    Specifications
    HS Code 388912
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Butene
    Density 0.918 g/cm³
    Meltindex 0.80 g/10 min (190 °C/2.16 kg)
    Meltflowratio 27
    Meltingpoint 121 °C
    Vicatsofteningpoint 94 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 26.2 MPa
    Elongationatbreak 700%
    Flexuralmodulus 0.241 GPa
    Hardnessshored 50
    Dartdropimpact 120 g
    Elmendorftearmd 240 g
    Elmendorfteartd 400 g
    Haze 12%
    Gloss 60

    As an accredited Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene-lined bags, palletized for shipment; also available in 1,000 kg bulk bags.
    Container Loading (20′ FCL) Container loading (20′ FCL): Dow TUFLIN™ HS-7021 NT 7 LLDPE resin in 25 kg bags, palletized, shrink-wrapped, and secured for transport.
    Shipping Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin ships as a non-hazardous solid in 25 kg bags, stretch-wrapped pallets, or bulk trucks/railcars. Store dry and clean, away from heat and direct sunlight. Not DOT/IMDG/IATA regulated; avoid package damage and moisture contamination. Handle per SDS.
    Storage Store Dow TUFLIN™ HS-7021 NT 7 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and moisture. Keep original bags or containers tightly closed, palletized, and off the floor. Avoid contamination, physical damage, and prolonged UV exposure. Maintain temperatures below 50°C, follow first-in, first-out rotation, and inspect containers regularly for leaks or damage.
    Shelf Life Shelf life is 12 months from date of manufacture when stored in original unopened packaging at temperatures below 50°C.
    Application of Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin

    At cast film line speeds above 180 m/min, the neck-in ratio of a linear low density polyethylene web is controlled more by air gap and melt curtain geometry than by the die temperature profile alone. TUFLIN™ HS-7021 NT 7 is evaluated as the core resin in a three-layer cast stretch film structure, where the two outer cling layers contain polyisobutylene or an ULDPE-rich blend at typical addition levels of 1–3 wt% or 20–30 wt% respectively. The die gap is normally set between 0.5 mm and 0.8 mm; wider gaps increase the melt bank thickness and are used only when die build-up produces local die lines. Melt temperature is held within 205–230 °C; below this window the melt curtain freezes too quickly and edge stability deteriorates, while above the window the cling additive may volatilise and create smoke deposits on the die lips. Air gap is reduced to 10–20 mm on wide cast lines to limit neck-in, but an air gap shorter than 10 mm is not common because it narrows the operating window for melt draw and makes thickness oscillation difficult to correct. The chill roll stack is run at 15–25 °C, and the cast web is drawn to a final thickness of 15–25 µm. Edge trim is generated at the die and is recycled into the core at levels up to 15 wt%; at higher trim re-feed, the melt elasticity shifts and the film may enter draw resonance, producing periodic transverse gauge bands that cannot be reduced by adjusting the die bolts. In converter trials on wide cast extrusion lines, the onset of draw resonance correlates with a reduction in melt curtain length and an increase in line speed, and the practical correction is to increase melt temperature, reduce draw ratio, or widen the air gap. No desiccant drying is required for this polyethylene resin, but pellets stored below the plant dew point must be conditioned to avoid surface condensation, which can generate splay in the cast film. Tensile properties are measured according to ASTM D882, puncture resistance according to ASTM D5748, and cling force according to ASTM D5458. The converted roll is used for machine pallet wrap for industrial unitisation; direct food contact is not the primary end use, and any food-contact over-wrap application must be validated under Regulation (EU) No 10/2011 and 21 CFR 177.1520. Published data for this specific grade in 30-layer nano-cast film structures is limited.

    What Limits Blown Film Output When HS-7021 NT 7 Is Positioned as the Core Layer in Frozen Food Laminations?

