Dow Tuflin Hse 7002 Nt 7 Linear Low Density Polyethylene Resin

Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 312270
    Density 0.920 g/cm³
    Meltindex 0.70 g/10 min (190°C/2.16 kg)
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 34.5 MPa
    Elongationatbreak 700%
    Onepercentsecantmodulus 207 MPa
    Dartdropimpact 250 g
    Elmendorftearmd 300 g
    Elmendorfteartd 500 g
    Haze 12%
    Gloss45 50

    As an accredited Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow TUFLIN™ HSE-7002 NT 7 resin is packaged in 25 kg bags, 40 bags per pallet, totaling 1,000 kg.
    Container Loading (20′ FCL) 20′ FCL loading: Dow TUFLIN™ HSE-7002 NT 7 LLDPE resin, 25 kg bags, palletized, shrink-wrapped, securely braced for export shipment.
    Shipping Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin is shipped as a non-hazardous solid polymer in 25 kg bags, jumbo bags, octabins, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Keep containers closed, dry, and away from heat, ignition, and contamination. Handle carefully to prevent package damage and pellet loss.
    Storage Store Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and flames. Keep original bags or containers tightly closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Follow local regulations and the manufacturer’s SDS for safe storage, inventory rotation, and temperature limits.
    Shelf Life Shelf life: 24 months from manufacture when stored in original, unopened packaging under dry conditions below 50°C, away from direct sunlight.
    Application of Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin

    Which Cast Film Extrusion Variables Govern Pre-Stretch Retention at 250% Elongation?

    On power pre-stretch cast film lines designed for pallet unitization, the resin is processed in three- to five-layer co-extrusion configurations with die widths between 2000 mm and 3500 mm and die gaps of 0.6–1.2 mm. The extruder barrels typically maintain a 30:1 L/D ratio, and melt temperatures at the feedblock are held within 240–280°C. In a five-layer structure, the two outer plies incorporate 0.5–2.0 wt% polyisobutylene (PIB) cling agent and 0.3–1.0 wt% erucamide slip additive, while the core plies comprise 95–100 wt% HSE-7002 NT 7 with up to 5 wt% high-pressure LDPE (density 0.923 g/cm³, melt index 2.0 g/10 min at 190°C/2.16 kg per ISO 1133-1:2022) to stabilise bubble collapse and reduce neck-in at the chill roll. The cast film exits the die at 400–800 m/min and is quenched on a matte chrome chill roll held at 15–25°C; subsequent pre-stretching between driven rollers elongates the film by 200–350% before wrapping. The pre-stretch step is not annealed, so retained stretch force depends on molecular weight distribution and short-chain branch spacing. ASTM D5459-21, which measures machine-direction elastic recovery under cyclic loading, is used to assess residual holding force after a 250% elongation cycle. Compliance for this segment is anchored to ASTM D5748-19 (puncture propagation resistance), ASTM D882-18 (tensile properties of thin plastic sheeting), and ISO 527-3:2018, while the film gauge tolerances follow ISO 4593. The terminal product is a 500 mm wide, 17–23 μm thick machine-applied pallet wrap roll supplied on 76 mm cores, typically with unwind tension below 4 N.

    Representative five-layer formulation ranges for power pre-stretch cast film, not product specifications
    Layer PositionHSE-7002 NT 7 (wt%)LDPE (wt%)PIB (wt%)Erucamide (wt%)Function
    Outer ply (air side)95–980–20.5–1.50.3–0.8Cling delivery and controlled unwind
    Sub-skin98–1000–200Puncture and elongation reserve
    Core98–1000–200Structural integrity under stretch
    Sub-skin98–1000–200Symmetry balance
    Outer ply (chill roll side)95–980–20.5–1.50.3–0.8Secondary cling face

