| HS Code | 110170 |
| Product Name | Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
| Density | 0.918 g/cm³ |
| Melt Index | 1.0 g/10 min |
| Melting Point | 123 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 26.2 MPa |
| Elongation At Break | 700% |
| 1 Secant Modulus | 190 MPa |
| Dart Drop Impact | 200 g |
| Elmendorf Tear Md | 300 g |
| Elmendorf Tear Td | 400 g |
| Haze | 10% |
| Gloss 60 | 80% |
As an accredited Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Packaged in 25 kg polyethylene bags, stacked on pallets, with optional 1,000 kg bulk bags. |
| Container Loading (20′ FCL) | 20′ FCL: approximately 18 MT (720 × 25 kg bags) floor loaded; palletized loads lower, subject to carrier weight limits. |
| Shipping | Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin is shipped as non-hazardous resin pellets, typically in 25 kg polyethylene bags on stretch-wrapped pallets. Bulk truck or railcar delivery may also be available. Store in a dry, cool, ventilated area away from direct sunlight, heat, and ignition sources. |
| Storage | Store Dow TUFLIN™ HS-7041 NT 7 in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture, dust, and contamination. Protect from prolonged UV exposure and extreme temperatures. Use clean, dedicated handling equipment. Follow local regulations and maintain good housekeeping to avoid slips from spilled pellets. |
| Shelf Life | Shelf life is 24 months from production when stored in original unopened packaging under cool, dry conditions. |
In three-layer cast stretch film lines running at 500–800 m/min, converter experience with hexene-LLDPE grades of 0.918 g/cm³ density and 1.0 g/10 min melt index indicates that die gap selection below 0.7 mm is critical for suppressing draw resonance when TUFLIN HS-7041 NT 7 linear low density polyethylene resin is used as the primary core component. Typical formulation for a machine-grade A/B/C structure is 70–85 wt% TUFLIN HS-7041 NT 7 in the core layer, 15–30 wt% skin-layer LDPE or plastomer for tack and cling, and 2–5 wt% polyisobutylene or metallocene tackifier masterbatch in the skin layers; single-layer converter structures may run the resin at 100 wt% neat, relying on the product’s built-in slip and antiblock formulation. Downstream production equipment includes a multi-channel feedblock and a coat-hanger manifold die, with a die gap of 0.5–0.8 mm, air gap of 60–120 mm, and chill roll temperatures maintained at 12–18°C. Melt temperatures at the die exit are typically held between 250 and 280°C, while electrostatic pinning is applied at 4–8 kV to stabilise the melt web against the primary chill roll. Gravimetric dosing of tackifier masterbatch at the skin extruder of a 55–75 mm single-screw extruder with an L/D ratio of 30:1 reduces batch-to-batch cling variation, and automatic gauge scanners normally hold film thickness variation within ±2% at 20 µm.
Compliance assessment for industrial stretch film made from this resin is performed under the European Packaging and Packaging Waste Directive 94/62/EC Article 11 heavy metal limits, REACH Annex XVII entries, and, where food contact is specified, FDA 21 CFR 177.1520(c) 3.1a and EU Regulation (EU) No 10/2011. The terminal product includes machine pallet wrap rolls in 350–500 mm width, hand stretch wrap in 100–150 mm width, and pre-stretched films produced at 150–300% draw ratio. A production-scale failure mode observed on cast lines running this polymer class is edge trim-induced gel formation when the melt temperature exceeds 300°C for more than 20 minutes; start-up purges should not exceed 290°C barrel set points without screw dry-running protection. The resin is not suitable for continuous exposure to aromatic hydrocarbons or chlorinated solvents, which may plasticise the film and reduce retained stretch force below load-stability requirements.
Because high-stalk blown film stability is governed by extensional viscosity rather than shear viscosity, the converter running TUFLIN HS-7041 NT 7 for heavy-duty shipping sacks will observe that lowering die lip exit temperature below 200°C can reduce bubble stability and create melt fracture at the die lip, while pushing die exit temperature above 230°C accelerates antioxidant depletion in the melt film. The extrusion window on a 65–90 mm single-screw extruder with an L/D ratio of 25:1–30:1 is set at 190–220°C for the rear zones and 210–230°C at the die; die gap is held at 1.6–2.0 mm for film thicknesses of 60–150 µm, and blow-up ratio is limited to 2.5:1–3.0:1 to control dart impact in the machine direction. Internal bubble cooling and a dual-lip air ring with a pressure differential of 0.05–0.10 bar allow frost line heights between 6 and 8 die diameters without destabilising the high-stalk configuration.
