Dow Tuflin Hs 7094 Nt 7 Linear Low Density Polyethylene Resin

Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 494738
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Melt Index 190 C 2 16 Kg 0.80 g/10 min
    Density 0.918 g/cm³
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 30.3 MPa
    Elongation At Break 700%
    1 Secant Modulus 200 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 65
    Slip No
    Antiblock No

    As an accredited Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaging: 25 kg polyethylene bags, 40 bags per pallet, totaling 1,000 kg; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL: 25 kg bags, loose loaded, 800 bags, 20 MT net of Dow TUFLIN™ HS-7094 NT 7 LLDPE Resin.
    Shipping Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin is a non-hazardous solid. It is not regulated for transport under DOT, IMDG, or IATA. Ship in sealed bags, boxes, or octabins; store dry, away from heat and UV. No UN number, hazard class, or packing group applies.
    Storage Store Dow TUFLIN HS-7094 NT 7 LLDPE resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers tightly closed, palletized, and off the floor. Protect from moisture, dust, oils, and chemical contamination. Avoid excessive stacking and prolonged UV exposure. Use first-in, first-out rotation and follow the SDS/local regulations.
    Shelf Life Shelf life is typically 24 months when stored in unopened original packaging under cool, dry, well-ventilated conditions away from direct sunlight.
    Application of Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin

    In heavy-gauge industrial liner and surface-protection film extrusion, TUFLIN™ HS-7094 NT 7 is introduced as the dominant linear low-density polyethylene phase rather than as a minor impact modifier. A three-layer coextrusion formulation for construction and chemical-packaging liners typically maintains a dry-blend loading of 60–85 wt% TUFLIN™ HS-7094 NT 7 with 15–40 wt% low-density polyethylene at a melt index of 0.25–0.50 g/10 min determined by ASTM D1238 at 190 °C/2.16 kg. Carbon black or mineral-filled UV masterbatch is added at 2.5–4.0 wt% where outdoor service, opacity, or light-shielding is specified; a fluoropolymer processing aid at 0.3–0.8 wt% is introduced on lines where die-lip build-up and melt fracture limit throughput. The blown-film equipment is commonly configured with a die diameter of 250–400 mm, die gap of 1.4–2.2 mm, blow-up ratio of 2.2–3.2, and frost line height held at 7–10 die diameters. Melt temperatures are maintained at 190–230 °C, with film thickness for liner stock typically between 100–250 µm. The dominant process conflict is the trade-off between bubble stability and dart impact resistance: raising the LDPE fraction toward 40 wt% widens the operating window on long campaigns, but low-temperature impact response measured by ASTM D1709-15a and tear propagation measured by ASTM D1922-15 usually shift relative to the neat LLDPE phase. Heavy-gauge liner compliance is verified against the packaging heavy-metal sum limit of 100 mg/kg for lead, cadmium, mercury and hexavalent chromium under Directive 94/62/EC. Puncture resistance is benchmarked with ASTM D5748, while tensile properties are checked with ISO 527-3:2018. Terminal products from this formulation include concrete formwork liners, demolition dust-containment sheeting, drum and intermediate bulk container liners, and heavy-gauge rubble sacks.

    Pre-drying of TUFLIN™ HS-7094 NT 7 is not normally required unless surface condensation has formed during storage at relative humidity above 60%; a hopper dryer set to 60–80 °C for 1–2 h is then sufficient to prevent screw surging and bubble instability. On multi-layer lines, the outer layers are often formulated at the higher LLDPE loading to maximize impact strength, while the core layer carries recycled edge trim or less costly LDPE. Thickness profiling by non-contact capacitance is maintained within a tolerance of ±10% around the nominal web thickness, because gage bands above 180 µm create hard wrinkles at the collapsing frame and increase the incidence of blocking under slit-roll compression. Converters using automatic feeding systems with gravimetric dosing and loss-in-weight calibration report fewer lot-to-lot melt-pressure variations when the additive masterbatches are pre-dispersed rather than added as powder alongside the pellets.

