Dow Tuflin Hse 1003 Nt 7 Linear Low Density Polyethylene Resin

Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 806671
    Density 0.920 g/cm³
    Melt Index 1.0 g/10 min
    Melting Temperature 124 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 700%
    Flexural Modulus 276 MPa
    Dart Impact Strength 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 400 g
    Haze 10%
    Gloss 60
    Coefficient Of Friction 0.2

    As an accredited Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Supplied in 25 kg polyethylene-lined bags, palletized with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with non-hazardous Dow TUFLIN™ HSE-1003 NT 7 LLDPE resin in 25 kg bags, palletized and secured.
    Shipping Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin ships as non-hazardous solid pellets. Typical packaging includes 25 kg bags, octabins, or bulk trucks/railcars. It is not DOT/IMDG/IATA regulated. Store dry, clean, away from heat, moisture, and contaminants. Handle to avoid bag damage and dust generation.
    Storage Store Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated warehouse. Keep original containers closed, off the floor, and away from direct sunlight, heat, ignition sources, moisture, dust, and oxidizing agents. Avoid prolonged UV exposure and excessive stacking. Maintain moderate temperatures, use first-in, first-out stock rotation, and follow local regulations and SDS recommendations.
    Shelf Life Typically 24 months from date of manufacture if stored unopened in a cool, dry place, protected from direct sunlight and moisture.
    Application of Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin

    For three-layer agricultural silage wrap and bale sheeting produced from Dow TUFLIN HSE-1003 NT 7, the extrusion line is typically configured with a 65 mm single-screw extruder using a barrier screw of L/D 24:1–30:1, a 200 mm spiral mandrel die, and a die gap of 1.6–2.0 mm. The resin has a melt index of 1.0 g/10 min per ASTM D1238-20 and a density of 0.918 g/cm³ per ASTM D792-20. Melt temperature at the die lip is controlled between 195°C and 215°C. A blow-up ratio of 2.2:1–2.8:1 and frost line height of 5–8 die diameters are set to balance MD/TD tear anisotropy in the finished 25–50 µm film.

    Black silage formulation requires a carbon black masterbatch at 2.0–3.0 wt% and a HALS concentrate at 0.8–1.5 wt% because the resin does not contain sufficient UV stabilizer for multi-month field exposure. Dispersion of the masterbatch is a process-critical variable; inadequate distributive mixing produces film defects that act as tear initiators under bale wrapping tension. Tensile break strength of a 25 µm monolayer film typically exceeds 30 MPa in MD and 25 MPa in TD when measured per ASTM D882-18. Elongation at break is generally above 600% in both directions. Dart impact measured per ASTM D1709-22 is typically above 150 g at 25 µm. Elmendorf tear measured per ASTM D1922-23 is typically above 200 g MD and 500 g TD at the same gauge.

    Water absorption measured per ASTM D570-22 is below 0.01%, so drying is not normally required. Resin stored below 10°C and transferred into a warmer extrusion area should be allowed to reach ambient temperature before rotation into the feed hopper to avoid condensation on pellets. Published data for the full three-layer silage structure is limited; individual line-specific qualification under actual UV exposure and bale tension is required because field performance depends on masterbatch quality, film gauge, and sealing layer formulation. The resin should not be considered a direct replacement for UV-stabilized silage film grades without confirmatory weathering data.

    How Blown Film Bubble Stability Responds to Die Pressure and Melt Elasticity

    Heavy-duty liner and shipping sack film at 75–150 µm gauge uses HSE-1003 NT 7 as the primary toughness component. Bubble stability in this gauge range is sensitive to die pressure and melt elasticity because thicker films retain more heat in the collapsing frame and respond slowly to air-ring changes. On a 75 mm grooved-feed extruder with L/D 30:1 and a 300 mm spiral mandrel die with 1.8–2.4 mm die gap, die pressure is controlled in the 25–38 MPa band at 210°C melt temperature. The use of a low-shear spiral mandrel die instead of a center-fed spider die reduces melt fracture and improves gauge uniformity. If die pressure falls below 20 MPa, output rate is usually too low to justify the line speed; if die pressure exceeds 40 MPa, melt temperature at the die exit can rise above the recommended 230°C ceiling and degrade the slip package.