The compounding ratio for this application is 70–85 wt% TUFLIN HS-7041 NT 7 and 15–30 wt% high-pressure LDPE with a melt index of 0.2–0.5 g/10 min; where bending stiffness must be raised, 10–20 wt% of an HDPE with density 0.954–0.960 g/cm³ can replace part of the LDPE. Compliance testing for heavy-duty sack constructions includes ISO 527-3:2018 tensile properties, ASTM D1709-16a dart impact, ASTM D1922-15 Elmendorf tear, and EN 13592:2017 for household waste sack dimensions and strength when the material is converted into waste sacks. Terminal products include heavy-duty shipping sacks of 25–50 kg capacity, FIBC liners, construction debris films, and agricultural salt bags. Operational boundaries for this blown film application are incompatible with long-chain branching degradation caused by excess cyclic acid scavengers; edge folds below the collapsing frame must also be avoided because cold-spot thickness variability above ±5% is a known cause of burst failure at the gusset fold during drop loading.
Typically, heat-seal initiation temperature in frozen food webs shifts downward when a sealant layer based on TUFLIN HS-7041 NT 7 is modified with lower-density plastomers; this allows the converter to maintain leak-rate integrity on vertical form-fill-seal machinery at sealing pressures of 0.3–0.7 MPa. Sealant layer addition is 80–90 wt% TUFLIN HS-7041 NT 7, 10–20 wt% metallocene plastomer with density 0.900–0.908 g/cm³, antiblock masterbatch at 0.3–0.8 wt%, and slip masterbatch at 0.1–0.3 wt%. Coextrusion on a 5-layer blown film line with die temperature 210–230°C, BUR 2.0:1–2.5:1, total web thickness 60–120 µm, and sealant layer thickness 8–15 µm produces a film that can be surface-treated to 38–42 mN/m on the reverse layer for print adhesion. Vertical form-fill-seal sealing jaws are run with a dwell time of 0.5–1.2 s and a cooling cycle of 1.0–2.0 s to prevent heat creep through the seal area as the web leaves the jaw at −20°C storage temperatures.
Compliance is anchored to the following matrix for food contact converters:
| Standard/Regulatory Reference | Assessment Parameter | Condition/Threshold |
|---|---|---|
| FDA 21 CFR 177.1520(c) 3.1a | Olefin polymer compositional compliance for direct food contact | Resin must meet olefin polymer density and extraction specifications; converter end-use film must pass extractives limitations under end-use food simulant conditions |
| EU Regulation (EU) No 10/2011 Annex I | Overall migration | 10 mg/dm² |
| Regulation (EC) No 2023/2006 | Good manufacturing practice for food contact materials | Documented risk-based production controls, change control on masterbatch additions |
| ISO 1133-1:2022 | Melt mass-flow rate | 190°C, 2.16 kg |
| ASTM D882-18 | Thin-film tensile properties | Grip separation 500 mm/min, specimen width 15 mm |
Terminal products include frozen fruit and vegetable pillow bags, quick-freeze seafood pouches, ice cream overwrap, and bakery frozen dough liners. The sealant web is not suitable for retort or autoclave service above 100°C, and prolonged contact with high-peroxide edible oil at elevated temperature may violate positive-list migration assumptions if tested outside frozen-food distribution conditions.
When TUFLIN HS-7041 NT 7 is run on an extrusion coating line at 290–315°C, the higher melt strength relative to conventional LDPE allows a reduction in coating weight from 20 g/m² to 15 g/m² only if the chill roll nip pressure is increased to 25–30 N/mm² and the air gap is maintained at 70–120 mm. The addition ratio is 95–100 wt% neat TUFLIN HS-7041 NT 7; the remaining 0–5 wt% is an acid copolymer tie resin when adhesion to aluminium foil is required. For paperboard adhesion, the extruder is fitted with a barrier mixing screw in a 90–120 mm cylinder with L/D 30:1, the die gap is held at 0.5–0.7 mm, and line speeds between 150 and 400 m/min are matched to chill roll water temperature of 10–15°C. Ozone treatment at 20–50 mW/m² is applied on the substrate side to promote primerless adhesion to paperboard and aluminium surfaces.
