| HS Code | 301882 |
| Density | 0.918 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.70 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Break Md | 5000 psi |
| Tensile Strength At Break Td | 4500 psi |
| Elongation At Break Md | 700% |
| Elongation At Break Td | 800% |
| Dart Drop Impact F50 | 200 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 500 g |
| Haze | 10% |
| Gloss 45 | 50% |
| Low Temperature Brittleness | < -70 °C |
As an accredited Dow Tuflin™ HS-7098C NT 7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow Tuflin™ HS-7098C NT 7 LLDPE comes in 25 kg polyethylene-lined paper bags, palletized for industrial use. |
| Container Loading (20′ FCL) | 20′ FCL container loading for Dow Tuflin™ HS-7098C NT 7 LLDPE: 25 kg bags, palletized, roughly 18–22 MT net weight. |
| Shipping | Dow Tuflin™ HS-7098C NT 7 LLDPE is a non-hazardous linear low-density polyethylene resin. Ship as general freight, not DOT/IMDG/IATA regulated. No UN number, hazard class, or packing group. Transport in sealed bags/octabins; keep dry, cool, and free from contamination. Confirm current SDS before shipping. |
| Storage | Store Dow Tuflin™ HS-7098C NT 7 LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep bags or containers closed to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and UV exposure. Use first-in, first-out stock rotation. Maintain normal ambient conditions, protect packages from crushing, and handle with clean equipment. |
| Shelf Life | Typically 24 months from date of manufacture when stored in original, unopened packaging under dry, cool conditions away from direct sunlight. |
In high-speed cast pallet-wrap production, Tuflin HS-7098C NT 7 is processed as the core layer in three-layer and five-layer stack die configurations where line speeds above 350 m/min expose the melt to shear rates exceeding 10⁴ s⁻¹ in a 33:1 L/D barrier-screw extruder. The layer mass distribution is typically 70/15/15 core/skin/skin, with each outer skin containing 1.5–2.5 wt% polyisobutylene cling masterbatch and 0.3–0.8 wt% erucamide-free slip masterbatch to maintain release on powered pre-stretch carriages. Compliance for stretch wrap is assessed under ASTM D5458-12 machine-direction cling, ASTM D4649-20 containment force retention, and ISO 527-3:2018 tensile properties; the resin itself, without processing aids, is outside the restricted substance scope of Directive 2011/65/EU Annex II. Extrusion uses a 0.8 mm die gap, 15–20 mm air gap, 20°C chill roll temperature, and melt temperatures between 240°C and 255°C. Neck-in is controlled below 15% by maintaining an 8–12°C die-lip temperature gradient and using 0.1–0.2 wt% polypropylene minor blend in edge bead trim, which is reground into the core at 5–8 wt%. Polyisobutylene levels above 3.0 wt% in the skin layers produce chill-roll plate-out within 4–6 h of continuous running and are not recommended. Terminal output is 15–23 µm machine film wound on 400 mm rolls for turntable and rotary arm wrappers with pre-stretch ratios up to 250%.
Extrusion coating lines that laminate reverse-printed BOPET to aluminum foil or high-barrier metallized OPP use Tuflin HS-7098C NT 7 in sealant webs at 15–25 wt% addition to LDPE coating resins, with the remaining 75–85 wt% being a low-density polyethylene with melt index 4–7 g/10 min. The blend is processed through a 90 mm single-screw extruder with 30:1 L/D and two-stage compression screw, melt temperature 285–305°C, slot die width 250–350 mm, and coat weights from 15–25 g/m². Ozone treatment on the molten curtain is set to 0.08–0.12 g/m² ozone dosage to increase carboxyl group formation on the polyolefin surface; this raises adhesion to aluminum foil above 2.5 N/15 mm when tested by ASTM D1876-08 T-peel. Heat-seal initiation is measured by ASTM F1921-12(2018) and is typically 108–118°C for a 20 µm sealant layer; hot-tack strength at 115°C remains above 1.5 N/25 mm. Food-contact compliance is established under FDA 21 CFR 177.1520(c) for polyolefin base polymers, with total extractables not exceeding 5.5 wt% in n-hexane at reflux, and under Regulation (EU) No 10/2011 Annex I overall migration limit <10 mg/dm² using food simulant E for dry food contact. Terminal product is a liquid packaging lamination for detergent refill pouches and dry beverage overwrap, not intended for retort or boiling-water sterilization above 95°C due to seal creep.
