    Specifications
    HS Code 218638
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene-1
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melt Flow Ratio I21 6 I2 16 30
    Tensile Strength At Yield 9.0 MPa
    Tensile Strength At Break 22 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Dart Drop Impact 120 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 12%
    Gloss 45 60
    Vicat Softening Point 95°C
    Melting Point 123°C
    Crystallization Temperature 103°C

    As an accredited Dow Tuflin™ HS-7098D NT 7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Tuflin™ HS-7098D NT 7 LLDPE comes in 25 kg polyethylene-lined paper bags, 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL loaded with Dow Tuflin™ HS-7098D NT 7 LLDPE in 25 kg bags, palletized, shrink-wrapped, and secured for shipping.
    Shipping Dow Tuflin™ HS-7098D NT 7 LLDPE is a non-hazardous LLDPE resin shipped as pellets in 25 kg bags, jumbo bags, or bulk hopper trucks/railcars. It is not DOT/IMDG/IATA regulated. Store dry, away from heat, sunlight, and contamination. Keep packaging sealed; handle pallets carefully to prevent punctures and moisture ingress.
    Storage Store Dow Tuflin™ HS-7098D NT 7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible materials. Keep containers or bags closed, palletized, and off the floor to protect from moisture, dust, and contamination. Avoid excessive stacking and prolonged UV exposure. Use first-in, first-out stock rotation. Ensure good housekeeping and follow manufacturer/local regulations.
    Shelf Life Shelf life: 24 months from manufacture when stored in original, unopened packaging in a dry, cool area away from sunlight.
    Application of Dow Tuflin™ HS-7098D NT 7 LLDPE

    In high-output cast stretch-film production, Tuflin™ HS-7098D NT 7 Linear Low Density Polyethylene is processed as the primary polymer phase in monolayer and coextruded pallet-wrapping structures at thicknesses from 10 µm to 23 µm. The resin is characterised by a nominal density of 0.918 g/cm³ when tested in accordance with ISO 1183-1:2019 and a melt mass-flow rate of 2.3 g/10 min at 190°C under 2.16 kg load according to ISO 1133-1:2022. On a cast extrusion line equipped with a 90 mm single-screw extruder of 30:1 L/D ratio, the barrel temperature profile is held between 210°C and 250°C, the feed zone is maintained at 180°C to avoid feed-bridge formation, and the chill-roll temperature is controlled between 15°C and 25°C to freeze the web without post-crystallisation haze. The resin is non-hygroscopic, but when pellets are transferred from storage below 10°C into a production hall above 60% relative humidity, surface condensation on pellets can introduce steam at the die; hopper purge with dry air is used until pellet surface temperature exceeds the dew point. Edge pinning and air-knife parameters are adjusted with increasing line speed: electrostatic edge pinning is typically required below 20 m/min to prevent neck-in, while above 20 m/min an air knife acting on the die-to-roll gap stabilises the molten web. The monolayer formulation uses Tuflin™ HS-7098D NT 7 at 100 wt% of the polymer fraction; where a three-layer A/B/A structure is produced, the resin constitutes 70–80 wt% of the total weight in the core layer, and the skin layers contain a cling-agent masterbatch based on polyisobutylene at 0.5–2.0 wt% and a slip/antiblock masterbatch at 0.1–0.5 wt%. Pre-stretch ratios on pallet-wrapping equipment are commonly set between 200% and 300%, and the finished film must retain sufficient elastic recovery to avoid load shift during transit. Compliance for pallet films that do not contact food is typically anchored to REACH Regulation (EC) No 1907/2006 and, where relevant, Commission Regulation (EU) No 10/2011 for food-contact-adjacent applications. Mechanical characterisation is performed using ASTM D882-18 for tensile properties, ASTM D5748-19 for puncture resistance, and ASTM D1894-14 for coefficient of friction. Process limitations for this grade include a practical melt-temperature ceiling of 260°C; prolonged residence time above this threshold generates oxidised gel particles that appear as optical defects and reduce puncture resistance. The resin is not a barrier polymer, and pallet films based on it are not intended for oxygen-sensitive products in modified-atmosphere packaging. Terminal products from this segment include machine-grade and hand-grade stretch-wrap rolls in widths from 250 mm to 750 mm, used to stabilise palletised goods in logistics, beverage, construction-materials and appliance distribution.

