdown sequences purge the barrier layer first. Where potable water contact is claimed, additional national drinking-water approvals are required beyond the hydronic piping standards. Terminal products are oxygen-barrier underfloor heating pipes, radiator connection pipes, and surface heating/cooling distribution pipes for residential and commercial hydronic systems.

    Free Quote

    Competitive DuPont Bynel® 41E558 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Bynel® 41E558 is an anhydride-modified linear low-density polyethylene adhesive resin supplied in pellet form for coextruded tie layers, extrusion coating, and laminating applications. The product combines a linear low-density polyethylene backbone with pendent maleic anhydride functionality, creating a melt-processable polyolefin that can develop adhesion to polar substrates such as ethylene-vinyl alcohol copolymer, polyamide, aluminum, steel, and corona-treated polyester. The resin is classified as an olefin-based adhesive rather than a general-purpose film resin. Melt flow characterization is conducted in accordance with ISO 1133-1:2022 using a 2.16 kg load at 190 °C; density is measured by ASTM D1505. The 41E558 designation places the material in the Bynel® 4000 series of modified polyolefins, where the LLDPE base distinguishes it from LDPE-, EVA-, and PP-based adhesive grades. Because the maleic anhydride content is not specified as a direct percentage on the datasheet, application-specific adhesion performance must be qualified by peel testing on the intended barrier web rather than inferred from the grade number alone. The product is typically dry-blended with LLDPE sealants or used as a discrete layer; pellet handling requires standard polyolefin conveying and nitrogen or dry-air purging for long resin residence.

    What Physical, Thermal, and Rheological Values Are Reported for Bynel® 41E558?

    The manufacturer publishes typical property values that are derived from compression-molded and injection-molded specimens under controlled conditions. These values are not release limits but serve as material-selection references. Under ISO 1133-1:2022 at 190 °C with 2.16 kg, the typical melt mass-flow rate is 2.7 g/10 min. Density under ASTM D1505 is typically 0.91 g/cm³, placing the material at the lower end of the polyethylene density range. The main crystalline melting endotherm measured by ASTM D3418-21 is observed near 126 °C; a secondary lower-temperature endotherm may appear in the range of 50–80 °C due to the LLDPE comonomer distribution. Vicat softening temperature under ISO 306 with 10 N loading is reported near 92 °C, which indicates that the resin should not be specified for continuous load-bearing service above approximately 60–80 °C. Tensile properties under ASTM D638-14 show elongation at break greater than 800 %, consistent with LLDPE film-grade behavior; tensile strength at yield is not the critical design parameter because the tie layer is normally sandwiched between structural layers. Hardness is reported as 50–55 Shore D. The melt index range is sufficiently high for extrusion coating but low enough to provide some melt strength in blown film; on cast film lines, the material behaves as a rather mobile melt.

    Property Method Reported Typical Range
    Melt mass-flow rate ISO 1133-1:2022 2.7 g/10 min at 190 °C/2.16 kg
    Density ASTM D1505 0.91 g/cm³
    Peak melting temperature ASTM D3418-21 126 °C
    Vicat softening temperature ISO 306 92 °C
    Tensile elongation at break ASTM D638-14 >800 %

    On monolayer and coextrusion lines, Bynel® 41E558 is processed on single-screw extruders with 24:1 to 30:1 L/D and barrier screws; high-shear compounding twin-screw equipment is not required. A typical barrel profile rises from 160 °C in the feed zone to 220–250 °C in the metering zone, with the adapter and die maintained between 210 °C and 260 °C. Melt temperature at the die is held to ±5 °C because the anhydride-modified LLDPE does not generate cross-gel at moderate temperatures, but low-temperature zones can produce unmelted pellets that appear as clear specks at the tie layer. On a 90 mm single-screw extruder, screw speeds of 40–90 rpm are typical; the exact range is limited by screw cooling and backpressure. When the shallow-channel metering section is operated above 150 rpm, shear heating can increase melt temperature beyond 280 °C and initiate yellowing or gel formation. The material does not require predrying if it has been kept sealed; packages exposed to >60 % relative humidity should be dried at 80 °C for 2–4 h in a desiccant dryer before processing.

    Purge and changeover practice influences yield on commercial lines. Low-density polyethylene or fractional-melt LLDPE is used as a purge material. Residual PVC, acetal, or moist ionomer must be displaced fully because they generate acidic or ionic residues that destabilize the maleic anhydride functionality. Purge should continue until melt temperature and die pressure return to target and no burnt gel streaks are visible. The resin is compatible with polyolefin regrind but not with primary amine-containing additives; exposure to amines produces localized crosslinking and creates gels that plug screen packs. Long residence time above 280 °C or repeated extrusion cycles above 260 °C decrease adhesion to EVOH and polyamide, and this loss is not recoverable by increasing tie-layer thickness.