    What Layer Ratios Preserve Low-Temperature Dart Impact in Frozen-Food Sealant Webs?

    Frozen-food lidding, pillow pouches, and quad-seal bags demand a sealant layer that resists impact below −20 °C without raising heat-seal initiation temperature. The structure commonly uses a polyethylene-rich skin based on 70–90 wt% TUFLIN™ HS-7094 NT 7 blended with 10–30 wt% LDPE having a melt index of 0.20–0.50 g/10 min measured under ISO 1133-1:2022. Slip and antiblock masterbatches are added at 0.05–0.10 wt% erucamide equivalent and 0.5–1.0 wt% silica type, respectively; the slip agent migrates to the film surface, but at frozen storage temperatures near −25 °C migration is kinetically slowed, so coefficient of friction measured by ASTM D1894 may remain above 0.40 for 24–72 h after extrusion. Published migration-rate data for this specific TUFLIN grade at deep-freeze conditions are limited, which forces converters to run roll-conditioning trials before sealing operations. The film is produced on a three-layer blown-film line with die gap 1.6–2.2 mm, blow-up ratio 2.5–3.0, melt temperature 195–225 °C, and final thickness 25–75 µm. Heat-seal jaw temperatures of 110–130 °C are typical for the sealant layer. Compliance is established under FDA 21 CFR 177.1520(c) for olefin polymers and under Regulation (EU) No 10/2011 annex requirements with overall migration below 10 mg/dm². Food-contact manufacturing also follows Regulation (EC) No 2023/2006 on good manufacturing practice. Oxygen and moisture transmission are benchmarked with ASTM D3985 and ASTM F1249 where the film forms a barrier web. Low-temperature fracture resistance is screened with ASTM D746 brittleness temperature and ASTM D1709-15a dart drop after conditioning at −20 °C, noting that the standard dart test is conducted at 23 °C unless the specification modifies conditioning. Terminal products include frozen vegetable pouches, seafood bags, and lidding films for thermoformed trays.

    The formulation boundary in this sector is controlled by the opposing demands of low blocking and high slip. If the silica antiblock loading exceeds 1.0 wt%, dart impact at frozen-food temperatures can deteriorate and the film can exhibit localized haze from void formation around particle interfaces. If erucamide slip is increased above 0.10 wt% to compensate for slow migration, the additive may build up on sealing jaws during extended runs and interfere with seal integrity. Converters typically monitor film-to-film blocking with ASTM D3354 and seal strength with ASTM F88/F88M before releasing a lot to high-speed horizontal or vertical form-fill-seal packaging lines.

    Greenhouse Film UV Stabilizer Retention and Condensation Management

    Long-term protected agriculture film formulations using TUFLIN™ HS-7094 NT 7 rely on stabilizer systems that remain effective under repeated UV exposure rather than on short-term optical performance alone. The base blend contains 75–85 wt% TUFLIN™ HS-7094 NT 7 with 15–25 wt% LDPE or ethylene-vinyl acetate copolymers to improve foldability, edge toughness, and low-temperature impact. Hindered amine light stabilizers are added at 0.20–0.60 wt% and a benzotriazole or triazine UV absorber at 0.10–0.30 wt%. Anti-fogging surfactant masterbatch is incorporated at 1.0–2.5 wt% to reduce condensed droplet formation on the inner surface and maintain light transmission. The blown-film process uses die diameters of 1200–2000 mm, die gap 2.0–2.6 mm, blow-up ratio 2.0–2.5, and melt temperatures of 200–240 °C; film thickness typically spans 150–200 µm. The extruder is often a mono-layer or three-layer line with internal bubble cooling to stabilize high-output runs and shorten cooling time. Compliance is anchored to EN 13206 for agricultural thermoplastic films, and weathering performance is evaluated according to ISO 4892-2 xenon-arc cycle conditions; tensile retention is measured with ISO 527-3:2018. Haze development and light transmittance are tracked with ASTM D1003. Terminal products include multi-season greenhouse covers, low tunnels, and silage bunker films.