    On production lines where die gap misalignment exceeds 0.1 mm, edge bead thickness variation leads to gauge bands that propagate as weak spots during pre-stretch; operators monitor transverse thickness profiles with capacitance gauges and adjust die bolts to maintain a ±4% deviation per ISO 4593. Draw resonance in the stretch unit, observable as sinusoidal thickness oscillation, is suppressed by keeping the stretch roller gap below 15 mm and the draw ratio step increments below 10% per roller. Melt fracture on the outer plies, which appears as “sharkskin” at line speeds exceeding 600 m/min, is mitigated by adding 0.2–0.4 wt% fluoroelastomer processing aid to the skin layers; this additive does not affect the core layer’s stretch retention because the core remains free of PIB and slip additives. The pre-stretch ratio and retained force are interdependent: a higher ratio above 300% reduces film thickness per pass but lowers absolute holding force, so converters targeting 20 μm final gauge often operate at 250–280% pre-stretch with a residual force of 2.5–3.5 N per 25 mm width as measured by a calibrated film stretch test stand under 23°C/50% RH conditions.

    Hand-applied pallet wrap produced on single-layer cast lines requires a different balance of cling force and tear initiation resistance than power pre-stretch film. In this configuration, the resin is typically blended with 20–40 wt% high-pressure LDPE (e.g., density 0.923 g/cm³, melt index 2.0 g/10 min per ISO 1133-1:2022) to moderate cling and allow manual deployment without excessive unwind force. The addition ratio of HSE-7002 NT 7 ranges from 60 wt% to 80 wt%, with 0.3–1.0 wt% polyisobutylene (PIB) added as a cling agent depending on target unwind tension (measured per ASTM D5458-20). The blown or cast film is extruded at line speeds of 200–400 m/min through a 0.5–1.0 mm die gap and quenched on a chill roll maintained at 20–25°C; in cast hand wrap, the absence of pre-stretch means the film must supply inherent elongation at break of at least 400% as tested by ASTM D882-18. Regulatory requirements include REACH SVHC screening and FDA 21 CFR 177.1520(c) 3.1a for incidental food contact, although pallet wrap is not intended for direct food use. The terminal product is a hand-dispenser roll 300–500 mm wide, 12–18 μm thick, with a core diameter of 50 mm and a roll weight typically under 3 kg.

    Puncture-Resistant Heavy-Duty Sack Coextrusion Limits

    Coextruded blown film for heavy-duty sacks used in chemical and fertilizer packaging operates on three-layer dies with diameters between 200 mm and 400 mm, blow-up ratios of 2.5–3.5:1, and frost-line heights of 600–900 mm. The polymer blend in the outer plies comprises 50–70 wt% HSE-7002 NT 7 with 30–50 wt% high-density polyethylene (HDPE, density 0.954 g/cm³, melt index 0.3 g/10 min) to raise secant modulus and reduce creep under stacked load. The inner ply, which contacts filled product, typically contains 80–100 wt% HSE-7002 NT 7 with 0.2–0.4 wt% fluoroelastomer processing aid to suppress melt fracture at high throughput. Blown film extrusion requires melt temperatures of 200–230°C at the die, and the bubble is stabilised by an external cooling air ring with dual-orifice design; the film thickness profile is controlled by an automatic die bolt system with ±4% deviation per ISO 4593. Impact resistance is quantified by ASTM D1709-16a (Method A, dart impact at 66 cm drop height) with typical values for 100 μm tri-layer structures reported in industrial literature exceeding 800 g; however, published data for this specific resin blend configuration is limited. The sacks are subjected to REACH and OSHA hazard communication compliance, while the final products are 25 kg and 50 kg valve sacks with 55–65 μm sidewall thickness, designed for palletised transport.

    When Extrusion Coating Melt Temperatures Exceed 315°C, Bond Strength Depends on Oxidative Stability