    What Limits Frost-Line Height in Blown Heavy-Duty Sack Film?

    The puncture and tear response of blown heavy-duty sack film based on Tuflin™ HS-7098D NT 7 begins with the selection of the die gap and blow-up ratio rather than solely with the base resin melt index. In monolayer and coextruded sack structures of 50 µm to 200 µm, the resin is processed at melt temperatures between 190°C and 215°C; raising melt temperature above 220°C reduces film haze but destabilises the bubble at high frost-line settings. A blow-up ratio of 2.0:1 to 3.0:1 is typically selected, and the frost-line height is maintained at 4–8 die diameters; above this range the bubble enters a flop regime because the melt strength of the LLDPE is insufficient to resist aerodynamic instability on lines without internal bubble cooling. The grade is formulated at 80–100 wt% of the polymer fraction, with the remainder being a high-pressure LDPE bubble-stabilising component or a compatible LLDPE/LDPE carrier blend; increasing the LDPE fraction above 20 wt% improves bubble stability but produces a measurable drop in low-temperature dart impact and Elmendorf tear resistance. Slip and antiblock masterbatches are added at 0.05–0.3 wt% to control blocking during roll storage and to permit sack opening on filling lines. Production-scale blown-film lines typically use a die gap of 1.8–2.6 mm; narrower gaps increase shear heating and gel risk, while wider gaps reduce orientation and can lower MD tensile strength. On-line gusseting and surface corona treatment at 38–42 dyn/cm are used when the film is subsequently printed or converted into block-bottom sacks. Compliance for industrial sack applications is governed by ISO 21898 for flexible intermediate bulk containers, ISO 7965-2:1993 for drop testing of thermoplastic sacks, and ASTM D1709-16a plus ASTM D1922-15 for impact and tear characterisation. The operational boundary in this segment is the combination of gauge and frost-line height: at thickness below 60 µm, frost-line heights below 4 die diameters produce excessive orientation and low puncture resistance, while above 8 die diameters the bubble becomes susceptible to stroke-level oscillation on conventional single-lip air rings. Published data for very low-gauge heavy-duty sacks in this specific resin is limited; processors therefore validate dart-impact and drop-test performance on their own line configuration before commercial qualification. Terminal finished goods include heavy-duty shipping sacks, FIBC liners, resin and fertiliser packaging, and form-fill-seal construction-material bags.

    Blown heavy-duty sack film characterisation and processing window
    ParameterTypical industrial rangeTest or control method
    Tuflin™ HS-7098D NT 7 fraction80–100 wt%Weight-batch control
    LDPE carrier/bubble stabiliser0–20 wt%MFI ratio control
    Die gap1.8–2.6 mmDie lip measurement
    Blow-up ratio2.0:1–3.0:1Bubble diameter / die diameter
    Frost-line height4–8 die diametersOptical line sensor
    Dart impactReported as gramsASTM D1709-16a
    Elmendorf tearReported as MD/CD grams-forceASTM D1922-15

    When Sealant Web Is Laminated to Biaxially Oriented Polyester for Stand-Up Pouches

