Dupont Bynel 4107 Anhydride Modified Lldpe Adhesive Resin

DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin

    • Product Name: DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 939697
    Product DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin
    Chemical Type Anhydride-Modified Linear Low Density Polyethylene (LLDPE)
    Modification Maleic Anhydride Grafted
    Form Pellets
    Color Natural
    Density 0.92 g/cm³
    Melt Flow Rate 190 C 2 16 Kg 2.0 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 89 °C
    Tensile Strength At Break 12 MPa
    Elongation At Break 500%
    Flexural Modulus 200 MPa
    Hardness Shore D 50
    Water Absorption <0.1%
    Thermal Stability Stable up to 300 °C
    Processing Temperature 260–300 °C
    Adhesion To Evoh High
    Adhesion To Polyamide High
    Adhesion To Polyethylene High

    As an accredited DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing DuPont Bynel® 4107 is packaged in 25 kg (55 lb) polyethylene-lined bags, typically palletized for shipment.
    Container Loading (20′ FCL) 20′ FCL: DuPont Bynel 4107 in 25 kg bags, palletized; about 20 metric tons, securely loaded.
    Shipping DuPont Bynel 4107 Anhydride-Modified LLDPE Adhesive Resin is not regulated for transport under DOT, IMDG, IATA, or ADR. No UN number, hazard class, or packing group is assigned. Ship in original sealed packaging, keep dry, and avoid excessive heat, moisture, and contamination. Consult the SDS for details.
    Storage Store Bynel® 4107 in a cool, dry, well-ventilated area in tightly closed original containers, preventing moisture absorption. Protect from direct sunlight, heat, flames, and static discharge. Keep away from strong oxidizers, amines, alcohols, and alkalis. Store separately from incompatible materials. Follow first-in, first-out rotation. Avoid prolonged storage above recommended temperatures. Contain spills and keep the area clean.
    Shelf Life Typically 24 months from manufacture if stored unopened in original packaging, cool, dry, and protected from moisture and direct sunlight.
    Application of DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin

    When the Sealant Skin Contains Slip Additives That Migrate to the Tie-Layer Interface

    Five-layer blown film lines running a symmetrical LDPE/LLDPE skin, Bynel® 4107 tie layer, EVOH core, Bynel® 4107 tie layer, and LDPE/LLDPE skin structure have shown interfacial delamination when the sealant skin is formulated with erucamide or oleamide at concentrations above 800 ppm. The amide slip additives bloom to the skin/tie boundary within the first 72 h after winding and occupy polar sites required for anhydride-mediated adhesion. The formulary countermeasure is to hold the Bynel® 4107 tie layer at 6–10 wt% of the total extruded curtain, corresponding to 5–9 µm per side in a 70–100 µm finished film, and to specify a sealant skin free of migratory slip where possible. If slip is unavoidable, the slip concentrate is limited to 300–500 ppm in the sealant skin. The coextrusion line is configured with 40:1 L/D grooved-feed extruders for the tie layer, barrel temperatures of 200–235°C, and a spiral mandrel die held at 225–235°C. The bubble blow-up ratio is maintained at 2.0–2.6, and frost-line height is kept at 1.2–1.8 die diameters so that cooling is complete before the bubble reaches the collapsing frame. Compliance for food-contact uses includes FDA 21 CFR 175.105 for the adhesive component and EU Regulation (EU) No 10/2011 migration testing under the intended temperature and time conditions. Oxygen transmission is evaluated under ASTM D3985-19 at 23°C and 0% RH or 85% RH to detect tie failure after retort; peel adhesion is measured by ASTM D1876-01(2015) with a 180° T-peel geometry and a 300 mm/min jaw separation rate. Terminal products include modified atmosphere packaging for raw meat, fresh pasta, shredded cheese, and coffee portion packs, where the tie layer must survive film stretching, print lamination, and cold-seal application without delamination.

