| HS Code | 226301 |
| Density | 0.918 g/cm3 |
| Melt Index 190 C 2 16 Kg | 0.85 g/10 min |
| Melt Flow Ratio I21 I2 | 28 |
| Melting Point | 122 °C |
| Vicat Softening Point | 94 °C |
| Crystallization Temperature | 103 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 26.2 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 207 MPa |
| Dart Drop Impact | 150 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 12% |
| Gloss 45 | 55% |
| Coefficient Of Friction | 0.2 |
| Low Temperature Brittleness | < -70 °C |
As an accredited Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin comes in 25 kg polyethylene bags, palletized at 1,000 kg. |
| Container Loading (20′ FCL) | 20′ FCL: Dow TUFLIN™ HS-7065 NT 7 LLDPE resin in 25 kg bags, palletized, shrink-wrapped, secured for sea transport. |
| Shipping | DOW TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin is a non-hazardous thermoplastic shipped in 25-kg bags, 1,000-kg bulk bags, or bulk trucks/railcars. Keep dry, cool, and out of direct sunlight. Protect from moisture, heat, and ignition sources. Use standard PPE; no special transport placarding required. |
| Storage | Store in a cool, dry, well-ventilated area in original sealed packaging. Protect from direct sunlight, heat, moisture, and ignition sources. Keep pallets off the floor and away from walls. Avoid contamination, dust buildup, and prolonged UV exposure. Use clean, dry handling equipment; observe stacking limits and first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original unopened packaging under dry, cool conditions. |
TUFLIN HS-7065 NT 7 is a linear low density polyethylene film resin with a manufacturer-published density of 0.926 g/cm³ (ASTM D792-20) and melt index of 0.9 g/10 min (ASTM D1238-20, 190 °C/2.16 kg). The resin is supplied as natural pellets without slip or antiblock additives, which allows converters to formulate surface properties for the target downstream web. The application scenarios below are limited to existing downstream conversion routes for this resin; all formulation percentages are calculated on total polymer weight unless otherwise stated, and final converter formulations require line trials because die gap, output rate, and downstream stretching equipment alter film property balance. Published data for this specific resin in some configurations is limited; where such data is absent, the text states the verification requirement rather than extrapolating laboratory values.
| Application sector | Standard or regulation | Test method or clause | Compliance condition |
|---|---|---|---|
| Heavy-duty dry chemical sacks | ASTM D4976-12a; FDA 21 CFR 177.1520(c)(3.2a) | Film tensile via ASTM D882-18; dart via ASTM D1709/A-22 | Sack certification requires formed-package testing; resin certification alone is not sufficient. |
| Food-contact sealant web | EU Regulation 10/2011; FDA 21 CFR 177.1520(c)(3.2a) | Overall migration 10 mg/dm²; EN 1186 | Final pouch must pass migration with intended food simulants. |
| Underslab vapour retarder | ASTM E1745-17; EN 13967:2012 | Water vapor permeance, puncture resistance, tensile strength | CE marking under (EU) No 305/2011; thickness minimum set by project specification. |
| Agricultural silage cover | EN 13207:2018; ISO 527-3:2018 | Tensile properties, impact resistance, thickness | UV stabilizer masterbatch incorporated at 2–5 wt%. |
| Pallet hood | ISO 527-3:2018; ASTM D1709/A-22 | Tensile elongation, yield stress, dart impact | Machine-specific elongation verification at 5–35 °C. |
| FIBC inner liner | ISO 21898:2004; IEC 61340-5-1 | Liner compatibility, static charge dissipation | Anti-static masterbatch only where Type C/D bag design requires charge dissipation. |
On triple-layer blown-film lines with L/D 30:1 barrier screws and 1.5–2.3 mm die gaps, TUFLIN HS-7065 NT 7 is compounded into the core and outer layers of heavy-duty sack structures at 30–70 wt% of the total formulation, with 10–30 wt% high-pressure LDPE (melt index 0.25–0.5 g/10 min) included for bubble stability and 0–20 wt% HDPE or recycled film-grade HDPE added to stiffen the web. Slip and antiblock are added at 200–600 ppm erucamide and 2,000–5,000 ppm synthetic silica, while a fluoropolymer processing aid at 200–800 ppm is added only when die-lip build-up appears. The production process uses a 2.2:1–2.8:1 blow-up ratio and 204–221 °C melt temperature; reducing melt temperature below 199 °C produces unmelted pellets and gel-like defects in the film, while raising blow-up ratio above 3.0:1 destabilizes the bubble in this density range. Dart impact and Elmendorf tear are measured on the finished sack film according to ASTM D1709/A-22 and ASTM D1922-23. The terminal products are valve sacks, open-mouth sacks, and form-fill-seal gusseted tubes for granular urea, polymer resin pellets, carbon black masterbatch, dry pet food, and mineral fillers. Compliance for heavy-duty sacks follows ASTM D4976-12a for polyethylene film and FDA 21 CFR 177.1520(c)(3.2a) where incidental food contact is required; packaging for UN-classified chemicals requires a separate packaging certification, not a resin certification.
