| HS Code | 517339 |
| Product Name | Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid |
| Product Code | GRSN-2070 NT |
| Chemical Name | Linear Low Density Polyethylene |
| Synonyms | LLDPE |
| Cas Number | 9002-88-4 |
| Physical State | Granular Solid |
| Color | Natural |
| Odor | Mild |
| Density | 0.920 g/cm3 |
| Melt Index | 2.0 g/10 min at 190 °C/2.16 kg |
| Melting Point | 120-135 °C |
| Bulk Density | 0.56 g/cm3 |
| Water Solubility | Insoluble |
| Autoignition Temperature | >300 °C |
| Decomposition Temperature | >300 °C |
| Vapor Pressure | Negligible |
As an accredited Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid is supplied in 25 kg polyethylene-lined bags, palletized for handling. |
| Container Loading (20′ FCL) | Container Loading (20′ FCL): Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid, 25 kg bags, palletized, securely stuffed. |
| Shipping | Linear low density polyethylene (LLDPE), granular solid, non-hazardous. Not regulated as dangerous goods by DOT, IMDG, IATA, or ADR; no UN number. Ship in clean, dry, sealed bags or bulk containers. Protect from moisture, contamination, and excessive heat; store in a cool, dry, ventilated area. |
| Storage | Store in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and open flames. Keep containers tightly closed. Minimize dust and control static with grounding/bonding during transfer. Segregate from oxidizing agents and incompatible materials. Protect from weather and UV. Do not store near food, feed, or drinking water. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Shelf life is 24 months from date of manufacture when stored in original, unopened packaging under cool, dry conditions. |
In cast stretch film manufacture, Dow GRSN-2070 NT linear low density polyethylene granular solid is introduced as the primary core layer resin at a formulation addition ratio of 65–80 wt% in three-layer A/B/C coextrusion structures, with the remaining mass split between metallocene-catalyzed LLDPE at 15–30 wt% and polyisobutylene or hydrogenated polybutene cling additives at 2–6 wt% in the skin layers. The granular solid is fed through a mass-flow hopper with a 70° cone angle and a low-friction liner because granular bulk density is 3–8% lower than pelleted resin and can bridge above a single-screw extruder throat. The line uses a 150 mm core extruder and 90 mm skin extruders, each with a 30:1 L/D barrier screw and Maddock dispersive mixing sections; screen packs are stacked at 40/60/100 mesh, melt temperature is held at 245–265°C, and the flat die gap is 0.5–0.8 mm. The melt curtain is pinned to a polished chill roll maintained at 18–24°C by a vacuum box and edge air knives; draw resonance appears when line speed exceeds 600 m/min or when melt temperature drops below 230°C, producing 3–8% gauge variation as measured by beta gauge scanners. The downstream process uses a die-to-chill-roll distance of 25–50 mm and a secondary cooling roll at 15–20°C before slitting and pre-stretching on 750 mm core winders. Barrel zone set points are 190/210/230/250/255°C; processing above 290°C is avoided because oxidation and gel speck formation increase. Surface moisture adsorbed above RH 60% can create microvoids, so a 70–80°C hopper dryer for 2 h is used only when condensation is observed. Finished product types are 12–23 µm machine wrap film, 8–15 µm hand wrap film, and pre-stretched cores with elongation retention of 70–85% after 200% stretch. Compliance for indirect food contact during palletizing operations is assessed under FDA 21 CFR 177.1520(c) and REACH Regulation (EC) No 1907/2006 Annex XVII; physical testing follows ASTM D882-18 for tensile properties, ASTM D1894-14 for static and dynamic coefficient of friction, ASTM D5748-19 for puncture resistance, ASTM D4321-09 for package yield, and ISO 527-3:2018 for film tensile anisotropy.
