    Specifications
    HS Code 820685
    Density 0.918 g/cm³
    Melt Index 0.80 g/10 min
    Melt Flow Ratio 30
    Tensile Strength At Break Md 6000 psi
    Tensile Strength At Break Td 5000 psi
    Tensile Strength At Yield Md 1500 psi
    Tensile Strength At Yield Td 1500 psi
    Elongation At Break Md 700%
    Elongation At Break Td 800%
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 12%
    Gloss 45 55%
    Melting Point 124°C
    Vicat Softening Point 100°C
    Brittleness Temperature < -70°C

    As an accredited Dow Tuflin™ HS-7098F NT 7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Tuflin™ HS-7098F NT 7 LLDPE is supplied in 25 kg polyethylene bags, palletized and wrapped for industrial shipping.
    Container Loading (20′ FCL) 20′ FCL container loading: palletized 25 kg bags of Dow Tuflin™ HS-7098F NT 7 LLDPE; approx. 18–20 metric tons.
    Shipping Dow Tuflin™ HS-7098F NT 7 LLDPE is shipped as non-hazardous solid pellets, typically in 25 kg bags or bulk containers. It requires dry, covered transport, protected from moisture, heat, and contamination. Not DOT/IMDG/IATA regulated. Follow SDS and local transport rules.
    Storage Store Dow Tuflin™ HS-7098F NT 7 LLDPE in a cool, dry, well-ventilated warehouse away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep bags or containers sealed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure. Use first-in, first-out rotation. Store at moderate temperatures and protect from physical damage. No special ventilation is normally required, but avoid inhaling dust.
    Shelf Life Shelf life is 24 months from date of manufacture when stored in original packaging in a cool, dry, well-ventilated area.
    Application of Dow Tuflin™ HS-7098F NT 7 LLDPE

    On a five-layer cast stretch film line configured with a 1,800 mm slot die, a 30:1 L/D barrier-screw extruder, and a polished chill roll held at 24 °C, Tuflin™ HS-7098F NT 7 is metered into the two sub-skin and core layers at 60–85 wt% of total polymer feed, with the balance divided between a metallocene-catalyzed LLDPE of 0.5–1.0 g/10 min melt index and a polyisobutylene cling additive concentrated at 0.8–2.2 wt% in the cling skin only. The cling layer is forced to the chill-roll side by a feedblock sequence that separates the tackifier-bearing melt from the outside layer for 24–72 h at 20–35 °C; this separation prevents tackifier transfer to the back side of the roll, which would otherwise raise unwind noise on high-speed pallet wrappers. Compliance for a pallet wrap that does not contact food directly is governed by EU Packaging Directive 94/62/EC, Article 11, with total lead, cadmium, mercury, and hexavalent chromium below 100 mg/kg, and by REACH Annex XVII entry 52 for phthalates; when the film is used as secondary wrap for packed food, the olefin layers must satisfy U.S. FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 with an overall migration limit below 10 mg/dm² at 40 °C for 10 days. Downstream processing requires a die gap of 0.6–0.8 mm, an air gap of 15–25 mm, and a chill roll temperature of 21–30 °C; a wider air gap above 28 mm causes transverse gauge oscillation exceeding 0.3 µm and pre-stretch failure at 200% elongation. Terminal product forms include 12–35 µm machine pallet wrap, pre-stretched hand wrap at 10–25 µm, and vented pallet covers with 0.5–1.5 wt% added silica anti-block.

    Application segmentRegulatory instrument / test methodIncoming QC numerical condition
    Non-food pallet wrapEU Packaging Directive 94/62/EC, Article 11Sum of Pb, Cd, Hg, Cr(VI) < 100 mg/kg
    Food-contact olefin layerU.S. FDA 21 CFR 177.1520(c); EU Regulation 10/2011Overall migration < 10 mg/dm² at 40 °C for 10 days
    Dangerous goods sack outer packagingUN Model Regulations Chapter 6.1Drop test per 6.1.5.3; leakproofness per 6.1.5.4
    Silage bale wrapEN 13207:2018Tensile and dimensional tolerance per standard tables
    Pharmaceutical blister liddingUSP <661.1>Extractable metals and organics per monograph

    What Processing Envelope Sustains BUR 2.8 with a 75 wt% Tuflin Core in FFS Sack Lines?