    Blends with HDPE or LDPE are used to modify bubble stiffness and end-use modulus. HDPE addition at 10–20 wt% increases modulus and reduces TD tear; plant trials commonly show that 20 wt% HDPE lowers Elmendorf tear TD by approximately 30% relative to a 100% HSE-1003 NT 7 control when measured per ASTM D1922-23. For sack film that must retain TD tear above 400 g at 100 µm, the HDPE content is usually limited to 15 wt% unless a downgauged structure is qualified. Dart impact per ASTM D1709-22 for unmixed 100 µm LLDPE film typically exceeds 400 g, but the exact value depends on blow-up ratio, frost line height, and web tension in the collapsing frame.

    On production-scale lines, gauge variation across the web is held below ±15% by using a dual-lip air ring and internal bubble cooling when available. Moisture on pellets from cold storage must be avoided because wet resin can create surface splay on the thick film. Published data for specific HDPE/LLDPE blend ratios in heavy-duty sacks is limited; each converter should determine the blend window by running a designed experiment with dart impact and Elmendorf tear as response variables per the cited ASTM methods.

    Because frozen-food form-fill-seal lines require a sealant layer that maintains seal integrity under low-temperature flexing, coextruded webs place HSE-1003 NT 7 in the 15–30 µm sealant layer. Seal strength is tested per ASTM F88/F88M-21. A seal-bar temperature of 110–115°C, dwell of 0.5 s, and jaw pressure of 0.30 MPa typically produce seal strength above 4 N/15 mm for a 20 µm sealant layer. Hot-tack performance is measured per ASTM F1921-18; the test should be run on the full coextruded structure because the outer layers affect heat transfer to the seal interface.

    Regulatory frameworkCitationTest conditionRequirement
    United States FDA21 CFR 177.1520(c) 3.1aOlefin polymer for food contactCompliant when used in accordance with GMP and intended for aqueous, acidic, alcoholic, and fatty foods
    European UnionRegulation (EU) No 10/2011Overall migration per EN 1186-1 and EN 1186-310 mg/dm² total migration
    European UnionRegulation (EU) No 10/2011Specific migration for additives used in formulationMust be verified for the final film because the base resin alone does not cover masterbatch-derived additives
    United States FDA21 CFR 177.1520(b)Granule or film extractionUse conditions and food types defined in 21 CFR 176.170(c)

    For aqueous foods, migration testing uses 10% ethanol; for acidic foods, 3% acetic acid; for fatty foods, 95% ethanol or isooctane under Regulation (EU) No 10/2011. The resin is not recommended as a retortable sealant layer above 100°C unless the complete laminate is tested for seal creep and seal-strength loss. Regrind addition above 20 wt% should be evaluated for gel formation and heat-seal consistency because repeated extrusion can consume the stabilizer package and increase oxidation products.

    If Under-Slab Vapor Retarder Specifications Call for Class A Permeance

    If under-slab vapor retarder specifications call for Class A permeance, HSE-1003 NT 7 is processed at 250–500 µm thickness. Blown film lines used for this gauge range typically run a 75–90 mm single-screw extruder with a barrier screw and a 300–350 mm die. Blow-up ratio is kept at 1.8:1–2.0:1 because lower BUR favors the MD tensile and puncture values required by concrete placement. Water vapor permeance is measured by the desiccant method at 23°C per ASTM E96/E96M-21; a 300 µm monolayer generally falls below 0.3 perm, which is within ASTM E1745 Class A requirements for polyethylene vapor retarders. Puncture resistance per ASTM E154/E154M-18 at 300 µm typically exceeds 200 N in production samples.

    Installation over sharp aggregate remains a field failure mode not fully predicted by laboratory puncture values. The membrane must be placed over compacted, smooth fill or a geotextile cushion if aggregate is present. Seaming is performed with polyolefin-compatible sealant tape or heat welding; seam overlap should be a minimum of 150 mm per project specification. The resin has low moisture absorption, but if stored in high-humidity conditions at RH > 60%, pellet surfaces may retain condensation and should be dried or surface-dried before extrusion to avoid splay. Radon diffusion resistance for polyethylene film increases with thickness; at 250–500 µm the membrane provides a diffusion barrier, but project requirements for radon control are governed by ANSI/AARST RMS-2018 or local code and must be verified with the final film structure.

