| HS Code | 768561 |
| Density | 1.61 g/cc |
| Water Absorption | 0.30 % |
| Hardness Shore D | 90 |
| Tensile Strength Ultimate | 70.0 MPa |
| Elongation At Break | 1.5 % |
| Tensile Modulus | 9.00 GPa |
| Flexural Strength | 120 MPa |
| Flexural Modulus | 9.00 GPa |
| Heat Deflection Temperature | 260 °C |
| Glass Transition Temperature | 280 °C |
| Coefficient Of Thermal Expansion | 30.0 µm/m-°C |
| Thermal Conductivity | 0.50 W/m-K |
| Dielectric Strength | 15.0 kV/mm |
| Dielectric Constant | 4.00 |
| Color | White |
As an accredited DSM Somos PerFORM Reflect Stereolithography Polymer, UV Postcure factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | |
| Shipping | |
| Storage |
Competitive DSM Somos PerFORM Reflect Stereolithography Polymer, UV Postcure prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618136850665 or mail to admin@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618136850665
Email: admin@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
DSM Somos PerFORM Reflect Stereolithography Polymer, UV Postcure, is a ceramic-filled vat-photopolymerization material formulated for 355 nm laser stereolithography systems. The grade consists of a stiff acrylate-epoxy matrix with dispersed ceramic filler; this formulation raises cured density to approximately 1.6 g/cm³ and places the material in the high-modulus, low-elongation class of SL resins. The Reflect designation denotes an adjusted surface response intended for optical interrogation methods such as particle image velocimetry, fringe projection, and retroreflective model tracking. Because the ceramic filler shifts fracture behavior toward brittle failure, stress concentrations at support contact points, sharp corners, and threaded inserts require greater attention than in unfilled SL resins. The laser-scanning step alone yields green parts with incomplete acrylate conversion; a subsequent UV post-cure cycle is required before the thermal and mechanical properties become stable under load.
Mechanical design allowables should be derived from lot-specific tests, but manufacturer-published typical values provide an initial screening envelope. Specimens are normally built in a vertical orientation and UV-postcured according to the resin supplier’s schedule; deviation from the specified irradiation dose changes conversion and can lower the values shown below. Table 1 lists representative ranges for the UV-postcured state under conventional test methods.
| Property | Test Method | Representative Range After UV Post-Cure |
|---|---|---|
| Tensile modulus | ASTM D638-14 | 9,500–10,500 MPa |
| Tensile strength | ASTM D638-14 | 40–80 MPa |
| Elongation at break | ASTM D638-14 | 0.5–2.0% |
| Flexural modulus | ASTM D790-17 | 9,500–10,500 MPa |
| Flexural strength | ASTM D790-17 | 80–120 MPa |
| HDT at 0.46 MPa | ASTM D648-18 | 250–268 °C |
| HDT at 1.82 MPa | ASTM D648-18 | 220–240 °C |
Values in Table 1 are not design allowables; build orientation, post-cure chamber uniformity, and filler settling can produce several hundred MPa of modulus difference within the same lot. The low elongation at break means that conventional yield criteria do not apply; failure is brittle, and notched Izod results under ASTM D256 are generally below 30 J/m for ceramic-filled SL grades. Hardness after full post-cure is in the high Shore D range, typically above 85 when measured per ASTM D2240. Compression properties are less frequently published; design for compressive loading should be qualified with coupon tests because filler orientation and layer-plane porosity can reduce compressive strength in flat build directions. Published data for this specific configuration is limited for fatigue and long-term creep.
In vat operation, the resin behaves differently from unfilled low-viscosity grades. A processing temperature near 28–32 °C is often maintained because filler loading raises viscosity and lowers recoating speed. The process window is constrained on both sides: low temperature increases viscosity and recoating force, while high temperature accelerates dark polymerization in the vat. After idle periods, filler settling can produce a resin-rich surface layer that does not carry the intended mechanical stiffening; the supplier’s mixing sequence should be followed, but mixing must avoid air entrainment. Unverified high-shear mixing can generate microbubbles that appear as pits on the reflective surface and remain after UV post-cure. Laser penetration is reduced by the ceramic fraction, so working curve parameters and layer exposure values must be taken from the resin-specific datasheet rather than copied from unfilled SL recipes. Typical layer thickness is between 50 µm and 100 µm; thicker layers reduce build time but produce more pronounced stair-step lines on curved aerodynamic surfaces. Support tip geometry, bridge spacing, and part orientation need to reflect the resin’s brittle failure mode. Heavy cross-sections can crack during recoater contact if the support strategy is too sparse, while overly dense supports leave nibs that act as fracture initiation sites during removal. Production facilities running filled Somos grades observe accelerated recoater-blade edge wear compared with unfilled resins; a nicked edge or contaminated vat film produces visible drag lines that are not eliminated by post-cure.