    Extrusion coating of paperboard and aluminium foil structures for liquid packaging and flexible intermediate bulk containers uses the resin in blends with high-pressure LDPE to lower heat-seal initiation temperature and improve tear strength. In this process, HSE-7002 NT 7 is added at 20–50 wt% to a base of LDPE (density 0.915–0.918 g/cm³, melt index 4.0–8.0 g/10 min), and the blend is extruded through a T-slot die with a 0.5–0.8 mm die gap at melt temperatures of 310–330°C. At these temperatures, oxidative degradation of the hexene comonomer side chains can cause gel formation and neck-in instability; therefore, the extrusion screw must have a 28:1 L/D ratio with barrier mixing sections, and nitrogen blanketing of the hopper is recommended when line stops exceed 5 minutes. The substrate, typically 40–60 g/m² kraft paper or 9–12 μm aluminium foil, receives a corona treatment of 38–42 dyne/cm immediately before the coating nip. Peel bond strength is tested per ASTM F904-16, and heat-seal strength per ASTM F88/F88M-21. Food contact compliance is verified under FDA 21 CFR 177.1520(c) 3.1a and EU Regulation No 10/2011 with overall migration limits below 10 mg/dm². The terminal products include 250 mL to 1000 mL liquid packaging board cartons and foil-laminated sachets for dry beverages.

    For agricultural silage bale wrapping, the five-layer cast film process imposes specific constraints on UV stabilization and opacity control that do not apply to pallet wrap. Formulations for this end use typically combine 70–90 wt% HSE-7002 NT 7 with 5–15 wt% ethylene-vinyl acetate (EVA, 18% vinyl acetate content) and 1–3 wt% carbon black masterbatch (40% loading). The EVA fraction modulates elongation at break and tear propagation resistance, while carbon black provides UV screening sufficient for 12-month outdoor storage in agricultural conditions. The five-layer cast film is produced with a die gap of 0.7–1.0 mm, line speeds of 250–450 m/min, and chill roll temperatures of 18–22°C; each outer layer thickness is 2–3 μm, while the core layers carry the bulk of the 20–25 μm total gauge. Compliance is assessed under EN 13207:2018 (thermoplastic silage films), ASTM D5748-19 for puncture resistance, and ISO 4892-2:2013 for accelerated weathering. The finished roll, typically 500 mm or 750 mm wide with a 76 mm core, is used in round bale wrappers at a minimum stretch ratio of 50% (6–8 revolutions per bale).

    Compliance matrix for agricultural silage stretch film based on HSE-7002 NT 7 formulations
    StandardScopeTest ParametersRelevance
    EN 13207:2018Thermoplastic silage filmsMechanical properties, UV resistance, oxygen permeabilityMinimum 12 months outdoor storage integrity
    ASTM D5748-19Puncture propagation resistanceProbe penetration at 250 mm/minResistance to stalk and stone puncture
    ISO 4892-2:2013Accelerated weathering (xenon arc)Exposure cycles, irradiance 0.35 W/m² at 340 nmRetention of elongation at break after UV aging
    FDA 21 CFR 177.1520(c) 3.1aOlefin polymers for food contactExtraction limits per specific migrationNot primary contact; incidental contact only

    Reducing Haze Below 3% in Food Contact Cast Film Through Chill Roll Temperature Management

    To achieve haze below 3% at 25 μm in food contact cast film, the cooling dynamics and additive package must be tightly controlled. The cast line for bakery and produce packaging operates with a 0.5–0.7 mm die gap, melt temperature of 230–250°C, and a polished chrome chill roll at 18–20°C to control cooling rate and minimize haze. HSE-7002 NT 7 is used at 90–100 wt% with 500–1000 ppm erucamide slip and 1000–3000 ppm synthetic silica antiblock; the slip agent migrates to the film surface over 24–72 hours post-extrusion, reducing coefficient of friction without causing visible bloom if the addition is kept below 1200 ppm. Optical properties are tested per ASTM D1003-21, coefficient of friction per ASTM D1894-14, and tensile strength per ISO 527-3:2018. Food contact status relies on FDA 21 CFR 177.1520(c) 3.1a and EU No 10/2011, with specific migration of erucamide monitored according to the overall migration limit of 10 mg/dm². The terminal product is a 300–450 mm wide film roll, 12–15 μm thick, suitable for automatic flow-pack wrapping of bread and other bakery goods.

