Dupont Bynel 41e532 Anhydride Modified Lldpe Adhesive Resin

DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 685689
    Productname DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin
    Polymertype Anhydride-Modified Linear Low Density Polyethylene
    Comonomer Maleic Anhydride
    Form Pellets
    Density 0.92 g/cm³
    Meltflowrate 2.5 g/10 min at 190 °C/2.16 kg
    Meltingpoint 124 °C
    Vicatsofteningpoint 94 °C
    Tensilestrengthatbreak 15 MPa
    Elongationatbreak 500%
    Flexuralmodulus 190 MPa
    Shoredhardness 50
    Waterabsorption 0.03%
    Volumeresistivity >1×10^15 ohm·cm
    Dielectricconstant 2.3
    Dissipationfactor 0.0005
    Thermalconductivity 0.25 W/m·K
    Brittlenesstemperature < -70 °C

    As an accredited DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin is supplied in 25 kg moisture-resistant bags, palletized, with 1,000 kg bulk bags available.
    Container Loading (20′ FCL) Container Loading (20′ FCL): DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin, in 25 kg bags, palletized, securely stowed, evenly distributed.
    Shipping DuPont Bynel® 41E532 is shipped as non-hazardous, solid resin pellets, typically in sealed 25-kg bags or octabins on stretch-wrapped pallets. Transport in clean, dry vehicles at moderate temperatures. Protect from moisture, heat, direct sunlight, and contamination. No UN dangerous-goods class applies; follow local regulations and keep containers closed until use.
    Storage Store DuPont Bynel® 41E532 in a cool, dry, well-ventilated area, away from heat, ignition sources, and oxidizing agents. Keep containers or bags tightly closed and palletized. Protect from moisture, direct sunlight, and contamination. Maintain moderate temperatures, avoid prolonged heat, and follow first-in, first-out stock rotation. Consult the Safety Data Sheet for specific local requirements.
    Shelf Life Shelf life is two years from date of manufacture when stored unopened in original packaging below 30°C, away from moisture, heat, and direct sunlight.
    Application of DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin

    Five-layer blown film structures combining linear low-density polyethylene skins, polyamide 6 or ethylene-vinyl alcohol barrier cores, and anhydride-modified polyethylene tie layers are produced on high-output coextrusion lines in which Bynel® 41E532 is metered as the neat adhesive layer between the non-polar polyethylene phase and the polar barrier polymer. In food-contact applications the adhesive resin is used under the compositional conditions of 21 CFR 175.105, while the polyethylene skins comply with 21 CFR 177.1500; for European Union migration compliance the finished symmetrical A/B/C/B/A film is assessed under Regulation (EU) No 10/2011, with overall migration testing performed in the appropriate fatty-food simulants assigned in Annex III of that regulation. Tie-layer thickness in meat-film and dairy-barrier constructions commonly ranges from 6 µm to 12 µm per side; below 6 µm, 90° peel adhesion measured under ASTM F904-16 becomes inconsistent because the interfacial contact area and the total anhydride functionality available for reaction with amide or hydroxyl end groups are insufficient. Above 12 µm, the additional material contributes to gauge non-uniformity without a detectable increase in lamination strength. The blown film line is configured with a 200–300 mm spiral mandrel die, a die gap of 1.6–2.2 mm, a 2.0:1–2.5:1 blow-up ratio, and die-head temperatures of 220–230°C. The tie-layer extruder is operated with barrel zones from 175°C to 220°C to avoid thermal degradation of the anhydride functionality, while the die-lip melt temperature is controlled within ±5°C of the nominal setpoint because viscosity mismatch with EVOH cores containing 32–38 mol% ethylene gives rise to interfacial waviness when the tie-layer-to-EVOH viscosity ratio at processing shear rate exceeds approximately 3:1. On production-scale lines, raising line speed beyond 120 m/min without adjusting the frost line above 350 mm shortens the available reaction time at the melt interface; published data for the exact PE/tie/PA6/EVOH stack at that speed are limited, but the corrective sequence is to increase die temperature within the specified window, reduce EVOH viscosity grade, or increase tie-layer thickness. Converted rollstock enters vacuum pouches, shrink bags for aged cheese, barrier liners, and modified-atmosphere flow-wrap packs.

    What limits the use of anhydride-modified LLDPE as an extrusion-coating tie layer on aluminium foil and paperboard?