    The operational boundary most frequently missed in this sector is the incompatibility of high anti-fog loadings with certain stabilizer carriers. Additive exudation can accumulate on collapsing frames and reduce light transmission if the masterbatch carrier is incompatible, or if the film is wound at excessive tension during the first 48 h after production. Heat management is also process-critical: a frost line position that is too low can lock in orientation imbalance and cause premature splitting along machine-direction folds. Converters serving this segment commonly require a weathering retention specification of at least 50% tensile elongation after the exposure interval specified by the buyer, with test data generated on the same gauge film used in the tunnel, because data generated on thinner laboratory specimens is not transferable.

    Application segmentPrimary regulatory or compliance anchorMechanical, barrier, or service test method
    Heavy-gauge industrial linersDirective 94/62/EC heavy-metal sum limit 100 mg/kgASTM D5748, ISO 527-3:2018
    Frozen-food sealant websFDA 21 CFR 177.1520(c); Regulation (EU) No 10/2011 OML 10 mg/dm²ASTM D1709-15a, ASTM D3985, ASTM F1249, ASTM D3354
    Greenhouse and silage filmsEN 13206; ISO 4892-2ISO 527-3:2018, ASTM D1003
    Heavy-duty shipping sacksFDA 21 CFR 177.1520(c) where food contact; ISO 7965-2ASTM D1709-15a, ASTM D1922-15
    Extrusion coating and laminationFDA 21 CFR 177.1520(c); Regulation (EU) No 10/2011ASTM D1876, ASTM F1249
    Inflatable void fillDirective 94/62/EC heavy-metal sum limit 100 mg/kgASTM D882, ASTM D1709-15a, ASTM D3354

    Where high-burst strength and melt-screen pressure interact during heavy-duty sack production, the blend is formulated to avoid rapid blow-hole formation at gusset folds while limiting extruder pressure swings. A three-layer coextrusion structure places 65–85 wt% TUFLIN™ HS-7094 NT 7 in the outer and inner layers and 15–35 wt% LDPE or clean post-industrial recycled polyethylene in the core, with a total film thickness of 100–180 µm. The die diameter is 200–350 mm, die gap 1.8–2.5 mm, blow-up ratio 2.0–2.8, and melt temperature 190–230 °C. A screen pack sequence of 120/80/120 mesh is used to protect the die from gel particles, but excessive recycled content increases screen pressure above the extruder’s maximum operating limit and can force a mid-campaign screen change. Mechanical acceptance uses ASTM D1709-15a dart impact, ASTM D1922-15 Elmendorf tear, and ISO 527-3:2018 tensile. Packaging of mineral, fertilizer, or polymer granule products requires puncture and burst resistance; drop tests on filled bags may follow ISO 7965-2 depending on the transport specification. Where food contact is required, compliance follows FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011. Terminal product types are side-gusseted sacks, valve bags, and heavy-duty open-mouth bags for construction materials or resin pellets.

    This sector is distinguished by the need to preserve fold-line toughness on gusseted tubing after inline flexographic printing and post-gusset winding. Excessive LLDPE loading above 85 wt% in the outer layer can reduce surface gloss and ink keying if corona treatment is not applied uniformly at 38–42 mN/m; however, excessive corona treatment increases roll blocking at the gusset fold. Tension-controlled winding with taper settings below 10–15% is used to prevent blocking over long storage periods. The recycled core must be screened through a melt filter fine enough to remove particles above 100 µm, because larger particles translate into pinholing at the fold line and lower drop-test performance. Converters serving the polymer granule and mineral sack market often test filled-bag performance on a production line using an incline impact test or a free-fall drop test specified by the end user.