    Formulating for form-fill-seal heavy-duty shipping sacks typically positions Tuflin™ HS-7098F NT 7 in the core layer at 70–85 wt%, diluted with 10–20 wt% LDPE of 0.25–0.35 g/10 min melt index and a 5–10 wt% post-industrial trim stream generated from edge trim and start-up film. The peelable seal layer is run separately at 12–18 wt% EVA with 12–18% vinyl acetate and a thickness of 12–18 µm. Compliance is driven by the fill product: for dangerous goods outer packaging, UN Model Regulations Chapter 6.1 applies, including drop and leakproofness tests defined in 6.1.5.3 and 6.1.5.4; for FIBC liner components, ISO 21898 governs; for non-hazardous polymer and fertilizer sacks, incoming tensile and tear testing is performed according to ISO 527-3 and ASTM D1922. The process is a three-layer blown film line using a 250–400 mm die, dual-lip air ring, BUR 2.2–3.0, frost line height 650–900 mm, melt temperature 190–215 °C, and output of 10–14 kg/h per centimetre of die circumference. At a BUR above 2.8 with 85 wt% Tuflin, vertical MD thickness oscillation appears when frost line height exceeds 850 mm; reducing screw speed by 8–12% restores gauge variation below ±4%. Terminal products include 50–100 µm valve sacks, pinch-bottom polymer pellet bags running at 1,200–1,600 bags/h, and 60–120 µm liner bags for boxed construction chemicals.

    Low-temperature puncture resistance at -25 °C in three-layer freezer film is obtained by maintaining the Tuflin™ HS-7098F NT 7 content in the core at 35–50 wt%, with the balance split between 30–40 wt% LDPE of 0.8–1.2 g/10 min melt index and 10–25 wt% metallocene LLDPE; the two skin layers are designed with 15–20 wt% EVA or ionomer for low-temperature seal initiation at 82–95 °C, producing a total film thickness of 55–90 µm. Food-contact compliance requires the olefin layer to meet U.S. FDA 21 CFR 177.1520(c) 3.1a or 3.2a and EU Regulation 10/2011, with overall migration below 10 mg/dm² under 40 °C for 10 days in aqueous, 3% acetic acid, and 20% ethanol simulants; when the structure includes a functional barrier, Article 13 of EU Regulation 10/2011 requires a barrier layer of at least 10 µm of an approved polymer such as PET or aluminium. Downstream processing is performed on a three-layer air-cooled blown film line with internal bubble cooling, a dual-lip air ring, BUR 1.8–2.4, die gap 1.0–1.8 mm, melt temperature 185–205 °C, and frost line height 500–700 mm; online corona treatment to 38–42 mN/m is applied before gravure lamination. Terminal product forms include 0.5–5 kg frozen vegetable pillow packs, vacuum skin packaging for frozen fish portions, and 2–10 kg ice cream bag-in-box liners.

    Agricultural Silage Bale Wrap Coextrusion and the UV Stabilizer Partitioning Boundary

    Silage bale wrap coextrusions position Tuflin™ HS-7098F NT 7 at 50–70 wt% across core and sub-skin layers, with a high-cling metallocene LLDPE skin containing 2.0–4.0 wt% polyisobutylene, 0.3–0.8 wt% hindered amine light stabilizer, and 0.2–0.5 wt% benzotriazole UV absorber. The standard film thickness is 25–40 µm, and the bale wrapper pre-stretch ratio is held to 60–75% of the laboratory elongation at break to limit neck-in below 12%. Compliance is defined by EN 13207:2018 for thermoplastic silage films, including dimensional tolerance and tensile requirements; because the film contacts animal feed indirectly, Regulation (EC) No 183/2005 Article 5 traceability and contaminant avoidance provisions are applied by converters. The cast extrusion process uses a melt temperature of 220–260 °C, a 0.5 mm die gap, a chill roll temperature of 18–22 °C, and line speeds of 300–500 m/min with air-knife edge pinning; the primary failure mode is cling-layer die lip deposit formation after 8–12 h, which is removed only by purging with a cast acrylic purge compound. Finished product types include 750 mm × 1,500 m round bale wrap rolls, 250 mm × 200 m mini-bale hand film, and 2–5 m wide silage sheets.