    In extrusion coating and extrusion lamination, Bynel® 41E532 functions as the intermediate tie layer between low-density polyethylene sealants and aluminium foil, metallised film, or paperboard in aseptic liquid carton precursors and laminated coffee packs. U.S. food-contact status of the finished board laminate is evaluated under 21 CFR 176.170 and 21 CFR 176.180 for the paperboard component, while the adhesive resin is used under the conditions of 21 CFR 175.105; in the European Union, the polyethylene-based layers are assessed under Regulation (EU) No 10/2011, and migration testing follows the food-simulant assignment in Annex III of that regulation. The tie layer is applied at 10–20 g/m², equivalent to 10–22 µm, between aluminium foil and LDPE; below 10 g/m², fibre-tear adhesion is not consistently achieved and the oxygen transmission rate of the laminate increases under ASTM D3985-17. When the tie layer is used in a four-layer liquid carton stack of LDPE/paperboard/Bynel®/LDPE or LDPE/foil/Bynel®/LDPE, the tie layer represents 6–10 wt% of the total polymer mass. Processing is conducted on an extrusion coating line with a 120 mm extruder having 30:1 L/D, a slot die with 0.6–1.0 mm opening, an air gap of 150–250 mm, and a matte-chromium chill roll held at 15–20°C. Melt temperature at the die exit is maintained at 235–260°C; above 260°C, low-molecular-weight oxidation products increase and can contaminate the chill-roll surface, while below 235°C, incomplete wet-out of the aluminium oxide surface reduces T-peel strength measured under ASTM D1876-08. Paperboard is preheated to 40–60°C to remove surface moisture, and aluminium foil is specified free of rolling oils rather than corona-treated, because the anhydride functionality reacts with the oxide surface without requiring additional oxidation. At line speeds above 250 m/min, the short residence time in the air gap limits thermal oxidation of the LLDPE backbone and shifts the adhesion mechanism toward the grafted anhydride groups; published data for Bynel® 41E532 at that line-speed threshold are limited, but converters commonly compensate by reducing the air gap or raising melt temperature within the upper range. Finished stocks are slit into aseptic beverage cartons, coffee brick packs, foil lidding sachets, and industrial membrane laminates.

    Application segmentPrimary regulatory referenceTest methodCritical process boundary
    Blown film food packaging21 CFR 175.105, 21 CFR 177.1500, (EU) No 10/2011ASTM F904-16Tie layer ≥6 µm
    Extrusion coating / lamination21 CFR 176.170, 176.180, 21 CFR 175.105ASTM D1876-08, ASTM D3985-17Melt 235–260°C
    Blow-moulded industrial bottlesUN Model Regulations Ch. 6.1ASTM D2684Tie layer ≥20 µm
    Cast film barrier webs21 CFR 175.105, (EU) No 10/2011ASTM F904-16Die-lip 230–245°C
    Coextruded sheet for MAP trays21 CFR 175.105, 21 CFR 177.1500, (EU) No 10/2011ASTM D1876-08Tie layer 20–35 µm

    Extrusion blow-moulded HDPE/EVOH barrier bottles for industrial chemical formulations

    Six-layer extrusion blow moulding of 1 L and 5 L HDPE/EVOH containers for agrochemical and solvent-based formulations uses Bynel® 41E532 as the neat tie layer between the high-density polyethylene structural layers and the ethylene-vinyl alcohol oxygen barrier. For dangerous-goods packaging, the finished container is certified under the UN Model Regulations Chapter 6.1 packaging framework, with the specific packaging code assigned by the certification holder after leakproofness and hydraulic-pressure tests; permeation screening is conducted according to ASTM D2684, and the HDPE layers meet the olefin compositional requirements of 21 CFR 177.1500 where the container is later used for food or food additives. In a six-layer HDPE/tie/EVOH/tie/regrind/HDPE wall of 600–1200 µm total thickness, each tie layer is held at 20–35 µm, or 2–4 wt% of the total container wall; below 20 µm, interfacial failure at the pinch-off and parting line is observed after conditioning at −18°C and tensile testing under ASTM D638-14. The multilayer intermittent line is equipped with a six-layer accumulator head, a diverging die, parison programming, and a clamp unit of 18–25 t for 5 L jerricans. Melt temperature at the die head is maintained at 210–225°C, while the HDPE extruder zones are operated from 180°C to 220°C; the EVOH layer temperature is kept below 225°C to avoid gel formation. The tie-layer resin is not pre-blended with the regrind stream because the anhydride functionality can be diluted below the concentration needed for adhesion. Processors control wall-thickness programming so that corner thickness does not fall below 500 µm, because EVOH core thinning below 25 µm creates oxygen-permeability spikes and localised delamination under ASTM D638-14 tensile testing of specimens cut from the container wall. Although the LLDPE backbone of Bynel® 41E532 is not hygroscopic, surface condensation on pellets stored in outdoor silos at RH > 60% can cause feed-zone slip and barrel output fluctuation; dry-air purge or hopper heating at 60°C is specified when pellet dew point exceeds 10°C. Containers from this process are filled with solvent-based agricultural formulations, pesticide concentrates, aqueous ammonia, or specialty cleaning chemicals.