Compliance for extrusion-coated substrates is assessed under EU Regulation (EC) No 1935/2004 and Regulation (EC) No 2023/2006 when the structure is intended for food contact; packaging waste heavy-metal limits are assessed under Directive 94/62/EC Article 11. Downstream product types include coated paperboard trays for frozen and chilled foods, sealant webs for sachets, multiwall sack liners, and industrial release papers. A process conflict observed on coaters is excessive web edge oxidation when the ozone generator exceeds 50 mW/m² at line speeds below 100 m/min, which raises seal initiation temperature and weakens fibre tear on peel. The resin is not recommended for direct extrusion coating onto PVC films because plasticiser migration from the substrate may reduce optical clarity and seal uniformity within 72 hours of lamination.
Across low-night-temperature agricultural bale wrapping operations, the film must retain tear resistance at −5°C to 5°C without becoming so soft that pre-stretch forces drop below the required 40–60 N per 750 mm width. TUFLIN HS-7041 NT 7 is formulated at 92–96 wt% with a UV/HALS masterbatch at 3–5 wt% and a mineral antiblock at 1–2 wt%; the UV package is usually a combined hindered amine light stabiliser and high-molecular-weight benzophenone system that provides 12–24 months of open-field weathering. The downstream production process for silage bale wrap uses a three-layer blown film line with internal bubble cooling, die gap 1.4–1.6 mm, BUR 3.0:1–3.5:1, and roll widths from 250 to 750 mm. Finished rolls are converted for round and square bale wrappers at 50–70% pre-stretch ratio; roll hardness is controlled to 75–85 Shore C to prevent telescoping during field handling.
Compliance for this agricultural film falls under REACH and national agricultural plastic recovery schemes; EN 17033:2018 is explicitly not applicable because the material is a non-biodegradable silage wrap rather than a biodegradable mulch film. Terminal finished product types include round bale wrap, square bale wrap, silage pit covers, and bunker silo covers. Process limitations include incompatibility with non-UV-stabilised recycle streams above 10 wt%, which accelerates surface haze and pre-stretch failure under ultraviolet exposure; also, the film should not be exposed to silage inoculant concentrates during storage because low-molecular-weight acids can migrate into the wound roll and alter cling force from batch to batch.
Under accelerated drop-test conditions at 0°C, impact failure in 25–50 µm industrial liner films is evaluated by filling a 55-gallon drum with 50 kg of dry crystalline material and dropping the liner from 1.5 m; TUFLIN HS-7041 NT 7 is typically blended with 10–20 wt% EVA containing 9–18% vinyl acetate to reduce low-temperature brittle fracture. The film is produced on a 45–65 mm blown film extruder with L/D 24:1–30:1, die gap 1.0–1.5 mm, BUR 2.0:1–2.5:1, and melt temperatures of 190–210°C. For static dissipative drum liners, the addition of conductive carbon black masterbatch at 6–12 wt% raises melt pressure by 10–25% and may require screw speed reduction to prevent film gauge variation; published data for this specific resin in conductive liner formulations is limited, so surface resistivity must be verified on the finished film according to IEC 61340-2-3 or ASTM D257.
Compliance testing for the non-conductive liner stock is anchored to ASTM D1709-16a for dart impact, ISO 7765-1 for puncture impact, and ASTM D882-18 for tensile properties. The terminal product range includes 55-gallon drum liners, pail liners, can liners, and antistatic liners for powder transfer operations. The liner film should not be used for continuous service above 60°C, nor with strong oxidisers, aromatic hydrocarbons, or high free-fatty-acid powders that may induce environmental stress cracking at fold lines during long-term storage.
Competitive Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow TUFLIN™ HS-7041 NT 7 Linear Low Density Polyethylene Resin is a natural-grade linear low density polyethylene supplied in pellet form for blown film extrusion. Published physical property data list a density of 0.920 g/cm³ at 23 °C according to ASTM D792 and a melt index of 1.0 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238. The model designation HS-7041 identifies the specific property balance within the TUFLIN™ series; the suffix NT 7 denotes the natural additive form, which is supplied without slip or antiblock masterbatch. Primary application areas include heavy-duty shipping sacks, industrial liners, lamination films, agricultural films, and monolayer or coextruded packaging structures in which the converter prefers to control surface additives through downstream dosing. The product differs from slip-agent-containing LLDPE film grades in that coefficient of friction, blocking force, and unwinding behavior are governed by converter-added masterbatch rather than by the neat resin.