    The output-limiting phase in frozen food laminations is bubble instability rather than extruder capacity when this resin is run as the core of a three-layer coextruded blown film. In vertical form-fill-seal packaging for frozen vegetables, seafood, and bakery products, the film structure commonly places an EVA or LDPE-rich sealant layer on the inside and the LLDPE core in the centre. The blown film line is run with a die gap of 1.4–2.0 mm and a blow-up ratio between 2.0:1 and 2.5:1; the frost-line height is kept at 8–12 times the die diameter to balance machine-direction and transverse-direction properties. The core layer is not required to provide seal initiation, but it controls the subzero dart impact and tensile energy absorption. The output limit is usually bubble instability rather than extruder capacity: if the frost line is raised too far above the die, the bubble becomes sensitive to plant air currents and the film gauge profile develops thick bands that are visible in the printed areas. Addition of 10–20 wt% LDPE to the core reduces this instability by increasing melt strength, but this same addition raises the seal initiation temperature of the sealant layer when the layers are coextruded in a single die. Seal initiation must therefore be re-checked by ASTM F88 seal strength and ASTM F2029 hot tack, because a seal that is acceptable at ambient may not close reliably through frozen product at a fill temperature of -25 °C to -5 °C. The end film is stored at -40 °C and must survive bag drop and puncture during distribution; dart impact is evaluated under ASTM D1709 and tear under ASTM D1922. The table below lists the regulatory references normally used by converters when validating frozen-food contact, but the listed references do not constitute a certification for this specific grade without migration test data.

    Regulatory referenceAnalytical endpointCondition relevant to frozen food packaging
    Regulation (EU) No 10/2011Overall migration and specific migration of authorised additivesSimulant D2 or food simulant according to frozen contact, ≤ 10 mg/dm² overall migration
    21 CFR 177.1520Olefin polymer extractives and density-based limitationsDirect food contact under the conditions of use specified by the converter
    GB 9685-2016Additive positive list for food contact plasticsAdditives in film layers must be listed under the relevant use conditions
    Japan MHLW Notification No. 370Polyethylene migration limits and food simulantsFrozen food contact if filled below 5 °C and stored frozen

    Because industrial bag converting involves high-speed continuous sealing, the side gusset film must retain toughness after the sack is loaded, closed, and stacked in warehouse conditions. TUFLIN HS-7021 NT 7 is processed as part of a blown film structure for valve sacks and block-bottom sacks used in dry chemical, resin pellet, and fertiliser packaging. The die gap is set at 1.8–2.4 mm and the blow-up ratio is held between 2.0:1 and 2.5:1; internal bubble cooling is used on lines with die diameters above 200 mm to remove the additional heat from LLDPE shear heating. The film is typically a blend of 80–90 wt% LLDPE and 10–20 wt% LDPE, because pure LLDPE on older grooved-feed extruders can produce melt pressure fluctuations at high throughput. Erucamide slip and synthetic silica antiblock are included at levels required for the target coefficient of friction, measured under ASTM D1894; the slip package must not be omitted when the sacks are run on automatic filling lines, because blocky film can cause vacuum pick-up failures. Seal integrity is the most frequent failure mode on filled sacks, not film tear; the seal is specified and tested under ASTM F88, and the film tear resistance is measured under ASTM D1922. The converted sack is not intended for direct steam sterilisation or retort use; continuous product temperatures above 60 °C can cause progressive loss of seal load and film deformation. The film is not a high-barrier structure, so moisture and oxygen transmission are controlled by thickness and inner liner selection rather than by the LLDPE itself. Published data for this specific grade in heavy-duty fertiliser sacks is limited, and the packaging technologist should validate seal strength on the actual vertical form-fill-seal configuration.

    Agricultural greenhouse film and anti-drip additive migration in a six-month northern exposure

    Six months of northern exposure alters the migration rate of anti-drip additives more than the initial film formulation does in greenhouse cladding. TUFLIN HS-7021 NT 7 is used as the outer or core layer in multilayer blown film that must retain mechanical integrity after repeated wind load and UV exposure. The extrusion process uses a die gap between 1.6 mm and 2.2 mm, a blow-up ratio around 2.0:1, and film thickness from 100 µm to 200 µm. UV stabiliser masterbatch is let down at the masterbatch supplier’s recommended active concentration, commonly 3–10 % for HALS-based packages in polyethylene, but the exact ratio depends on the masterbatch carrier and the intended service life. Anti-drip additives, typically ethoxylated amine or sorbitan ester compounds, migrate to the film surface to form a continuous water-sheeting layer; this migration is temperature-dependent and is slowed at low outdoor temperatures. If the additive loading is too high, the film surface becomes tacky and dust accumulation increases, which reduces visible light transmission measured according to ASTM D1003. The film may be judged under EN 13206:2017 for agricultural films. The converted product is used for greenhouse covers, low tunnels, and silage protection. Since anti-drip additives and HALS packages are not always food-contact-approved, this agricultural film is generally separated from food packaging regrind streams, and disposal is managed under Directive 94/62/EC.