    When cast-film line speed exceeds 200 m/min in five-layer nylon/EVOH structures

    In five-layer cast-film coextrusion for flexible barrier webs, Bynel® 41E532 is inserted as the tie layer between polyethylene skins and a polyamide 6 or EVOH core, with the line operating above 200 m/min requiring tighter control of die geometry and melt temperature than blown film. Food-contact status is anchored to 21 CFR 175.105 for the adhesive layer and 21 CFR 177.1500 for the polyethylene skins; in the EU, the final film is assessed under (EU) No 10/2011, with migration testing according to Annex III food simulants. The tie layers are run at 4–8 µm each, or 3–5 wt% of the 50–100 µm total web. At line speeds above 200 m/min, the melt draw between the die lip and the chill roll reduces web width unless the die-lip temperature is held in the 230–245°C window; below 230°C, the nylon core solidifies prematurely and the tie layer cannot wet the polar surface, while above 245°C, neck-in increases and edge trim loss rises. The cast-film line is equipped with a flat slot die at 0.8–1.2 mm gap, a 18–25°C chromium chill roll, and an air knife or vacuum box for edge pinning. Adhesion is monitored by ASTM F904-16 on samples conditioned at 23°C and 50% RH for 48 h. Published data for Bynel® 41E532 at casting speeds above 250 m/min in five-layer nylon-containing structures are limited; when converters observe intermittent edge delamination, the corrective sequence is to raise die temperature within the specified window, reduce die gap, or increase tie-layer thickness to 10 µm. Finished cast webs are used as lamination base films, stand-up pouch backsheets, and high-clarity barrier overwrap.

    Coextruded polyolefin barrier sheet for refrigerated modified-atmosphere packaging trays is produced on flat-die sheet lines in which Bynel® 41E532 joins a food-contact LDPE/LLDPE sealing layer to a central EVOH or polyamide 6 barrier. In food-contact tray applications the adhesive layer is permitted under 21 CFR 175.105, the sealing layer complies with 21 CFR 177.1500, and the total structure is evaluated under (EU) No 10/2011 for overall migration using the appropriate food simulant for refrigerated aqueous and fatty foods. Total sheet thickness for thermoformable barrier trays ranges from 500 µm to 1000 µm, with tie layers of 20–35 µm on each side of the barrier core, equivalent to 4–6 wt% of the total sheet. The sheet line uses a multi-layer flat die with restrictor-bar adjustment, a polished three-roll stack maintained at 50–70°C, and melt temperatures of 220–240°C at the die exit. Thermoforming is performed downstream at surface temperatures of 120–150°C, with plug-assisted drawing at a 3:1 depth-to-diameter ratio; the tie layer must remain above 15 µm in the thinnest corner region or the EVOH core delaminates under tensile stress during drawing. Processors measure sheet adhesion by cutting 25 mm-wide strips and testing under ASTM D1876-08; the acceptance threshold is set by the converter based on downstream puncture resistance, not a universal adhesive strength value. Finished trays are used for case-ready red meat, poultry, seafood, and cheese packaging under modified-atmosphere conditions.

    Free Quote

    Competitive DuPont Bynel® 41E532 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Bynel® 41E532 is an anhydride-modified linear low-density polyethylene adhesive resin supplied as free-flowing pellets. The material is specified as a discrete tie layer in coextruded multilayer films, sheet, extrusion coating, and blow-molded container structures where a non-polar polyethylene or polypropylene-based layer must be bonded to a polar barrier layer such as polyamide 6, polyamide 66, ethylene-vinyl alcohol copolymer, or an ionomer. The anhydride functionality is grafted onto the polymer backbone rather than copolymerized as a separate monomer phase, which leaves the base resin primarily linear while providing reactive adhesion sites at the interface during melt processing.