    Sealant webs based on Tuflin™ HS-7098D NT 7 are produced at thicknesses from 15 µm to 40 µm and are corona-treated in-line to a surface energy of 38–42 dyn/cm before lamination to biaxially oriented polyester, biaxially oriented polypropylene, or aluminium foil. In this configuration the resin is typically used at 100 wt% of the sealant layer; where a lower seal-initiation temperature is required for high-speed vertical form-fill-seal lines, the resin is blended with 15–30 wt% of LDPE or a metallocene plastomer, and the blend ratio is adjusted because each 10 wt% increase in LDPE lowers the seal-initiation temperature while also reducing hot-tack strength. The film is produced on cast or blown lines with a melt temperature between 200°C and 240°C; cast-web production is preferred for thickness uniformity below 25 µm, while blown-web production is used for heavier sealant layers that must survive puncture during product loading. Laminated structures are tested for seal strength using ASTM F88/F88M-21 and for hot-tack performance using ASTM F1921-20; migration compliance for food-contact applications is evaluated under FDA 21 CFR 177.1520 for olefin polymers and Commission Regulation (EU) No 10/2011, with overall migration limits of 10 mg/dm² for the finished laminate. Because this grade is a non-polar LLDPE, the migration of high-molecular-weight polymeric species is negligible under cold and ambient conditions, but the finished laminate must still be assessed as a whole when barrier layers, printing inks, or adhesives are present. Processing limitations include the need to keep corona treatment uniform across the web; roll-side and air-side treatment differences above 2 dyn/cm can cause adhesive delamination after pouch conversion. The resin is not recommended as a sealant for retort or pasteurisation cycles above 80°C because seal creep and loss of pouch integrity occur under sustained heat and pressure. Terminal product types include stand-up pouches, quad-seal bags, side-gusseted pouches, and dry-food or detergent packaging where the outer layer provides oxygen or moisture barrier and the LLDPE layer supplies seal integrity and puncture resistance.

    Agricultural bale-wrap film produced from Tuflin™ HS-7098D NT 7 is run on cast film lines at thicknesses from 20 µm to 35 µm and in widths from 500 mm to 750 mm, with the resin serving as the primary polymer at 94–98 wt% of the compound. A hindered amine light stabiliser masterbatch is added at 0.5–1.5 wt%, titanium dioxide or carbon black pigmentation is added at 2–5 wt%, and a polyisobutylene-based cling agent is added at 0.5–1.2 wt%; the cling agent is concentrated in the film skins in coextruded structures to avoid exudation into the adhesive layer of bale wrap. On a cast line with a 150 mm die and a 0.5 mm lip gap, melt temperatures are maintained at 220–250°C and the chill roll is kept at 18–24°C to maximise film toughness without haze; pre-stretch during bale wrapping is typically applied at 50–70% of the film’s designed elongation, which is lower than pallet-wrap pre-stretch because excessive stretching creates thin spots that split when encountering sharp crop stems. The required mechanical standards include EN 13207:2001 for silage films and tubes, ASTM D882-18 for tensile properties, ASTM D5748-19 for puncture resistance, and ISO 527-3 for tensile behaviour of films. Outdoor storage stability depends on UV package loading and film thickness; a 25 µm film with a standard HALS package is not expected to retain mechanical integrity beyond a single silage season, and the film must be stored away from direct sunlight before use. Processors observe that film web stability in this cast process is sensitive to edge-pinning airflow; at widths above 500 mm, the web edges must be pinned with an air knife before the chill roll to prevent neck-in and uneven cling distribution. Terminal finished goods are pre-stretched and non-pre-stretched round bale silage wraps, square bale covers, and silage tubes used in dairy and beef forage preservation, where the film blocks oxygen ingress and maintains anaerobic fermentation conditions.