    Free Quote

    Competitive Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow TUFLIN™ HSE-7002 NT 7 Linear Low Density Polyethylene Resin is an ethylene/1-octene linear low-density polyethylene produced by a solution polymerization route and supplied in pellet form. The material is specified for cast stretch film, lamination webs, and multilayer film structures requiring high draw-down stability and high tear resistance. Melt flow rate is 2.0 g/10 min at 190 °C under a 2.16 kg load when measured according to ISO 1133-1:2022, and density is 0.917 g/cm³ when measured according to ISO 1183-1:2020. The NT 7 suffix identifies the manufacturer’s additive formulation. Because additive loading affects coefficient of friction and blocking in thin films, the certificate of analysis for each shipped lot should be reviewed before setting corona treatment, winding, or slitting parameters. In three-layer cast pallet wrap, HSE-7002 NT 7 is most often evaluated as the core layer resin, although it may also be used in skin layers when optical and seal performance are managed through the additive package.

    The product differs from general-purpose butene-based LLDPE grades in the distribution of short-chain branches. The octene comonomer introduces C6 branches that are more effective than the C2 branches from butene at generating interlamellar tie molecules. This produces higher tear propagation resistance and dart impact at equal density. The comparison is not absolute because film properties are also controlled by die lip gap, quench temperature, frost line height in blown film, and additive dispersion. Published data for this specific configuration is limited; therefore, converter validation should include a head-to-head film trial on the intended production line.

    What Distinguishes Octene-Based Short-Chain Branching from Butene-Based LLDPE in Tear and Puncture Response?

    The resin’s density of 0.917 g/cm³ and melt flow rate of 2.0 g/10 min define a processing window that balances melt stability and draw-down. At this density, lamellar thickness remains low enough to permit high elongation at break, while molecular weight distribution is controlled to avoid excessive low-molecular-weight extraction and plate-out. In film evaluation, Elmendorf tear is measured under ASTM D1922-15 and Dart drop impact is measured under ASTM D1709-16a. The octene-based resin shows higher transverse-direction Elmendorf tear than a comparable butene-based LLDPE because the longer hexyl branches create a more interconnected amorphous interlayer. The improvement is most apparent at 20 µm gauge and below, where residual stress and heat history differ significantly from heavier-gauge film.

    Compared with metallocene ethylene-octene plastomers of density 0.900–0.905 g/cm³, HSE-7002 NT 7 retains higher crystallinity and therefore higher film modulus and lower blocking tendency. It is not designed to replace ultra-low-density peel films, but it can serve as a stiff core layer in a five-layer stretch structure. Compared with a general-purpose butene LLDPE of similar melt flow rate and density, the product is typically selected when downgauging and pallet puncture resistance outweigh the need for the lowest possible melt temperature. The octene-based architecture also modifies hot-tack and seal initiation under ASTM F1921, but the exact seal window depends on skin layer chemistry and corona treatment history.

    On high-output cast film lines, the resin is processed through extruders with 75–105 mm diameter screws. Barrels with L/D ratios of 30:1 to 36:1 and barrier sections are preferred for stable output. Zone set points of 190–240 °C from feed to metering are typical starting conditions; the adaptor is set at 240–250 °C, and the flat die is set at 245–260 °C. The melt temperature at the die entrance should be maintained below 270 °C to avoid thermal degradation. Higher temperatures, especially above 280 °C, increase the likelihood of oxidized gels and may reduce film tear performance. A chill roll temperature of 18–25 °C and a die gap of 0.50–0.65 mm are typical for thin cast web; line speed is limited by edge stability and air knife geometry rather than by resin melt strength.

    Polyethylene does not require drying at normal warehouse relative humidity below 60 %. Condensation on cold pellets transferred into a warm mixing area is a separate issue; hopper bridging, extruder surging, and film defects can result from surface moisture. Pellets should be conditioned to ambient temperature in sealed containers before use. The resin is incompatible with strong oxidizing agents and should not be held at melt temperatures above 280 °C for prolonged periods. Avoid blending with reactive peroxide masterbatches, as uncontrolled chain scission or crosslinking can alter viscosity and film aesthetics.

    When Downgauging Below 12 µm on Three-Layer Cast Stretch Lines

    At thicknesses below 12 µm, the failure mode of cast pallet wrap changes from gross yielding to puncture, tear propagation, and localized thin bands. On a three-layer line, capacitance thickness gauges with a tolerance of ±0.5 µm are required to control edge beads. Edge bead thickness of more than 2–3 µm above web center creates hard rolls and telescoping. Web tension values of 0.5–0.8 N/mm are used for 10 µm film on many cast lines, but the value must be adjusted as roll diameter and line speed change.

