Dow Tuflin Hs 7066 Nt 7 Linear Low Density Polyethylene Resin

Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin

    • Product Name: Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 584961
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.70 g/10 min
    Melt Flow Ratio I10 I2 28
    Melting Temperature Dsc 123 °C
    Vicat Softening Temperature 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 25.5 MPa
    Elongation At Break 800 %
    Flexural Modulus 1 Secant 255 MPa
    Hardness Shore D 50
    Low Temperature Brittleness < -70 °C
    Dart Drop Impact F50 190 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 450 g
    Haze 14 %
    Gloss 45 55 %

    As an accredited Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow TUFLIN HS-7066 NT 7 LLDPE resin is packaged in 25 kg (55 lb) polyethylene bags, usually palletized.
    Container Loading (20′ FCL) 20′ FCL container loaded with Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin, palletized bags, secured for shipment.
    Shipping Dow TUFLIN™ HS-7066 NT 7 LLDPE resin ships as non-hazardous solid pellets in moisture-barrier bags, octabins, or bulk trucks/railcars. Keep dry, shaded, and at ambient temperature; avoid UV, heat, and package damage. No special UN dangerous-goods classification is required.
    Storage Store Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, flames, and ignition sources. Keep packages clean, closed, and off the floor to prevent moisture, dust, and contamination. Protect from prolonged UV exposure. Use first-in, first-out rotation and avoid excessive stacking or high temperatures. Always follow supplier instructions.
    Shelf Life Dow TUFLIN HS-7066 NT 7 resin has a shelf life of about two years when stored cool, dry, and in original unopened packaging.
    Application of Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin

    In machine-grade cast pallet wrapping, TUFLIN™ HS-7066 NT 7 is introduced as an additive-rich outer-skin modifier in five-layer coextruded film rather than as a single-layer polymer. Typical addition rates in the outer skin lie between 18 wt% and 25 wt% of total film mass; the metallocene-catalysed LLDPE core accounts for 50–60 wt%, and the reverse skin is blended from LDPE and non-slip LLDPE at 15–20 wt%. The 25 wt% ceiling is process-defined. On a five-layer cast line with 33:1 L/D barrier screws and 150 mm extruders running at 250–265°C die temperature, raising the HS skin layer to 30 wt% produces measurable die lip bloom and winder-side blocking; the migratory oleamide/erucamide slip package increases film-to-metal friction on idle rollers so severely that web wander exceeds 1.5 mm at 300 m/min and edge trim waste rises above 6%. The cast process uses a 0.5–0.8 mm die gap, 25–40 mm air gap, 18–24°C chill roll temperature, and dual-stack vacuum pinning to stabilise melt web boundaries before the primary nip. The winder is programmed with a taper target of 20–25%; higher taper on film younger than 72 h aggravates blocking because the slip additive has not completed its surface migration. Batch-to-batch variation in slip concentration can shift aged film-to-film COF by 0.03–0.05; therefore, incoming lots are screened after 72 h ageing using ASTM D1894-14. Property release testing references ASTM D5748-19 for protrusion puncture resistance, ASTM D882-18 for tensile elongation at break, ASTM D1922-15 for Elmendorf tear, and ISO 1133-1:2022 for melt mass-flow rate. Regulatory surveillance includes EU Packaging and Packaging Waste Directive 94/62/EC heavy-metal limits and Regulation (EC) No 1907/2006 (REACH) for SVHC content. Terminal products are machine-applied pallet wrap rolls in 18–23 µm thickness, slit to 450–500 mm web width, pre-stretched at 150–250% on turntable, rotary arm, and orbital wrappers used in logistics hubs. Published machine-specific data for this exact grade in five-layer cast pallet wrap is limited; the window above is derived from solution LLDPE cast film practice and should be confirmed on a pilot line.

    Test methodPropertyTypical release band
    ASTM D1894-14Film-to-film kinetic COF, 72 h ageing0.15–0.25
    ASTM D5748-19Protrusion puncture resistance, 20 µm2.5–4.0 N/µm
    ASTM D882-18MD ultimate elongation350–450%
    ASTM D1922-15MD Elmendorf tear8–14 g/µm
    ASTM D1003-13Haze1.5–3.0%

    What Governs Neck-in and Tear Propagation in Down-Gauged Hand Stretch Wrap?

