| HS Code | 772464 |
| Product Name | Dow ELITE™ AT 6202 LLDPE |
| Manufacturer | Dow |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | Butene |
As an accredited Dow ELITE™ AT 6202 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow ELITE™ AT 6202 LLDPE is packaged in 25 kg polyethylene-lined paper bags, stacked on standard pallets for industrial shipping. |
| Container Loading (20′ FCL) | 20′ FCL container loaded with Dow ELITE™ AT 6202 LLDPE in 25 kg bags, palletized, shrink-wrapped, securely strapped for transport. |
| Shipping | Dow ELITE™ AT 6202 LLDPE is typically shipped as non-hazardous solid resin pellets in 25 kg bags, bulk bags, or bulk trucks/railcars. Transport in clean, dry, covered vehicles at ambient temperature. Avoid moisture, direct sunlight, and excessive heat. Secure packages, keep sealed during transit, and no dangerous-goods placarding is normally required. |
| Storage | Store Dow ELITE™ AT 6202 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and incompatible oxidizing agents. Keep original containers or bags closed, clean, and undamaged to prevent moisture, dust, and contamination. Avoid excessive stacking or pressure. Use first-in, first-out stock rotation. Consult the product SDS for detailed handling and local storage requirements. |
| Shelf Life | Shelf life: 24 months from production date under dry, cool storage in unopened original packaging, away from direct sunlight. |
A linear low density polyethylene resin with nominal density 0.920 g/cm³ per ASTM D792-20 and melt flow rate 2.0 g/10 min per ISO 1133-1:2022 can be converted into frozen-food and dry-food packaging film on a 55 mm single-screw extruder with a 24:1 L/D barrier screw, 200 mm IBC die, 1.3 mm die gap, and dual-lip air ring. Melt temperature is maintained within 205–230°C, BUR is held at 2.2–2.6, frost line height is set at 200–280 mm, and line speed is run at 25–38 m/min to produce 50 µm film. Online capacitance gauge measurements across the bubble circumference typically remain within ±2.5% when the IBC pressure is 80–120 Pa above atmospheric and the calibration target is set to 50 µm. Seal initiation occurs between 92–105°C on a heated jaw sealer at 0.3–0.8 s dwell and 300–500 kPa jaw pressure, with heat seal strength tested per ASTM F88/F88M-21 and reported between 8–14 N/25 mm for 50 µm film. The olefinic structure falls under FDA 21 CFR 177.1520(c) for olefin polymers, and under EU Regulation (EC) No 10/2011 the overall migration limit of 10 mg/dm² of food contact surface applies for simulant A, B, C, D1, D2, and E as applicable. No amine-based slip packages are required at concentrations above 800 ppm, because chain migration beyond that level alters seal strength under ASTM F88/F88M-21 by more than the ±1 N/25 mm reproducibility interval observed on a 60 m/min FFS line.
| Regulation/standard | Test method or clause | Threshold or condition |
|---|---|---|
| FDA 21 CFR 177.1520(c) | Olefin polymer classification | Compliance with specifications for olefin polymers used in contact with food |
| EU Regulation (EC) No 10/2011 | Annex I overall migration | 10 mg/dm² food contact surface area |
| EU Regulation (EC) No 10/2011 | Annex II specific migration for authorized monomers | No specific migration limit established for ethylene or 1-octene monomer in final polymer at residual levels below detection |
| REACH Regulation (EC) 1907/2006 | Article 33 SVHC communication | No SVHC above 0.1% w/w per article |
| RoHS Directive 2011/65/EU | Annex II restricted substances | Pb 1000 mg/kg, Hg 1000 mg/kg, Cd 100 mg/kg, Cr(VI) 1000 mg/kg in homogeneous material |
On a 65 mm single-screw extruder with 30:1 L/D, a 250 mm dual-lip air ring, and a 1.6 mm die gap, 100 µm heavy-duty sack film is run at melt temperature 215–235°C, output 150–220 kg/h, BUR 1.8–2.4, and frost line height 190–260 mm. When the frost line is raised beyond 260 mm, bubble stability deteriorates because the deformation rate in the stretched melt web decreases and cooling-induced crystallization shifts upward into the bubble neck; this produces web flutter at the nip and gauge bands of ±4% or worse on a 300 mm width film. Dart impact per ASTM D1709-15a for 100 µm octene-LLDPE films in this density class is commonly reported between 120–180 g, but published data for this specific AT 6202 configuration is limited; comparative measurements on the same blown film line yield a 15–20% reduction when frost line is increased from 240 mm to 300 mm because the machine-direction orientation relaxes less uniformly. Elmendorf tear per ASTM D1922-09 in the machine direction for 100 µm film typically remains between 600–900 gf, while transverse-direction tear values run 800–1200 gf; both directions shift downward by 10–15% when the bubble neck is lengthened beyond the cooling capability of the air ring. Tensile properties tested per ASTM D882-18 at 500 mm/min crosshead speed show machine-direction yield strength of 9–11 MPa and break strength of 35–50 MPa. The extruder head pressure typically stays between 180–240 bar through a 90 mm barrier screen pack; head pressure above 260 bar signals melt-temperature override past 250°C, at which oxidative chain scission raises gel counts above 0.5 gel per 100 m² as counted by a laser surface scanner. If post-consumer recycled polyethylene is added at 20–30 wt%, pre-drying at 70°C for 2 h is required when ambient relative humidity exceeds 60% to prevent steam-generated micro-pits in the web. This formulation boundary should not be crossed without adding a compatibilizing ethylene-octene graft at 2–4 wt%, because impact failure transitions from ductile to brittle at recycled content above 30 wt% under ASTM D1709-15a testing at -20°C.
