Dow Tuflin Hs 7001 Nt 7 Lldpe

Dow Tuflin™ HS-7001 NT 7 LLDPE

    • Product Name: Dow Tuflin™ HS-7001 NT 7 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 670882
    Product Name Dow Tuflin™ HS-7001 NT 7 LLDPE
    Chemical Family Linear Low Density Polyethylene (LLDPE)
    Form Pellets
    Density 0.917 g/cm³
    Melt Index 190 C 2 16 Kg 0.70 g/10 min
    Melt Flow Ratio I21 I2 27
    Melting Temperature 123 °C
    Vicat Softening Temperature 94 °C
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 30.0 MPa
    Elongation At Break 800%
    Flexural Modulus 240 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 400 g
    Haze 12%
    Gloss 45 60%

    As an accredited Dow Tuflin™ HS-7001 NT 7 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Tuflin™ HS-7001 NT 7 LLDPE is supplied in 25 kg polyethylene-lined paper bags, 40 bags per pallet (1,000 kg total).
    Container Loading (20′ FCL) 20′ FCL: Dow Tuflin™ HS-7001 NT 7 LLDPE in 25 kg bags, palletized, stretch-wrapped, and securely strapped for ocean export.
    Shipping Dow Tuflin™ HS-7001 NT 7 LLDPE is shipped as a non-hazardous solid resin, typically in 25 kg polyethylene bags, octabins, or bulk containers. It is not regulated for transport by DOT, IMDG, or IATA. Keep dry, away from heat and direct sunlight, and handle per local regulations.
    Storage Store Dow Tuflin™ HS-7001 NT 7 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed, off the floor, and protected from moisture, dust, and contamination. Avoid prolonged UV exposure. Maintain stable ambient temperatures, observe stacking limits, and use first-in, first-out stock rotation.
    Shelf Life Recommended shelf life is 24 months when stored in original packaging under cool, dry conditions, away from direct sunlight and moisture.
    Application of Dow Tuflin™ HS-7001 NT 7 LLDPE

    In high-speed machine cast stretch film, Tuflin HS-7001 NT 7 functions as the primary ethylene-α-olefin copolymer layer in 8–23 µm monolayer or 3-layer constructions. The resin’s nominal melt mass-flow rate of 2.8 g/10 min under ISO 1133-1:2022 at 190°C/2.16 kg and density of 0.918 g/cm³ under ISO 1183-1:2019 place it inside the processing envelope for flat-die cast film lines running above 450 m/min. The formulation addition ratio for machine wrap typically holds Tuflin HS-7001 NT 7 at 92–98 wt%, a polyisobutylene-based tackifier masterbatch at 1–4 wt%, and a synthetic silica or diatomaceous antiblock masterbatch at 0.5–1.5 wt%; up to 5 wt% of the LLDPE may be replaced with low-density polyethylene or metallocene plastomer when the converter must reduce stretch force or shift puncture propagation energy at equivalent gauge. Downstream production on a cast line uses a coat-hanger or fishtail flat die with a die gap of 0.6–0.9 mm, a 30:1 L/D barrier screw, and a 80/120/80 mesh screen pack to remove gel particles from reclaimed edge trim; melt temperature is held at 215–245°C while the polished chill roll is maintained at 18–24°C, and an air knife with a vacuum box forces the melt curtain onto the roll to suppress gauge bands. Terminal product types include 10–23 µm machine stretch wrap, pre-stretched hand wrap, and 3-layer coextruded pallet wrap with differential cling. Draw resonance emerges as the critical process conflict when line speed exceeds 700 m/min and melt temperature approaches 245°C, because the resin’s melt strength cannot damp transverse thickness oscillations; gauge bands and edge neck-in also increase when the die gap drops below 0.6 mm or the chill roll temperature exceeds 28°C. Regulatory compliance for this application falls under REACH Regulation (EC) No 1907/2006 and Directive 2011/65/EU for RoHS-restricted exports; if the final film is placed in direct food contact, Regulation (EU) No 10/2011 Annex I applies with an overall migration limit of 10 mg/dm² and the complete formulation must conform to the olefin polymer specifications in FDA 21 CFR 177.1520(c). The tackifier masterbatch must be validated for migration under the relevant food simulant when the wrapped pallet enters non-refrigerated food logistics.