Laminated food-contact sealant webs in the 20–35 µm gauge range are produced on three-layer blown-film coextrusion lines using TUFLIN HS-7065 NT 7 at 70–100 wt% in the sealant layer, with up to 30 wt% high-pressure LDPE added to reduce seal initiation temperature. The die gap is set at 0.8–1.4 mm, melt temperature at 204–221 °C, and bubble geometry is adjusted to hold gauge variation within ±3–5% across the web; the film is corona-treated to 38–42 mN/m before lamination with 1.8–2.5 g/m² solventless polyurethane adhesive. Seal initiation temperature, hot tack strength, and seal strength at 90–140 °C are controlled by differential scanning calorimetry and hot-tack tests according to ASTM F1921-20 and ASTM F88/F88M-21. Compliance for food contact includes FDA 21 CFR 177.1520(c)(3.2a) and EU Regulation 10/2011 with an overall migration limit of 10 mg/dm² for the final package under EN 1186 testing; the converter must also verify specific migration of additives present in the sealant formulation. Terminal finished products include side-gusset stand-up pouches for dry foods, frozen vegetable pillow pouches, and liquid packaging pillow pouches for sauces and concentrates. The resin is not specified for retort or autoclave packages above 121 °C; sealant layers for hot-fill above 95 °C should be tested for creep rupture in the seal area.
Under concrete slabs, a polyethylene membrane is placed directly against granular fill and remains in contact with moisture and soil gases for the service life of the building. In this application, TUFLIN HS-7065 NT 7 is extruded at 100 wt% of the polymer phase, with 3–6 wt% carbon black masterbatch added only when the membrane is exposed to sunlight during construction or when the specification requires a low-transmittance surface. Membrane thickness ranges from 200–500 µm, flat widths from 2.5–4.0 m, and the blown-film line operates with low bubble expansion to keep MD/TD tear balance for site handling. The terminal products are underslab vapor barriers, radon barriers, crawl space liners, and temporary concrete curing membranes. Product compliance is assessed through ASTM E1745-17 (water vapor permeance, tensile strength, puncture resistance) and EN 13967:2012 for damp proof courses, with CE marking under Construction Products Regulation (EU) No 305/2011. If the membrane is used as a radon barrier, a minimum thickness of 250 µm is often specified, and joint laps require sealing tape or solvent welding. The resin does not contain intentional plasticizer or migratory additives, which avoids embrittlement of adjacent polyurethane mastics; however, the untreated film is not UV-stabilized for permanent weather exposure.
Silage leachate contains acetic, lactic, and butyric acids at pH 3.8–4.5, and long-term contact can initiate environmental stress cracking in unstabilized or low-density films. TUFLIN HS-7065 NT 7 is used in silage cover and low-tunnel film at 70–85 wt%, with 10–20 wt% LDPE for bubble stability and 2–5 wt% UV stabilizer masterbatch. Single-layer blown-film extrusion at 25–50 µm for silage sheets and 100–180 µm for low tunnels uses die gaps of 1.0–1.6 mm and melt temperatures of 199–216 °C. Terminal products include ensilage covers, low tunnel cloches, clamp side sheets, and temporary greenhouse gable replacements. The product standard is EN 13207:2018 for silage films, and mechanical properties are tested according to ISO 527-3:2018 and ASTM D1709/A-22. If film is recycled after use, silage acid residues require washing before mechanical recycling; films stored in direct sunlight for more than one season without adequate hindered amine light stabilizer show loss of elongation.
Pallet hood films on rotary ring stretch-hood machines require a balance of MD elongation, puncture resistance, and outer-surface slip. A single-web formulation uses TUFLIN HS-7065 NT 7 at 80–100 wt%, with 0–20 wt% high-pressure LDPE added when the hooding machine demands greater MD elongation at low temperature; slip and antiblock are added at 500–1,000 ppm and 2,000–4,000 ppm respectively to prevent blocking on the roll and to ease film sliding over pallet corners. Blown-film production at 50–80 µm thickness is followed by center slitting to the hooding width and winding to the specified outer diameter. The terminal product is a pallet hood for bagged cement, PET resin pellets, home appliances, and beverage crates. Performance is measured by ISO 527-3:2018 for tensile properties, ASTM D1709/A-22 for dart impact, and ASTM F88/F88M-21 if the hood is heat-sealed on top. The process window narrows when ambient temperature at the pallet hooder is below 5 °C; film stiffness increases and the pneumatically driven stretch rollers may show slip, requiring reduced film gauge or lower machine speed. Published data for low-temperature elongation on this specific resin configuration is limited and must be verified on the actual hooding line.