    On a coil-fed three-layer polyethylene pipe coating line running at 2.5 m/min to 4.5 m/min, the anhydride-modified LLDPE is applied as the intermediate adhesive layer between a fusion-bonded epoxy primer and a high-density polyethylene topcoat. The steel substrate is first dry-blast cleaned to ISO 8501-1 Sa 2.5 with an anchor profile of 50–90 µm, after which the fusion-bonded epoxy is sprayed at a pre-heat temperature of 180–230°C to a cured thickness of 60–100 µm. Bynel® 4107 is extruded at a melt temperature of 210–240°C through a flat die positioned between the epoxy spray and the topcoat application, and it is deposited as a 100% neat tie layer at a nominal thickness of 220–300 µm. No carrier resin dilution is used in the primary adhesive layer, although a dry blend of 10–25 wt% Bynel® 4107 into the HDPE topcoat is sometimes run to recover interfacial shear on thick-wall pipe. The HDPE topcoat is applied at 2.0–3.5 mm to complete the three-layer coating. The production process is a single-pass side extrusion and roller pressing sequence, and the adhesive layer must retain sufficient melt viscosity to avoid being squeezed out at the rollers; melt-index control therefore governs the available line-speed window. Compliance is anchored to ISO 21809-1:2018 for external polyolefin coatings on buried or submerged pipeline systems and to DIN 30670 for three-layer PE coating. Peel adhesion is tested by ASTM D4541-17 pull-off or by ISO 21809-1 peel requirements at 23°C and after hot-water immersion. Terminal finished product types include oil and gas transmission pipelines, gas distribution lines, water transmission mains, and firewater piping where the coating must resist cathodic disbondment over 28 days at 23°C and 65°C. Bynel® 4107 is not selected for three-layer polypropylene systems where topcoat melt temperatures exceed 250°C; a PP-grafted tie resin is substituted in that configuration.

    What Constrains Residence Time in Six-Layer Blow Molded Barrier Containers?

    The primary processing hazard in six-layer extrusion blow molding of HDPE/regrind/tie/EVOH/tie/HDPE containers is not low initial adhesion but progressive gelation of the anhydride-functionalized LLDPE when it is held in the accumulator head above 220°C for more than 10 min. This condition arises in barrier jerrycan production for agricultural chemicals and solvent-based inks where the machine operates with intermittent parison ejection and long cycle time. Bynel® 4107 is maintained at 5–8 wt% of the total container wall weight, with each tie layer typically 0.08–0.15 mm thick in a 1.0–1.5 mm finished wall. The extrusion system consists of six separate extruders feeding a spiral accumulator head; the tie-layer extruders are operated at 200–225°C barrel temperature, and the die head is held at 210–220°C. The parison is dropped at a mold closing speed that maintains 0.8–1.2 s open time to reduce overheating of the EVOH layer and to limit contact of the molten tie resin with atmospheric moisture. Clamp force is typically 1,800–2,500 kN for a 20 L jerrycan. Compliance for chemical packaging is evaluated against the UN Recommendations on the Transport of Dangerous Goods and ADR/RID packaging provisions, while food-contact barrier containers require EU Regulation (EU) No 10/2011 and FDA 21 CFR 175.105 for the adhesive tie layer. Interlayer adhesion is tested after filling by drop impact on filled containers at -18°C and by hydrostatic burst-permeation testing of the barrier wall. Terminal finished product types include HDPE/EVOH six-layer jerrycans for agrochemicals, solvent-based cleaning fluids, fuel additives, and industrial oils where EVOH provides a hydrocarbon permeation barrier and the tie layer prevents layer separation during stacking and transport.

    ScenarioCompliance anchorAdhesion/barrier test methodBynel® 4107 proportion
    Five-layer EVOH barrier filmFDA 21 CFR 175.105; EU Regulation (EU) No 10/2011ASTM D3985-19; ASTM D1876-01(2015)6–10 wt% of total web
    Three-layer PE steel pipe coatingISO 21809-1:2018; DIN 30670ASTM D4541-17; ISO 21809-1 peel100% neat adhesive layer; 220–300 µm
    Six-layer barrier jerrycanUN Recommendations; ADR/RID; EU 10/2011Drop impact at -18°C; hydrostatic burst-permeation5–8 wt% of container wall
    Aseptic carton foil laminationFDA 21 CFR 175.105; EU Regulation (EC) No 1935/2004ASTM D903-98(2017)5–15 g/m²; 5–10% of total polymer coating
    Retortable thermoformed barrier trayEU Regulation (EU) No 10/2011; FDA 21 CFR 175.105ASTM D638-14; ISO 527-3:20187–9% of total sheet thickness
    Multilayer barrier tubeEU Regulation (EC) No 1223/2009; EU 10/2011; FDA 21 CFR 175.105ASTM D1876-01(2015) after 40°C/75% RH aging5–10 wt% of sleeve wall