    Published data for this specific monolayer configuration in radon service is limited. The mechanical values cited are typical for LLDPE film of this density and gauge but should not replace project-specific test reports.

    In pallet unitization lines where stretch hood equipment pre-stretches film by 55–70%, film produced from HSE-1003 NT 7 is run at 50–80 µm gauge on a blown film line using a 70 mm barrier screw and a 250 mm die with 2.0–2.4 mm die gap. A blow-up ratio of 2.5:1–3.0:1 is maintained to raise TD elongation and reduce corner puncture failures. Tensile yield strength at 25 µm is near 10 MPa per ASTM D882-18. Elongation at break is above 600% per ASTM D882-18, which accommodates the corner stretch cycle without film rupture. Dart impact per ASTM D1709-22 at 25 µm is typically above 150 g.

    Gel count is measured per ASTM D3596-23; the target threshold is set by the pre-stretch ratio because contaminant gels form pinholes at high pre-stretch ratios and cause load collapse during transport. The film web is corona-treated on the external layer to 38–42 dyn/cm per ASTM D2578-23 for print or anti-slip coating adhesion. Coefficient of friction is measured per ASTM D1894-23; slip packages are adjusted to maintain a COF between 0.20 and 0.40 on the outer surface. If the film is used as a replacement for shrink hood, the processor must verify holding force recovery after the stretching cycle because LLDPE does not shrink and the load is secured by elastic recovery.

    Water absorption measured per ASTM D570-22 is below 0.01%, so no pre-drying is required for resin stored in dry ambient conditions. Published data for HSE-1003 NT 7 in stretch hood film is limited; line-specific field trials under the actual pallet wrapping machine stretch ratio are required to set final gauge and slip targets.

    Edge-Tear Resistance in Coextruded Mailer Film Tracks LLDPE Skin Orientation

    Edge-tear resistance in coextruded e-commerce mailer film tracks LLDPE skin orientation and total gauge. A typical mailer film at 60–90 µm total gauge places HSE-1003 NT 7 in the two outer skin layers with an HDPE or HDPE-rich core for stiffness. Elmendorf tear TD at 75 µm total thickness is typically above 500 g when tested per ASTM D1922-23, with MD tear above 200 g. The blow-up ratio of 2.0:1–2.5:1 shifts tear resistance toward the TD direction, which is critical for edge-tear resistance in mailer fabrication. Maximum tensile strength in MD is typically above 30 MPa and TD above 25 MPa at 25 µm when measured per ASTM D882-18.

    Surface treatment is applied at 38–42 dyn/cm per ASTM D2578-23 to prepare the skin layer for flexographic printing. Coefficient of friction is controlled in the 0.20–0.40 range per ASTM D1894-23 to permit automated mailer line feeding. If low noise is specified, the core layer formulation and skin thickness must be adjusted; the LLDPE skin has a higher flex-crack resistance than brittle HDPE-rich films, but published data for this exact coextruded structure is limited. Processors should not substitute HDPE skins without evaluating edge-tear and drop performance per ASTM D1922-23 and ASTM D1709-22.

    Processing limits include a melt temperature ceiling of 230°C to avoid slip additive degradation and gel formation. Regrind use above 20 wt% should be evaluated for coefficient of friction shifts and odor in the final mailer.

    Free Quote

    Competitive Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow TUFLIN™ HSE-1003 NT 7 Linear Low Density Polyethylene Resin is a solution-polymerized ethylene-octene copolymer supplied as natural pellets for extrusion coating, lamination, and cast film applications. The product is defined by a melt index of 7.0 g/10 min when tested at 190 °C under a 2.16 kg load in accordance with ASTM D1238 and a density of 0.918 g/cm³ in accordance with ASTM D792. These two values establish the processing window for commercial coating lines: the melt index lowers extruder head pressure and supports thin-gauge drawdown at high line speed, while the density maintains sealant flexibility without introducing the stiffness typical of high-density polyethylene.

