Dow Elite 5500g Enhanced Polyethylene Resin

Dow ELITE™ 5500G Enhanced Polyethylene Resin

    • Product Name: Dow ELITE™ 5500G Enhanced Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 620187
    Productname Dow ELITE™ 5500G Enhanced Polyethylene Resin
    Manufacturer Dow
    Resintype Enhanced Polyethylene
    Density 0.955 g/cm³
    Meltindex 0.85 g/10 min
    Meltflowratio 100
    Meltingpoint 134 °C
    Vicatsofteningpoint 127 °C
    Tensileyieldstrength 31 MPa
    Tensilebreakstrength 52 MPa
    Elongationatbreak 600%
    Onepercentsecantmodulus 1100 MPa
    Dartimpact 200 g
    Elmendorftearmd 20 g
    Elmendorfteartd 250 g
    Haze 12%
    Gloss45 45%
    Coefficientoffriction 0.2

    As an accredited Dow ELITE™ 5500G Enhanced Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5500G Enhanced Polyethylene Resin comes in 25 kg polyethylene bags, palletized and stretch-wrapped for safe storage and transport.
    Container Loading (20′ FCL) 20′ FCL container loaded with Dow ELITE™ 5500G Enhanced Polyethylene Resin, palletized 25 kg bags, shrink-wrapped, secured for ocean transport.
    Shipping Dow ELITE™ 5500G Enhanced Polyethylene Resin is shipped as non-hazardous solid pellets. Typical packaging includes 25 kg bags, 1,000 kg bulk bags, and bulk trucks or railcars. Store in a cool, dry, ventilated area; keep containers closed and away from heat or ignition.
    Storage Store Dow ELITE™ 5500G Enhanced Polyethylene Resin in a cool, dry, well-ventilated area, away from direct sunlight, heat, and ignition sources. Keep original bags or containers closed and palletized off the floor. Protect from moisture, dust, and contamination. Avoid prolonged storage above 50°C. Do not stack excessively. Practice first-in, first-out rotation and use within recommended shelf life.
    Shelf Life Shelf life: 24 months from date of manufacture when stored in a cool, dry place in unopened containers.
    Application of Dow ELITE™ 5500G Enhanced Polyethylene Resin

    In frozen food primary packaging converted on high-stalk blown film lines, ELITE 5500G is let down into low-density polyethylene at 20–40 wt% to raise dart impact resistance measured under ASTM D1709-16a Method A while maintaining haze below 8% under ASTM D1003-13. The food-contact compliance position is established under FDA 21 CFR 177.1520(c)3.1a for olefin polymers and EU Regulation (EU) No 10/2011 Annex I, with overall migration below 10 mg/dm² under the frozen-food simulant condition of 10 days at 40°C. On a production line using a 65 mm grooved-feed extruder with L/D 30:1, a 250 mm spiral mandrel die, and die gap 1.4 mm, stable bubble geometry is observed at melt temperatures of 199–216°C, blow-up ratio 2.5:1–3.0:1, and frost line height 500–650 mm. Bubble instability occurs when the let-down exceeds 50 wt% unless the frost line is raised to 700 mm and the external air ring is shifted from single-lip to dual-lip configuration, because the higher molecular-weight tail of the enhanced resin increases melt strength but also increases bubble sag at low internal bubble pressure. Terminal products include frozen vegetable pillow bags, fish fillet freezer packs, ice cream overwrap, and poultry portion pouches; these structures are typically printed gravure or flexo on the outer LDPE-rich skin, while the inner sealant layer contains the higher ELITE 5500G fraction. Pre-drying is not required below 60% relative humidity, but silo transfer systems with high fines carry-over must be vented to avoid angel-hair formation in the hopper.

    What Limits Seal Initiation Temperature in Coextruded Liquid Pouch Structures?