    For aseptic carton structures that combine paperboard, aluminum foil, and a low-sealing LLDPE, the extrusion coating line operates under an entirely different adhesion mechanism from blown film: the anhydride groups of Bynel® 4107 interact with hydrated aluminum oxide sites on the foil surface to produce primerless adhesion when the polymer undergoes oxidative grafting during the air gap. The tie resin is extruded at 235–245°C through a T-slot die onto the foil web at line speeds of 150–300 m/min, with the air gap set at 100–180 mm and the chill roll maintained at 15–25°C. Coating weight is held at 5–15 g/m²; when Bynel® 4107 is coextruded with a bulk LDPE layer, the tie layer constitutes 5–10% of the total polymer coating weight. The process is a single-pass tandem extrusion lamination, with the paperboard and foil webs unwound under a combined tension control window that limits foil wrinkling while maintaining web-path stability. Compliance for aseptic packaging laminates is documented under FDA 21 CFR 175.105 and EU Regulation (EC) No 1935/2004; migration testing follows EU Regulation (EU) No 10/2011 for plastic materials in contact with food. Peel strength between the foil and the extrusion laminate is measured by ASTM D903-98(2017) with a 180° peel angle at 300 mm/min. Published data for this specific configuration under high line-speed trial conditions is limited, so initial validation on the customer’s tandem line is required to establish the lower coating weight limit before commercial approval. Terminal finished product types include aseptic brick packs for dairy and juice, pharmaceutical sachet lidding, and dry food pouch laminates where foil integrity and tie adhesion determine shelf-life without refrigeration.

    A Narrow Thermal Processing Window Beneath 235°C for Retort-Tolerant Thermoformed Barrier Trays

    Coextruded sheet for retortable trays enters a property cliff when the tie-layer melt temperature exceeds 235°C because the anhydride functionality begins oxidative degradation, reducing peel strength after the tray is exposed to 121°C overpressure retort for 30 min. The sheet structure is typically HDPE/tie/EVOH/tie/HDPE with the Bynel® 4107 tie layers held at 7–9% of total sheet thickness, approximately 40–70 µm per tie layer in an 800–1,200 µm sheet. The downstream production process starts with a sheet extrusion line using a 45:1 L/D single-screw extruder for the tie resin and a coextrusion feedback block feeding a 1,200 mm slot die at 225–235°C. The molten web is polished through a three-roll stack at 70–85°C and wound into mother rolls for subsequent thermoforming. Thermoforming is operated at 110–130°C sheet surface temperature with plug-assisted pressure forming; this temperature stays below the onset of EVOH moisture-foaming but above the tie layer’s activation threshold. Compliance for food-contact use is anchored to EU Regulation (EU) No 10/2011 and FDA 21 CFR 175.105. Mechanical integrity after retort is quantified by ASTM D638-14 tensile yield and ISO 527-3:2018 peel delamination testing on microtomed cross-sections. Terminal finished product types include ready-meal retort trays, soup and sauce bowls, and medical disposable trays that are sterilized at 121°C and must resist layer separation during steam purge cycles.

    In a multilayer barrier tube line, the sleeve is coextruded as a five-layer composite of sealant-grade LDPE, Bynel® 4107, EVOH, Bynel® 4107, and LDPE, then cut into blanks on an indexing conveyor before shoulder injection molding. The tie layer is set at 5–10 wt% of the sleeve wall, which translates to 15–35 µm per side in a 300–500 µm tube wall. The tube coextrusion die is held at 210–230°C, and the sleeve line speed is typically 30–60 m/min for tube diameters of 25–50 mm. The downstream production process continues with automatic shoulder molding at 220–250°C, in which the adhesive tie resin must tolerate proximity to the hot sprue and maintain adhesion to EVOH without generating interfacial gas splay. Compliance for the finished tube is evaluated under EU Regulation (EC) No 1223/2009 for cosmetic product packaging safety, EU Regulation (EU) No 10/2011 for food-contact migration, and FDA 21 CFR 175.105 for the adhesive resin. Peel adhesion between the EVOH barrier and the LDPE skin is tested by ASTM D1876-01(2015) after accelerated aging at 40°C and 75% RH for 14 days. Terminal finished product types include toothpaste tubes, cosmetic cream and lotion tubes, pharmaceutical ointment tubes, and hair colorant packaging where the EVOH barrier prevents flavor or fragrance loss and the adhesive layer resists delamination during repeated squeezing.