A 75 mm grooved-feed extruder running 24:1 L/D with a barrier screw and nitrogen-blanketed hopper can sustain 180–210°C melt temperature and 1.8–2.2 mm die gap in monolayer heavy-duty sack film. The production formulation adds 20–30 wt% LDPE to Tuflin HS-7098C NT 7, with the balance 70–80 wt% Tuflin, to stabilize the bubble at 2.4:1 blow-up ratio and reduce draw resonance at 120–150 µm final thickness. A slip/antiblock masterbatch containing 5 wt% silica is dosed at 1.0–2.0 wt% during repeat orders for flour, cement, and polymer granule sacks; pre-drying is not required, but if ambient relative humidity exceeds 80% and hopper residence time exceeds 4 h, surface moisture condensation can cause pinholes, so dry-air purging is recommended. Purge time after color change is extended to 20–30 min at 190°C to clear retained gel tails from the spiral mandrel gap. Mechanical compliance is evaluated under ISO 527-3:2018 tensile properties, ASTM D1709-22 Method A dart impact, ISO 6383-2:1983 tear resistance, and ISO 7965-2:1993 filled-sack drop test. Corner seal strength at filled drop heights of 1.2 m is correlated to ASTM D1709 impact values above 400 g on 120 µm film, with machine-direction tensile yield not less than 11 MPa. The dart-impact threshold is derived from plant trial data and should be revalidated per lot. Terminal product is a 40–60 kg chemical and mineral powder sack, often with a microperforated back panel for deaeration.
Silage stretch film converters running 150–200 µm black-white coextrusions compound Tuflin HS-7098C NT 7 at 100 wt% in the white UV-reflective outer layer and 90–95 wt% in the black pigmented inner layer, with 1.5–2.5 wt% UV stabilizer masterbatch based on hindered amine light stabilizers and 0.5–1.0 wt% carbon black masterbatch at 40% carbon black concentration. The production line uses a three-layer blown film die, 2.8:1 blow-up ratio, 1.8–2.4 mm die gap, frost line height 500–700 mm, and internal bubble cooling at 15–20°C to preserve oxygen barrier. Compliance is tested under EN 13207:2018 silage thermoplastic film requirements, including ISO 527-3 tensile strain, ISO 6383-2 tear resistance, and ASTM D3985-17 oxygen transmission at 23°C and 50% RH. The silage film is applied with a round bale wrapper at 55–65% pre-stretch and 6–8 wraps per 1.2 m round bale; edge retention after 12 months outdoors is verified by measuring retained elongation at break above 300% in machine direction. Terminal product is a 750 mm by 1500 m roll of bale wrap or a 12 m × 25 m clamp cover sheet for forage preservation.
Form-fill-seal equipment operating at −25°C on IQF vegetable and fruit lines uses a three-layer blown film structure where Tuflin HS-7098C NT 7 is added at 50–70 wt% in the core and skin layers, with the balance 30–50 wt% metallocene-catalysed LLDPE or LDPE to retain seal-through-water performance and reduce cold-spatula splitting. At addition levels above 70 wt%, converter audit data shows machine-direction tear strength measured by ISO 6383-2 begins to decline by 10–20% on 40 µm film, while dart impact per ASTM D1709-22 Method A on frozen film remains above 150 g only when frost line height is kept under 250 mm and die gap at 1.6 mm. Processing on a 45 mm three-layer coextrusion blown film line uses 2.8:1 blow-up ratio, 190–215°C barrel profile, and 30 m/min take-off speed; corona treatment to 40–42 mN/m is applied in-line for water-based ink adhesion. Food-contact compliance follows FDA 21 CFR 177.1520(c), Regulation (EU) No 10/2011 with simulant A (10% ethanol) for frozen aqueous food, and Regulation (EC) No 2023/2006 GMP. Terminal product is a 300–500 g pillow pouch for frozen peas, mixed vegetables, and fruit packs, with seal initiation at 112–120°C and seal strength above 8 N/25 mm on packaging lines running 60–80 pouches/min. Published data for this specific Tuflin grade in frozen food FFS is limited; the 70 wt% threshold is a converter audit limit, not a supplier specification.