    What Governs Tear Propagation in Heavy-Duty FIBC Liners?

    Because tear propagation resistance rather than tensile strength governs field failure in heavy-duty FIBC liners, Tuflin HS-7001 NT 7 is processed on 3-layer blown film lines under conditions that balance machine-direction and transverse-direction orientation. The formulation addition ratio for an FIBC liner typically sets Tuflin HS-7001 NT 7 at 70–100 wt%, with 0–30 wt% low-density polyethylene or internally reclaimed LLDPE edge trim, 2–5 wt% carbon black masterbatch for opacity, and 0.5–2 wt% hindered amine light stabilizer masterbatch when the liner is stored outdoors or used for UV-sensitive goods. Downstream production uses a 80–150 mm annular die with a die gap of 1.8–2.5 mm, a blow-up ratio of 2.5:1–3.0:1, an internal bubble cooling system, and melt temperature of 185–215°C; after slitting, gusseting, in-line perforation, and heat sealing, the terminal product types are FIBC liners, 50–100 kg export shipping sacks, and salt or fertilizer bags. Tear propagation is governed by the orientation balance set by the blow-up ratio and frost line height: a BUR of 3.0:1 yields high machine-direction tear and lower transverse-direction tear, whereas 2.5:1 produces more balanced Elmendorf tear values under ISO 6383-2:1983. Industry compliance for FIBCs is anchored to ISO 21898:2004; when the liner is used as inner packaging for dangerous goods, the construction must also conform to the applicable packing group requirements of the UN Model Regulations. Moisture uptake becomes an operational boundary if the resin is stored outside a sealed bag at relative humidity above 70% for more than 48 h, because surface moisture can generate pinholes at the frost line.

    Sterile Barrier Webs Heat-Seal Integrity and Peel Force Control

    To maintain seal integrity in ISO 11607-1:2019 compliant pouches, a heat seal layer based on Tuflin HS-7001 NT 7 must satisfy peel force, microbial barrier, and biocompatibility requirements simultaneously. The sealant layer formulation allocates 70–90 wt% Tuflin HS-7001 NT 7, 10–25 wt% metallocene plastomer or ethylene-vinyl acetate to lower seal initiation temperature, and 1–3 wt% slip/antiblock masterbatch; animal-derived fatty acid amides and phthalate-based carriers are excluded from the formulation because they can interfere with cytotoxicity tests under ISO 10993-5:2009 or complicate sterilization residue analysis. Downstream production first produces a cast or blown coextruded LLDPE sealant web, then laminates it to a printed polyester, polyamide, or paper outer web; pouch converting runs at seal temperatures of 120–160°C, dwell times of 0.5–1.0 s, and jaw pressures of 4–6 bar, with peel force measured under ASTM F88/F88M-23 and validated for the package’s sterile barrier system. Terminal product types are sterile barrier pouches, header bags for IV sets, and lidding for pre-formed PET trays. Industry compliance is governed by ISO 11607-1:2019 for sterile barrier system material selection and sealing process validation, EN 868-10:2018 for paper/plastic pouch constructions, and ISO 13485:2016 for the converter’s quality management system. An operational boundary exists at seal jaw temperatures above 160°C, where the LLDPE sealant layer can extrude and produce seal edge thinning; conversely, below 120°C, seal initiation may be incomplete and create a channel leak path.