    When Melt-Curtain Geometry Limits Extrusion Coating Output

    Extrusion coating and lamination lines running TUFLIN™ HS-7094 NT 7 as a sealant web require a high enough melt temperature to maintain curtain stability over the air gap. The resin is blended at 50–100 wt% with LDPE at 0–50 wt%, depending on whether the target is high seal strength or higher line speed; an antioxidant masterbatch at 0.05–0.15 wt% is included because the melt temperature reaches 285–320 °C. A single-screw extruder with L/D 28:1–32:1 and a barrier screw is standard, supplying a flat die of up to 2600 mm width. The air gap is set at 100–200 mm, and the chill roll temperature is maintained at 12–18 °C. Melt-curtain instability appears as neck-in or draw resonance above 250–450 m/min; reducing the air gap or raising the melt temperature within the degradation threshold restores edge stability. Adhesion to paper or aluminium foil is measured with ASTM D1876 T-peel; moisture-barrier performance is tested with ASTM F1249. Food-contact compliance is verified under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, with overall migration below 10 mg/dm². Terminal products include extrusion-coated paper sacks, flexible stand-up pouches, and sealant layers for medical packaging. Published peel adhesion values for this specific TUFLIN grade on low-density kraft paper are limited, so converters characterize each paper lot with ASTM D1876 after priming.

    The production limit in this application is not usually extruder throughput but die-lip cleanliness and chill-roll release. At melt temperatures above 320 °C, oxidative degradation can form gel-like deposits at the die edge, producing edge tear in the coated web. At melt temperatures below 285 °C, draw resonance and melt-curtain sag can cause uneven coating weight, especially at grammages below 20 g/m². The vacuum box and nip roll geometry must be aligned to minimize air entrapment at high line speed, and back-up roll pressure is adjusted to prevent gauge banding in the molten web. When a coextruded tie layer is required, the TUFLIN™ HS-7094 NT 7 layer is normally the sealant skin rather than the adhesion layer.

    Blown-Film Production of Inflatable Void Fill with Controlled Blocking

    Air pillow and bubble cushion webs are typically monolayer films with a high proportion of TUFLIN™ HS-7094 NT 7 to balance impact toughness and roll-to-roll blocking. The blend ratio is 85–100 wt% TUFLIN™ HS-7094 NT 7 with 0–15 wt% LDPE for easier bubble stability during gauge transitions. Slip/antiblock masterbatch is dosed at 0.5–1.2 wt% to keep film-to-film blocking below converter tracking tolerances; excessive slip reduces inflation-channel sealing later. Processing uses a monolayer blown-film line with die diameter 100–250 mm, die gap 1.2–1.8 mm, blow-up ratio 2.5–3.5, melt temperature 190–220 °C, and film thickness 35–70 µm. Corona treatment is set to 38–44 mN/m only when the web undergoes printing; on inflation machines, the treated film may exhibit higher blocking at elevated unwind tension. Mechanical acceptance follows ASTM D882 tensile and ASTM D1709-15a dart impact. Packaging waste compliance is checked under Directive 94/62/EC heavy-metal limits of 100 mg/kg. Terminal products are void-fill air pillows, padded mailers, and bubble cushion replacement webs. The main operational boundary is the incompatibility between high corona treatment levels and low blocking: converters must confirm surface tension decay and blocking via ASTM D3354 before large runs.

    Gauge uniformity is the most critical production parameter in this sector because pillow inflation machines seal individual channels at high speed. A film thickness variation greater than ±8% can produce non-uniform channel inflation, weak seal points, or premature bursting under stack load. The air ring and internal bubble cooling are tuned to maintain a frost line between 3–6 die diameters; too low a frost line increases film-blocking tendency, while too high a frost line reduces bubble stability and worsens gauge banding. Unwind torque on the converter machine is kept low to avoid blocking after corona treatment, and slip performance is checked after 48–72 h of roll ageing. The application does not require a food-contact declaration unless the inflated pillows are used in direct contact with food, in which case the same FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011 migration limits apply.