Blown film lines running Dow GRSN-2070 NT as the primary resin at 80–95 wt% of total formulation produce monolayer food bags in which Elmendorf tear anisotropy is set by bubble geometry and freeze line height rather than by resin density alone. The formulation addition ratio combines the granular LLDPE with high-pressure LDPE at 5–20 wt% for bubble stability, antiblocking silica masterbatch at 2–5 wt%, and slip additive masterbatch at 1–3 wt%; for 30 µm bread bag film the LLDPE:LDPE ratio is typically 70:30 to 90:10 by weight. Melting is carried out in a 100–150 mm single-screw extruder with a 25:1 barrier screw, melt temperature of 210–230°C, an annular die gap of 1.5–2.2 mm, and a rotating die and haul-off system for gauge randomization. Blow-up ratio is held at 2.2:1 to 2.8:1, while freeze line height is set at 6–10 die diameters and internal bubble cooling is adjusted between 40–60% of blower capacity; exceeding 60% cooling air can destabilize the stalk and create periodic thickness bands of ±4–7% on high-speed towers. The granular solid does not require drying below RH 60%; surface condensation is removed by 70°C air before entering the extruder throat. Finished product types are primary bread bags, frozen vegetable bags, and produce films in thicknesses of 18–70 µm. Compliance for food contact uses FDA 21 CFR 177.1520(c) for olefin copolymers, EU Regulation No 10/2011 Annex I with a total migration limit of 10 mg/dm², and specific migration limits for slip and antiblock additives under the same regulation. Mechanical acceptance tests are performed to ASTM D1922-15, ISO 6383-2:1983, ASTM D1709-16a, and ISO 527-3:2018; melt flow rate is verified per ISO 1133-1:2022 against the granule certificate of analysis.
Extrusion coating of liquid paperboard uses Dow GRSN-2070 NT as a 20–40 wt% blend partner in high-melt-strength LDPE to control neck-in and impart seal and abrasion resistance to gable-top and aseptic carton structures. For a 300 g/m² liquid packaging board, the LLDPE fraction is maintained at 25–35 wt% of a 15 g/m² coating layer; for thinner 12 g/m² heat-seal layers, the ratio is reduced to 20–25 wt% because higher LLDPE fractions above 40 wt% increase edge neck-in beyond 100 mm on conventional coating dies. The line is a 4.5 m tandem extrusion coating unit with a 120 mm 30:1 single-screw extruder, melt temperature of 305–320°C, a flat die gap of 0.6–0.8 mm, and a mirror-finished chill roll at 13–18°C. Corona treatment is applied at 1.5–2.5 kW/m and ozone at 1.5–3.0 kW/m immediately before the nip to raise adhesion of the molten polyethylene to the primed polyolefin layer. Downstream forming takes the coated board through score bending, longitudinal heat sealing, and cross-sectional sealing in filling lines. Terminal finished product types are gable-top dairy cartons, aseptic juice bricks, and hot-fill paperboard containers with edge wicking resistance. Regulatory compliance relies on FDA 21 CFR 176.170(c) for paper and paperboard coatings intended for aqueous and fatty food contact, EU Framework Regulation (EC) No 1935/2004 Articles 3 and 17, and REACH Regulation (EC) No 1907/2006 Annex XVII for lead, cadmium, and phthalate restrictions. Melt flow and density are verified by ISO 1133-1:2022 and ISO 1183-1:2019; blocking resistance of coated board is evaluated per ASTM D3354-15.
Injection moulding of thin-wall food-service lids and dispensing closures uses Dow GRSN-2070 NT at a letdown ratio of 10–35 wt% in a polypropylene or high-density polyethylene base resin to increase environmental stress cracking resistance and low-temperature impact without reducing cycle time below the mold cooling limit. The granulate is dry-blended with the base resin and additives before hopper loading; for a 0.6 mm wall deli lid the LLDPE fraction is 20–30 wt%, the base resin is a 12 g/10 min HDPE blow moulding grade, and a calcium stearate acid scavenger is dosed at 500–1,000 ppm. Process equipment includes a hydraulic injection moulding machine with clamp force of 150–250 tonnes, a 20:1 L/D general-purpose screw with check ring, hot runner manifold with valve gates, and mold temperature held at 15–25°C for rapid solidification. Injection pressure is set at 800–1,200 bar, back pressure at 5–10 bar, screw speed at 100–150 rpm, and booster time at 0.2–0.5 s; total cycle time is 18–28 s. The terminal product types are thin-wall deli lids, tamper-evident overcaps, dispensing closures for dry food canisters, and lids for dairy tubs. Food-contact compliance is determined under FDA 21 CFR 177.1520(c), EU Regulation No 10/2011, and migration testing according to Commission Regulation (EU) 2016/1416 for plastic materials in contact with food. Melt flow rate is tested by ASTM D1238-20 at 190°C/2.16 kg, Izod impact per ASTM D256-10, and tensile properties per ASTM D638-14.