    Neck-in and tear propagation in hand stretch wrap are governed by melt elasticity, air-gap distance, and edge pinning, not by thickness alone. A starting formulation containing TUFLIN™ HS-7066 NT 7 at 55–65 wt%, a metallocene-catalysed LLDPE at 20–30 wt%, and an LDPE homopolymer at 10–15 wt% is run on a three-layer cast line with 30:1 L/D screws, die temperature 255–265°C, die gap 0.6–0.8 mm, and an air gap of 20–30 mm with compressed-air edge pinning. At 200 m/min, neck-in is kept below 8 mm per edge if the die lip exit temperature is held within ±3°C of the setpoint; deviations of ±5°C widen neck-in to 12–15 mm and shift shrinkage behaviour. Tear propagation is assessed after 72 h ageing because the migratory slip package in HS-7066 NT 7 changes surface crystallinity and interlayer entanglement; ASTM D1922-15 is used for Elmendorf tear, ASTM D5748-19 for puncture, and ASTM D882-18 for MD/TD elongation. The slip migration interval also imposes a packaging hold time: rolls wound before 48 h aging may display film-to-film kinetic COF above 0.45 on ASTM D1894-14, which alters hand unroll force. Downstream converters slit and rewind the hand wrap into 400–450 mm wide rolls of 10–15 µm film; terminal products are manual pre-stretch rolls used in low-throughput packaging stations where operator-applied extension is normally below 80%, not the 150–250% seen in machine wrap. Compliance for these industrial logistics films follows EU Packaging and Packaging Waste Directive 94/62/EC heavy-metal limits and Regulation (EC) No 1907/2006 for SVHC content; direct food contact is outside this scenario unless the final structure is separately certified under food-contact regulations.

    Food-contact overwrap seal initiation and migration potential

    Food-contact overwrap produced from a three-layer cast structure places TUFLIN™ HS-7066 NT 7 in the sealant layer at 70–85 wt% of that layer, diluted with 15–30 wt% LDPE to lower seal initiation. On a ram-type heat sealer, the layer reaches seal initiation below 105°C at 0.4 MPa pressure and 0.5 s dwell; seal strength is measured per ASTM F88/F88M-15 after 24 h. The HS slip package in the resin migrates to the surface and creates a non-blocking, low-COF overwrap; however, this migration kinetics imposes a 24–72 h ageing window before the target film-to-film COF of 0.15–0.25 under ASTM D1894-14 is reached. Converters that convert film into rollstock immediately after slitting may observe blocking because migrated slip has not yet formed a continuous surface layer. The cast process uses die temperature 240–260°C, a 0.5–0.6 mm die gap, 20–30 mm air gap, and a chill roll setpoint of 15–20°C for optical uniformity; gauge variation across the web is held below ±3% by automatic air-bolt profile systems. Tensile properties are additionally screened by ISO 527-3:2018 for thin-film elongation under machine and transverse directions. Direct food-contact suitability is evaluated under FDA 21 CFR 177.1520(c), EU Regulation 10/2011 with overall migration limit 10 mg/dm² and its Annex I simulant assignments, plus Regulation (EC) No 1935/2004 Article 3. Terminal products are transparent food-service and retail overwrap rolls of 8–15 µm, used for wrapping meat trays, cheese, and produce at chilled retail counters; the film is not specified for retort, microwave-in-pack, or hot-fill above 85°C because seal strength and migration behaviour are not validated for those thermal loads.