    Extrusion lamination for high-speed vertical form-fill-seal pouch sealant webs is a process where 10–25 wt% Tuflin™ HS-7098F NT 7 is dry-blended into a 7.0–10.0 g/10 min LDPE carrier resin to produce an 18–25 µm sealant layer at 200–280 m/min on a 90 mm single-screw extruder with a 32:1 L/D and a 150 mm flat die. The hexene LLDPE reduces neck-in from 55 mm to 35 mm at an air gap of 150 mm and raises hot-tack strength measured by ASTM F1921 by 18–25% over an LDPE-only sealant, which is the decisive parameter at sealing jaw temperatures of 120–150 °C and dwell times below 0.2 s. Food-contact compliance is maintained through U.S. FDA 21 CFR 177.1520 for the olefin component and EU Regulation 10/2011 Annex II positive list, with overall migration below 10 mg/dm² at 40 °C for 10 days in aqueous and 3% acetic acid simulants; pharmaceutical blister lidding additionally requires USP <661.1> extractables testing. The downstream process requires corona treatment of the primary paper, aluminium, or OPP web at 40–44 mN/m and a chill roll temperature of 15–20 °C; on a 2,000 mm line at 250 m/min, coating weight variation remains below 0.8 g/m² only when screw speed stability is within ±0.5 rpm. Terminal product forms include 4–8 g/m² sealant webs on aluminium foil for seasoning sachets, 60–100 g/m² multi-layer structures for frozen dairy lidding, and 50–70 µm stand-up pouch sealant films.

    When 40 µm Can Liners Must Exceed 160 g Dart Impact by ASTM D1709 Method A Without HDPE Surface Matte

    When 40 µm can liners must exceed 160 g dart impact by ASTM D1709 Method A without the surface matte of high-density polyethylene, the formulation imposes a 65–85 wt% loading of Tuflin™ HS-7098F NT 7 in the core and non-seal layers, with 10–20 wt% LDPE of 0.25 g/10 min melt index and 5–15 wt% recycled LLDPE from post-industrial trim. Compliance for refuse sacks in the EU falls under EU Packaging Directive 94/62/EC Article 11, limiting lead, cadmium, mercury, and hexavalent chromium to below 100 mg/kg aggregate, and under REACH Annex XVII for specific phthalates; in North America, state-level toxics in packaging model legislation enforces the same four-metal threshold. Downstream blown film extrusion on a 75 mm single-screw extruder with a 24:1 L/D, 200 mm die, BUR 2.5–3.5, die gap 0.9–1.2 mm, and melt temperature 175–205 °C reaches 38–42 µm at 80–110 kg/h. The main processing bottleneck is bubble flutter at high BUR and low frost line height, which creates gauge variation above ±4% and causes dart impact failure below 160 g; lowering BUR to 2.8 and raising the frost line to 500–700 mm restores process stability. Terminal products include 20–80 µm star-sealed refuse sacks, 40–60 µm wheelie bin liners, and 3–10 mil drum liners for non-hazardous industrial waste.

    Free Quote

    Competitive Dow Tuflin™ HS-7098F NT 7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Tuflin™ HS-7098F NT 7 LLDPE is a linear low-density polyethylene resin assigned to the supplier’s Tuflin film-grade portfolio. The grade is supplied as natural pellets and is intended for blown-film and cast-film processes where elongation, impact resistance, and heat-sealing performance are specified. The complete designation includes the film-grade indicator HS-7098F and the suffix NT 7, the latter of which identifies a particular additive and lot-control configuration in the manufacturer’s product-management system. The certificate of analysis should be consulted for lot-specific melt flow rate, density, and additive loadings. The polymer is an ethylene–α-olefin copolymer with a linear backbone and short-chain branches introduced by comonomer insertion. This architecture distinguishes it from high-pressure low-density polyethylene, which contains long-chain branching and a broader short-chain branching distribution.