    The limiting factor in liquid pouch sealing is not enthalpy recovery at the seal bar but migration of high-melting constituents from the outer HDPE or BOPP layer into the sealant. In coextruded cast film, ELITE 5500G is used as the sealant layer at 100 wt% or as a 50–70 wt% blend with metallocene plastomer to reduce seal initiation to 82–90°C under ASTM F1921-18 hot tack testing at 0.5 N/mm² seal pressure and 500 mm/s peel speed. The downstream process is a 3-layer cast coextrusion line with 80 mm primary extruders, L/D 28:1, a 1,200 mm slot die, and chill roll temperature 18–24°C; the sealant layer is maintained at 18–22 µm to limit coefficient of friction while preserving seal-through-contamination resistance. Industry compliance includes EU Regulation (EU) No 10/2011 Annex I and FDA 21 CFR 177.1520(c)3.1a, with specific migration of the polyolefin comonomer species checked under EN 1186-1:2002 migration protocols. Terminal product types include vertical form-fill-seal pouches for sauces, 1–5 L liquid liner bags in corrugated boxes, and stand-up spouted pouches for dairy and fruit beverages. The seal layer formulation must avoid amine-based slip masterbatches because secondary amine migration into the heat-seal interface causes erratic hot-tack strength loss above 115°C; instead, erucamide slip is added at 500–1,000 ppm and the coefficient of friction is verified under ASTM D1894-14 to remain below 0.35.

    Heavy-Duty Sack Film with Post-Industrial Recyclate and Gauge Reduction

    Monolayer heavy-duty sack film produced on large-scale blown film lines uses ELITE 5500G at 15–25 wt% in a matrix of low-density polyethylene and post-industrial recyclate, enabling gauge reduction from 150 µm to 125 µm while maintaining tear resistance above the minimum accepted under ASTM D1922-15 Elmendorf tear testing. The production process is a 90 mm single-screw extruder with L/D 30:1, 400 mm die, die gap 1.8 mm, output 280–320 kg/h, and external bubble cooling with a dual-lip air ring at air temperature 10–18°C; blow-up ratio is kept near 2.0:1 to preserve machine-direction tear orientation. Recyclate addition above 30 wt% introduces gels and volatile residues that raise melt pressure at the screen changer, requiring a continuous screen changer with 100–150 mesh screens and vacuum venting. Compliance is governed by ASTM D4976-12a for polyethylene specification, REACH Regulation (EC) No 1907/2006 for post-industrial recyclate content, and EU Packaging and Packaging Waste Directive 94/62/EC for heavy metal concentration below 100 ppm total for lead, cadmium, mercury, and hexavalent chromium. Terminal products include fertilizer sacks up to 50 kg, resin shipping bags, polymer granule FIBC liners, and bulk mailing envelopes. The primary processing defect is bubble snapping at the frost line when the melt temperature falls below 190°C; therefore, head temperature is held at 205–210°C.

    Compliance matrix for standard designations cited in first three application zones
    Application zoneStandard/regulationProperty measuredTest condition or limit
    Frozen food blown filmFDA 21 CFR 177.1520(c)3.1aFood-contact olefin polymerClearance for frozen food contact
    Frozen food blown filmEU Regulation (EU) No 10/2011 Annex IOverall migration10 mg/dm²
    Liquid pouch sealantASTM F1921-18Hot tack seal force0.5 N/mm² seal pressure
    Liquid pouch sealantEN 1186-1:2002Migration of plasticsFood simulant protocol
    Heavy-duty sack filmASTM D1922-15Elmendorf tearGauge-dependent minimum
    Heavy-duty sack film94/62/ECHeavy metal concentration100 ppm total