    On a three-layer blown film line with 80 mm grooved-feed extruders, a 400 mm die diameter, BUR 2.2–2.8, and frost-line height 500–700 mm, TUFLIN™ HS-7066 NT 7 is added at 25–35 wt% of the total formulation; the remainder of the blend is LDPE at 55–65 wt% and EVA with 14–18% vinyl acetate at 8–12 wt%. The blown-film route provides biaxial orientation sufficient for temporary protection film applied to polycarbonate sheet, float glass, and acrylic panels during storage and site transport. The target thickness of 25–50 µm is controlled by gravimetric yield, and the film is tested for Elmendorf tear using ASTM D1922-15 and haze using ASTM D1003-13; haze above 5% is rejected when the film is specified for optically clear glazing surfaces. Surface tension after corona treatment must remain above 38 dyn/cm for masking adhesion, but the migratory slip package in HS-7066 NT 7 can depress retreatment effectiveness if the film is stored longer than 90 days; converters therefore re-confirm wetting tension by ASTM D2578-17 before slitting. Regulatory compliance for the protection film follows Regulation (EC) No 1907/2006 for SVHC content; Directive 2011/65/EU may apply only if the protection film is incorporated into electrical or electronic equipment. Terminal products are surface protection rolls in 1500–2000 mm slit widths with solvent-free adhesive coating applied downstream by converters, not by the film producer.

    Stretch hood load retention after 200% pre-stretch and winder taper control

    Stretch hood load retention after 200–250% pre-stretch is measured with ASTM D5459-17 for machine-direction elastic recovery and permanent deformation; load retention loss above 12% after 30 min indicates unsatisfactory elastic recovery for palletized building insulation or brick packs. A five-layer cast structure for hood film uses TUFLIN™ HS-7066 NT 7 in the outer skin at 20–25 wt%, a metallocene-catalysed LLDPE core at 45–50 wt%, and a blended LDPE/plastomer inner skin at 25–30 wt%. The outer skin is the blocking-critical surface: the HS package must complete its diffusion to the surface before film-to-film contact at the winder; rolls wound with taper above 35% at line speeds above 250 m/min exhibit blocking layers within the first 20 mm of core diameter. The cast film line uses a 0.9–1.2 mm die gap, die temperature 260–270°C, MDO pre-stretch ratios of 160–220%, and a layflat width of 1.8–2.2 m before weld-bar conversion. The weld bar operates at 150–180°C and must deliver a seal that does not fail during vertical hood application; weld seam strength is verified by ASTM F88/F88M-15 on 25 mm specimens. Terminal products are stretch hood bags or continuous hood stock applied by stretch hooders in construction material packaging, appliance logistics, and palletized beverage lines. Published data for the exact TUFLIN HS-7066 NT 7 hood structure is limited; the above parameters are therefore screened against general cast film practice and should not be used as a release specification without pilot verification. Compliance is assessed under EU Packaging and Packaging Waste Directive 94/62/EC and Regulation (EC) No 1907/2006.

    When TUFLIN HS-7066 NT 7 Is Diluted as a Low-Seal-Temperature Sealant Web in Laminated Dry-Food Packaging

    When TUFLIN™ HS-7066 NT 7 is diluted to 15–25 wt% in a cast sealant web blended with 70–80 wt% LDPE and 5–10 wt% EVA, the seal initiation temperature shifts low enough for lamination to metallized oriented polypropylene or PET without distorting the print web. The cast sealant web is extruded through a 0.5 mm die gap at 240–260°C with 25–35 mm air gap and 15–20°C chill roll; it is then adhesive-laminated in-line before pouch conversion. Seal bar temperature at the converter is set at 105–120°C with 0.35–0.55 MPa pressure and 0.4–0.8 s dwell; seal strength is measured per ASTM F88/F88M-15. The HS additive package continues to migrate after lamination, so finished pouches should not be stacked under high humidity above 60% RH until the 72 h ageing window has closed or the outer slip effect may cause inter-pouch slippage. Direct food-contact suitability is evaluated under FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 with overall migration limit 10 mg/dm². Terminal products are dry-food pouches for granular products such as rice, pulses, or powdered beverage mixes; the sealant web is not specified for retort, microwave, or high-grease-fatty-food contact above 40°C unless specific migration testing is completed on the final laminate.

    Free Quote

    Competitive Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow TUFLIN™ HS-7066 NT 7 Linear Low Density Polyethylene Resin is a natural-pellet ethylene-alpha-olefin copolymer supplied for film extrusion where impact resistance, tear propagation resistance, and stable blown-film bubble geometry are required. The product is used in heavy-duty shipping sacks, industrial liners, agricultural silage covers, and certain high-integrity food packaging applications when film thickness is below 125 µm and the converter requires a resin that can hold a uniform bubble on large-diameter dies. The values given in this technical description are nominal supplier-published values and should be confirmed against the lot certificate of analysis because additive package, production site, and sampling conditions can shift delivered properties.