    The designation HSE-1003 identifies a high-speed extrusion grade within the Dow TUFLIN™ line. The suffix NT 7 denotes a natural pellet product form. The resin is not formulated with intentionally added slip or antiblock additives; downstream operations that require coefficient-of-friction control must introduce masterbatch or compounded additives under separate validation.

    What Property Profile Distinguishes HSE-1003 NT 7 from High-Pressure LDPE Coating Resins?

    Conventional high-pressure LDPE coating resins of similar melt index possess long-chain branching that produces strain hardening and low neck-in on a coat-hanger die. HSE-1003 NT 7 is linear and lacks significant long-chain branching. The short-chain octene branches disrupt crystallinity enough to achieve the 0.918 g/cm³ density, but they do not create the extensional-thickening behavior that stabilizes LDPE at high draw-down ratios. A processor moving from LDPE to this LLDPE must therefore adjust deckle settings, reduce air gap, or blend with high-pressure LDPE to maintain equivalent web width.

    Rheologically, the 7.0 g/10 min melt index corresponds to a lower melt viscosity than a 2.0 g/10 min LLDPE film resin, but the zero-shear viscosity of a linear resin remains higher than that of an LDPE of identical melt index at low shear rates. In a 90 mm single-screw extruder with a barrier screw and L/D 30:1, the practical consequence is lower screw speed for the same throughput than with high-pressure LDPE, although excessive head pressure is not typically observed at melt temperatures above 290 °C. Published data for this specific configuration is limited; processors should verify screw design and torque requirements with the extruder manufacturer.

    Thermally, the melting peak of the resin is near 124 °C by differential scanning calorimetry, compared with approximately 110 °C for many high-pressure LDPE coating grades. This difference raises the heat-seal initiation temperature but improves resistance to hot-tack failure on warm substrates. The seal window should be mapped on the intended packaging line using heat-seal test methods such as ASTM F1921 or ASTM F2029, because seal bar pressure and dwell time interact with the melting range.

    Typical values used for grade selection are summarized in the following table. These values are manufacturer-reported and should not be interpreted as batch release specifications.

    Typical Physical Properties
    PropertyTest methodTypical value
    Melt indexASTM D1238 / ISO 1133-1:20227.0 g/10 min (190 °C, 2.16 kg)
    DensityASTM D792 / ISO 1183-1:20190.918 g/cm³
    Melting peakISO 11357-3:2018124 °C

    When Draw-Down Ratios Exceed 100:1 on Coextrusion Lines

    On a coextrusion coating line fitted with a 120 mm barrier-screw extruder and an automatic die with a lip gap of 0.5 mm to 0.8 mm, draw-down ratios above 100:1 can induce draw resonance when the melt temperature at the adapter is below 290 °C or the air gap is greater than 250 mm. Because the linear architecture of HSE-1003 NT 7 provides less strain hardening than LDPE, the web is more sensitive to periodic variation in extruder output. Operators typically narrow the deckle to 5 mm to 10 mm inside the substrate edge and increase chill-roll speed in steps while monitoring coat-weight variation by beta-gauge scanning.

    In multi-layer structures, the melt index of the skin layer affects interfacial stability. A low-viscosity 7.0 g/10 min stream adjacent to a high-viscosity barrier resin can create wavy interfaces if the viscosity ratio exceeds 4:1. Processors avoid this by matching the temperature of adjacent extruders or by placing the HSE-1003 NT 7 layer against the substrate rather than against a high-viscosity tie resin. These conditions are line-specific; published data for this specific configuration is limited.

    In extrusion lamination of aluminum foil or metallized film, adhesion depends on melt oxidation. At a melt temperature of 300 °C to 315 °C, the surface of the molten web oxidizes rapidly in the air gap, creating polar carbonyl species that wet the foil. The air gap is therefore not simply a neck-in control parameter; it also controls the extent of oxidation. An air gap shorter than 150 mm may reduce oxidation enough to lower peel strength, while an air gap longer than 250 mm may over-oxidize the melt and generate pinholes from low-molecular-weight debris on the chill roll. T-peel adhesion of the laminate is evaluated under ASTM D1876 using conditioned substrates.