    Supplier-published nominal values list a melt flow rate of 2.7 g/10 min determined at 190 °C under a 2.16 kg load in accordance with ISO 1133-1 or ASTM D1238, and a density of 0.91 g/cm³ per ISO 1183-1 or ASTM D1505. Representative thermal values include a differential scanning calorimetry peak melting point of 125 °C per ISO 11357-3 and a Vicat softening temperature of 95 °C per ISO 306 or ASTM D1525. These values are nominal guide values, not batch-release specifications, and should be confirmed against the current supplier certificate of analysis for the specific lot.

    PropertyNominal valueTest method
    Melt flow rate2.7 g/10 minISO 1133-1 / ASTM D1238
    Density0.91 g/cm³ISO 1183-1 / ASTM D1505
    DSC peak melting point125 °CISO 11357-3
    Vicat softening temperature95 °CISO 306 / ASTM D1525

    In a typical five-layer cast film structure of linear low-density polyethylene / Bynel® 41E532 / EVOH / Bynel® 41E532 / linear low-density polyethylene, the tie layers are commonly specified at 5–15 µm per layer within a 50–150 µm total gauge. In a seven-layer blown film line equipped with a 250 mm spiral mandrel die and a blow-up ratio of 2.2:1–2.8:1, the same material is processed as a discrete sub-skin layer between a polyethylene skin and a polyamide core. These thickness values are process-dependent and must be confirmed by interlayer adhesion testing after coextrusion, typically using a 180° T-peel method derived from ASTM F904 or an equivalent internal specification.

    In extrusion coating and cast film lines, Bynel® 41E532 is processed as a thin tie layer between a polyethylene-based substrate and a barrier layer. The resin is typically fed from a dedicated 45–65 mm single-screw extruder with a 24:1–30:1 L/D ratio, and the melt is combined in a feedblock before the die. Layer distribution is controlled by selective adjustment of extruder output and takeoff speed; tie-layer thickness is verified by cross-sectional microscopy using ISO 12509 or an equivalent optical method.

    Anhydride Grafting Occurs on a Linear Low-Density Polyethylene Backbone

    The adhesion mechanism of Bynel® 41E532 relies on pendant maleic anhydride groups grafted onto the LLDPE chain. During melt contact with polyamide, the anhydride functionality can react with terminal amine groups to form amide or imide linkages. With EVOH, the anhydride can form ester linkages with hydroxyl groups. These reactions are diffusion- and contact-time-dependent; they occur within the interfacial layer only when the melt temperature is high enough to allow chain segment mobility and when the tie layer and barrier layer are in uninterrupted contact through the feedblock, selector plug, or multi-manifold die. Interfacial adhesion therefore depends not only on anhydride content, but also on melt contact temperature, line speed, and solidification rate at the chill roll or air ring.

    The grafted anhydride concentration is not separately specified in the public datasheet; published data for the exact grafted level are limited. However, the practical adhesion response is strongly influenced by the anhydride content and by the carrier resin’s molecular architecture. Because the carrier is an LLDPE, the molten resin retains sufficient melt strength for cast film and blown film coextrusion while maintaining a lower sealing temperature and greater low-temperature toughness than an anhydride-modified HDPE tie layer of equivalent melt flow rate. This behavior is suitable for flexible barrier packaging where the tie layer must not dominate the overall film stiffness.

    What Distinguishes Bynel® 41E532 from Unmodified LLDPE and Ethylene-Acrylic Acid Copolymers?

    Unmodified linear low-density polyethylene has no polar functionality capable of forming covalent bonds with polyamide or EVOH. Interlayer adhesion in structures that omit a functionalized tie resin is typically low and fails adhesively at the polyethylene/polar-barrier interface in peel testing. Bynel® 41E532 differs by introducing reactive anhydride functionality without shifting the base resin into the higher-density, higher-modulus range characteristic of anhydride-modified HDPE grades. Compared with ethylene-acrylic acid copolymers, the anhydride-modified LLDPE generally provides a broader processing window in polyolefin coextrusion and lower water sensitivity at the interface; however, specific peel strength depends on the barrier polymer type, melt contact temperature, and cooling rate. Within the Bynel® 4000 series, 41E532 is commonly selected when an LLDPE carrier is required for blown film toughness and lower heat-seal initiation. Grades based on EVA or acid copolymers are selected when foil adhesion or lower-temperature sealing is specified; grades based on HDPE are selected when higher stiffness and temperature resistance are specified. Published direct comparative peel data for all potential counterparts are limited.