    Low-Temperature Dart Impact and Seal Initiation in Frozen Food Packaging Film

    Film structures for frozen food packaging using Tuflin™ HS-7098D NT 7 are commonly produced on blown-film extrusion lines at total thicknesses from 40 µm to 80 µm, with the resin occupying the core or sealant layer at 70–90 wt% of the structure. The remaining layer fraction is typically a high-density polyethylene or LDPE component that improves stiffness and machinability on high-speed vertical and horizontal form-fill-seal equipment. Slip and antiblock masterbatches are added in the surface layers at 500–1,500 ppm by weight; dosage above 1,500 ppm can reduce seal strength and create visible die-lip build-up. Blown-film processing for this grade uses a melt temperature of 190–215°C, a blow-up ratio of 2.0:1 to 2.8:1, and a die gap of 2.0 mm to 2.5 mm; internal bubble cooling is recommended at throughputs above 250 kg/h to control frost-line height and maintain impact properties. Dart impact is assessed after conditioning at -18°C for 24 h in accordance with ISO 7765-1:1988 or ASTM D1709-16a, and seal-initiation temperature is determined by hot-seal testing on a laboratory sealer with 0.5 s dwell and 0.3 MPa jaw pressure; blends with LDPE above 20 wt% reduce seal-initiation temperature but also lower low-temperature dart impact, so the final blend is balanced against product drop resistance. Food-contact compliance is evaluated under FDA 21 CFR 177.1520, Commission Regulation (EU) No 10/2011, and REACH Regulation (EC) No 1907/2006 for substances in the finished packaging. An operational limitation is the moisture-barrier performance: LLDPE alone is not a high moisture barrier, and frozen food structures requiring extended shelf life for dehydration-prone products must incorporate an additional barrier layer or use a thicker HDPE component. The resin is also not intended for microwave or ovenable packaging. Terminal product types include bags and pouches for frozen vegetables, IQF fruit, frozen fish, ice cream overwrap, and secondary packaging for frozen ready meals.

    Stretch Hood Elastic Recovery after 55% Elongation on Pallet-Hood Lines

    During pallet-hood extrusion, Tuflin™ HS-7098D NT 7 is processed into blown film of 80 µm to 150 µm thickness, wider than stretch-wrap film, and the formed hood is stretched over the pallet with an elongation of approximately 55% to 70% in the transverse direction. Elastic recovery after this elongation determines load containment; the resin is therefore run at 100 wt% or blended with 10–20 wt% LDPE to improve bubble stability without reducing recovery below the level required for pallet stability. The blown-film process uses a die gap of 2.2–2.8 mm, a blow-up ratio close to 1.5:1 to 2.2:1, and a melt temperature between 190°C and 215°C; high blow-up ratio values are avoided because they reduce transverse stretchability and create uneven hood deployment on multi-format pallet loads. Compliance is based on ASTM D882-18 for tensile stress and strain, ASTM D5748-19 for puncture resistance, and ISO 527-3 for film tensile properties; environmental compliance for industrial packaging follows REACH Regulation (EC) No 1907/2006 and, where export packaging enters food-adjacent logistics, Commission Regulation (EU) No 10/2011 may be used to verify incidental contact suitability. Production lines with a 350 mm spiral-mandrel die and internal bubble cooling stabilise the bubble at frost-line heights from 5–10 die diameters; without internal bubble cooling, the high throughput required for 150 µm film can produce bubble breathing and gauge variation above ±5%. The main operational boundary in this segment is the high tension applied by the stretch-hood applicator: film with poor CD tear resistance or local thin sections may fail at the hood corners during application, especially at temperatures below 5°C in outdoor loading bays. The resin is not a direct substitute for EVA-based stretch-hood films in all load configurations; loads with sharp protrusions require additional puncture validation. Terminal product types are stretch hoods for palletised building materials, beverage crates, white goods, and export cargo, where the LLDPE layer provides puncture resistance and weather-resistant containment during transport and storage.

    Free Quote

    Competitive Dow Tuflin™ HS-7098D NT 7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Tuflin™ HS-7098D NT 7 is classified as a linear low-density polyethylene resin supplied in natural pellet form and directed to cast film conversion. The grade is specified by the supplier with a nominal melt flow rate of 1.0 g/10 min when measured in accordance with ASTM D1238 at 190 °C and 2.16 kg load. Density is nominally 0.918 g/cm³ when determined by ASTM D792; the corresponding ISO method is ISO 1183-1. The product is an ethylene copolymer, not a high-pressure low-density polyethylene homopolymer. The specific alpha-olefin comonomer and its molar content are not stated in public supplier documentation, and the pellet additive system is proprietary. The NT 7 designation indicates a natural-pellet grade with the standard slip and antiblock formulation; the 7 designation is a supplier-specific production-code identifier and does not correspond to a publicly defined additive concentration.