    Downstream extrusion lamination lines running solvent-free polyurethane adhesives onto white-machine-glazed kraft or aluminium foil use ELITE 5500G as the extrudate at 12–18 µm coating weight, with melt temperature at the die of 305–320°C to promote adhesion to the substrate without ozone pretreatment; adhesion is tested under ASTM F904-16 with a required cohesive failure mode. The resin is processed neat or with 1–3 wt% adhesion-promoting masterbatch containing low-acid-value polyolefin copolymers; addition above 3 wt% increases melt fracture and reduces draw-down stability at line speeds above 300 m/min. Compliance for food board lamination includes FDA 21 CFR 177.1520(c)3.1a and EU Regulation (EU) No 10/2011, with migration testing under EN 1186-1:2002 for aqueous and fatty food simulants. The process line is a tandem extrusion lamination coater with a 105 mm extruder, L/D 30:1, 1,650 mm slot die, and a chill roll at 15–20°C; the air gap is limited to 90–120 mm to control neck-in and maintain edge bead uniformity. Terminal products include aseptic liquid cartons, paper-based dry food pouches, and cup stock lamination for hot-fill closures.

    When ELITE 5500G Replaces Conventional Butene LLDPE in Collation Shrink Film

    When ELITE 5500G replaces conventional butene LLDPE in collation shrink film at 20–30 wt% of the total PE blend, the increased short-chain branching from the comonomer distribution produces a more gradual crystal size distribution that lowers shrink initiation stress while maintaining free-shrink values of 40–50% in both machine and transverse directions under ASTM D2732-14. The downstream process is double-bubble blown film extrusion; the primary bubble is produced at 190–205°C and the secondary orientation bubble is reheated to 105–115°C with bubble expansion ratio 2.5:1 in the transverse direction and 2.0:1 in the machine direction. A processing conflict occurs at orientation temperatures below 100°C: the film fails at the second-bubble air ring due to insufficient mobility in the crystalline domains, causing bubble oscillation and gauge bands. Compliance for distribution packaging is limited to ASTM D4976-12a and RoHS Directive 2011/65/EU for electrical and electronic equipment packaging; if food is present, FDA 21 CFR 177.1520(c)3.1a applies. Terminal products include supermarket multi-pack shrink canopies, bottled water collation wraps, and carton overwrap film. The formulation typically includes 0.5–1.0 wt% of an antiblock masterbatch with synthetic silica to prevent blocking under storage temperatures above 30°C.

    Surface Protection Film for Sheet Metal and Flat Glass: Peel Initiating Force and Residue Control

    Surface protection film produced by cast coextrusion uses ELITE 5500G as the core and outer skin at 70–85 wt%, with a peelable adhesive skin based on an ethylene-vinyl acetate copolymer at 15–30 wt%; the addition ratio of ELITE 5500G is reduced to 50–65 wt% when a separate adhesive layer is coextruded, because the adhesive layer itself contributes to total film tensile strength. The production line is a 3-layer cast film line with 90 mm extruders, L/D 30:1, a 1,500 mm slot die, and corona treatment of the adhesive skin at 38–42 mN/m surface energy under ASTM D2578-17. Compliance includes REACH Regulation (EC) No 1907/2006 for substances of very high concern, RoHS Directive 2011/65/EU for electrical equipment applications, and ASTM D4976-12a for polyethylene resin specification. Peel initiation is verified under ASTM D3330/D3330M-04 Method A at 0.5–2.5 N/25 mm; inadequate corona dose or die-lip contamination causes low peel force and adhesive transfer. Terminal products include stainless steel sheet masking, flat glass transit protection, polished aluminium panel protection, and protective film for polycarbonate glazing during laser cutting. Published data for this specific configuration is limited; processor validation by differential scanning calorimetry and peel aging at 40°C for 7 days is required before setting specification limits.

    Free Quote

    Competitive Dow ELITE™ 5500G Enhanced Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5500G Enhanced Polyethylene Resin is an ethylene/alpha-olefin copolymer supplied as a pelletized resin for blown film, cast film, and coextruded packaging structures. The manufacturer classifies the grade within the enhanced polyethylene portfolio, which designates polymer architectures produced with a single-site catalyst platform rather than a conventional Ziegler-Natta system. The nominal melt flow rate is 1.0 g/10 min when determined at 190°C under 2.16 kg load according to ISO 1133-1, and the nominal density is 0.917 g/cm³ determined according to ISO 1183-1. These two values establish the resin as a low-melt-index linear-low-density polyethylene with a density below the 0.920 g/cm³ threshold often used in medium-duty packaging. The grade is positioned for applications requiring a balance of low-temperature toughness, optical clarity, and seal consistency rather than maximum stiffness or maximum melt strength.