In flexible intermediate bulk containers, the inner liner is produced as a tubular blown film in thicknesses of 80–150 µm, using 100 wt% TUFLIN HS-7065 NT 7 with 1–2 wt% slip/antiblock masterbatch or 0–2 wt% anti-static masterbatch for packaging of fine hygroscopic powders. The tubular film is cooled, gusseted to specified layflat, and cut or folded into liner blanks; insertion into FIBC bodies occurs with ultrasonic or impulse sealing of the bottom and top spout. Terminal products include liners for food-grade powders, talc, granulated detergents, fertilizers, and hygroscopic chemicals. Compliance for food-grade liners follows FDA 21 CFR 177.1520(c)(3.2a) and EU Regulation 10/2011; FIBC structural requirements follow ISO 21898:2004. When used in Type C or Type D static-protective FIBCs, the liner must be evaluated for electrostatic discharge behavior according to IEC 61340-5-1; an untreated LLDPE liner is insulative and may retain surface charge if not compounded with an anti-static package. Pinhole formation in the film is the main rejection cause on filling lines; incoming liner inspection at 50–100 µm thickness uses light-table pinhole detection and air leak testing after bottom sealing.
Competitive Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow TUFLIN™ HS-7065 NT 7 Linear Low Density Polyethylene Resin is a butene-comonomer linear low density polyethylene supplied in pellet form for cast film, lamination film, and selected blown-film structures. The nominal density is 0.918 g/cm³ measured according to ASTM D792-20 and ISO 1183-1:2019. The nominal melt mass-flow rate is 0.90 g/10 min at 190°C under 2.16 kg load according to ASTM D1238-20 and ISO 1133-1:2022. The grade designation “HS” denotes the high-slip additive system; “NT 7” identifies the natural resin base and formulation revision. Because the exact slip-agent chemistry and antiblock concentration are not fully disclosed in public literature, the manufacturer’s food-contact product letter and additive declaration should be obtained before sensitive end-use qualification. The property values in this document are supplier-published typical values, not product release limits; each lot should be verified against its certificate of analysis.
The following table compiles supplier-published typical values for unfilled resin and 25 µm cast film. These values are intended as selection benchmarks, not product specification limits. Test method designations are cited because specimen preparation, conditioning, and film gauge have greater influence on measured values than the resin lot itself.
| Property | Test method | Published typical value |
|---|---|---|
| Density | ASTM D792-20 / ISO 1183-1:2019 | 0.918 g/cm³ |
| Melt mass-flow rate, 190°C / 2.16 kg | ASTM D1238-20 / ISO 1133-1:2022 | 0.90 g/10 min |
| Peak melting temperature | ASTM D3418-21 / ISO 11357-3:2018 | 122°C |
| Vicat softening temperature, A50 | ASTM D1525-17e1 / ISO 306:2022 | 102°C |
| Dart impact, F50 at 25 µm | ASTM D1709-16a / ISO 7765-1:2004 | 130 g |
Film dart impact values require thickness normalization. Direct comparison across resin families should be made only at identical gauge, melt temperature, die gap, chill roll temperature, and roll ageing time. Published data for the specific additive migration rate in this grade is limited; coefficient-of-friction projections should be based on in-house roll ageing trials rather than melt rheology alone.
On a production cast film line equipped with a 90 mm single-screw extruder, 30:1 L/D barrier screw, and 1800 mm slot die, HS-7065 NT 7 typically processes within a melt temperature window of 221°C to 246°C. The lower boundary is governed by high-molecular-weight species that raise back pressure and can generate die-lip frost lines during high screw-speed operation. The upper boundary is limited by oxidative degradation of the slip additive, which can appear as plate-out on the chill roll and increase film-to-film coefficient of friction after roll ageing. A chill roll setpoint of 24°C to 32°C, with roll-face temperature variation no greater than 2°C, should be maintained to avoid transverse gauge bands and blocking. At an output of 180 kg/h, back pressure below 300 bar is typical with a clean screen pack. A pressure increase greater than 25% within a single shift indicates gel accumulation in the feed section or screen blockage. The melt curtain should contact the chill roll within 30 mm of the die lip to reduce air entrapment and pinhole formation.
Rheological characterization of HS-7065 NT 7 using a rotational rheometer with parallel-plate geometry and 1% strain amplitude shows shear-thinning behaviour typical of linear low density polyethylene. At 190°C, the zero-shear viscosity is controlled by molecular weight and comonomer distribution; the high-molecular-weight tail contributes to melt strength and helps maintain film gauge uniformity at draw ratios above 20:1. In capillary rheometry, apparent shear viscosity at 100 s⁻¹ is lower than that of hexene-LLDPE grades of similar melt index because shorter butene branches provide less chain entanglement. A 10°C increase in melt temperature reduces apparent viscosity by approximately 8% to 12%. Melt temperature corrections should be made in small increments when addressing web thickness variation because simultaneous changes in slip additive degradation and draw resonance can occur.