    Free Quote

    Competitive DuPont Bynel® 4107 Anhydride-Modified LLDPE Adhesive Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DuPont Bynel® 4107 is an anhydride-modified linear low-density polyethylene adhesive resin used as a tie layer in coextruded barrier structures. The carrier resin is an LLDPE backbone functionalized with maleic anhydride, producing a polyolefin that retains film toughness while forming polar interactions with polyamide, ethylene vinyl alcohol copolymer (EVOH), and ionomer barrier surfaces. The resin is supplied in pellet form for cast film, blown film, extrusion coating, sheet coextrusion, and blow molding. Typical melt flow rate at 190 °C/2.16 kg is reported as 1.0–1.2 g/10 min per ISO 1133-1:2022, with density at 23 °C of 0.910–0.920 g/cm³ per ISO 1183-1:2019. These values are typical ranges, not lot-specific specification limits.

    PropertyTypical rangeTest method
    Melt flow rate, 190 °C/2.16 kg1.0–1.2 g/10 minISO 1133-1:2022
    Density, 23 °C0.910–0.920 g/cm³ISO 1183-1:2019
    Peak melting temperature, DSC, 10 °C/min120–126 °CISO 11357-3:2018
    Vicat softening temperature, A50, 10 N93–100 °CASTM D1525-17e1
    Shore D hardness, 15 s50–55ISO 868:2003
    Tensile stress at yield, 50 mm/min10–12 MPaASTM D638-14
    Elongation at break, 50 mm/min>700%ASTM D638-14
    Flexural modulus, 1% secant200–300 MPaASTM D790-17

    Because the resin is an LLDPE-based adhesive, its melt behaviour differs from unmodified LLDPE primarily in the presence of low-level grafted anhydride groups. At the tie-layer processing temperature of 210–250 °C, the anhydride functionality is thermally available for reaction with terminal amine groups in polyamide and hydroxyl groups in EVOH. The grafting level is kept low enough to preserve melt processability but high enough to raise short-term peel adhesion above the cohesive strength of LLDPE skins in typical five-layer structures. Peel testing is commonly conducted under ASTM F88-21; exact peel values depend on adjacent layer grades, tie-layer thickness, and die temperature, and published data for this specific configuration is limited.

    What Process Variables Govern Tie-Layer Melt Curtain Stability?

    Melt curtain stability in cast film coextrusion is controlled by the viscosity ratio between the tie layer and the adjacent LLDPE skin at the die lip. At 240 °C, Bynel® 4107 has a shear-thinning profile similar to LLDPE of 0.9–1.3 g/10 min melt flow rate, but the grafted species can raise die-pressure sensitivity when low processing temperatures are selected. A flat-to-slightly-rising extruder temperature profile from feed zone 160–180 °C to metering zone 220–240 °C is used to maintain melt temperature at 220–250 °C. Barrel cooling in the feed throat zone is maintained at 20–30 °C to prevent pellet bridging. Production-scale single-screw extruders with 30:1 L/D and barrier screws typically show melt pressure fluctuations of ±0.5–1.5 bar when melt temperature is controlled within ±2 °C. Die temperatures below 215 °C can produce thickness variation of more than ±2 µm across a 500 mm flat die, while sustained temperatures above 260 °C accelerate oxidative degradation of the anhydride graft.

    Screw selection for Bynel® 4107 differs from unmodified LLDPE in that low-work barrier screws with Maddock mixing sections are preferred on 24:1 to 30:1 L/D extruders. The melt is not pre-dried at storage relative humidity below 60%; surface moisture on cold pellets exposed to higher humidity is removed by an air-knife or desiccant hopper dryer at 60–70 °C for 2–4 h only when condensation is visible. Prolonged exposure to humid air hydrolyzes some anhydride grafts and reduces barrier adhesion. Edge trim and start-up film can be reclaimed into the tie layer at 20–30 wt% of the feed provided that the trim is dry and free of barrier layer contamination; higher reclaim percentages may alter melt viscosity and reduce peel strength.