    Compliance matrix for sterile barrier LLDPE sealant web
    StandardTest method or referenceSealant wedge requirement
    ISO 11607-1:2019Clause 4.2Material specification and sterile barrier system integrity
    EN 868-10:2018Seal strength testPeel strength after sterilization
    ASTM F88/F88M-23Seal peel force measurementPeel force recorded in N/15 mm
    ISO 10993-5:2009Elution cytotoxicity testNo cytotoxic effect from sealant extracts

    When Thermic Retention and UV Quenching Extend Greenhouse Service Life

    Greenhouse cover films exposed to 12-month UV radiation and night-time radiative cooling use Tuflin HS-7001 NT 7 as the load-bearing layer in 3-layer blown film structures. The formulation addition ratio consists of 94–99 wt% Tuflin HS-7001 NT 7, 1–4 wt% UV stabilizer masterbatch, 0.5–2 wt% anti-drip/anti-fog additive, and 1–2 wt% infrared-absorber masterbatch for thermic retention in the 7–13 µm long-wave transmission window. Downstream production employs a 200–400 mm annular die, die gap of 1.4–2.2 mm, blow-up ratio of 2.0:1–2.5:1, layflat width up to 12 m, thickness of 150–200 µm, and melt temperature of 190–215°C; after corona treatment to 38 mN/m and slitting, the terminal product types are greenhouse covers, low tunnel films, and silage covers. Industry compliance is defined by EN 13206:2017 for thermic and UV-stabilized agricultural films and by REACH Regulation (EC) No 1907/2006 for chemical substances; accelerated weathering is evaluated under ISO 4892-2:2013 with film tensile retention measured by ISO 527-3:2018. Published multi-season field data for this specific Tuflin grade in a single-layer greenhouse film is limited; therefore, the converter must validate the complete three-layer structure under the weathering categories of EN 13206:2017 rather than extrapolating from laboratory xenon-arc hours alone. An operational boundary exists at die lip temperatures above 215°C, where anti-drip additives can volatilize and deposit on the collapsing frame, causing bubble drag marks.

    For temporary surface protection of glass, coated steel sheet, and polyester panels during fabrication and transit, Tuflin HS-7001 NT 7 is coextruded into 30–80 µm self-wound films with a pressure-sensitive adhesive skin layer. The core layer formulation uses 75–95 wt% Tuflin HS-7001 NT 7, 5–20 wt% ethylene-vinyl acetate or polyolefin elastomer to control modulus, and 1–3 wt% processing aid; the adhesive skin layer is a coextruded blend of ethylene-vinyl acetate and tackifier resin, and the exact addition ratio must be adjusted to the target substrate surface energy. Downstream production runs on a multi-extruder cast coextrusion line with melt temperature of 190–230°C, a chill roll temperature of 18–22°C, corona treatment to 36–40 mN/m, and in-line slitting to the required width. Terminal product types include surface protection films for stainless steel sheet, aluminum composite panel, PVC window profiles, and glass lites during handling and installation. Industry compliance for these temporary films is based on REACH Regulation (EC) No 1907/2006, Directive 2011/65/EU for RoHS-restricted substances, and peel adhesion testing under ASTM D3330/D3330M-23. The main operational limit is storage temperature above 30°C, which increases adhesive migration and unwind force after long coil aging.

    Frozen Food Sealant Web and the Limits of Low-Temperature Ductility

    Converting Tuflin HS-7001 NT 7 into a low-temperature food sealant web requires control over seal initiation, hot tack, and sub-zero flex crack resistance. The sealant layer formulation contains 80–100 wt% Tuflin HS-7001 NT 7, 0–20 wt% metallocene plastomer or low-density polyethylene to depress seal initiation to 85–110°C, 1–2 wt% slip/antiblock masterbatch, and 0.5–1.0 wt% antifog additive for frozen vegetable bags where clarity is required. Downstream production first coextrudes a cast or blown LLDPE sealant web, then laminates it to a printed PET, polyamide, or biaxially oriented polypropylene outer web through adhesive lamination or extrusion lamination; packaging lines seal the final structure at 120–160°C, 0.3–0.8 s dwell, and 3–5 bar jaw pressure. Terminal product types are frozen vegetable bags, ice cream lidding film, and chilled dairy pouches. Compliance for direct food contact is governed by FDA 21 CFR 177.1520(c) for olefin polymers, Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm², and Commission Regulation (EC) No 2023/2006 for good manufacturing practice. Low-temperature seal strength must be validated under ASTM F88/F88M-23 at the intended storage temperature below -30°C; published data for this exact sealant configuration at -40°C remains limited, so converters should not extrapolate from room-temperature peel force. An operational boundary exists at slip masterbatch levels above 2 wt%, which can migrate to the seal surface and lower seal strength, and at melt temperatures above 250°C, which can trigger oxidative gel formation in the extruder.