    ParameterBynel® 41E532Unmodified LLDPEEthylene-acrylic acid copolymerAnhydride-modified HDPE
    Functional groupAnhydrideNoneCarboxylic acidAnhydride
    Density0.91 g/cm³0.918–0.922 g/cm³0.93–0.96 g/cm³0.94–0.96 g/cm³
    Melt flow rate2.7 g/10 minGrade-dependentGrade-dependentGrade-dependent
    Adhesion to PA/EVOHReactive covalent/acid-baseLow, adhesive failureModerate to goodGood
    Processing window210–260 °C190–240 °C180–260 °C220–280 °C

    When Melt Temperature Deviates Beyond the 210–260 °C Processing Window in Coextruded Film Lines

    Melt temperature control is critical for reactive tie-layer performance. At melt temperatures below 210 °C, the viscosity of Bynel® 41E532 remains elevated, interfacial wetting of polyamide or EVOH is incomplete, and the residence time available for anhydride reaction may be insufficient. This condition can produce weak interlayer adhesion that is detected only after secondary converting, when the laminated structure is flexed, thermoformed, or heat-sealed. On a cast film line, the condition may appear as a visible boundary between the tie layer and barrier layer in cross-sectional microscopy even when the extruder pressure remains stable.

    Above 260 °C, the anhydride graft can participate in chain extension and crosslinking reactions. Production-scale cast film lines with 75 mm single-screw extruders at 30:1 L/D have shown gel accumulation when melt temperatures exceeded 260 °C for residence times beyond 10–15 min. The first visual indication is usually fisheye formation in the polyethylene skin layer or interfacial gel streaks at the feedblock merge point. If the temperature is raised above 280 °C, discoloration and odor can develop, and the material may begin to deposit carbonaceous residue on screw flights and die lips.

    Barrel zone settings are commonly established from 180 °C at the feed throat to 240 °C in the metering zone, with adapter and die temperatures held at 230–250 °C. Because the carrier resin is a polyolefin, drying is not required at ambient relative humidity below 60%. Pellets exposed to condensation or stored in an environment above 60% relative humidity should be dried in a desiccant dryer at 80 °C for 4 h to reach a surface moisture level below 0.05 wt%. Line purging with unmodified LLDPE of melt index 1.0–2.0 g/10 min is recommended before shutdown to displace reactive material and limit carbonaceous deposits in the feedblock and die.

    Because the material contains reactive anhydride groups, it should not be dry-blended or coextruded with additives that contain free primary or secondary amines. Such amines can react during melt processing and produce localized gel particles, shift the adhesion balance, or generate odor. Any antioxidant or processing aid used in the tie layer must be selected for compatibility with anhydride functionality, and changes to the additive package should be validated on a pilot line before production use.

    Regulatory Compliance and Food-Contact Documentation

    Food-contact suitability must be established for the finished multilayer structure, not for the resin alone. For United States applications, the olefin polymer fraction of this type is generally reviewed under 21 CFR §177.1520; the anhydride modification may require additional adjuvant or food-contact notification review depending on the final use, food type, and temperature condition. In the European Union, compliance is assessed under Commission Regulation (EU) No 10/2011, including the overall migration limit of 10 mg/dm² measured under EN 1186 test conditions appropriate to the intended contact time and temperature. For industrial and non-food applications, the material is subject to REACH Regulation (EC) No 1907/2006; a written confirmation from the supplier is required to confirm the absence of substances of very high concern above 0.1 wt% under the current candidate list.

    The product is not supplied as a medical-grade or pharmaceutical-grade material. No compliance statement should be transferred to a final application without verifying the exact coextrusion structure, layer distribution, and use conditions against the current regulatory list for the intended market. Compliance documentation for the base resin does not automatically cover the functionalized grade because the anhydride modification can alter migration behavior and food-contact status.