| HS Code | 399077 |
| Polymertype | Anhydride-Modified Linear Low Density Polyethylene (LLDPE) |
| Anhydridemodifier | Maleic Anhydride |
| Density | 0.92 g/cm3 |
| Meltindex | 5.0 g/10 min at 190°C/2.16 kg |
| Meltingpoint | 126°C |
| Vicatsofteningpoint | 95°C |
| Tensilestrengthatbreak | 18 MPa |
| Elongationatbreak | 700% |
| Flexuralmodulus | 200 MPa |
| Hardnessshored | 50 |
| Waterabsorption | 0.03% |
| Thermalconductivity | 0.33 W/m·K |
As an accredited DuPont Bynel® 41E557 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DuPont Bynel® 41E557 adhesive resin is supplied in 25 kg polyethylene-lined multi-wall bags, palletized and stretch-wrapped for transport. |
| Container Loading (20′ FCL) | 20′ FCL: DuPont Bynel® 41E557 in 25 kg bags, 20–22.5 MT net, palletized/floor-loaded, shrink-wrapped and securely braced for ocean shipment. |
| Shipping | DuPont Bynel 41E557 Anhydride-Modified LLDPE Adhesive Resin is shipped as non-hazardous plastic pellets in moisture-resistant bags, boxes, or bulk containers. It is not classified as dangerous goods for DOT, IMDG, or IATA transport. Keep containers sealed and store in a cool, dry area away from excessive heat and sunlight. |
| Storage | Store DuPont Bynel® 41E557 in a cool, dry, well-ventilated area. Keep containers tightly closed and protect from moisture, direct sunlight, heat, sparks, and open flames. Maintain recommended storage temperatures, generally 5–35°C (41–95°F). Keep away from strong oxidizing agents. Follow first-in, first-out stock rotation and consult the safety data sheet for specific handling and shelf-life requirements. |
| Shelf Life | Typically two years from manufacture when stored unopened in original packaging at ≤30°C, dry, and away from direct sunlight. |
| Application | Bynel® 41E557 layer | Total structure | Key bond interface |
|---|---|---|---|
| Blown-film EVOH barrier | 3–10 µm per side | 55–120 µm | EVOH / LLDPE |
| Retort-stable film | 4–12 µm | 70–140 µm | EVOH / sealant PE |
| 3LPE steel pipe | 170–250 µm | 2.6–3.7 mm | FBE / PE topcoat |
| Foil lamination | 15–25 g/m² | 60–120 g/m² plus foil | Aluminium foil / LLDPE |
| Blow-moulded fuel tank | 3–8% wall | 5–12 mm wall | HDPE / EVOH |
| MAP sheet | 3–5% sheet | 350–800 µm | EVOH / polyolefin |
| Standard / Regulation | Application scope | Relevant test or clause |
|---|---|---|
| FDA 21 CFR 177.1395 | Laminate adhesives for food contact | Extraction testing in food simulants |
| EU 10/2011 | Plastic materials for food contact | Overall migration 10 mg/dm²; substance-specific limits |
| ISO 21809-1:2018 | Three-layer PE external pipe coating | Peel strength, cathodic disbondment, impact |
| DIN 30670 | Polyethylene coatings on steel pipe | Peel strength, indentation, impact resistance |
| ASTM D1876 | T-peel adhesion of laminates | Bond separation at controlled crosshead speed |
| ASTM D1238 | Melt flow rate of polyethylene | 190 °C / 2.16 kg |
| REACH 1907/2006 | Substances in EU market | SVHC screening, registration obligations |
| RoHS 2011/65/EU | Electrical and electronic equipment | Lead 0.1%, cadmium 0.01% |
Competitive DuPont Bynel® 41E557 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DuPont Bynel® 41E557 is an anhydride-modified linear low-density polyethylene adhesive resin supplied for coextruded tie-layer service in multilayer packaging and industrial laminates. The molecular architecture combines an LLDPE backbone with pendant anhydride groups, producing a material that processes like a conventional LLDPE while offering adhesion to polar barrier polymers and metal oxide surfaces. In a coextrusion structure, Bynel® 41E557 is typically placed between a polyolefin skin layer and an EVOH or polyamide core. The product is identified by the model designation 41E557; grade-specific values for melt mass-flow rate, density, thermal transitions, and mechanical properties are controlled on the manufacturer’s certificate of analysis and lot release documentation. Publicly available technical bulletins for this exact grade are limited; therefore the processing envelope described here is based on the broader class of anhydride-modified LLDPE tie-layer resins and should be confirmed against the current supplier datasheet.