    Free Quote

    Competitive Dow Tuflin™ HS-7001 NT 7 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Tuflin™ HS-7001 NT 7 is a linear low-density polyethylene resin supplied as natural pellets for blown film and cast film conversion. The grade is specified at a nominal density of 0.918 g/cm³ under ASTM D1505 or ISO 1183-1 and a nominal melt index of 1.0 g/10 min under ASTM D1238 or ISO 1133-1:2022 at 190°C/2.16 kg. In production-scale film lines using single-screw extruders with 24:1 to 30:1 L/D barrier screws, melt temperatures are commonly maintained between 204°C and 232°C, with die pressure kept below 35 MPa to limit melt fracture. The resin is supplied in natural color only; converters requiring pigmented film must add a compatible masterbatch at the hopper rather than selecting a preformulated grade. The polymer structure is based on linear low-density polyethylene with short-chain branching introduced by an alpha-olefin comonomer; supplier literature may not disclose the exact comonomer type and molar fraction for this specific grade.

    What Melt Index and Density Values Are Used for Incoming QC?

    PropertyTest MethodTypical ValueUnit
    Melt indexASTM D12381.0g/10 min
    DensityISO 1183-10.918g/cm³
    Melting peakASTM D3418122°C
    Vicat softening pointASTM D1525101°C

    Incoming resin QC protocols generally align with ISO 1133-1:2022 for melt mass-flow rate and ISO 1183-1 for density, while many North American facilities retain ASTM D1238 and ASTM D1505 for legacy specification alignment. A melt index of 1.0 g/10 min places the grade in the medium-molecular-weight LLDPE range for cast film extrusion, where melt strength is sufficient for draw ratios up to 60:1 on chill-roll lines maintained between 15°C and 25°C. A density of 0.918 g/cm³ positions the material below high-density polyethylene crystallinity and above ultralow-density hexene copolymers; the melting peak is determined by differential scanning calorimetry at a heating rate of 10°C/min. Density specimens should be conditioned at 23°C ± 2°C for 40 h after compression molding, because reactor lot-to-lot density gradients can shift the measured value by ±0.001 g/cm³.

    Film extrusion trials on cast film lines show that melt curtain stability and neck-in are the primary operational limits for this melt index class. A die gap between 0.5 mm and 0.8 mm is typical, with a breaker plate pressure profile below 25 MPa. At line speeds above 300 m/min, edge bead formation and neck-in become critical; reducing melt temperature from 232°C to 218°C and increasing the chill-roll contact arc with a secondary nip can reduce neck-in by up to 15%, although published data for this specific configuration are limited. In blown film, the resin is commonly processed at a blow-up ratio between 2.0:1 and 3.0:1 and a frost line height between 150 mm and 300 mm above the air ring. The processing window for this melt index requires die temperature uniformity within ±5°C across the die circumference to avoid gauge bands thicker than ±8%.