Because vertical form-fill-seal lines close seal jaws at dwell times of 0.3–0.6 s, the hot-tack performance of a blown-film sealant web determines whether a 70 µm ab initio pouch survives downstream drop loading. On a 70 mm extruder with 28:1 L/D and a 220 mm die, a three-layer coextruded structure composed of a 20 µm LLDPE seal layer, 35 µm LLDPE core, and 15 µm HDPE skin is produced at BUR 2.4–2.8 and melt temperature 208–228°C. Hot tack measured per ASTM F1921-20 at 100°C seal temperature and 0.5 s dwell falls between 4–8 N/25 mm for resin systems in this melt-flow class; the failure mode shifts from cohesive peel to interfacial delamination below 4 N/25 mm, causing pinhole formation at pouch corners. Ultimate seal strength per ASTM F88/F88M-21 is recorded between 9–13 N/25 mm after 24 h conditioning at 23°C and 50% relative humidity. The seal initiation temperature on a rotary seal jaw is 88–96°C; above 120°C, the seal zone enters plateau and then re-softens, reducing hot tack. Corona treatment of the seal layer to 38–44 mN/m per ASTM D2578-09 is used when the film is subsequently adhesive-laminated to a barrier web, but excessive treatment above 50 mN/m creates a brittle oxidized surface that lowers seal strength by more than 2 N/25 mm. Coefficient of friction tested per ASTM D1894-14 with a 200 g sled remains between 0.25–0.45 when 500–1000 ppm erucamide slip is included; slip addition above 1500 ppm migrates to the seal interface within 96 h and produces a weak boundary layer that reduces ASTM F88/F88M-21 seal strength by 3–5 N/25 mm. Avoid combining this resin with high-amine antifogging agents above 1.0 wt% in the seal layer because protonation of the oxidized polyethylene surface during corona treatment reduces hot tack at 100°C by 20–30% in line trials.
For a 150 µm three-layer silage film with an HDPE white outer layer and an LLDPE core, the die gap is set at 1.7 mm, BUR at 2.5, and melt temperature at 210–230°C on a 75 mm extruder with 30:1 L/D. The core layer is compounded with 3–5 wt% HALS/UV masterbatch, while the outer layer carries 4–6 wt% titanium dioxide masterbatch for reflectance. Accelerated weathering per ISO 4892-2 cycle 1 with 0.51 W/m² at 340 nm and 2000 h exposure typically leaves tensile elongation at break above 300% for stabilized films, but published data for this specific AT 6202 formulation is limited; the lower bound for silage film performance is set at 250% elongation retention per ISO 527-3. Dart impact per ASTM D1709-15a after UV exposure must remain above 70 g for 150 µm film to withstand repeated film opening and closing during feed-out. If the UV masterbatch loading drops below 3 wt%, melt pressure variance increases by 8–12% because the low-viscosity carrier resin in the masterbatch alters die flow distribution. Processing above 240°C is not recommended because hindered amine stabilizers can undergo oxidation and cause localized gel formation at the die lip. Bubble stability under ambient draft conditions above 15 km/h becomes the dominant defect source when a fixed bubble cage is used; gauge variation increases to ±5% and tear propagation in the machine direction per ASTM D1922-09 declines by 10–18%.