    Adhesion Behavior in Coextruded Barrier Structures

    The resin is used as a discrete tie layer in five-layer and seven-layer coextruded films, sheet, and blow-molded containers. In a typical PE/tie/EVOH/tie/PE structure, the tie layer is coextruded at 2–8 µm; below 2 µm, melt instability and gauge variation can create discontinuous tie coverage. Interlayer adhesion is measured by peel testing under ASTM F904 or equivalent T-peel methods; a cohesive failure in the polyethylene layer is preferred over interfacial delamination at the tie/EVOH boundary. With EVOH containing 27–44 mol% ethylene, adhesion is developed when the interfacial temperature exceeds approximately 220 °C, but maximum peel strength is generally reached between 230 °C and 260 °C. At lower melt temperatures, the maleic anhydride groups do not react sufficiently with hydroxyl or amide end groups, leading to low peel and possible tunnel formation during downstream forming. With polyamide barrier layers, the resin is functional up to standard PA6 processing temperatures; PA66 grades requiring melt temperatures above 280 °C exceed the recommended stability window unless inert-gas blanketing is used.

    In extrusion coating and extrusion lamination, Bynel® 41E558 is applied to aluminum foil, metallized film, and primed polyester at coating weights from 10 g/m² to 25 g/m². Line speeds above 150 m/min are possible but edge-bead formation and neck-in increase compared with LDPE-based adhesives. Die temperatures should be profiled across the width to maintain ±5 °C uniformity; uneven die temperature produces adhesion hot spots and odor. When coating on aluminum foil, foil preheating to 60–90 °C before the nip improves wet-out and reduces pinhole tunneling at thin coating weights. Published data for this specific configuration is limited at coating weights below 10 g/m², so a pilot-scale coating trial is recommended before commercial conversion.

    Compared with anhydride-modified LDPE tie resins, Bynel® 41E558 exhibits higher elongation at break and improved environmental stress-crack resistance under ASTM D1693 when placed adjacent to LLDPE skin layers. The LLDPE backbone provides better dart impact retention in coextruded films but lower melt strength than LDPE-grafted grades at equivalent melt index. On cast film lines, draw resonance and edge-beading can occur above approximately 120 m/min unless the die gap, air-jet, and melt temperature are adjusted. Against EVA-based tie layers, Bynel® 41E558 has lower equilibrium moisture uptake and does not release acetic acid during prolonged processing at temperatures above 230 °C. However, EVA and ethylene-acrylate copolymers often wet PET, inks, and corona-treated polyester more readily; therefore, Bynel® 41E558 is not a universal replacement in print-primed laminations. Compared with anhydride-modified polypropylene adhesives, Bynel® 41E558 has a lower continuous-use temperature limit and is not appropriate for retort structures requiring sustained exposure above 121 °C. Its polyolefin base limits continuous service to about 60–80 °C depending on load and sealant geometry.

    When Barrier Structures Demand LLDPE-Based Adhesion Instead of EVA or LDPE Grafted Resins

    Selection of Bynel® 41E558 is technically justified when the adjacent bulk layer is LLDPE or metallocene polyethylene and the barrier layer is EVOH with ethylene content between 27 mol% and 44 mol%. Under these conditions, the shrinkage and expansion coefficients of the LLDPE adhesive remain close to those of the adjacent LLDPE layer, reducing interfacial stress during cooling and subsequent film winding. When EVOH grades with lower ethylene content are used, the barrier layer must be extruded at higher temperatures; prolonged exposure above 240 °C may embrittle the EVOH boundary and reduce measured peel adhesion, even if the tie resin is not chemically degraded. With polyamide barrier layers, the resin is compatible with PA6 and PA6/66 copolymers up to the normal melt-temperature window. If the structure must operate in retort or autoclave conditions, an anhydride-modified PP-based tie resin is required because LLDPE-based adhesives soften above 92 °C and lose load-bearing capability above 121 °C. The resin is also less effective when the substrate is unprimed PET film because the anhydride-LLDPE system does not wet polyester as readily as EMA- or EVA-based tie resins. In those structures, a printed or primed surface is typically needed before extrusion coating.

    Regulatory compliance for finished structures must be established against the full construction, not the adhesive alone. Bynel® 41E558 is typically evaluated under U.S. FDA 21 CFR 177.1520 for olefin polymers and may meet EU Regulation (EU) No 10/2011 under migration conditions specified by the manufacturer; REACH obligations are managed under Regulation (EC) No 1907/2006. Specific end-use suitability for food contact should be confirmed with the supplier’s Food Contact Statement. Because maleic anhydride functional resins can release trace free maleic anhydride at elevated processing temperatures, local exhaust ventilation is recommended. Store pellets in original sealed packaging below 40 °C and away from ultraviolet light; under these conditions, the manufacturer typically indicates a 24-month shelf life. Avoid blending with amine-containing additives, primary-amine processing aids, or moist regrind, because these materials react with anhydride groups to form gel particles and crosslinked domains. Recycled edge trim is usable if kept clean and dried; repeated extrusion above 280 °C increases oxidized gel content and reduces adhesion to polar substrates. Any material that has been exposed to ambient humidity above 60 % for more than 8 h should be re-dried before blending into a barrier structure.

    Top