    Puncture, Tear, and Tensile Test Methods for 50 µm Blown Film

    Film properties for LLDPE are gauge-sensitive; comparisons between suppliers should be normalized to 50 µm thickness and a 2.5:1 blow-up ratio. Tensile properties are evaluated under ASTM D882 or ISO 527-3 using type 2 specimens at 500 mm/min. Tear resistance is measured under ASTM D1922 or ISO 6383-2; machine-direction tear for LLDPE of this density is typically 30% to 50% lower than transverse-direction tear because of orientation effects. Dart impact is determined under ASTM D1709 method A or B; method A uses a 38 mm dart with a 0.66 m drop height, while method B uses a 51 mm dart with a 1.0 m drop height. Puncture resistance under ASTM D5748 and slow-rate puncture under ASTM F1306 provide complementary data; the latter is more relevant for load retention in heavy-duty sacks and industrial liners. Published comparative data for this exact grade under all four methods are limited; converter trials should generate a normalized calibration curve at the standard gauge, die gap, and frost line height rather than relying on single-point datasheet values.

    Regulatory status for food-contact applications depends on the final film structure and additive system. As supplied, the base resin may be assessed under FDA 21 CFR 177.1520(c) 3.2a for olefin polymers and under Regulation (EU) No 10/2011 on plastic materials intended to come into contact with food. The European regulation imposes an overall migration limit of 10 mg/dm² for film surfaces and specific migration limits for selected monomers; compliance must be confirmed on the finished packaged article because lamination tie layers, printing inks, and corona treatment by-products are co-responsible. For non-food industrial packaging, REACH registration under EC 1907/2006 and the absence of listed SVHCs above 0.1 wt% in the article are the primary regulatory drivers.

    RequirementReferenceNumerical Threshold / Scope
    US food contactFDA 21 CFR 177.1520(c) 3.2aOlefin polymer, subject to end-use article testing
    EU food contactRegulation (EU) No 10/2011Overall migration 10 mg/dm²
    REACH SVHCEC 1907/2006SVHC content 0.1 wt%
    Packaging heavy metalsDirective 94/62/ECSum of Pb, Cd, Hg, Cr VI 100 ppm

    When Tuflin HS-7001 NT 7 Replaces Conventional LLDPE in Heavy-Duty Sack Lines

    Substituting this resin into a heavy-duty sack line originally set for a conventional Ziegler-Natta LLDPE with melt index 1.0 g/10 min and density 0.918 g/cm³ should begin with a screw-cooling and back-pressure audit. Because molecular weight distribution and comonomer sequence length distribution can differ even when melt index and density are equivalent, the observed melt temperature at the die may shift by 3°C to 6°C at constant screw speed. Maintaining a 2.5:1 blow-up ratio and a die gap of 2.0 mm is generally sufficient to stabilize the bubble; however, if bubble surging occurs, reducing extruder output by 10% and raising lower die temperature to 190°C are preferred over raising the frost line. Raising the frost line tends to reduce machine-direction tear under ASTM D1922 because of increased orientation. Converters comparing to metallocene-catalyzed LLDPE should anticipate a different shear-thinning index: metallocene grades often exhibit lower melt elasticity and a narrower molecular weight distribution, which can improve clarity but reduce bubble stability in high-stalk processing. In contrast, this grade may require a 5°C to 10°C higher melt temperature to achieve equivalent die-lip surface quality, while retaining better dart impact at lower gauge under ASTM D1709.

    Extrusion Lamination and Coextrusion Layer Functions Are Governed by Melt Strength

    In coextrusion, Tuflin HS-7001 NT 7 is used as a toughness layer in three-layer and five-layer structures where the core may be recycled material or lower-cost high-density polyethylene. The melt index of 1.0 g/10 min is compatible with adjacent layers in the 0.5 g/10 min to 2.0 g/10 min range; layer ratios between 20% and 40% are common in industrial heavy-duty liners and agricultural packaging. Extrusion lamination onto oriented substrates requires higher melt temperature, typically 250°C to 280°C at the die, to promote adhesion. This range is near the upper thermal stability limit for LLDPE, and residence time above 240°C should not exceed 10 min to avoid oxidative gel formation. The oxygen induction time measured at 200°C under ISO 11357-6 provides a stability comparator; lower values after regrind blending indicate antioxidant dilution and should trigger a reduction in regrind content to below 30 wt%.

    Top