    Free Quote

    Competitive Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow TUFLIN™ HS-7094 NT 7 Linear Low Density Polyethylene Resin is a hexene-based, Ziegler-Natta-catalysed ethylene copolymer supplied in natural pellet form. The nominal melt mass-flow rate is 0.80 g/10 min when measured at 190 °C under a 2.16 kg load according to ISO 1133-1:2022, and the nominal density is 0.925 g/cm³ according to ISO 1183-1:2019. The grade is positioned for monolayer and coextruded film structures in which stiffness, tensile strength, and tear resistance are required. Typical converting formats include heavy-duty shipping sacks, industrial liners, laminating film, and agricultural film. The NT 7 designation identifies a natural, unpigmented pellet; the slip and antiblock package should be verified against the lot-level certificate of analysis because additive levels can be adjusted in downstream compounding.

    As a linear low density polyethylene, the resin has a short-chain branched backbone and no significant long-chain branching. The comonomer distribution influences the level of strain-induced orientation in blown-film and cast-film drawing. In applications where puncture and tear resistance are governed by molecular orientation, the longer short-chain branching in this grade contributes to tie-chain density after film stretching. Comparisons with conventional butene-based LLDPE therefore require identical gauge, die gap, and blow-up ratio. Published data for this specific configuration is limited, but converter trials on a 90 mm grooved-feed extruder showed that the hexene grade retained transverse-direction Elmendorf tear after gauge reduction from 50 µm to 35 µm more consistently than a butene-based control of equivalent density.

    The following nominal physical properties are compiled from manufacturer-published data and are not lot-specific guarantees.

    PropertyTest StandardUnitNominal Value
    Melt mass-flow rateISO 1133-1:2022g/10 min0.80
    DensityISO 1183-1:2019g/cm³0.925
    Melting temperatureISO 11357-3:2018°C122
    Vicat softening temperatureISO 306:2022°C102
    Tensile modulusISO 527-2:2012MPa320
    Shore D hardnessISO 868Shore D56

    What Separates Hexene-Based TUFLIN HS-7094 NT 7 from a Comparable Butene-Based LLDPE?

    The principal structural distinction lies in the side group introduced by the comonomer: 1-hexene contributes a butyl branch, whereas butene contributes an ethyl branch. For a given density, the longer side group modifies the crystal morphology and increases the amount of tie molecules that bridge lamellae after orientation. This effect translates into higher Elmendorf tear and dart impact in film when measured under ASTM D1922-15 and ISO 7765-1:2004. The difference is not linear with density; comparisons at equivalent melt flow rate and film gauge showed transverse-direction tear improvements of no more than 15% to 25% over typical butene-based resins, with the upper end observed at low frost-line heights where transverse orientation is limited.

    Because Ziegler-Natta catalyst systems produce a distribution of comonomer placements, the grade is not as compositionally uniform as a metallocene-catalysed LLDPE. This broader composition distribution lowers hot-tack strength and raises the seal initiation temperature relative to many metallocene grades. However, the same distribution can improve bubble stability in certain high-output blown-film lines because the higher-molecular-weight fraction retains melt tension during inflation. These differences should be evaluated with seal-strength curves generated under ASTM F88 and not inferred from the resin density alone.

    In five-layer coextruded structures, the resin is frequently paired with an ethylene vinyl acetate or polyolefin plastomer skin to improve heat-seal response. The core layer carrying the load-bearing fraction can contain 60 to 80 wt% of this LLDPE, while the outer layers contribute seal initiation and slip. A five-layer blown-film line with a 350 mm die and 2.5:1 blow-up ratio has been used to produce 60 µm heavy-duty sacks, with gauge bands held within ±5% by internal bubble cooling. In this structure, the stiffness contribution of HS-7094 NT 7 is measurable through an increase in machine-direction secant modulus when compared with a butene-based LLDPE of the same melt index.

    On a high-output cast-film line built around a 120 mm 30:1 single-screw extruder and a 1400 mm slot die, the resin is typically processed at melt temperatures from 220 °C to 250 °C. Chill-roll temperatures between 15 °C and 25 °C provide adequate quench without excessive condensation. Draw resonance in edge regions has been recorded when the draw ratio exceeded 20:1; reducing the die-gap-to-chill-distance and increasing melt temperature to 240 °C delayed the onset. These observations are from production-scale trials and are not intended as universal limits because die geometry and winder tension differ among installations.