    Chemical Structure of the Anhydride Graft on an LLDPE Backbone

    Maleic anhydride grafting onto an LLDPE backbone introduces succinic anhydride functions at low concentrations along the polymer chain. These polar moieties react with terminal amines in polyamide and with hydroxyl groups in EVOH during melt contact, forming covalent linkages and hydrogen bonds. Unmodified LLDPE fails at the tie-barrier interface with peel loads below 15 N/m in typical film configurations because it has no polar functionality. Bynel® 4107 is designed to shift failure to cohesive film tearing or substrate deformation. The degree of adhesion depends on contact time, melt temperature, and barrier-layer terminal group availability. For EVOH with 38 mol% ethylene content, a tie-layer thickness of 8–15 µm in a five-layer cast film is usually sufficient to avoid interfacial delamination when the interface melt temperature is held above 220 °C. Peel adhesion is assessed by ASTM F88-21 on coextruded films or by ASTM D1876-08(2015)e1 on pressed laminates; both methods require conditioning at 23 ± 2 °C and 50 ± 5% relative humidity for at least 40 h before testing.

    Relative to anhydride-modified LDPE tie resins, Bynel® 4107 exhibits higher melt tension and dart impact resistance in blown films, which permits thinner tie layers in freezer-to-microwave packaging. Relative to HDPE-based tie layers, the linear low-density backbone lowers flexural modulus and improves low-temperature interlayer adhesion to LLDPE skins. Bynel® 4107 is not a substitute for maleated polypropylene when the adjacent skin layer is polypropylene; the molecular compatibility with PP is insufficient at typical coextrusion temperatures. In applications requiring adhesion to unprimed aluminium foil, an anhydride-modified polyolefin may require corona or silane surface treatment of the foil; otherwise an acid copolymer resin or ionomer tie resin may perform more consistently under retort conditions. These differences arise from the carrier resin morphology rather than from a change in graft concentration.

    When Coextruded with Polyamide 6, Interfacial Temperature Differentials Require Calibration

    In a five-layer cast film structure of LLDPE/tie/PA6/tie/LLDPE, polyamide melt temperature is commonly set at 240–260 °C, while the tie layer is set at 215–240 °C. The lower tie-layer temperature preserves anhydride graft integrity but creates an interfacial temperature differential that can cause edge encapsulation if die land velocities differ by more than 1.5:1. Melt pumps and adjustable flex-lip die settings are used to keep the tie-layer thickness uniform within ±1 µm. On blown film lines with blow-up ratios of 2.0:1 to 2.5:1, bubble stability improves when the tie-layer frost line height is matched to the LLDPE skin frost line, because premature crystallization in the tie layer increases melt stiffness and produces gauge bands at the bubble edge. Coextrusion operators have observed that reducing the tie-layer die gap by 0.2–0.5 mm relative to the polyamide layer can compensate for the higher melt elasticity of the LLDPE carrier and reduce encapsulation defects on high-speed cast lines running above 150 m/min.

    Regulatory Status and Food-Contact Verification Matrix

    For food-contact use, Bynel® 4107 is commonly referenced under 21 CFR 175.105 for adhesives and may be used as a component of multilayer food packaging provided the finished structure meets the end-use limitations of that section. In the European Union, compliance must be evaluated under Regulation (EC) 1935/2004 and plastics-specific Regulation (EU) No 10/2011, including overall migration and specific migration limits for any reaction products. The migration behaviour is structure-dependent; therefore the current supplier food-contact statement must be obtained for the exact skin and barrier materials. The resin should not be used in direct contact with foods unless an appropriate functional barrier or authorised layer is present.

    Regulatory referenceRelevanceVerification requirement
    21 CFR 175.105Adhesive component in food packagingCurrent Bynel® food-contact certification for intended use
    Regulation (EU) No 10/2011Plastic materials in food contactOverall and specific migration testing on final laminate
    Regulation (EC) 1935/2004Framework for food-contact materialsDeclaration of compliance for the finished article
    EN 1186-1:2002Overall migration test methodLaboratory extraction per food simulant selected for the laminate

    Storage should be in sealed original bags at ambient temperature not exceeding 40 °C. The resin may be stored for 24 months from the date of production when kept dry; beyond this interval, rheological and adhesion properties should be re-verified. Incompatibilities include prolonged contact with amine-based masterbatches and certain high-nitrogen barrier coatings, which can consume grafted anhydride groups before the tie layer reaches the barrier interface. If coextruding with flame-retardant PA grades, brominated additives may require a polyolefin purge compound run at 180–220 °C to remove acidic residues. Do not weld or seal the tie layer as a monolayer food-contact surface. The maximum processing temperature should not exceed 260 °C for more than 10 min to limit gel formation and loss of adhesion. These operational boundaries are material limitations, not defects of the specific formulation.