Many unfilled stereolithography resins exhibit tensile modulus in the 2.5–3.2 GPa range, elongation at break above 5%, and HDT at 0.46 MPa below 120 °C. PerFORM Reflect shifts the envelope to a tensile modulus near 10 GPa and HDT at 0.46 MPa above 250 °C after full UV post-cure. This supports brief exposure to aerodynamic heating or tooling temperatures that would soften unfilled SL parts. The trade-off is the loss of ductility: ABS-like or elastomeric SL resins absorb demolding strain, whereas this material fractures at low strain. The coefficient of thermal expansion below the glass transition is on the order of 50 × 10⁻⁶ °C⁻¹; aluminum is near 23 × 10⁻⁶ °C⁻¹. In composite layup tooling, that CTE difference can produce thermal stress at the tool skin if heating and cooling cycles are rapid. Unfilled SL resins often show CTE values above 80 × 10⁻⁶ °C⁻¹ below the glass transition, so the filled ceramic system provides measurable dimensional stability improvement. Compared with the standard Somos PerFORM grade, the Reflect variant does not change the high-temperature stiffness class; the difference is the tuned optical surface behavior and filler-matrix morphology. The two grades should not be substituted without requalification of the optical measurement path. Against metal tooling, PerFORM Reflect has lower thermal conductivity and much lower fracture toughness than aluminum or steel. It is not appropriate for high-cycle injection mold cores subjected to repeated ejection loads; it is applied in short-run tooling, low-pressure molds, and sacrificial or proofing fixtures where the end-use thermal environment is more demanding than the mechanical load case.
Wind tunnel test models and high-temperature fixtures are the main use cases. In aerodynamic testing, the surface is evaluated under the specific illumination wavelength, camera angle, and exposure setting of the measurement system; the material is not a specular mirror and should not be specified as such. Thin-shell models with wall thickness below 1 mm can survive the thermal environment but are fragile during support removal and handling. Internal cavities should include drain holes to avoid residual liquid resin exotherming during the UV post-cure. In composite tooling, the material has been used for layup and cure tooling exposed to elevated temperatures; published data for this specific configuration is limited, so thermal cycling trials should be performed with the intended laminate schedule and bagging pressures. Threaded inserts and bushings require stress-relief bosses and generous fillets because the low elongation at break does not permit local plastic deformation around a press fit. Machining should be done with carbide or diamond tooling; generated dust from sanding or machining should be controlled as for any filled polymer dust. The reflective surface can be polished, but polishing removes the as-built skin and may alter the optical response; if the end-use qualification includes primer, paint, or pressure-sensitive paint, the coated surface should be tested rather than assuming the unpainted reflectance value remains valid.
Under-cured PerFORM Reflect may show a hard surface and a softer core if the UV-A chamber delivers insufficient dose or non-uniform irradiance. Because the matrix is a hybrid acrylate-epoxy system, residual acrylate groups and ongoing dark polymerization can continue after the part leaves the chamber. This means critical dimensions should not be accepted immediately after post-cure; conditioning for at least 24 h under controlled temperature is a reasonable control point. The post-cure chamber should be mapped with a radiometer calibrated in the 350–410 nm band. LED flood arrays in the 365–405 nm range provide stable irradiance but may require longer dose times; arc lamps add infrared heating that can distort thin sections. Broad-spectrum UV-A sources with significant output above 410 nm may not excite the photoinitiator efficiently and can cause thermal load without conversion. Oxygen inhibition at low irradiance in ambient air can produce a tacky surface layer and reduce reflectivity; nitrogen purging or higher-intensity UV-A lamps reduce this effect. Thick monolithic sections require periodic rotation or split-dose cycles because the low thermal conductivity of the ceramic-filled polymer traps exothermic heat. A single continuous high-dose exposure can drive internal temperature above the glass transition of the partially cured network and create residual stress. Process engineers can embed thermocouples in sacrificial blocks to establish a split-dose schedule rather than transferring a fixed time from another photopolymer. Under-cured cores can also be checked by sectioning a witness plate and measuring Shore D on the cut surface, not only on the exterior skin. Operational boundaries should include solvent restrictions: aggressive ketone wiping and amine-based mold releases can attack the acrylate-containing matrix and should be avoided unless compatibility is demonstrated. If a release agent is necessary, a grade validated for filled SL materials should be used, and the effect on post-cure conversion should be checked by hardness or extraction testing.
Dimensional stability in humid conditions is better than many unfilled SL resins, but precision wind tunnel models held to tolerances below 25 µm should be stored in a desiccated cabinet at 20–23 °C when not in test. The uncured liquid is a skin and eye irritant; handling requires nitrile gloves and local exhaust. Spills should be cleaned before exposure to sunlight or shop UV sources, which can initiate exothermic polymerization. Workshop lighting containing UV or blue-violet content can slowly skin the liquid in an open vat, so machine covers should remain closed. The resin’s filler content also increases wear on vat films and recoater blades; production facilities should log recoater-blade condition and vat haze after long runs. The material is not a drop-in replacement where impact toughness, high thermal conductivity, or high fracture strain is required. It is selected when the thermal and stiffness requirements of the part exceed the limits of unfilled SL resins and when the brittle failure mode can be accommodated by the design.