Conversion of the resin on single-screw blown film lines is typically carried out on extruders with 25:1 to 30:1 L/D ratios, grooved feed sections, and barrier or Maddock mixing screws. Melt temperature is maintained between 190 °C and 240 °C; sustained operation above 240 °C can increase gel formation and reduce film appearance. Die gaps from 1.5 mm to 2.5 mm and blow-up ratios from 2.0:1 to 3.0:1 are common for monolayer and skin-layer processing. Frost line height is adjusted between 250 mm and 500 mm depending on cooling air temperature, output rate, and film gauge; a longer frost line reduces quench rate and can shift the tensile-impact balance. Output stability on grooved-feed extruders is sensitive to feed-throat temperature, and water cooling of the feed section is recommended to prevent pellet bridging. Pre-drying is not required when storage conditions remain below 60% relative humidity. If pellets have been exposed to ambient humidity above 70% for more than 24 h, drying at 70 °C for 2 h to 4 h in a desiccant-bed dryer is sufficient to reduce surface moisture defects. The resin should be purged with a low-melt-index polyolefin before shutdown; direct transition from polar polymers can leave carbonized residues in the die lip area. Post-industrial regrind may be incorporated only after film property validation because haze per ASTM D1003, dart impact per ASTM D1709 Method A, and seal initiation temperature shift with regrind concentration and thermal history.
Screen packs of 40/60/100 mesh are commonly used with grooved-feed extruders processing 1.0 g/10 min LLDPE. Pressure drop across the screen pack should be monitored against the die pressure rating; a rising differential indicates gel or contaminant accumulation. Film bubble stability is improved by internal bubble cooling, but equipment-specific stabilization must be validated on the line because published data for this exact configuration is limited.
After film production at 25 µm to 50 µm gauge, mechanical evaluation is performed on specimens conditioned for at least 40 h at 23 °C ± 2 °C and 50% ± 5% relative humidity according to ASTM D618. Tensile properties are measured according to ASTM D882 or ISO 527-3; machine-direction and transverse-direction values are reported separately because LLDPE blown film is anisotropic. Dart impact resistance is evaluated using ASTM D1709 Method A; because impact values scale with thickness, comparisons require matched gauge and blow-up ratio. Elmendorf tear is measured per ASTM D1922; the machine-direction and transverse-direction tear ratio is process-dependent. Optical haze is quantified per ASTM D1003. The absence of slip and antiblock in the NT 7 form does not inherently reduce transparency, but roll blocking can induce surface defects that appear as haze after unwinding. Surface treatment for lamination and printing should achieve a minimum wetting tension of 38 mN/m per ASTM D2578; for some water-based ink systems, 42 mN/m is specified. Kinetic and static coefficients of friction are measured per ASTM D1894. Converters targeting low coefficient of friction must add slip masterbatch; erucamide or oleamide concentrate doses in the range of 500 ppm to 2,000 ppm by weight are common in industry, but the required dose depends on film gauge, storage temperature, and contact time.
The primary distinction is additive packaging. Slip/antiblock film grades contain surface-active agents such as erucamide or oleamide and particulates such as synthetic silica; those agents migrate to the film surface and lower coefficient of friction. HS-7041 NT 7 in the NT 7 form is specified without those surface additives, which transfers surface-property control to the converter. Coefficient of friction measured per ASTM D1894 on neat film is therefore higher than on a slip-grade film of equivalent density and melt index; blocking tendency increases with roll tension, storage temperature above 30 °C, and contact time. This distinction is relevant for lamination: a high slip-agent concentration can impair solventless or water-based adhesive bond strength, whereas an untreated film may require corona treatment and primer. Compared with higher-melt-index LLDPE film grades, the 1.0 g/10 min melt index provides greater melt strength and bubble stability but may reduce output on shallow-channel screws. Compared with lower-melt-index grades, it offers better drawdown and reduced motor load. Compared with high-pressure low-density polyethylene, the resin has higher tensile and dart impact values at comparable gauge but lower melt elasticity; this changes bubble shape and requires grooved-feed extrusion. The HS-7041 model number is not a direct substitute for grades containing pre-compounded slip and antiblock, and film property equivalence must be verified by side-by-side conversion at matched blow-up ratio, die gap, and frost line height.