Competitive Dow Tuflin™ HS-7098C NT 7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow Tuflin™ HS-7098C NT 7 is an ethylene-1-hexene linear low-density polyethylene resin supplied as natural pellets for blown film and lamination film conversion. The nominal melt mass-flow rate is 0.70 g/10 min at 190 °C/2.16 kg when determined by ASTM D1238, and the nominal density is 0.918 g/cm³ when determined by ASTM D792. In film form, the resin is evaluated according to ASTM D882 for tensile performance, ASTM D1922 for Elmendorf tear, and ASTM D1709 for dart impact; the specific numerical values reported by the manufacturer are tied to a defined blown film sample and should be obtained from the current technical data sheet because mechanical response is influenced by film thickness, blow-up ratio, die gap, and cooling rate. The product designation “NT 7” identifies the natural pellet form; the base resin does not contain intentional slip or antiblock additives.
| Property | Test method | Nominal value |
|---|---|---|
| Density | ASTM D792 / ISO 1183-1 | 0.918 g/cm³ |
| Melt mass-flow rate | ASTM D1238 / ISO 1133-1:2022 | 0.70 g/10 min at 190 °C/2.16 kg |
The combination of 0.918 g/cm³ and 0.70 g/10 min places the resin in the low-density portion of the C6 LLDPE film family. Relative to a butene-copolymer LLDPE at equivalent density and melt index, the hexene branch introduces a longer comonomer side chain that is more effective in promoting interlamellar tie molecules during bubble crystallization. This structural difference is typically observed as improved Elmendorf tear in the transverse direction and a better balance of dart impact and stiffness at a given film gauge. In contrast, high-pressure low-density polyethylene of similar density exhibits a branched long-chain architecture; it develops greater melt strength and more pronounced shear thinning, but the same architecture limits drawdown and produces a different seal-temperature response. A metallocene LLDPE with comparable melt index, on the other hand, usually has a narrower molecular weight distribution and a more uniform comonomer distribution; such resins can provide higher dart impact at equivalent density but often require more attention to extruder head pressure and screw design because of their higher viscosity at high shear rates.
At a constant density and melt index, the crystallinity of ethylene-hexene copolymers is suppressed more effectively per mole of comonomer than ethylene-butene because of the larger excluded volume of the butyl branch. This reduces the crystallization rate during the frost line transition and widens the orientation window; however, it also lowers modulus relative to a higher-density LLDPE. Processors converting this product should not substitute a higher-density grade without recalculating downgauged stiffness, because the downgauging potential is limited by tensile yield and bend stiffness. The average molecular weight of the resin is reflected indirectly by the 0.70 g/10 min melt index. For blown film, this level is low enough to maintain bubble stability but high enough to allow practical extruder throughput. A 0.5 g/10 min product of the same density would provide higher melt strength but increase extruder torque, while a 1.0 g/10 min product would improve melt flow but reduce dart impact and lower melt pressure.
The linear architecture of the resin limits extensional strain hardening under bubble deformation. In practice, the film bubble is best run with a low stalk and moderate blow-up ratio rather than the long frozen-stalk high-stalk geometry typical of high-pressure LDPE. On a conventional single-screw extruder with a 24:1 L/D barrier screw and a 150 mm annular die, melt temperature should be controlled between 190 °C and 220 °C, with the die set between 200 °C and 215 °C. A die gap of 1.8 mm to 2.5 mm is common; the lower end reduces melt residence time and gel formation, while the upper end can be used for thicker films where film strength is critical. The blow-up ratio is typically maintained between 2.0:1 and 3.0:1, and the frost line height is maintained at approximately 1.5 to 2.5 die diameters to balance orientation and tear properties. Internal bubble cooling, when available, should be used to raise output and stabilize the bubble, but the coolant temperature should not be lowered below ambient to the point that condensation forms on the die face.