    Material Identity and Specification Profile

    The resin is classified in the 0.918 g/cm³ density class of linear low density polyethylene. The melt index of 0.90 g/10 min places it on the higher-viscosity side of normal film grades, increasing die pressure and melt strength relative to cast-film grades in the 1.5–2.0 g/10 min range. Table 1 lists the resin properties that define the material specification; film mechanical properties are not fixed because dart impact, tear, tensile, and haze are controlled by fabrication.

    PropertyNominal ValueTest Standard
    Melt index0.90 g/10 minASTM D1238, 190°C/2.16 kg; ISO 1133-1:2022
    Density0.918 g/cm³ASTM D1505; ISO 1183-1:2019
    Crystalline melting temperature122°CASTM D3418; ISO 11357-3

    The crystalline melting temperature is measured by differential scanning calorimetry at a heating rate of 10 K/min. Lot-to-lot variation for solution-processed LLDPE commonly falls within ±0.001 g/cm³ for density and ±0.05 g/10 min for melt index, though the certificate of analysis is the controlling document.

    For reproducible melt-index determination, pellet samples are conditioned at 23±2°C and 50±5% relative humidity according to ISO 291 or ASTM D618. If pellets are tested immediately after storage in a humid warehouse, surface water can produce slight apparent melt-flow variation and internal bubbles in the extrudate. Density specimens are prepared by compression molding and annealed to remove thermal history before measurement in a gradient column.

    Rheologically, the low melt index corresponds to a higher shear viscosity than general-purpose cast-film resins. On a standard 90 mm grooved-feed single-screw extruder with a 30:1 L/D barrier screw, melt temperatures of 190–225°C are maintained at the die, and die pressure is typically below 35 MPa at outputs up to 220 kg/h when the die gap is 2.0 mm. The lower melt index raises motor load relative to a 1.0 g/10 min LLDPE because shear heating is a stronger contributor to the energy balance; converters changing grades should monitor thermocouple readings and screw speed rather than relying solely on barrel set-point temperature.

    Capillary rheometry at 190°C and shear rates of 100–1000 s⁻¹ is recommended for die design because the public datasheet does not provide a full viscosity curve. Melt elasticity is lower than that of high-pressure LDPE, which reduces draw resonance but also reduces bubble self-healing.

    Why does this grade demand more bubble stabilization than high-pressure LDPE?

    Linear low density polyethylene of this type contains limited long-chain branching. Extensional viscosity at high strain is therefore lower than that of high-pressure LDPE, making the bubble more sensitive to air-ring instability, ambient drafts, and frost-line movement. A typical starting window on a 250 mm three-layer die with dual-lip air ring is a blow-up ratio of 2.0:1–2.8:1, an external air-ring pressure of 4–6 kPa, and a frost-line height of 600–900 mm. If internal bubble cooling is used, the supply air temperature is usually held at 10–20°C. Frozen-film stability is reduced when the melt temperature at the die exceeds 240°C, because thermal degradation can simultaneously reduce viscosity and generate gel particles.

    When bubble instability persists at normal conditions, the first checks are die alignment, air-ring centering, and frost-line height. Vortex instability in the melt can be aggravated by die gaps below 1.4 mm or output rates above 250 kg/h without internal bubble cooling. The upper practical melt temperature of 240°C should not be exceeded for more than 10 min; repeated thermocouple excursions above 250°C produce oxidative gels that appear as arrowhead defects.

    On cast-film equipment, the product can be processed as a core or sealant layer in stretch wrap and industrial film. Because the melt index is below 1.0 g/10 min, melt curtain sag and edge neck-in require attention. A die-to-nip distance of 10–15 mm and a chill-roll temperature of 15–25°C are common starting points; lower roll temperatures increase surface gloss but can increase retained stress and blocking. Published data for this specific configuration is limited, and pilot-line trials are required to define the exact window for a given die, winder, and gauge-control system.