    Because the product is an LLDPE film resin, incoming-material verification commonly includes density, melt flow index, melting peak, Vicat softening point, and thin-film tensile properties. Representative values for the product class are summarised below. These ranges are process-relevant data, not a substitute for the certificate of analysis, and they can shift with thermal history and film-forming conditions.

    Table 1. Representative property envelope for Tuflin™ HS-7098F NT 7 LLDPE film resin
    PropertyTest methodValue/range
    DensityASTM D792 or ISO 1183-10.916–0.920 g/cm³
    Melt flow indexASTM D1238 or ISO 1133-1 at 190°C, 2.16 kg0.5–1.0 g/10 min
    Melting peak temperatureASTM D3418 or ISO 11357-3120–125°C
    Vicat softening pointASTM D1525 or ISO 30695–105°C
    Tensile stress at break, filmASTM D88230–50 MPa
    Elongation at break, filmASTM D882600–900%
    Dart drop impact, Method AASTM D1709150–250 g
    HazeASTM D10035–10%

    On blown-film lines using a single-screw extruder with a grooved-feed section and L/D 24:1–30:1, the resin is normally started with a temperature profile of 170–180°C in the feed zone, 190–210°C in the compression zone, 210–220°C in the metering zone, and 215–225°C at the die. A die gap of 1.8–2.5 mm and a blow-up ratio of 2.0:1–3.0:1 are used for blown film; the frost line is maintained at 2–4 die diameters below the air ring when bubble stability is the limiting factor. Melt temperature should not remain above 240°C for extended periods because oxidation accelerates and gel particles can form in stagnant die areas. Internal bubble cooling at air temperatures of 10–20°C raises throughput but reduces the cooling-air differential at the frost line, shifting the bottleneck from extruder capacity to bubble ventilation.

    In cast film, chill-roll temperatures between 20°C and 30°C are typical, with a die-to-roll gap of 0.5–1.0 mm. Neck-in is controlled by die width, melt temperature, and line speed rather than by the polymer antioxidant package. At die-exit shear stresses above 0.1–0.3 MPa, linear polyethylenes can exhibit sharkskin melt fracture. The onset is sensitive to die-lip geometry; a polished chromium die surface and a wider die gap reduce the frequency of melt fracture. On lines producing film below 25 µm, gauge uniformity becomes difficult to maintain if die-lip variation exceeds ±0.05 mm.

    Melt rheology, density, and the specification envelope

    Because the linear backbone reduces long-chain branching, the shear-thinning response is less pronounced than in high-pressure LDPE. The melt flow index range of 0.5–1.0 g/10 min places the resin in a medium-viscosity film-extrusion window. Extruder backpressure is typically higher than for LDPE at the same melt temperature, and screw power per kilogram increases. The grade is therefore processed on screws designed for LLDPE, with a compression ratio around 2.5:1–3.5:1 and a mixing section that does not generate excessive shear heating. The density range of 0.916–0.920 g/cm³ balances stiffness and impact; moving below 0.916 g/cm³ would raise dart impact but lower film modulus, while moving above 0.920 g/cm³ would raise stiffness but reduce draw and toughness.

    The melt flow index and density are not independent quality indicators. A shift in either parameter alters gauge uniformity, bubble stability, and film optical properties. In blown-film conversion, lot-to-lot melt flow index variation of more than 0.2 g/10 min from the established baseline has been observed to shift frost line height and require rebalancing of internal bubble cooling. Therefore incoming resin should be charted against the supplier certificate of analysis, and blending of multiple lots should be verified before a production campaign.

    How does the α-olefin comonomer alter film toughness relative to butene LLDPE?

    Compared with a butene-comonomer LLDPE of equivalent density and melt flow index, the higher α-olefin comonomer used in this Tuflin grade produces a more uniform distribution of tie chains after film blowing. That difference is typically observed as higher dart drop impact and improved low-temperature puncture resistance at the same film thickness. In laboratory comparisons using ASTM D1709 on 25 µm blown film, the transition from butene comonomer to a higher α-olefin comonomer generally raises the dart drop impact envelope from below 150 g to above 180 g, although absolute values depend on frost-line height, blow-up ratio, and die gap. Tear resistance measured by ASTM D1922 also improves, particularly in the transverse direction, because the tie-chain network redistributes stress away from the initial tear tip.