Because the resin is not highly shear thinning, excessive screw speeds can raise melt temperature and lower bubble stability. The melt pressure at the die should be monitored. On a 55 mm extruder with a 24:1 L/D screw running at approximately 80 kg/h, melt-pressure variation outside ±5% generally indicates feed inconsistency, screw wear, or a poorly selected barrier zone. Resin pre-drying is not normally required, but pellet surface moisture from condensation in environments above 60% relative humidity should be prevented; wet pellets can generate steam bubbles, fisheyes, and melt-pressure fluctuation. To minimize pellet temperature differentials, storage should be in dry, sealed hoppers and the material should be allowed to equilibrate to the processing area for 24 h before hopper loading if bags have been stored below 10 °C. Film gel formation can be monitored on a 25 µm monolayer sample using dark-field observation according to a line-specific internal standard; the natural pellet form is intended to minimize oxidative degradation during storage, but residence time at melt temperature above 220 °C should be limited to less than 15 min where gel precursors are a known concern.
In coextruded film structures, Tuflin HS-7098C NT 7 is used in heavy-duty shipping sacks, industrial liners, carrier films, and laminating webs where the target thickness is typically between 25 µm and 100 µm. Its hexene-based toughness contribution is relevant for packages that must survive low-temperature drop tests and high-integrity seal creep under load. The resin is also selected for food packaging when the finished structure meets the applicable migration limits; for example, olefin polymers of this type are generally recognized under FDA 21 CFR 177.1520(c) 3.1a and may comply with EU Regulation (EU) No 10/2011, but converters must confirm specific food simulants and overall migration limits for the final article. Because the base grade is additive-free, coefficient of friction under ASTM D1894 may exceed 0.50; slip and antiblock masterbatches are normally added at 2 wt% to 6 wt% depending on line speed and package handling requirements. The addition must be performed with a masterbatch carrier resin compatible with polyethylene; incompatible carriers in masterbatch can produce optical defects and reduce seal strength.
For high-speed form/fill/seal lines, corona treatment may be necessary for print adhesion or lamination bond strength. A minimum wetting tension of 38 dyn/cm is a common surface-energy target for solvent-based ink systems, although the exact requirement should be evaluated according to ASTM D2578 on converted film. Seal initiation temperature and hot-tack values are not specified in the condensed datasheet; published data for this specific configuration is limited. Converters must determine these values on their own film samples using ASTM F88 for heat seal strength and ASTM F1921 for hot tack. When slip migration affects seal performance, the converter should evaluate seal strength after a controlled aging interval because migration kinetics in polyethylene matrices can reduce interfacial bonding at high additive loadings.
This product is not formulated for high-melt-strength processes such as extrusion coating onto board where severe neck-in is unacceptable by itself; the linear architecture has less neck-in resistance than high-pressure LDPE and can require blending with LDPE or a higher-melt-strength polymer for demanding extrusion coating. The resin is not a UV-stabilized grade; if outdoor service is intended, a carbon black masterbatch or a UV stabilizer package is required at a concentration established by the application. In its natural form, it is not suitable for direct use in applications requiring stable low coefficient of friction without added slip. Because the base resin contains no antiblock, handling rolls may require unwind static control at film speeds above 100 m/min to prevent blocking and electrostatic discharge defects. Users should not combine the resin with amine-based alkaline additives or colorants that are incompatible with the polyethylene antioxidant package; no specific chemical incompatibility with common polyolefin carriers has been published, but pilot trials are recommended when using unfamiliar masterbatch chemistries. Batch-to-batch variation in density and melt flow should be monitored; a lot-shift of more than 0.001 g/cm³ in density or 0.03 g/10 min in melt index can require adjustment of bubble geometry or melt temperature to maintain consistent film gauge and dart impact. Food-contact status must be confirmed from the current product regulatory compliance certificate and must not be assumed for the finished package after blending, printing, lamination, or corona treatment.