    On five-layer blown film lines running polyamide or EVOH barrier layers, the rheological mismatch between LLDPE and anhydride-modified tie resins is the primary source of interfacial instability. TUFLIN HS-7021 NT 7 is run as the outer contact layer and inner sealant layer in barrier packaging for processed meat, cheese, and coffee. The die gap is set at 1.2 mm to 1.8 mm, the blow-up ratio at 2.0:1 to 2.2:1, and the LLDPE layers are each maintained at 30–40 % of total film thickness. The tie layers and barrier layer occupy the remaining 20–40 %; precise layer ratios are adjusted to keep the barrier layer continuous because any thinning below the critical layer thickness produces a rapid loss of oxygen barrier. Interfacial sharkskin is more likely when the LLDPE layer runs below 10 % of total thickness or when the melt temperature of the LLDPE skin is below 190 °C. The film must be corona treated on the outer LLDPE surface to 38–42 mN/m before lamination or printing, and wetting tension is measured under ASTM D2578. Oxygen transmission is measured under ASTM D3985 and water vapour transmission under ASTM F1249. The final package is not retortable above 100 °C unless the barrier layer and tie resins are specifically selected for high temperature; standard EVOH structures may delaminate in boiling water. Direct food contact compliance must be validated under Regulation (EU) No 10/2011 and 21 CFR 177.1520; the sealant layer present in contact with food must also meet the specific migration limits of the tie resin used.

    When high-speed surface printing and ceramic-coated rollers reduce film slip during converting

    High-speed surface printing on ceramic-coated rollers changes the slip additive migration profile of printed overwrap film. TUFLIN HS-7021 NT 7 can be used as the print web or the inner web in non-food overwrap for tissue paper, magazine packaging, and industrial rolls. The film is blown or cast, then print-treated to a wetting tension of 38–42 mN/m under ASTM D2578; ink adhesion is checked with tape-release tests. Ceramic-coated idler rollers with high contact area can raise the film temperature and bring the slip additive to the surface faster, which lowers the coefficient of friction measured under ASTM D1894 but can also create transfer marks on the printed side. When corona treatment is applied too aggressively, the surface bonds polar functional groups and the static coefficient of friction can rise above 0.40; this value is not a specification but a converter control limit derived from high-speed track requirements. The film must not be stored for extended periods after corona treatment before printing because surface oxidation decays and the treatment level falls below 36 mN/m. The converted overwrap is typically not intended for direct food contact, and compliance is limited to industrial use unless the ink and coating system are validated under Regulation (EU) No 10/2011 or 21 CFR 177.1520. Published data for this specific grade in high-speed ceramic-roller converting lines is limited.

    Free Quote

    Competitive Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow TUFLIN™ HS-7021 NT 7 Linear Low Density Polyethylene Resin is identified in supplier technical documentation as a pelletized linear low density polyethylene film grade for thin-gauge cast film conversion and extrusion coating. The complete alphanumeric designation separates this product from adjacent TUFLIN™ grades; the NT suffix indicates a natural, unpigmented pellet, and the trailing numeral identifies a proprietary additive package. The HS modifier is conventionally associated with a high-slip surface system, though the exact slip and antiblock composition must be confirmed from the current supplier datasheet. Specification review begins with the lot certificate of analysis, where melt flow rate and density are reported against the supplier’s controlled test platform. Published property tables for linear low density polyethylene of this density class should not be substituted for the grade-specific datasheet; class-level data are used here only to frame conversion behavior and comparative product positioning.

    What Specification Limits Apply to Melt Index and Film Density?