Mineral-filled masterbatch production based on Dow GRSN-2070 NT places the resin as the carrier phase at 25–40 wt% of the formulation, with ground calcium carbonate or talc at 55–70 wt% and a compatible wax or functionalized polyolefin dispersant at 3–8 wt%. The addition ratio is set to maintain a melt mass-flow rate above 2 g/10 min after filler loading so that the concentrate can be let down in film and moulding resins without creating viscosity stratification. The downstream compounding process uses a co-rotating twin-screw extruder with 40:1 L/D, a side-stuffer at L/D 24–28, atmospheric venting before the side-stuffer and vacuum venting at -0.08 MPa after mixing, screw speed of 500–800 rpm, and melt temperature of 200–230°C. Specific energy input is typically 0.18–0.25 kWh/kg; below 0.18 kWh/kg filler dispersion measured as screen pack pressure rise can become unacceptably high. The melt is filtered through a 100–150 mesh breaker plate and strand pelletized or underwater pelletized into 3 mm cylindrical granules. Terminal finished product types are filled masterbatch pellets for blown film antiblock, antifibrillation concentrates for cast stretch film, and carrier resin for liquid colour concentrates. Published data for this specific resin in mineral-filled concentrates is limited; the process window is derived from LLDPE carriers of comparable density class and must be validated on the production line. Regulatory compliance for the compounded output is referenced to REACH Regulation (EC) No 1907/2006 Annex XVII, EU Packaging and Packaging Waste Directive 94/62/EC for heavy metals, and ISO 1133-1:2022 for melt flow rate; ash content is determined by ASTM D5630-13, and density by ISO 1183-1:2019.
For seven-layer forage preservation film, agricultural film lines run Dow GRSN-2070 NT as the polyolefin barrier and puncture layer at 60–90 wt% in outer layers and 50–75 wt% in internal abuse layers; when a polyamide barrier layer is present, it remains at 5–10 wt% of total structure, and the LLDPE-rich layers account for 65–80% of total film mass. The addition ratio of polymer processing aid fluoroelastomer is 0.05–0.10 wt% to suppress melt fracture on high-output towers. The downstream process uses three-layer, five-layer, or seven-layer blown film lines with internal bubble cooling, oscillating haul-off, annular die gap of 1.8–2.4 mm, blow-up ratio of 2.0:1 to 2.5:1, and melt temperature of 220–245°C. For silage bale wrap, total thickness is 25–40 µm, and the cling layer contains 2–6 wt% of a low-melt-index polyisobutylene or EVA-based cling additive; greenhouse covers are coextruded at 150–200 µm with hindered amine light stabilizer packages at 0.15–0.30 wt% to prevent UV embrittlement. Terminal finished product types are silage bale wrap film, greenhouse cover film, and mulch film in 20–50 µm thicknesses. Standards include EN 13206:2017 for agricultural film definitions and requirements, ASTM D5748-19 for puncture resistance, ASTM D4833-07 for index puncture resistance, ASTM G154-16 for UV weathering, and ISO 527-3:2018 for tensile properties. Food-contact relevance is limited to silage wrap in direct feed preservation, evaluated under EU Regulation No 10/2011 only where migration from film to fermented fodder is within specified overall migration limits.
Competitive Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow GRSN-2070 NT Linear Low Density Polyethylene Granular Solid is supplied as a natural, unpigmented granular feedstock within the manufacturer’s linear low density polyethylene portfolio. The product class is distinguished from conventional low density polyethylene by a predominantly linear backbone with short-chain branches introduced through ethylene-alpha-olefin copolymerization, and by the practical absence of long-chain branching. This structural arrangement changes crystallization, shear thinning, melt extension, tensile properties, impact resistance, and environmental stress-crack resistance. Relevant test methods include ASTM D792-20 for density, ASTM D1238-20 for melt flow rate, ASTM D638-14 for tensile properties, ASTM D1709-16a for dart impact, and ASTM D1693-21 for environmental stress-crack resistance. Grade-specific values for GRSN-2070 NT density, melt flow rate, comonomer type, additive package, and thermal transitions are controlled by the supplier certificate of analysis and technical data sheet; those documents govern lot release and should not be replaced by class-level literature data. Publicly available data for general-purpose butene-comonomer linear low density polyethylene grades commonly place density between 0.918 g/cm³ and 0.922 g/cm³ when measured under ISO 1183-1:2019, and melt flow rate between 1.0 g/10 min and 3.0 g/10 min under ISO 1133-1:2022 at 190 °C and 2.16 kg. These ranges are not product specifications but provide a comparative frame for downstream process design.