    Relative to high-pressure LDPE, the LLDPE architecture reduces long-chain branching and therefore reduces melt strength. The practical consequence is a larger neck-in and lower tolerance for high stalk-height bubbles in blown film. The resin is not a direct drop-in for LDPE in applications requiring high bubble stability at low blow-up ratios. However, the LLDPE film can be down-gauged while retaining tensile strength and puncture resistance. This differentiation is important in dunnage bags, heavy-duty sacks, and agricultural films where down-gauging reduces mass per unit area without sacrificing tear resistance.

    Seal initiation temperature is governed by the melting range. When a 25 µm film is sealed at 0.35 MPa for 0.5 s, initial seal strength exceeding 0.5 N/15 mm is commonly observed in the 100–110°C range. Hot-tack strength measured by ASTM F1921 increases with temperature and can become limiting above 120°C when sticking and film distortion occur. The resin is therefore suited to high-speed vertical form-fill-seal lines where seal-bar contact time is short.

    Sealing performance and laminate integrity in flexible packaging

    In multilayer films, Tuflin HS-7098F NT 7 LLDPE is placed in skin or sealant layers where its seal strength and puncture resistance are functional. Tie-layer adhesion to ethylene vinyl acetate or polar substrates should be confirmed by the film converter because the LLDPE surface is nonpolar and may require corona treatment to reach a wetting tension above 38 mN/m. Lamination bonds are evaluated by ASTM F904 or equivalent peel-test methods. In laminates exposed to frozen-food distribution, the low-temperature toughness of the LLDPE layer reduces brittle cracking at temperatures below −20°C. Published data for this specific configuration is limited; converters should validate final laminate performance under the intended storage and transport conditions.

    Film properties are measured after sample conditioning at 23°C ± 2°C and 50% ± 5% RH. Dart drop impact values in the range of 150–250 g for 25 µm film are common for this product class. Haze is usually reported at 5–10% at 25 µm, and the product is expected to exhibit higher haze than an LDPE of equivalent density but lower haze than many recycled-content LLDPE compounds. Gloss measured by ASTM D2457 at 45° tends to fall in the range of 60–75 for blown film, depending on die-lip finish and cooling-air flow.

    When replacing LDPE in high-integrity dunnage or agricultural film

    When the grade replaces high-pressure LDPE in puncture-critical dunnage or greenhouse film, the converter typically maintains a higher frost line and reduces stalk height to compensate for lower melt strength. A single-screw extruder with L/D 30:1 and a barrier screw improves melt-temperature control at high output. The die gap may be increased from 1.8 mm to 2.2 mm to reduce melt fracture. Blending with LDPE is common to improve bubble stability; ratios of 70–80% LLDPE have been used, but the exact ratio must be established on the production line because the two resins differ in shear viscosity and extensional behavior.

    For cast-film replacement of LDPE, the linear resin requires higher melt temperatures to reduce draw resonance. At a chill-roll temperature of 25°C and line speed above 150 m/min, draw resonance can appear as periodic thickness variation in machine direction. Reducing the die-to-roll gap or increasing the melt temperature by 5–10°C usually suppresses the instability. Operators should not exceed the 240°C melt-temperature limit while making these adjustments.

    Food-contact compliance is assessed against FDA 21 CFR 177.1520 and European Union Regulation EU No 10/2011. The converter is responsible for overall migration and specific migration testing on the final article. The resin is supplied under REACH; end-use articles should be screened against RoHS 2011/65/EU or IEC 61249-2-21 where halogen restrictions apply. The product should not be combined with additive packages containing high levels of primary amines if the intended food-contact use imposes low migration limits for amine derivatives.

    Resin storage in sealed hoppers at 20–25°C and 40–60% RH is recommended. If surface condensation occurs, drying at 60–70°C for 2–3 h in desiccant-air equipment is generally sufficient. The resin is not designed for rotational molding or injection molding with long flow lengths; its narrow molecular weight distribution and linear architecture limit low-shear melt flow. In extrusion, purging with LDPE after the campaign reduces start-up contamination when the next product requires lower melt temperatures. The final grade should not be exposed to direct steam-heated hoppers, and regrind should be limited to 10–15% by weight unless property retention is validated by film testing.