Downgauging and layer control in coextruded films require the tie layer to maintain consistent thickness under high shear. The resin is typically run as a discrete layer at 5–12 µm in blown film and 3–8 µm in cast film. Below these thicknesses, interfacial contact time decreases and adhesion to EVOH or PA can become process-dependent. The anhydride group must reach the interface during the brief melt contact before quenching; therefore melt temperature and die gap are as important as nominal layer ratio.
The anhydride functionality contributes adhesion through ring-opening reactions or hydrogen bonding with hydroxyl groups on EVOH, amide groups on polyamide, and oxide/hydroxide sites on aluminum foil. Unlike unmodified LLDPE, which relies on weak dispersion forces and fails adhesively, Bynel® 41E557 can shift interfacial failure toward cohesive or mixed-mode. Acid-copolymer tie resins such as ethylene-acrylic acid contain carboxylic acid groups that also bond to polar substrates but differ in moisture sensitivity, thermal stability, and seal behavior. Anhydride-modified LLDPE generally retains a processing window closer to LLDPE skin layers; a typical melt pump set point on a cast film line is 220–230°C, while the same process for an acid copolymer may require 205–215°C due to lower thermal stability. These ranges are line-specific and should be established with melt temperature probes at the adapter and die.
Compared with maleic anhydride-grafted polypropylene tie resins, the LLDPE backbone in Bynel® 41E557 produces lower flexural modulus and improved low-temperature impact resistance in film structures. PP-g-MAH grades are usually selected for retortable rigid containers or high-temperature applications where the tie layer must withstand long-term service above 80°C. In flexible packaging that must remain ductile at freezer temperatures, the LLDPE-based adhesive resin avoids the stiffening observed with polypropylene-based tie layers. These differences are quantified by dynamic mechanical analysis; published data for this specific grade is limited.
In seven-layer cast film for fresh red meat, the tie layers may each represent 8–12% of total film thickness. The resin is fed to a satellite extruder with a 30:1 L/D barrier screw and no Maddock mixing section; additional high-shear mixing is not required because the grafted anhydride distribution is already controlled by the manufacturer. If layer distribution exceeds ±1% of nominal, the edge trim recyclability decreases due to the multiple heat histories of EVOH and adhesive. Operators should not exceed 15% edge trim re-feed in the polyolefin skin extruder when Bynel® 41E557 is present. This limit derives from the need to avoid gel specks in the final film.
The simultaneous demand for low seal initiation temperature, oxygen barrier, and interlayer adhesion makes tie-layer selection process-critical. In a nine-layer blown film, Bynel® 41E557 may be positioned adjacent to EVOH and an LLDPE skin. The die temperature is typically held at 210–230°C. If the die temperature is below 200°C, the EVOH layer can cool too quickly at the merge point, reducing interfacial diffusion and creating delamination points at the tie/EVOH boundary. In contrast, die temperatures above 250°C increase the risk of anhydride scission and crosslinked gel formation. Melt temperature should be checked with an immersion thermocouple at the die lip, not estimated from barrel zone settings.
Typical layer ratios for high-barrier blown film are 25–35% polyolefin skins, 5–10% tie layers, and 10–15% EVOH core. The oxygen transmission rate of the final structure is measured according to ASTM D3985 at 23°C and 0% RH or 50% RH, depending on the package use. Because Bynel® 41E557 is non-barrier, its thickness contributes to packaging oxygen permeability only indirectly; excessive tie-layer thickness dilutes the barrier core and increases raw material cost without improving adhesion. When peel strength is evaluated using ASTM F904, the failure mode should be noted because a high numerical peel force with adhesive failure at the tie/EVOH interface still indicates a weak boundary layer.
Anhydride-modified LLDPE resins of this class require a stable melt pump pressure because melt viscosity is close to that of the adjacent polyolefin. Extruders with a 24:1–30:1 L/D ratio and a barrier screw with a compression ratio of 2.5:1–3.5:1 are generally suitable. The barrel temperature profile may be flat or gradually rising, such as feed 175°C, early compression 195°C, metering 210°C, adapter 215°C, and die 220°C. These values are class-level starting conditions; line-specific optimization is required because thermocouple placement and screw wear shift actual melt temperatures by 5–15°C.