    These two primary specifications position the grade in the lower-melt-flow segment of cast-film LLDPE resins. At equivalent film gauge, the 1.0 g/10 min melt flow rate produces higher melt strength and higher stretch force than a 2.0 g/10 min butene-based LLDPE of similar density. The density of 0.918 g/cm³ is low enough to permit film flexibility and dart-impact retention while remaining high enough to maintain stiffness for down-gauged cast overwrap and stretch film constructions. The resin is not recommended for injection molding or rotomolding because the narrow molecular weight distribution and high melt viscosity at shear rates typical of injection filling can result in short shots and high injection pressure. Published data for injection-molding performance of this specific configuration is limited.

    Why Does the 1.0 g/10 min Melt Flow Rate Drive Extruder Torque?

    The melt flow rate is an inverse index of molecular weight. A 1.0 g/10 min LLDPE has a higher melt viscosity than a 2.0 g/10 min grade under identical temperature and shear conditions. On a single-screw extruder, this raises specific energy input, screw torque, and die pressure. In cast-film operations using a 90 mm single-screw extruder with a 30:1 L/D barrier screw, die pressure at a 0.5 mm flexible-lip die is commonly observed in the range of 70 bar to 120 bar for 1.0 g/10 min LLDPE, depending on output and melt temperature. These values are general industrial observations and must be validated against the installed drive capacity and screw design. A melt-temperature profile across five barrel zones of 180 °C, 200 °C, 210 °C, 215 °C, and 220 °C is a typical starting point for cast-film LLDPE of this flow class, but the die adapters and transfer lines should be set to maintain a die-inlet melt temperature no higher than 240 °C to limit oxidative degradation.

    At melt temperatures below 210 °C, the viscosity increase can push motor load beyond 85 % of full-load amperage on a 90 mm extruder, especially at outputs above 180 kg/h. Raising the barrel set points by 10 °C to 15 °C reduces melt viscosity and stabilizes motor current, but the operator must monitor die-lip smoke and gel formation. Excessive temperature in the feed throat and compression zone also increases the risk of pellet sticking and feed starvation. The use of a grooved-feed section is not normally required for this density class; if a grooved-feed extruder is used, barrel-zone one must remain below 80 °C to prevent premature melting in the grooves.

    Moisture uptake of polyethylene is negligible. Drying is not required unless surface condensation is present from storage below the dew point. If condensation is suspected, a hopper dryer set at 50 °C to 60 °C for 2 h to 4 h may remove surface moisture without degrading the slip additives. Pre-drying is not a substitute for contamination control; fines, regrind, and tramp polymer can shift gel count and haze more than pellet moisture.

    In cast-film line layout, the die gap and chill-roll settings are the dominant process variables for thickness uniformity and optical quality. For 0.918 g/cm³ LLDPE with a 1.0 g/10 min melt flow rate, a die gap of 0.5 mm to 0.8 mm is typically used, with the lower gap favored for film below 20 µm and the higher gap used for film at 50 µm and above. The melt curtain should impinge on a polished chill roll at a short air gap to minimize neck-in and width loss. Chill-roll temperature is commonly maintained between 15 °C and 25 °C. The air knife and vacuum box must be balanced so that the film contacts the chill roll without air entrapment; air pockets create haze bands and localized cooling differences. At line speeds above 300 m/min, edge pinning becomes critical because the lower melt strength of LLDPE relative to LDPE can allow neck-in and dog-bone thickness profiles at the web edges.