Hot tack and seal initiation temperature for this exact grade are not listed in the published data sheet; converters must evaluate them on packaging lines using ASTM F1921 or ASTM F2029 because seal performance depends on sealant thickness, dwell time, and contamination.
Use in heavy-duty shipping sacks typically involves film gauges from 75 µm to 150 µm. The 1.0 g/10 min melt index supports bubble stability at high frost-line heights; converter-added anti-block concentrates are required to prevent blocking during winder lay-flat. In industrial liners, dart impact and tear resistance are evaluated by ASTM D1709 and ASTM D1922, with comparisons performed at matched gauge. In lamination films, the absence of slip agents reduces interference with polyurethane adhesives; surface treatment to a minimum of 40 mN/m per ASTM D2578 is required before coating. In agricultural film, UV stabilizer masterbatch and pigments are added by the converter, and retention of mechanical properties after weathering is evaluated separately by ASTM D882 following controlled UV exposure. Silo storage and pellet conveying systems should be grounded to prevent static accumulation; these are standard polyolefin handling practices, not product-specific limitations.
For regulatory compliance, the resin can be evaluated under the following framework. Compliance statements on a final article require converter verification because migration, film thickness, and additive additions affect the legal status.
| Regulation/Standard | Designation | Applicability | Converter Verification Requirement |
|---|---|---|---|
| U.S. FDA food contact | 21 CFR 177.1520(c)3.2a | Olefin polymer film in food-contact articles | Extractives and end-use migration limits must be confirmed by converter |
| EU food contact plastics | Regulation (EU) No 10/2011 | Plastic materials and articles intended to contact food | Overall migration ≤ 10 mg/dm² per Article 12; specific migration limits apply |
| U.S. Pharmacopeia | USP <661.1> | Plastic packaging systems for pharmaceuticals | Extractable profile depends on drug product and sterilization |
| EU REACH | Regulation (EC) No 1907/2006 | Chemical registration and SVHC communication | Article 33 disclosure duty if SVHC > 0.1% w/w in article |
| EU RoHS | Directive 2011/65/EU | Restriction of hazardous substances in electrical equipment | Neat LLDPE not typically in scope; final article must be assessed |
The absence of slip and antiblock in NT 7 does not by itself confer food-contact compliance; specific migration testing is required for each final film structure, sealant layer, and printing ink combination.
In three-layer or five-layer barrier films, the LLDPE layer is often combined with polyamide or ethylene vinyl alcohol through tie resins. If the LLDPE skin layer is processed too cold or the contact time in the die is too short, interlayer adhesion can fall below target, as measured by T-peel adhesion according to ASTM D1876. The resin is typically run at melt temperatures of 210 °C to 240 °C when coextruded with ethylene vinyl alcohol because higher thermal input at the interface increases chain interdiffusion across the tie layer. Melt temperature above 240 °C can degrade the barrier polymer and generate oxidized gels; the adapter and die are therefore maintained within a 210 °C to 235 °C balance in many barrier film operations. Interfacial adhesion in the machine direction and transverse direction can differ by 10% to 20% depending on die rotation speed and frost line height; published data for this specific configuration is limited and line-specific validation is required. Blow-up ratio above 3.0:1 can improve transverse orientation but may reduce adhesion when the frost line is too short. Corona treatment of the outer layer to at least 42 mN/m per ASTM D2578 is necessary before lamination or printing; without it, solventless adhesives and water-based inks may wet unevenly.
Resin pellets should be stored in sealed containers at temperatures below 50 °C and protected from ultraviolet exposure. Prolonged storage at elevated temperatures can deplete the thermal stabilizer and shift melt index; incoming lots should be checked by melt flow rate according to ISO 1133-1:2022 and by density according to ISO 1183-1 if a lot-to-lot issue is suspected. The hopper and conveying system should be grounded to prevent static accumulation, and purge air should be dry. These are standard polyolefin handling practices, not product-specific limitations.
The melt index value of 1.0 g/10 min is a single-point viscosity descriptor; it does not fully define shear-thinning behavior. For die design and troubleshooting, capillary rheometry per ISO 11443 is used to generate viscosity curves at 190 °C, 210 °C, and 230 °C at shear rates from 10 s⁻¹ to 1,000 s⁻¹. The power-law index for LLDPE in this melt index range is typically between 0.5 and 0.7, but published data for this specific resin is limited. Film property comparisons should use specimens of matched gauge and conditioning per ASTM D618 because LLDPE properties are sensitive to orientation and thermal history.