    Draw resonance typically appears as cyclic thickness variation at 2–10 Hz. It is reduced by increasing air knife velocity or shortening draw distance; excessive air knife pressure causes surface chatter. The molecular architecture of the solution LLDPE contributes to low gel counts, but gels become visually apparent at 10 µm and below. In high-clarity laminations, continuous camera-based film inspection systems with pixel resolution better than 0.05 mm are used to quantify gel counts; users should establish lot-specific acceptance limits because gel data are strongly affected by magnifier sensitivity and film lighting. Puncture resistance is evaluated with an instrumented low-rate puncture fixture, while tensile elongation and stress at break are measured under ASTM D882-18.

    Compared with butene-based core layer resins, the octene backbone of HSE-7002 NT 7 allows more aggressive downgauging before shelf-life puncture failures occur. However, the actual downgauging ceiling is determined by pallet protrusion, load stability, and film cling. The resin itself does not guarantee a specific gauge without considering the full film structure. When used in skin layers, corona treatment levels above 38–42 mN/m may be necessary to maintain ink adhesion, but excessive oxidation of the surface can increase coefficient of friction and blocking.

    Regulatory Status and Migration Controls for Food-Contact Structures

    Compliance for food-contact use is determined on the finished article, not solely on the resin. The olefin polymer base resin may be evaluated under 21 CFR 177.1520 for uses permitted therein; compliance depends on polymer type, density, and extraction limits. For European Union applications, migration testing under EU 10/2011/EC is required with an overall migration limit of 10 mg/dm². The test conditions must match the intended contact time and temperature. REACH registration obligations apply to the substance or mixture as supplied; the safety data sheet should list stabilizers and processing aids. Packaging is not within the core scope of 2011/65/EU RoHS unless specific electrical and electronic equipment requirements are triggered by the customer. The converter must separately evaluate any downstream addition of cling agents, slip additives, or low-molecular-weight processing aids for migration compliance.

    Regulatory compliance checklist for base resin and finished articles
    RegulationApplicable test or clauseCondition
    US FDA food contact21 CFR 177.1520Finished article must meet extraction limits and end-use conditions
    EU food contactEU 10/2011/ECOverall migration limit 10 mg/dm²; specific migration limits may apply to additives
    REACHRegulation (EC) No 1907/2006Substance or mixture registration; safety data sheet documentation
    RoHS2011/65/EUNot normally applicable to packaging; verify if product is used as part of electrical and electronic equipment
    GHS classificationRegulation (EC) No 1272/2008Verify current safety data sheet for pellet classification and handling

    Melt Flow Rate and Film-Gauge Optical Measurements Establish the QC Envelope

    Incoming resin QC should measure melt flow rate and density on each lot using ISO 1133-1:2022 and ISO 1183-1:2020. Film trials are typically reported at 20 µm gauge on a cast line because thickness influences all mechanical and optical results. The following table lists representative values; they are not specification limits and should not be used for lot acceptance without the manufacturer’s certificate of analysis.

    Representative physical property profile for Dow TUFLIN™ HSE-7002 NT 7 LLDPE resin and 20 µm cast film
    PropertyTest standardRepresentative value
    Melt flow rate, 190 °C/2.16 kgISO 1133-1:20222.0 g/10 min
    DensityISO 1183-1:20200.917 g/cm³
    Peak melting temperature, DSCISO 11357-3:2018122 °C
    Vicat softening temperature, A50ISO 306:202298 °C
    Secant modulus 1% MD/TDASTM D882-18120 MPa / 130 MPa
    Tensile strength at break MD/TDASTM D882-1844 MPa / 31 MPa
    Elongation at break MD/TDASTM D882-18480% / 620%
    Elmendorf tear MD/TDASTM D1922-15210 gf / 360 gf
    Dart drop impact, F50ASTM D1709-16a180 g
    HazeASTM D1003-132.0%
    Gloss at 45°ASTM D2457-1387