    At the molecular level, the single-site catalyst produces a more uniform distribution of short-chain branches across the molar mass distribution than a Ziegler-Natta LLDPE of comparable density. In a Ziegler-Natta resin, the low-molar-mass fraction is typically more highly branched and the high-molar-mass fraction is more linear. This compositional heterogeneity creates a broader melting range and a greater population of low-melting material. The enhanced polyethylene architecture reduces the low-melting fraction, which alters the crystallization behaviour during blown film cooling. The practical consequences include lower haze at equivalent film thickness, a narrower seal initiation window relative to the melting peak, and a different response to orientation during bubble stretching. Film processors should not treat the material as a simple one-for-one replacement for a conventional LLDPE; rheology, melt strength, and extrusion back-pressures must be evaluated on the target line.

    What separates the 5500G grade from a conventional Ziegler-Natta LLDPE of identical density?

    The difference is not the density or the melt flow rate; those values can be matched to a conventional grade. The difference is the composition distribution and the resulting solid-state behaviour. A Ziegler-Natta LLDPE at 0.917 g/cm³ and 1.0 g/10 min typically contains a broad distribution of comonomer content. The Dow ELITE™ 5500G grade has a narrower distribution, which reduces the fraction of very low-melting material and improves the film's resistance to blocking at typical warehouse temperatures. When a film is produced at the same gauge, blow-up ratio, and die gap, the 5500G film will generally show lower haze as measured by ASTM D1003 and higher dart impact as measured by ASTM D1709/A, but the absolute values depend on processing conditions. The single-site architecture also lowers the concentration of high-molar-mass, low-comonomer chains that can contribute to high melt viscosity and gel-like defects. The resin may exhibit less shear thinning than a high-pressure LDPE, so die pressure on a given blown-film die is not the same as an LDPE of identical MFR.

    Melt strength is especially important in high-stalk bubble configurations. A high-pressure LDPE provides strain hardening in the melt that stabilises the bubble; an enhanced polyethylene such as 5500G generally has lower extensional viscosity. In processes that rely on melt strength, such as high-stalk blown film or extrusion coating, blending with 10–20 wt% of a high-pressure LDPE is a common technical remedy. The blend will reduce dart impact and increase haze relative to the neat 5500G film, but it may restore acceptable bubble stability and neck-in behaviour. The trade-off should be quantified on the production line.

    Physical property envelope under ISO 1183 and ISO 1133-1

    The following table consolidates typical physical properties reported for the neat resin in manufacturer technical literature. The values are not specification limits; they are single-point typical values from a production campaign and are not to be used for lot acceptance without a defined specification.

    PropertyTest methodTypical value
    Melt flow rate at 190°C/2.16 kgISO 1133-11.0 g/10 min
    DensityISO 1183-10.917 g/cm³
    Melting temperature, DSC peakISO 11357-3124 °C
    Vicat softening temperatureISO 306/A50103 °C

    The density of 0.917 g/cm³ corresponds to a crystalline fraction lower than a 0.926 g/cm³ medium-density polyethylene, which contributes to higher dart impact and lower secant modulus. The melting temperature of 124°C is the differential scanning calorimetry peak, not the processing setpoint. Film extrusion is conducted above the melting point, typically between 190°C and 220°C, to lower viscosity and to ensure that all high-melting species are molten. The Vicat softening temperature of 103°C is a measure of the temperature at which a flat-ended needle penetrates the sample under load; it is not a continuous-use temperature. These thermal values are useful for comparing grades but do not determine the maximum service temperature of a fabricated bag or pouch.