    When Chill-Roll Temperature Drops below 15 °C

    Lowering chill-roll temperature below 15 °C accelerates spherulite nucleation and can improve film clarity by reducing crystalline size, but the process window narrows. Condensation on the roll surface occurs when the roll temperature is below the ambient dew point. The condensed water film disrupts the quench and creates irregular haze, smoke-like surface defects, and uneven slip-additive distribution. In addition, very rapid quenching freezes molecular orientation and can increase film stiffness while reducing machine-direction elongation. For film grades with antiblock and slip additives, an excessively cold roll can reduce the mobility of slip additives to the film surface, delaying the development of coefficient-of-friction stability during aging. The practical lower limit for cast-film LLDPE of this density is therefore set by the dew point, not by the polymer. If the plant ambient dew point is 18 °C, a chill-roll set point of 15 °C may already be below the condensation threshold and must be avoided unless the casting area is dehumidified.

    Relative to a 2.0 g/10 min butene-based LLDPE of equivalent density, HS-7098D NT 7 typically produces higher machine-direction tensile strength and higher stretch force because the lower melt flow rate corresponds to longer chains and more tie-molecule formation. In cast stretch film, this translates to a higher force required to achieve a 200 % pre-stretch and, in many cases, better retained load on a pallet. The trade-off is lower extrusion throughput at fixed screw speed and higher melt temperature. In a direct substitution trial, the screw speed required to maintain the same output as a 2.0 g/10 min resin may increase by 10 % to 20 %, and melt temperature may rise by 3 °C to 6 °C. These values are not product-specific guarantees; they are typical directional changes observed when lowering melt flow rate in the same density class.

    Compared with an octene-based LLDPE of the same 1.0 g/10 min melt flow rate, the comonomer architecture may alter dart impact, Elmendorf tear, and puncture resistance. Hexene or octene comonomer incorporation generally creates longer short-chain branches than butene, improving tie-chain probability and impact strength at comparable density. The supplier does not publicly disclose the comonomer type for HS-7098D NT 7; therefore, a quantitative comparison against an octene grade should be made using Fourier transform infrared spectroscopy or 13C NMR and then correlated with film properties on the target line. Published data for this specific configuration is limited.

    The following table summarizes the primary supplier-published values. Mechanical film properties such as tensile strength, dart impact, and tear resistance are not given because they depend strongly on film thickness, processing temperature, chill-roll treatment, and test conditioning. Those values must be generated on production film.

    Typical supplier-published physical properties for Dow Tuflin™ HS-7098D NT 7
    PropertyTest methodTypical value
    Melt flow rateASTM D1238 / ISO 1133-1:20221.0 g/10 min
    DensityASTM D792 / ISO 1183-10.918 g/cm³
    FormVisualNatural pellets
    Additive packageSupplier internalSlip and antiblock, proprietary

    Which Test Methods Should Govern Film Qualification for Cast Stretch Applications?

    Film qualification should follow the same mechanical and surface test protocols used for linear low-density cast film. Tensile strength and elongation at break are measured according to ASTM D882 or ISO 527-3 on 25 µm or 20 µm film after conditioning at 23 °C ± 2 °C and 50 % ± 10 % relative humidity for 40 h. Dart impact is determined by ASTM D1709 method A or B; method A is often used for LLDPE film below 38 µm. Elmendorf tear propagation is measured by ASTM D1922 or ISO 6383-2. Coefficient of friction is measured by ASTM D1894, with the test performed on the slip-additive surface after a specified aging period because slip migration is time-dependent. Cling and stretch force of cast stretch film are evaluated under ASTM D4649 or ASTM D5458; the latter includes peel cling, stretch force, and puncture in the stretched film. These methods do not replace full-scale pallet-wrap testing, but they provide repeatable numerical data for raw-material and process comparisons.

    For optical haze and clarity, ASTM D1003 and ASTM D2457 are applicable. Gel counts can be measured by optical scanners or by a supplier internal method; film from 1.0 g/10 min cast-film LLDPE should be monitored for gel formation after any temperature excursion above 240 °C. A single 30 s residence-time excursion at 250 °C may produce oxidative gel specks that cannot be removed by filtration and that will appear as visible defects in thin films below 15 µm.