    For linear low density polyethylene film resins, melt flow rate is measured at 190 °C and 2.16 kg using ISO 1133-1:2022 or ASTM D1238-23. Density is determined on compression-moulded plaques by ISO 1183-1:2019 or ASTM D1505-18. Commercial cast film LLDPE grades of this type generally fall between 1.0 g/10 min and 3.5 g/10 min in melt index and between 0.916 g/cm³ and 0.920 g/cm³ in density; narrower specification windows are lot-specific and are certified on the supplier’s CoA. A shift of 0.1 g/10 min in melt index can alter cast film drawdown, melt pressure, and chill roll contact length. A density shift of 0.001 g/cm³ can produce measurable changes in secant modulus under ASTM D882-22 at 500 mm/min crosshead speed. The following matrix contains the specification and qualification methods used for film-grade LLDPE.

    PropertyStandard MethodSpecimen or ConditionControl Function
    Melt flow rateISO 1133-1:2022, ASTM D1238-23190 °C, 2.16 kg, 10 minExtruder screw design and melt pressure
    DensityISO 1183-1:2019, ASTM D1505-18Compression-moulded plaqueCrystallinity, stiffness, sealing temperature
    Film tensile yield and breakASTM D882-22, ISO 527-3:201825 µm film, 500 mm/minDownweb load and drawdown
    Dart impactASTM D1709A-22, ISO 7765-1:200425 µm film, clamped specimenHigh-speed puncture resistance
    Elmendorf tearASTM D1922-23, ISO 6383-2:198325 µm film, notchedTear propagation in packaging
    HazeASTM D1003-2125 µm filmOptical clarity
    GlossASTM D2457-21, ISO 2813:201460° geometrySurface appearance
    Coefficient of frictionASTM D1894-21, ISO 8295:1995Film-to-film, 25 µmSlip additive migration and packaging line speed

    Resin conversion on a chill-roll cast film line requires control of melt temperature, die gap, air knife flow, and chill roll surface temperature. In production practice, a 90 mm single-screw extruder with 30:1 L/D barrier-flight geometry and a Maddock mixing section is often used; screen pack configurations of 40/60/100 mesh or finer protect the die from gels and raise backpressure. Barrel zone profiles are commonly stepped from 180 °C in the feed zone to 260–290 °C at the die adapter. The flat die gap is set from 0.4 mm to 1.0 mm, with film thickness drawn to 15–100 µm. Chill roll surface temperature is maintained between 18 °C and 30 °C, with tighter ±3 °C loops for high-slip packaging grades. Temperature drift beyond ±5 °C is a processing-window threshold because the migration rate of erucamide and oleamide slip agents changes with lamellar crystallinity; an increase in chill roll temperature accelerates surface bloom, while a decrease traps slip additive below the skin layer. The practical consequence is a coefficient of friction shift from approximately 0.10 to 0.30 as measured under ASTM D1894-21, which is sufficient to mischaracterize batch performance. Drying is not routinely required because polyethylene pellets have low equilibrium moisture below 0.01 wt%; however, cold-stored pellets should be allowed to reach ambient temperature and, if surface condensation is visible, dried at 80 °C for 2 h before extrusion.

    Slip and antiblock additives in TUFLIN™ HS-7021 NT 7 are not permanently fixed in the polymer matrix. Erucamide and similar primary amides diffuse to the film surface over hours to days, with published diffusion coefficients in semicrystalline polyethylene commonly falling between 10-13 m²/s and 10-15 m²/s at 23 °C. Migration rate accelerates with storage temperature; a film stored at 40 °C reaches stable coefficient of friction faster than at 23 °C. This creates a specification timing issue: immediate measurements under ASTM D1894-21 may overreport friction because the slip bloom has not equilibrated. A conditioning period of 48 h at 23 °C and 50% relative humidity under ISO 291 is a common minimum before certification. The opposite boundary is excessive bloom, which can occur after prolonged storage above 35 °C; surface haze can increase and seal strength can decline because slip species act as a transfer layer during heat sealing. These two boundaries define the practical quality window in converted film.