    For film properties, no universal value can be stated because dart impact, Elmendorf tear, tensile strength, haze, and gloss depend on film thickness, die gap, blow-up ratio, melt temperature, frost-line height, and post-extrusion handling. A typical 25 μm monolayer blown film produced at a 2.5:1 blow-up ratio is often used as a reference point in technical data sheets. Processors comparing 5500G with a conventional LLDPE should prepare both films on the same line at the same gauge and measure dart impact according to ASTM D1709/A, Elmendorf tear according to ASTM D1922, tensile properties according to ASTM D882, haze according to ASTM D1003, and gloss according to ASTM D2457. The resin's comparative advantage is largest when the comparison is made at equivalent density and MFR; comparing a higher density or lower MFR grade will confound the effect of the catalyst architecture.

    On a three-layer blown-film line with a 400 mm annular die and a 1.2 mm die gap, the 5500G resin is typically run as a skin layer or core layer in a coextrusion structure. The melt temperature at the die is set between 190°C and 220°C; the extruder barrel profile is often set from 170°C in the feed zone to 210°C at the metering zone. A grooved-feed extruder with an 30:1 L/D ratio and a barrier screw with a compression ratio of 3.0:1 is typical for high-output operation. The resin's shear-thinning behaviour is less pronounced than that of high-pressure LDPE; therefore, the pressure drop across a die at a given output may be higher than a converter expects from an LDPE of the same melt index. The die pressure should be recorded during the first production campaign and compared against the baseline resin. If melt-temperature override is observed at high screw speeds, the screw speed should be reduced or the barrel temperature profile adjusted before reaching the maximum allowable melt temperature.

    In cast film, the resin is processed at slightly higher melt temperatures, typically 220°C to 240°C, with an air gap of 100 mm to 150 mm and a chill roll temperature of 15°C to 25°C. Draw resonance and neck-in are greater when 5500G replaces a high-pressure LDPE because the melt strength is lower. A blend of 80 wt% 5500G with 20 wt% LDPE is a practical starting point to restore draw behaviour, but the blend ratio should be adjusted based on neck-in measurements at the die and film width control. Film property testing after extrusion should follow ISO 291 conditioning for at least 40 h at 23°C ± 2°C and 50% ± 5% relative humidity to stabilise crystal orientation and residual stresses.

    Processing parameterBlown film typical rangeCast film typical range
    Melt temperature at die190–220 °C220–240 °C
    Die gap / air gap0.8–1.6 mm100–150 mm
    Blow-up ratio / draw ratio2.0:1–3.0:1equipment-dependent, typically 20:1–40:1
    Chill roll temperaturenot applicable15–25 °C
    Typical film thickness for evaluation25–100 μm20–80 μm

    These processing ranges are starting points derived from general film-processing practice for a linear-low-density polyethylene with a melt flow rate of 1.0 g/10 min. The die gap and blow-up ratio interact: a narrow die gap increases shear and can improve optical properties but may raise die pressure, while a wider die gap reduces pressure but may require a higher blow-up ratio to achieve balanced film orientation. Published data for specific equipment configurations and exact draw limits is limited; the values must be verified on the production line.

    When 5500G is used as the sealant web in a coextruded barrier structure

    A common use of the resin is in a sealant layer of a laminate containing oriented PET, aluminium foil, or metallised film. The sealant web may be a neat 5500G layer or a blend with a lower-density PE to reduce seal initiation temperature. Seal strength is measured according to ASTM F88 on a 25 μm film after sealing at a defined pressure and dwell. The resin's narrow composition distribution produces a seal plateau that is reached at a lower temperature than a conventional Ziegler-Natta LLDPE of the same density; the difference is frequently in the range of 5°C to 10°C, but must be verified because sealing pressure, dwell time, and film thickness change the measured value. Hot-tack performance is evaluated according to ASTM F1921 or an internal packaging-line test because the seal must resist opening forces before full crystallization. In food-contact structures, the converter is responsible for verifying that the finished article complies with FDA 21 CFR 177.1520 and, where applicable, EU Regulation (EU) No 10/2011. The base resin may support such compliance, but the presence of adhesives, primers, and additives in the final laminate requires end-use migration testing according to EN 1186 and the relevant food simulant conditions.