    The chill-roll finish and temperature define the sealed surface gloss and blocking behavior. A polished roll maintained at 15 °C to 25 °C is typical for high-speed coating, with a water circulation system sized to remove heat fast enough to prevent roll release defects. Because HSE-1003 NT 7 contains no antiblock, blocking can occur on warm rolls or in rewind if the laminate is wound above 35 °C.

    Regulatory Compliance and Food Contact Matrix

    The resin is used in food packaging only if the converting plant validates the finished article under the applicable framework. Compliance is defined at the article level, not by resin certification alone. The following matrix summarizes the relevant regulatory references.

    Regulatory References for Polyethylene Food Contact
    FrameworkCitationRelevant condition
    U.S. FDA olefin polymers21 CFR 177.1520(c)(3.2a)Complies as an olefin polymer when extraction limits are met
    EU plastic food contactCommission Regulation (EU) No 10/2011Overall migration limit 10 mg/dm² for plastic multilayers
    REACHRegulation (EC) No 1907/2006Polymer exempt from registration; monomer registration required
    RoHSDirective 2011/65/EUNo restricted substances intentionally added

    Polyethylene Homopolymer Blending Alters Neck-In and Seal Initiation

    The addition of 10 wt% to 30 wt% high-pressure LDPE restores strain hardening at the die exit and reduces neck-in, but it also lowers the melting peak and shifts the seal initiation temperature downward. The exact blend response depends on the LDPE grade and its long-chain branching content; a high-clarity autoclave LDPE produces a different draw-down limit than a tubular LDPE of identical melt index. Because published data for this specific resin blend is limited, line trials should vary LDPE addition in 5 wt% increments while recording deckle width, web width, coat weight, and motor current.

    Compared with DOWLEX™ film-grade LLDPE of 0.918 g/cm³ density and 1.0 g/10 min melt index, the 7.0 g/10 min melt index of HSE-1003 NT 7 reduces head pressure and permits lower coat weights without raising melt temperature. The lower molecular weight reduces unsupported film toughness; dart impact strength under ASTM D1709 is lower than that of a 1.0 g/10 min film resin, and tear resistance in the transverse direction is reduced when the coating is highly oriented in the machine direction.

    Relative to metallocene-catalyzed LLDPE grades with similar density, HSE-1003 NT 7 may exhibit a broader molecular weight distribution and lower film clarity. That broader distribution reduces melt fracture at high screw speeds and improves single-screw motor stability, but it also lowers dart impact and can increase haze in unsupported cast film. The product is not designed as a high-clarity shrink film resin; converters requiring optical clarity should evaluate a metallocene LLDPE or a high-pressure LDPE blend.

    Because the resin is supplied without slip or antiblock, the dynamic coefficient of friction of the final film or coating is controlled entirely by downstream additives. If no masterbatch is used, blocking can occur in roll form at temperatures above 35 °C or at high winding tension. Addition of a silica antiblock masterbatch at 0.5 wt% to 2.0 wt% is common in cast film, but the food-contact status of the masterbatch must be verified separately.

    Storage Boundaries Under High Humidity and Re-Extrusion

    Pellets do not require drying for moisture removal. Surface condensation can develop if bags are opened in warm, humid conditions and then held in a cooler area; a relative humidity above 60% during bag opening is a practical threshold. If condensation is visible, the pellets can be dried at 60 °C to 80 °C for 2 h to 4 h in a desiccant or hot-air dryer with a dew point below -20 °C. Drying beyond 4 h provides no measurable benefit and can oxidize the pellet surface if oxygen is not excluded.

    Re-extrusion of edge trim and start-up scrap is possible up to 20 wt% if the trim is clean, dry, and free of slip or antiblock additives. Higher recycle levels reduce draw-down stability because oxidative degradation during the first pass shortens chains and lowers melt viscosity. Avoid combining HSE-1003 NT 7 with PVC decomposition products, ionomer melt streams, or amine-based antifog additives without trial validation; these species can destabilize the melt or shift heat-seal performance. For continuous service above 60 °C, oxidative stabilization must be confirmed on the finished article because the base resin is not formulated for high-temperature engineering applications.

    Top