Granular solid feedstocks differ from pelletized linear low density polyethylene in particle aspect ratio, bulk density, cohesive flow function, and dust generation. Typical bulk densities measured under ISO 60:1977 for granular polyolefin resins range from 0.45 g/cm³ to 0.55 g/cm³, while sieve retention under ASTM D1921-18 commonly shows a mean particle width between 2 mm and 5 mm. These values affect hopper outlet sizing and mass-flow design. In conical hoppers with half-angles greater than 30° from vertical, granular linear low density polyethylene can exhibit funnel-flow discharge and bridging when outlet diameter is below 150 mm. On gravimetric feeders equipped with vertical agitators, production-scale observations report feed rate fluctuations of ±3% to ±5% as feeder hopper level falls below 20% and rat-holing develops above the screw flights. Feed throat temperature on a 65 mm single-screw extruder is typically maintained below 40 °C to prevent premature granule sintering under screw precompression. For loss-in-weight feeding, refill intervals shorter than 2 min and hopper agitation speed above 30 min⁻¹ can introduce air entrapment and density variability that appear as extruder output fluctuation measured at the die lip by gravimetric throughput sensors.
At the macromolecular level, linear low density polyethylene incorporates short-chain branches that interrupt crystalline lamellae. Butene-comonomer grades carry ethyl branches of 2 carbons; hexene and octene grades carry branches of 4 carbons and 6 carbons, respectively. Longer comonomer branches reduce crystalline lamella thickness and increase tie-molecule concentration, which changes Elmendorf tear strength under ASTM D1922-15, puncture resistance under ASTM D5748-19, and slow crack growth resistance under ASTM F1473-21. Compared with low density polyethylene, the linear backbone and short-chain branch architecture produce a narrower molecular weight distribution and reduced shear thinning at extrusion shear rates. Capillary rheometry under ISO 11443:2021 at 210 °C shows that linear low density polyethylene retains a higher fraction of low-shear viscosity at shear rates above 1000 s⁻¹ than long-chain-branched low density polyethylene. This requires higher torque on twin-screw compounding lines and can increase melt temperature rise across restrictive screen packs and gear pumps. In blown film, lower melt extension hardening reduces bubble tension retention and narrows the stable operating window between bubble sag and extensional rupture.
Butene-comonomer linear low density polyethylene occupies a thermal and mechanical position between low density polyethylene and high density polyethylene. Differential scanning calorimetry under ISO 11357-3:2018 commonly reports peak melting temperatures from 120 °C to 124 °C for butene linear low density polyethylene, while low density polyethylene peaks are near 105–112 °C and high density polyethylene peaks are near 130–137 °C. The crystalline fraction is lower than high density polyethylene, which reduces density, flexural modulus, and softening temperature. Table 1 summarizes class-level comparative property ranges; these ranges are compiled from public technical references and are not specification values for GRSN-2070 NT.
| Resin class | Density (g/cm³) | Tensile yield strength (MPa) | Flexural modulus (MPa) | Dart impact (g) | Peak melting temperature (°C) |
|---|---|---|---|---|---|
| LDPE | 0.917–0.930 | 10–20 | 150–350 | 50–150 | 105–112 |
| LLDPE butene | 0.918–0.922 | 15–25 | 200–450 | 80–300 | 120–124 |
| HDPE | 0.940–0.965 | 22–35 | 800–1600 | <50 | 130–137 |
Test references for Table 1 are density ASTM D792-20, tensile yield strength ASTM D638-14, flexural modulus ASTM D790-17, dart impact ASTM D1709-16a, and melting temperature ISO 11357-3:2018. Published data for this specific configuration is limited regarding grade-specific additive interactions; direct comparative trials on production equipment are required for lot-level substitution decisions.
Published data specific to GRSN-2070 NT across coextruded film die geometries is limited; the following film-extrusion references are therefore class-level linear low density polyethylene process settings. Blown film conversion of butene linear low density polyethylene commonly uses single-screw extruders with 24:1 to 30:1 L/D ratio, barrier screws, and annular die gaps from 1.0 mm to 2.5 mm. Melt temperature is maintained between 190 °C and 230 °C, while die pressure ranges from 20 MPa to 35 MPa. Blow-up ratios of 2.0:1 to 3.0:1 and frost line heights from 200 mm to 600 mm are typical. The lower melt extension hardening of linear low density polyethylene relative to low density polyethylene narrows bubble stability; addition of 5 wt% to 10 wt% low density polyethylene is frequently used to control bubble flutter at line speeds above 80 m/min. High stalk heights above 800 mm can amplify edge-wave defects and gauge variation unless dual-lip air-ring flow is adjusted. In cast film, chill roll temperatures from 18 °C to 30 °C reduce surface tack and improve thickness uniformity measured under ASTM D6988-21. For coextruded sealant layers, linear low density polyethylene heat-seal initiation temperature is typically 10–20 °C lower than high density polyethylene but higher than metallocene linear low density polyethylene grades of equivalent density; hot-tack performance under ASTM F1921-12 is therefore grade-dependent and sensitive to seal-bar temperature, dwell time, and contamination.