    When Sealant Web Layers Are Coextruded Against Propylene Copolymer Substrates

    Sealant layer performance separates an octene-based high-slip LLDPE from generic butene-based LLDPE and high-pressure LDPE when coextruded onto propylene copolymer substrates for flexible packaging. Heat seal strength is measured under ASTM F88/F88M-23; hot tack is measured under ASTM F1921/F1921M-23. An octene-copolymer LLDPE of similar density can produce a seal initiation temperature 5–10 °C lower than a butene-copolymer LLDPE at equal film gauge, because octene comonomer defects reduce the crystalline lamellar thickness and broaden the melting endotherm. The effect is observable in hot tack curves as a wider plateau and cohesive failure mode down to lower seal bar temperatures. For a high-slip additive package, slip migration to the sealant surface competes with interfacial wetting; seal initiation measurements should be repeated after ageing at 40 °C for 7 days under ISO 291. Published data for TUFLIN™ HS-7021 NT 7 in this specific coextruded configuration is limited; processors are advised to generate film samples on the target line and compare against supplier reference curves before committing to specifications. Blending with LDPE is common for neck-in control on extrusion coating lines; however, LDPE addition above 15 wt% can reduce Elmendorf tear and raise seal initiation temperature, so the blend is not a direct property substitute for a dedicated high-slip LLDPE sealant grade. Differential scanning calorimetry under ISO 11357-3 at 10 °C/min can be used to compare the melting peak and lower-temperature shoulder as a faster qualification parameter than a full hot tack matrix.

    Polymer ClassChain ArchitectureDensity RangeMelt Index RangeSeal Initiation Relative to High-Slip LLDPEMechanical Character
    Butene-based LLDPELinear ethylene-butene copolymer0.916–0.920 g/cm³1.0–3.5 g/10 minHigher by approximately 5–10 °CLower dart and tear at equal gauge
    Octene-based LLDPELinear ethylene-octene copolymer0.916–0.920 g/cm³0.5–3.5 g/10 minLower and broader hot tack plateauHigher dart and tear at equal gauge
    High-pressure LDPELong-chain branched polyethylene0.919–0.924 g/cm³0.2–8 g/10 minLower initiation but lower hot tack plateauLower tensile strength, lower dart
    Metallocene plastomerEthylene-olefin copolymer, very low density0.860–0.910 g/cm³0.5–5 g/10 minLower initiationHigher impact but lower stiffness

    Comparative mechanical performance across resin families is meaningful only when specimen preparation follows the same standard. For example, ASTM D1709A-22 dart impact values are sensitive to film gauge, cooling rate, and additive loading; a 25 µm cast film made on a chill roll line will differ from a blown film of the same gauge. When evaluating whether TUFLIN™ HS-7021 NT 7 can replace another grade, the comparison should fix extruder type, die gap, melt temperature, chill roll temperature, and winding age. A change of 5 °C in melt temperature can alter measured impact and tear values more than the difference between two similar LLDPE grades. Release specifications are therefore paired with sample preparation methods rather than treated as intrinsic polymer constants.

    Food-contact status is established through regulatory testing rather than resin designation alone. In the United States, the base olefin polymer may be evaluated under 21 CFR § 177.1520(c) for food contact subject to end-use temperature and food-type limitations; extraction tests use food simulants and total nonvolatile extractable fraction as specified in the section. In the European Union, Regulation (EU) No 10/2011 governs plastic materials intended to contact food. Overall migration is tested under BS EN 1186-1:2002 with an overall migration limit of 10 mg/dm² or 60 mg/kg, whichever is higher; specific migration of additives is evaluated under Annex II restrictions. Compliance documentation should include the supplier’s product stewardship declaration for REACH registration status and any restrictions under Annex XVII. For electronic applications where RoHS applies, 2011/65/EU and Annex II hazardous substance thresholds must be checked against the actual formulation. These standards do not certify the film structure; the downstream converter retains responsibility for migration testing of the final printed, adhesive-laminated, or coated article.

    Operational boundaries include storage and handling conditions. The pellet should be protected from ultraviolet exposure and moisture condensation; cold-stored material should be allowed to reach ambient temperature before opening to avoid surface moisture uptake. Fines generation during high-speed conveying can increase dust and feed variation; low-velocity dense-phase conveying is preferred. The resin is not intended for medical implant applications or for use as a direct food-contact material without post-processing qualification. Lot-to-lot variation in melt index and additive loading is controlled through supplier certificates of analysis; downstream converters often apply moving-range charts for film dart impact and coefficient of friction to detect batch variation that cannot be resolved from melt flow rate alone.