Flow surging and interfacial waviness often appear when the viscosity ratio between the tie layer and the adjacent EVOH or PA exceeds 3:1 at the local shear rate. If the tie-layer extruder is dedicated to Bynel® 41E557, screw speed should be controlled by a gravimetric feeder with better than ±0.5% feed-rate stability. A melt pump with gear-pump inlet pressure of 70–100 bar is commonly used on cast film lines to damp extruder pulses. Without a melt pump, output variations caused by pellet feed irregularity can produce tie-layer thickness variation of ±2 µm, which is large enough to affect peel uniformity in thin-gauge structures.
Interfacial stability also depends on the die land length and the location where the layers merge. When Bynel® 41E557 is combined with high-viscosity polyamide in a feedblock, the tie layer may be pushed into the barrier layer if the tie-layer melt is too low in viscosity. A similar materials class with a melt-flow rate at 2.16 kg below 1.5 g/10 min can create viscosity mismatch in the opposite direction. The selection of the 41E557 grade therefore balances adhesion and a melt-flow rate close enough to the adjacent polyethylene skin to minimize layer deformation. Processors verify this by cutting cross-sections with a microtome and examining layer geometry under an optical microscope at 100× magnification.
| Property or regulatory dimension | Class-level envelope or assessment scope | Reference method |
|---|---|---|
| Melt mass-flow rate | 2.0–3.5 g/10 min at 190°C/2.16 kg | ASTM D1238 / ISO 1133-1 |
| Density | 0.910–0.920 g/cm³ at 23°C | ASTM D1505 / ISO 1183-1 |
| Peak melting temperature | 120–126°C | ASTM D3418 / ISO 11357-3 |
| Melt temperature at die | 210–240°C | Plant process measurement |
| Storage relative humidity | ≤60% RH | Supplier handling guidance |
| Food-contact adhesive component | Functional barrier required for direct food contact | 21 CFR 175.105 |
Food-contact status for Bynel® 41E557 is application-specific. In the United States, adhesive components may be evaluated under 21 CFR 175.105 when separated from food by a functional barrier; the polyolefin backbone may also fall within 21 CFR 177.1520(c). In the European Union, plastic materials in food contact are assessed under Commission Regulation (EU) No 10/2011 and its amendments; compliance is confirmed at the final article level, not solely by the resin datasheet. REACH registration and heavy-metal limits should be confirmed through the supplier’s safety data sheet. These regulatory references are not sufficient by themselves for production release.
Anhydride groups on the polyethylene backbone can undergo thermal and hydrolytic reactions when held at elevated temperature for extended periods. The practical consequence on coextrusion lines is that Bynel® 41E557 should not be left in a hot extruder during line stoppages. If a line must stop for more than 10 minutes, the tie-layer extruder should be purged with LLDPE or the barrel temperatures reduced to 150°C. Start-up purging after long shutdowns should be conducted with unmodified LLDPE for 20–30 minutes until the melt is clear and free of discolored streaks.
Moisture exposure before processing is also a process limitation. The material should be stored in sealed containers at or below 60% relative humidity. If sacks are left open in a humid plant for more than 24 hours, surface condensation can hydrolyze a portion of the anhydride functionality to the acid form, reducing adhesion to EVOH and polyamide without necessarily changing melt-flow rate. In such cases, drying for 2–4 hours at 60–75°C in a desiccant hopper dryer is used before processing. Avoid amine-based additives, including certain processing aids and purge compounds, because amine groups can react with anhydride and create infusible gel deposits on screw surfaces and die lips.
Bynel® 41E557 is supplied in multi-layer bags or bulk containers, depending on region. Bulk handling systems should use stainless steel or aluminum piping and avoid long-radius bends; pellet abrasion can generate dust. Pellet conveying with plant compressed air should maintain a dew point below -20°C to prevent condensation on the pellets at high humidity. These measures preserve the dry-as-supplied condition of the anhydride functionality before melt processing.
For extrusion lamination of aluminum foil to polyethylene, Bynel® 41E557 is applied at coating weights between 15 g/m² and 25 g/m² through a T-slot die. The air gap is kept as short as practical, typically 100–200 mm, to reduce oxide cooling and maintain adhesion. The substrate should enter the nip at 20–40°C to maximize thermal quench. If the melt curtain is run above 240°C, the resin can smoke and deposit degraded material on the backside of the foil; if below 210°C, the anhydride groups lack sufficient interfacial mobility to wet the metal oxide surface. Peel strength measured after lamination can vary with coating weight and cooling rate; therefore lot-to-lot adhesion should be screened with a standard T-peel method before full production.