When injection molding tools are transitioned from low density polyethylene to linear low density polyethylene, the lower melt-extension behavior and slower crystallization of linear low density polyethylene change filling and packing requirements. Parts with wall thickness from 2 mm to 4 mm often require 10% to 20% longer hold time at constant gate freeze temperature. On hydraulic injection molding machines with clamp force between 150 t and 300 t, screw back pressure is set at 5 MPa to 10 MPa, and injection velocity is maintained at 60 mm/s to 120 mm/s to avoid flow marks and gate blush. Nozzle melt temperature is typically 200–220 °C for general-purpose butene linear low density polyethylene; mold temperature is held at 20–40 °C. Because linear low density polyethylene has higher viscosity than low density polyethylene at low shear rates, runner and gate cross-sections should be evaluated for 10–15% enlargement to maintain equivalent filling pressure. Processing above 260 °C or residence time exceeding 10 min can increase thermo-oxidative chain scission and gel formation, visible as black specks or surface melt fracture. For thin-wall packaging with flow length to thickness ratios above 150:1, melt temperature can be raised to 240 °C only if screw geometry provides sufficient mixing without excessive viscous heating. Published data for this specific configuration is limited for very thin-wall GRSN-2070 NT applications; mold-flow validation using grade-specific viscosity curves is required.
For food-contact packaging, the regulatory status of linear low density polyethylene depends on base resin, comonomer, stabilizer package, and end-use conditions. Compliance is typically evaluated under FDA 21 CFR 177.1520(c) for olefin polymers when the product is supplied under applicable good manufacturing practice. European food-contact compliance is evaluated under EU Regulation 10/2011 with overall migration limits of 10 mg/dm² using food simulants and test conditions described in the EN 1186 series. Industrial transparency declarations may also require REACH EC 1907/2006 SVHC confirmation and Directive 2011/65/EU RoHS substance restrictions. Table 2 provides the compliance matrix for documentation review.
| Standard or regulation | Scope | Relevant limit or method |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer food-contact uses | End-use temperature and food-type restrictions |
| EU Regulation 10/2011 | Plastic food-contact materials | Overall migration 10 mg/dm²; EN 1186 series |
| REACH EC 1907/2006 | Registration and SVHC content | Substance and article concentration thresholds |
| RoHS Directive 2011/65/EU | Electrical and electronic equipment restrictions | Pb 1000 mg/kg, Hg 1000 mg/kg, Cd 100 mg/kg, Cr(VI) 1000 mg/kg, PBB/PBDE 1000 mg/kg |
Granular solid transfer introduces a dust fraction that pelletized resin does not carry. Sieve analysis under ASTM D1921-18 often reports fines below 500 µm at 0.5–2.0 wt% in granular polyolefins. In vacuum conveying systems, fines reduce filter bag efficiency and can accumulate in rotary airlock clearances, eventually raising motor current draw on dilute-phase blowers. Conveying line velocity for granular linear low density polyethylene is typically maintained between 18 m/s and 25 m/s to balance pressure drop and particle attrition. Lower velocities increase slugging and line plugging, while higher velocities generate electrostatic surface charge. Metal piping should be grounded to resistance below 10⁶ Ω to dissipate charge. The resin should not be stored in direct contact with copper-based flame retardant residues or strong oxidizing agents; copper ions can accelerate oxidative degradation of polyethylene. Long-term storage in direct sunlight can raise granule surface temperature above 50 °C and consume phenolic or phosphite antioxidants before processing. Polyethylene is not hygroscopic; drying is usually unnecessary. If cold granular material is moved into a warm processing area with relative humidity above 60%, condensation on granule surfaces can produce flow instabilities and visual surface defects. For those conditions, desiccant drying at 80 °C for 2 h with dew point below −20 °C is applied before hopper loading. Avoid combination with amine-based additive carriers in color concentrates without compatibility testing, because amine chemistry can interact with oxygenated surface species and alter color stability in unpigmented films.