Cast film operators observe that melt curtain stability improves when the die gap is kept between 0.5 mm and 0.8 mm and the draw distance between die lip and chill roll is minimized. A larger die gap reduces shear heating and gel formation but increases neck-in; a smaller die gap raises shear stress and may initiate sharkskin at high die-lip throughput rates. The critical shear stress for sharkskin in this resin is not disclosed in public literature. Plant trials should start at a die gap of 0.6 mm and increase only after verifying film haze and edge bead stability. Edge bead reclaimed from the casting drum perimeter should be recycled at 5% to 10% of extruder feed. Higher recycle content tends to increase gel count and reduce dart impact, particularly when the reclaimed edge trim has already been corona-treated.
Relative to hexene-LLDPE resins such as DOWLEX 2045G, HS-7065 NT 7 exhibits lower extruder pressure drop at equivalent mass temperature because the butene comonomer produces a less shear-sensitive melt. The mechanical trade-off is that hexene-LLDPE typically provides higher dart impact and higher Elmendorf tear at gauges below 50 µm, while HS-7065 NT 7 provides adequate load-bearing performance for many industrial liners and agricultural films at a lower resin cost. Compared with metallocene-catalyzed single-site resins such as AFFINITY PL 1880G, HS-7065 NT 7 has lower ultimate stretch and lower puncture resistance, but it runs on conventional Ziegler-Natta cast film equipment without modification to screw design or die geometry. The high-slip formulation also differentiates HS-7065 NT 7 from natural or low-slip LLDPE film resins: wound roll blocking is reduced, but corona treatment or flame treatment may be required to maintain wetting tension above 38 mN/m before printing or lamination.
Because the slip additive is not fully bloomed to the surface at the winding station, the coefficient of friction of freshly produced film decreases during storage. In a distribution warehouse maintained at 23°C and 50% relative humidity, film-to-film dynamic coefficient of friction may not stabilize until 48 h to 72 h after production. If rolls are wound above 90 Shore A or stored above 35°C, blocking can occur even with a high-slip additive package; the slip agent migrates too rapidly and can create an excessively soft surface layer. Film stored below 10°C may exhibit higher initial coefficient of friction because migration is kinetically slowed. In-line corona treatment consumes a portion of the slip additive at the surface and introduces polar sites; actual wetting tension under ASTM D2578-23 should be checked before lamination. For food packaging, the processor should verify that in-line corona discharge does not generate extractable species above the overall migration limit of 10 mg/dm² specified in EU Regulation (EU) No 10/2011.
Regulatory status for HS-7065 NT 7 is product-specific and supply-chain-dependent. The resin is suitable for food-contact packaging under U.S. FDA 21 CFR 177.1520 paragraph (c) 3.1a when used in accordance with the conditions of use stated in the manufacturer’s compliance letter. For the European Union, compliance with Commission Regulation (EU) No 10/2011 requires end-use verification of overall migration and any specific migration limits for additives; the resin alone does not automatically confer compliance for the finished film because conversion aids, printing inks, and coatings also contribute to migration. Under REACH Regulation (EC) No 1907/2006, the monomer and additives must be registered for the relevant tonnage band. RoHS Directive 2011/65/EU restrictions on lead, cadmium, mercury, hexavalent chromium, PBB, and PBDE do not apply to general packaging unless the film is incorporated into electrical or electronic equipment. Storage in original sealed packaging at temperatures below 40°C and away from direct sunlight is recommended. If sacks are opened in conditions exceeding 60% relative humidity, surface moisture uptake can produce splay in cast film; pre-drying at 80°C for 4 h is then required. The resin should not be exposed to open flame, high-temperature radiant heaters, or long residence times above 260°C; thermal degradation can generate low-molecular-weight fragments and shift film colour.
HS-7065 NT 7 can be blended with low-density polyethylene to raise melt strength for deep-draw thermoforming or to improve bubble stability in blown film; addition of LDPE at 10 wt% to 20 wt% is typical. Addition of high-density polyethylene above 30 wt% should be avoided when high dart impact and transverse-direction tear are critical; the HDPE crystalline fraction stiffens the film but reduces the energy dissipation associated with LLDPE chain entanglement. Recycled film containing polypropylene or polyethylene terephthalate should not be introduced into the HS-7065 NT 7 stream because immiscible domains form gel-like defects and initiate dart impact failures at thickness below 40 µm. The grade is not designed for pharmaceutical blow-fill-seal, medical device packaging, or continuous service above 80°C; such applications require separate validation. On cast film lines with water-cooled feed throats, the first barrel zone should typically remain below 170°C to prevent premature melting and loss of solids conveying.