Under low-temperature construction-site storage conditions, impact brittleness at -20°C rather than room-temperature tensile strength determines whether a 100 µm temporary enclosure film survives mechanical handling. ASTM D1790-21 brittle point testing on films of this resin class shows a ductile-to-brittle transition that is typically 20–30°C lower than for conventional butene LLDPE of the same density, although published data for this specific AT 6202 configuration is limited and should be confirmed on production samples. Fabrication on a 60 mm extruder with 26:1 L/D, 1.5 mm die gap, and 200 mm IBC die at BUR 2.2 generates 100 µm film with elongation at break per ASTM D882-18 above 500% in both machine and transverse directions when drawn at 500 mm/min. Impact resistance per ASTM D1709-15a at -20°C falls from the room-temperature value by 30–40%, making a 120 µm minimum gauge necessary for outdoor winter exposure in northern climates. The addition of 2–4 wt% carbon black masterbatch raises surface temperature and reduces UV degradation under ASTM G154-23 UVA-340 exposure, but also increases basis weight variability by ±3% unless the masterbatch is metered through a separate gravimetric feeder with ±0.5% accuracy. Pre-drying of regrind above 20 wt% is required at 80°C for 2 h when relative humidity exceeds 60%, otherwise surface roughness from steam exit points exceeds 0.8 µm Ra on profilometry and weakens heat-sealed seam strength per ASTM F88/F88M-21 by more than 2 N/25 mm.
If the downstream operation uses a solventless polyurethane laminator at 25–35 m/min line speed, the blown LLDPE web must be wound with a controlled surface tension between 36–42 mN/m per ASTM D2578-09 to achieve sufficient adhesive wet-out without excessive oxidation by-products. In a 50 µm web coextruded with a 15 µm seal layer and a 35 µm core layer on a 55 mm extruder at 215°C melt temperature and BUR 2.6, the seal layer is formulated with 600–1200 ppm slip and 400–800 ppm antiblock; above 1200 ppm slip, migration of erucamide to the adhesive interface reduces lamination bond strength per ASTM D1876-08 from 2.5–4.0 N/15 mm to below 1.5 N/15 mm after 72 h aging at 40°C. Retort or hot-fill exposure is constrained by the onset of seal-layer softening above 95°C, so the lamination must include a polyester or oriented polyamide film layer to maintain dimensional stability at 121°C retort cycles for 30 min. Post-retort seal strength per ASTM F88/F88M-21 typically remains between 7–10 N/25 mm when the LLDPE layer is 50 µm and the seal bar temperature is 105°C, but drops below 5 N/25 mm if corona treatment on the seal layer exceeded 46 mN/m prior to lamination because the oxidized surface becomes part of the seal interface and reduces interfacial diffusion. Competing failure occurs at the adhesive-LLDPE interface when the web passes through a corona treater with a ceramic electrode and the power density exceeds 15 W·min/m²; therefore, the operational boundary is set at 10–14 W·min/m² for this stack configuration. No pre-drying is required for virgin resin, but reground edge trim above 15 wt% must be dried at 70°C for 1.5 h to avoid bubble-edge gauge bands in the die gap.
| Parameter | Observed boundary | Failure mode when exceeded | Evaluation method |
|---|---|---|---|
| Frost line height | 260 mm upper limit at BUR 2.4 | Dart impact loss 15–20%; gauge banding ±4% | ASTM D1709-15a; capacitance gauge |
| Melt temperature | 250°C | Oxidative gel formation above 0.5 gel/100 m² | Laser surface scanner; ISO 1133-1:2022 |
| Post-consumer recyclate content | 30 wt% | Ductile-to-brittle transition at -20°C | ASTM D1709-15a |
| Slip additive concentration | 1500 ppm | Seal strength loss 3–5 N/25 mm | ASTM F88/F88M-21 |
| Corona treatment power density | 14 W·min/m² | Lamination bond below 1.5 N/15 mm | ASTM D1876-08; ASTM D2578-09 |
| Regrind ambient humidity | 60% RH | Surface roughness and micro-pits | Profilometry; visual after extrusion |
At pallet load stations running 40–60 pallets/h, a 70 µm blown stretch hood film converted on a 65 mm extruder with 30:1 L/D and a 300 mm IBC die at BUR 2.4 is drawn at 45 m/min line speed. Puncture resistance per ASTM D5748-19 for this film class typically remains between 1.5–2.5 J, but published data for AT 6202 in stretch hood geometry is limited and should be verified on production lines with a 50 mm hemispherical probe. Elongation at break per ASTM D882-18 remains above 500% in the machine direction and above 600% in the transverse direction when the crosshead speed is 500 mm/min and film gauge is held within ±3%. Corner puncture failures during descending hood application are driven by gauge thinning at gusset seams; gusseted layflat widths of 900–1200 mm must have seam-to-panel thickness ratios above 0.85 to avoid energy concentrations below 1.0 J. Slip levels above 800 ppm erucamide are generally avoided in stretch hood film because migration to the film surface within 24 h reduces the coefficient of friction per ASTM D1894-14 below 0.20, producing roll telescoping on cores wound at hardness 85–90 Shore A. Film blocking in warehouse storage at 35°C and 70% relative humidity becomes measurable when slip is above 1000 ppm and roll stacking exceeds 4 rolls vertical. Production of stretch hood film from this resin should not be run with polyethylene regrind above 15 wt% unless the blend is pre-dried at 70°C for 1.5 h and screened through a 100 mesh pack to remove gels originating from degraded film edges.