    Hexane extractable content is a critical parameter for fatty-food packaging under 21 CFR 177.1520. The enhanced polyethylene architecture of 5500G typically reduces the low-molecular-weight, high-comonomer extractable fraction compared with some conventional LLDPE grades, but the converter must not rely on generic statements. A lot-specific extraction test should be performed on the final film or laminate because extrusion temperature and regrind use can shift the extractable level.

    In a heavy-duty shipping sack or industrial liner, the resin can be used as a core layer between HDPE skins. The gauge is typically 100 μm to 150 μm, and the mechanical targets include dart impact and Elmendorf tear resistance. The film is tested according to ASTM D1709/A for dart impact and ASTM D1922 for tear. The balance of machine-direction and transverse-direction tear can be changed by the blow-up ratio: a lower blow-up ratio, such as 2.0:1, increases MD orientation, while a higher blow-up ratio, such as 3.0:1, increases TD orientation. The narrower composition distribution improves low-temperature impact behaviour relative to conventional LLDPE at the same density; however, the actual product must be tested at the target cold condition because seal seams and notches may fail before the film body. The resin is also used in agricultural films where light transmission and mechanical durability are evaluated over extended exposure. For those applications, the effect of UV stabilizers on the base resin's viscosity and film properties should be evaluated with ASTM D792, ASTM D1238, and ASTM D882 after accelerated weathering or outdoor exposure.

    The grade imposes specific storage and handling boundaries before film conversion

    Polyethylene pellets are not hygroscopic to the extent of PET or polyamide, but surface condensation is a processing issue. If cold pellets are opened in a warm processing bay, moisture can condense on the pellet surface and cause bubble instability or lens-like defects in film. The resin should be kept in its sealed packaging until its temperature equilibrates with the processing area. Storage below 40°C is typical, and extended storage above that temperature can accelerate oxidative changes. The resin contains an antioxidant stabilizer package; if regrind is used, the stabilizer concentration is diluted proportionally. The processor should verify stabilizer concentration if regrind levels exceed 30 wt% of the feed. The pellets are not intended for direct food contact; compliance applies to the fabricated film article.

    The pellet shape and bulk density are controlled for reliable conveying. Bridging or pellet fracture in pneumatic conveying can occur if the conveying air temperature exceeds 60°C or if line velocities are too high. Material-handling audits on a production line should verify the transfer-line dew point and the pellet surface temperature before blending additives such as slip and antiblock masterbatches. The resin can be blended in-line with a gravimetric blender, but the additive masterbatch carrier resin should be compatible with the single-site polyethylene matrix to prevent premature loss of slip agent or uneven dispersion.

    In direct comparison with a high-pressure LDPE of the same melt index, the 5500G resin provides higher tensile elongation, higher Elmendorf tear resistance, and lower haze at the same film thickness, but it has lower melt strength and lower shear thinning. This makes it unsuitable as a direct replacement for LDPE in extrusion coating and high-stalk blown film unless an LDPE blend is used. Compared with a conventional Ziegler-Natta LLDPE, the 5500G resin typically yields lower haze, more uniform seal performance, and lower extractables, but the die pressure may be higher at the same output. Within the ELITE family, the 0.917 g/cm³ density of 5500G positions it between lower-density grades that offer greater impact and flexibility and higher-density grades that offer greater stiffness and thermal softening resistance. The selection between 5500G and another enhanced polyethylene should be based on the measured secant modulus, dart impact, tear balance, and seal initiation temperature of the target film structure. A converter should not infer product performance from density and melt flow rate alone; pilot-line verification remains the most reliable method for material substitution.

    In a direct substitution trial, the converter should collect die pressure, screw speed, melt temperature, film gauge, haze, dart impact, and seal strength data from both the incumbent resin and 5500G under the same line conditions. Without this matched trial, differences in processing aids, additive packages, and pellet conveying can mask the effect of the resin architecture.

    Top