    Barrier screws with mixing pins or Maddock mixers are used to homogenize the high-viscosity melt. Conventional three-zone screws may produce melt-temperature heterogeneity when the resin is run at high output. If unmelted pellets appear in the film, the barrier flight clearances should be checked before increasing barrel temperature.

    When a converter evaluates HS-7066 NT 7 against butene and metallocene grades

    Against a butene-copolymer LLDPE of similar density and melt index, this grade is expected to show higher dart impact and higher Elmendorf tear because hexene-derived short-chain branches create a more efficient tie-chain network in blown film. The effect is especially visible in films above 50 µm; below 25 µm, the thickness itself limits the tear zone and the difference is smaller. Against a metallocene-catalyzed hexene LLDPE, this grade typically exhibits a broader molecular weight distribution, higher melt strength, and lower clarity. Gloss measured per ISO 2813 and haze measured per ISO 14782 on a 50 µm film will be inferior to metallocene grades at the same density, but bubble stability on large dies is generally better because the melt resists sag and sway more effectively.

    Compared with DOWLEX™ 2045G, a general-purpose Dow LLDPE with nominal density 0.920 g/cm³ and nominal melt index 1.0 g/10 min, this resin has a lower density and a lower melt index. The density reduction of 0.002 g/cm³ corresponds to a measurable reduction in crystalline volume fraction and therefore a shift toward lower modulus and higher low-temperature stress-crack resistance. The melt-index reduction from 1.0 g/10 min to 0.90 g/10 min is small but sufficient to raise screw torque and die pressure on an existing line; no universal screw-speed correction is available, and the converter should record pressure, melt temperature, and output during grade transition.

    In coextruded heavy-duty sacks, the resin is placed in the core layer to provide toughness while LDPE or metallocene skins provide heat seal and optical surface quality. In a three-layer A/B/A structure, the core layer can be 60–70% of total thickness, with skin layers containing slip and antiblock to control coefficient of friction per ISO 8295.

    Operational Boundaries for Moisture, Regrind, and Thermal History

    Surface moisture is the main handling constraint. Pellets stored in unheated silos or exposed to relative humidity above 60% can accumulate condensation on the pellet surface, which produces splay and bubble defects. A hopper dryer set at 70–80°C for 4–6 h removes surface water. Regrind of this resin may be incorporated at 15–30 wt% if the regrind is free of gel contamination and has not been subjected to more than three heat histories. Thermal exposure above 250°C for more than 10 min should be avoided because oxidative chain scission and crosslinking can produce gel particles and reduce impact properties. During a shutdown, the extruder should be purged with a lower-viscosity LDPE before barrel temperatures drop below 160°C to prevent solidification of high-viscosity material in the die.

    In food-contact applications, the converter must verify compliance under 21 CFR 177.1520(c) for olefin polymers, including end-use temperature and food-type restrictions. Regional requirements such as EU Regulation 10/2011 and GB 9685-2016 may require additional migration testing. In heavy-duty sacks and silage covers, 10–20 wt% high-pressure LDPE is often added to improve bubble stability and reduce block wear. For high-gloss and low-haze packaging, the resin is less suitable than metallocene LLDPE or LDPE-rich blends because the broader crystallite size distribution increases surface haze. The final film specification is confirmed by testing production film per ASTM D1709 or ISO 7765-1:2003 for dart impact, ISO 6383-2 for tear, and ISO 527-3 for tensile properties.

    Sealing of this grade in coextruded structures is controlled by seal-bar temperature and dwell. Lower density LLDPE typically shows seal initiation near 95–105°C; converters should confirm the actual heat-seal curve because the surface-layer additive package and film gauge shift seal initiation. Hot-tack strength is evaluated per ASTM F1921 or JIS Z 1707 on production film.

    For agricultural exposure exceeding one season, the base resin requires UV stabilization. Carbon black masterbatch at 2–3 wt% or hindered amine light stabilizer packages are used to control chain scission; the exact dosage is determined by exposure region, film thickness, and expected service life. Without UV stabilization, rapid loss of elongation is observed in outdoor weathering per ISO 4892-2.

    Top