    Melt-Rheology Signatures and Blown-Film Instability Envelope

    At 230 °C, the resin’s viscosity is high enough to generate melt pressure in the 250 bar to 400 bar range on a monolayer blown-film die, depending on output and lip gap. Processors running 24:1 L/D extruders may need to reduce screw speed or increase barrel set-points to keep the pressure below 400 bar. A dual-lip air ring with adjustable lower-lip jet provides the best gauge control at high throughput. A frost-line height below 300 mm from the die face tends to raise machine-direction tear but reduce dart impact in 25 µm film tested by ISO 7765-1:2004.

    Because the resin has lower melt strength than a high-pressure LDPE of similar melt index, the stable bubble envelope narrows when the blow-up ratio exceeds 2.8:1. A common remedy is to blend 5 to 15 wt% of a high-pressure LDPE, which increases bubble stability but reduces ultimate tensile strength and tensile modulus. The converter must decide whether the added toughness of the LLDPE component justifies the stiffness loss of the LDPE addition.

    For blown film at 25 µm gauge, a die gap of 1.5 mm to 2.5 mm and a blow-up ratio of 2.0:1 to 2.5:1 are common. Gauges below 20 µm may increase the occurrence of gels and die lines if the melt temperature is not maintained above 230 °C. If the film is used in food contact, the final article must satisfy the overall migration limits of Regulation (EU) No 10/2011, irrespective of the resin’s intrinsic compliance.

    In cast film, edge trim recycle of this resin can be added back at 10 to 30 wt% without measurable loss of dart impact at 25 µm, provided that the recycled fraction is not contaminated with polypropylene or paper fiber. Extruder filtration through a 100 mesh screen pack is recommended to protect narrow die lips from gels. The resin’s thermal stability permits a hold time of up to 20 minutes at 240 °C before measurable yellowing appears; this boundary is shorter than some C8 metallocene grades with higher stabilizer loading.

    When Additive Selection Determines Film Surface Performance

    Because the natural grade may not include a high slip level, coefficient of friction measured by ISO 8295 can remain above 0.50 unless slip additives are introduced. In high-speed form-fill-seal operations, film blocking at back-side guides has been traced to static charge and low slip, not to resin mechanical failure. Addition of 500 ppm to 1500 ppm of an erucamide or oleamide masterbatch reduces the coefficient of friction but may raise the seal initiation temperature and increase surface bloom. Antiblock loading of 1000 ppm to 4000 ppm is typical when the film is wound at high tension or stored in warm warehouses.

    Published data for optically demanding cast film below 15 µm is limited for this specific configuration; pilot-line verification is required before commercial production. Haze and clarity depend on quench rate, die-land finish, and additive bloom, not solely on resin density.

    The resin’s regulatory profile is summarized below; each requirement applies to the final article or the resin as part of a compound, not to the pellet in isolation.

    Regulatory ReferenceScopeVerification Boundary
    21 CFR 177.1520(c) 3.1bPolyethylene for food-contact applicationsVerification on finished article; conditions of use per 21 CFR 176.170(c)
    (EU) No 10/2011Plastic food-contact materialsOverall migration per Annex II; verification on final food-contact article
    Regulation (EC) No 1907/2006REACHPolymer registration exempt under Article 2(9); monomer and additive registration required
    Directive 2011/65/EURoHSHomogeneous-material thresholds for lead 1000 ppm, cadmium 100 ppm; final component must be tested

    Pellets should be stored in a dry, dust-free environment at ambient temperatures below 40 °C and relative humidity below 60%. Pre-drying is not normally required for sealed, dry shipments; if condensation from cold storage has occurred, a hopper dryer at 70 °C for 2 h can be used. Avoid melt temperatures above 280 °C to reduce oxidative yellowing and gel formation. The resin is not compatible with high levels of free-radical-generating peroxides or certain amine-based additives that can initiate premature crosslinking and reduce film tear.

    Top