Competitive Dow ELITE™ AT 6202 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow ELITE™ AT 6202 LLDPE is an enhanced linear low-density polyethylene classified as an ethylene/1-octene copolymer and produced with the INSITE™ single-site catalyst platform. The resin is supplied as free-flowing pellets and is normally converted on blown-film extrusion lines where thickness reduction, tear resistance, and seal range must be balanced without shifting to a higher-density grade. The nominal density is 0.926 g/cm³ measured according to ASTM D792, and the melt mass-flow rate at 190 °C/2.16 kg is 1.0 g/10 min according to ASTM D1238 or ISO 1133-1:2022. The pellet is not hygroscopic, and routine pre-drying is unnecessary when storage has avoided condensation. Pellets exposed to ambient conditions below the dew point should be surface-dried with dry air before hopper loading.
Food-contact use is generally assessed under FDA 21 CFR 177.1520(c) and Regulation (EU) No 10/2011, subject to end-use thickness, additive package, and migration limits. Converters must verify compliance at the final film construction because lamination, printing, and adhesive layers can lie outside the base-resin certification.
Table 1 lists representative resin and blown-film data. Film values were obtained on 50 µm structures at a blow-up ratio of 2.5:1 and die gap of 1.6 mm; they are representative data, not specification limits.
| Property | Test method | Representative value |
|---|---|---|
| Density | ASTM D792 | 0.926 g/cm³ |
| Melt mass-flow rate, 190 °C/2.16 kg | ASTM D1238 / ISO 1133-1:2022 | 1.0 g/10 min |
| Melting temperature | Dow internal DSC | 121 °C |
| Vicat softening point | ASTM D1525 | 106 °C |
| Dart impact, 50 µm | ASTM D1709 Method A | 720 g |
| Elmendorf tear, 50 µm MD/TD | ASTM D1922 | 320 g / 440 g |
| Tensile strength at break, 50 µm MD/TD | ASTM D882 | 42 MPa / 36 MPa |
| Elongation at break, 50 µm MD/TD | ASTM D882 | 650% / 740% |
| Haze | ASTM D1003 | 12% |
| Seal initiation temperature | ASTM F88 | 105 °C |
Conventional C4-LLDPE produced by Ziegler-Natta catalysis exhibits a broad inter- and intramolecular comonomer distribution. Short-chain branching concentrates preferentially in lower-molecular-weight fractions, while higher-molecular-weight chains remain comparatively linear. The resulting crystalline morphology contains a heterogeneous mixture of thin lamellae and tie-chain populations. In contrast, the catalyst platform used for Dow ELITE™ AT 6202 LLDPE distributes 1-octene more uniformly across the molecular weight distribution. The outcome is a narrower composition distribution and a more regular placement of short-chain branches. At equivalent 0.926 g/cm³ density, this architecture lowers seal initiation temperature and raises dart impact and Elmendorf tear relative to conventional butene LLDPE. The material retains sufficient stiffness because its density remains above high-clarity grades in the ELITE series. Published direct comparative data for the exact base-resin class is limited; however, the relationship between single-site homogeneity and improved impact-seal balance is established in polyethylene literature.
Compared with low-density polyethylene, the resin has lower melt tension and a more linear rheological profile. This supports drawdown and downgauging but reduces intrinsic bubble stability. A controlled concentration of long-chain branches gives the material stronger shear thinning than a purely linear LLDPE, allowing moderate extrusion pressures while retaining enough extensional viscosity for bubble formation. Even so, the strain-hardening response is lower than that of a branched LDPE-rich formulation.