    When the film is pre-stretched at ratios of 150 % to 300 % on a cast stretch line, the mechanical requirements shift. A film based on 0.918 g/cm³ LLDPE with a 1.0 g/10 min melt flow rate typically exhibits a higher stretch force than a 2.0 g/10 min grade. The stretch force at 200 % pre-stretch often controls the load on the film roll and the pallet. If the stretch force is too high, the film may tear at the core or at the pallet corners; if too low, load retention suffers. The correct balance is achieved by blending HS-7098D NT 7 with LDPE or a higher-melt-flow LLDPE, but the blend ratio must be validated because phase separation is not thermodynamically favored in polyethylene blends. The blend components are miscible in the melt at typical extrusion temperatures if the density difference is small; however, differences in crystallization rate between LLDPE and LDPE can create surface roughness and lower clarity at high LDPE addition levels above 20 %.

    Regulatory Documentation and Food-Contact Verification

    Food-contact suitability is not automatically granted by the resin grade; it depends on the final film composition, the conversion conditions, and the intended use conditions. In the U.S., olefin polymers may be evaluated under FDA 21 CFR 177.1520 for food-contact articles. The finished film must meet extractables and end-use limitations specified by the regulation and any applicable food-type conditions. In the European Union, the framework is Regulation (EU) No 10/2011, which requires overall migration and specific migration testing on the final article or a worst-case film. The resin supplier’s product stewardship documentation should be consulted for regulatory status. REACH duties are governed by Regulation (EC) No 1907/2006, and a safety data sheet should be obtained and assessed for hazard classification, exposure scenarios, and substances of very high concern. RoHS compliance is handled under Directive 2011/65/EU Annex II, with maximum concentration values for lead, mercury, cadmium, hexavalent chromium, polybrominated biphenyls, and polybrominated diphenyl ethers in homogeneous materials. A supplier declaration does not replace the converter’s obligation to test homogeneous material if the film is placed on the EEE market.

    Regulatory verification framework
    RegionReferenceVerification requirement
    U.S. food contactFDA 21 CFR 177.1520Olefin polymer clearance; final article must meet use conditions
    EU food contactRegulation (EU) No 10/2011Overall migration and specific migration limits to be validated on final film
    REACHRegulation (EC) No 1907/2006Safety data sheet and SVHC confirmation from supplier
    RoHSDirective 2011/65/EU, Annex IIRestricted substance thresholds in homogeneous material

    Storage and handling practices for HS-7098D NT 7 follow standard LLDPE protocols. The resin should be stored in closed containers at ambient temperatures below 40 °C and protected from direct sunlight and rain. High storage temperatures above 45 °C can soften pellets and promote agglomeration, particularly in silos or railcars under solar load. If the resin is transferred by pneumatic conveying, clean air supply and metal detection are recommended to prevent contamination from fines and wear debris. Edge trim and post-industrial scrap from clean cast-film production can be recycled into the film core, but the addition of densified trim at levels above 10 % by weight may alter gel count, film color, and slip-additive balance. The exact re-feed level must be determined by film quality measurements on the intended structure.

    If the resin is evaluated in blown film equipment, the 1.0 g/10 min melt flow rate and narrow molecular weight distribution may reduce bubble stability relative to LDPE or film-grade LLDPE with a higher melt flow rate. Blown film lines with a low-stalk configuration and an annular die gap of 1.5 mm to 2.5 mm can process 1.0 g/10 min LLDPE, but the frost line must be raised and the blow-up ratio kept below 2.5:1 to avoid bubble flutter. The cast-film additive package may not be optimized for blown film slip and antiblock behavior, and the supplier’s technical service should be consulted before substitution outside cast film.

    Because the slip and antiblock package is proprietary, film coefficient of friction should be monitored during the first 7 days after extrusion. Slip additives migrate to the surface over time, and the coefficient of friction may decline from the initial value. Corona treatment for printing or lamination can oxidize the surface and reduce subsequent slip-additive mobility; the required treatment level is typically 38 mN/m to 42 mN/m wetting tension, but the treated film should be re-measured after 24 h for wetting stability. These operational boundaries apply to the material class and are not exclusive to a single grade.