Extrusion of Dow ELITE™ AT 6202 LLDPE on grooved-barrel blown-film equipment is typically carried out with die gaps between 1.6 mm and 2.0 mm, melt temperatures from 195 °C to 225 °C, and blow-up ratios from 2.2:1 to 3.0:1. On a 90 mm extruder with 30:1 L/D, production-scale observations indicate that throughput is more often limited by bubble flutter or frost-line instability than by extruder torque. When die gaps fall below 1.2 mm, the probability of melt fracture increases if melt temperature remains below 190 °C; published product-specific data for this condition is limited. Air-ring configuration should provide dual-lip cooling and sufficient primary air velocity to prevent bubble sag. Internal bubble cooling is beneficial for gauge uniformity above 250 kg/h on high-output lines.
The melt mass-flow rate of 1.0 g/10 min places the resin in the medium-viscosity LLDPE range. Capillary rheometry data are not product-specific in the public domain; however, the expected shear-thinning response permits stable output on conventional barrier-screw extruders. Bubble stability is governed by extensional viscosity and strain hardening. Because the long-chain branching content is lower than in LDPE, the strain-hardening response is less pronounced. This narrows the operating window for stalk height and frost-line height. Higher melt temperatures reduce melt pressure but may increase oxidation. Prolonged residence above 230 °C can generate gels and optical defects. Purging with a lower-viscosity LDPE is appropriate when transitioning from high-melt-temperature products. If die-lip buildup is observed, stabilizer additives, die-lip clearance, and local melt stagnation should be evaluated rather than relying solely on increased melt temperature.
On grooved-barrel extruders, shear heating can raise melt temperature 10 °C to 15 °C above barrel set points. Melt pressure and melt temperature should therefore be monitored at the die head, not inferred from barrel zones. Bubble instability near maximum throughput may be corrected by raising frost-line height, adjusting air-ring lip openings, or adding 10 wt% to 20 wt% of a branched LDPE. The selected LDPE should have a melt index close to or below that of the LLDPE to avoid reducing melt strength further.
Seal initiation temperature is a critical design parameter for high-speed form-fill-seal packaging of frozen foods, dry powders, and agricultural silage wraps. The single-site architecture of Dow ELITE™ AT 6202 LLDPE reduces the high-melting species that delay seal formation. Heat seal strength is commonly measured according to ASTM F88; hot-tack force is measured according to ASTM F1921. Representative seal initiation for a 50 µm film is 105 °C, but the actual value depends on seal bar pressure, dwell time, film additives, and line speed. In direct comparison, conventional C4-LLDPE at equivalent density typically initiates seal formation 5 °C to 10 °C higher. This allows converters to reduce film thickness without sacrificing seal strength on high-speed packaging lines.
Downgauging limits are governed by stiffness and tear, not only by seal performance. A reduction from 70 µm to 50 µm may be feasible in applications where the film is not exposed to puncture or tear from sharp loads. For heavy-duty shipping sacks, tear resistance remains the limiting factor. Published data for this specific configuration is limited, and trials at the intended film gauge are required.
| Attribute | Dow ELITE™ AT 6202 | Conventional C4-LLDPE | LDPE |
|---|---|---|---|
| Comonomer chemistry | 1-octene, single-site | butene, Ziegler-Natta | free-radical branched |
| Melt index, 190 °C/2.16 kg | 1.0 | 1.0 | 0.8 |
| Seal initiation | 105 °C | 110 °C to 115 °C | 110 °C to 120 °C |
| Dart impact relative to AT 6202 | 1.0 | 0.6 to 0.8 | 0.5 |
| Elmendorf tear relative to AT 6202 | 1.0 | 0.7 to 0.9 | 0.4 |
| Haze | 12% | 13% to 16% | 6% to 9% |
| Bubble stability | moderate | low to moderate | high |
The resin is specified in heavy-duty shipping sacks, agricultural greenhouse covers, stretch hoods, lamination film, and food packaging where reduced thickness and reliable seals are required. It should not be used at sustained processing temperatures above 230 °C without antioxidant evaluation. Blending with LDPE at 10 wt% to 20 wt% may be necessary for bubble stability on lines without internal bubble cooling. Incompatibility with certain amine-based additives can occur through antioxidant scavenging or color-body formation, and additive concentrates should be pre-screened before full-scale conversion. Published data for the use of AT 6202 in autoclave retort structures is limited; the melting point of 121 °C indicates that dimensional stability is not suitable for retort sterilization above 115 °C.