    HS Code 710779
    Density 0.918 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melt Flow Ratio I10 I2 8.5
    Melting Point 121 °C
    Vicat Softening Point 102 °C
    Tensile Strength At Yield 9.7 MPa
    Tensile Strength At Break 31.0 MPa
    Elongation At Break 600%
    Flexural Modulus 207 MPa
    Dart Impact 200 g
    Elmendorf Tear Md 250 g
    Elmendorf Tear Td 450 g
    Haze 8%
    Gloss 60 90
    Coefficient Of Friction 0.2
    Comonomer Octene-1
    Material Type Enhanced Polyethylene Resin
    Catalyst Constrained Geometry

    As an accredited Dow ELITE™ 5401G Enhanced Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5401G Enhanced Polyethylene Resin comes in 25 kg (55 lb) polyethylene bags, palletized for industrial shipment.
    Container Loading (20′ FCL) 20′ FCL: 18 pallets, 25 kg bags, 1,375 kg/pallet, 24.75 MT; Dow ELITE™ 5401G resin, dry, secure, non-DG.
    Shipping Dow ELITE™ 5401G Enhanced Polyethylene Resin is typically shipped as pellets in moisture-barrier bags, boxes, octabins, or bulk trucks/railcars. Transport in clean, dedicated equipment under ambient conditions. Keep containers closed, dry, and away from heat, sunlight, and ignition sources. Follow local transport regulations and avoid spills or dust generation.
    Storage Store Dow ELITE™ 5401G Enhanced Polyethylene Resin in a cool, dry, well-ventilated area in tightly closed original containers. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, and odorous materials. Avoid excessive stacking, prolonged high temperatures, and physical damage. Reseal opened packages promptly. Follow local regulations and good housekeeping practices to preserve resin quality.
    Shelf Life Typically 24 months from date of manufacture when stored in original packaging, cool, dry, away from direct sunlight and contaminants.
    Application of Dow ELITE™ 5401G Enhanced Polyethylene Resin

    On three-layer high-stalk blown film lines configured with a 350 mm dual-spiral die and a 1.6 mm die gap, the abrasion-resistant inner ply of a heavy-duty shipping sack is extruded using a 100 wt% ELITE 5401G seal layer over a core containing recovered edge trim. The outer abuse layer is a blend of 70 wt% high-density polyethylene with 30 wt% low-density polyethylene; the core layer contains 60 wt% butene-LLDPE and 40 wt% in-house recycled film flake. The ELITE 5401G layer, with a nominal density of 0.916 g/cm³ per ASTM D1505 and a melt index of 1.0 g/10 min per ASTM D1238 at 190°C and 2.16 kg, permits the converter to operate at a melt temperature of 215°C without inducing shark-skin melt fracture in the nip-flattened bubble at haul-off speeds above 35 m/min. The total film thickness is maintained at 140 µm with a gauge spread of ±5% under capacitive scanning; blow-up ratio is held at 2.2:1 and frost line height at 1.2 m above the die. The finished sacks are converted on a hot-bar bottom-seal unit at 135°C, 0.8 s dwell, and 0.4 MPa jaw pressure, and the filled sack must survive drop tests according to ISO 21898 / UN 13M1 protocols without seal rupture. Dart impact is evaluated per ASTM D1709-16A, Elmendorf tear per ASTM D1922-15, and seal strength per ASTM F88. The practical limitation of the recycled-containing core is cumulative dust contamination at the screen changer; when screen-push frequency exceeds one push per 90 kg of extruded polymer, the core pellet blend requires filtration through a 250 µm mesh before entering the hopper. Pre-drying is unnecessary at pellet moisture below 0.1 wt%; however, when the silo relative humidity exceeds 60%, a 1 h purge with dried air at 30°C before the extruder throat prevents surface condensation that can cause melt film micro-voids at 215°C.

    When Does Frozen Food Seal Integrity Depend More on Hot Tack Plateau Than on Ultimate Seal Strength?

    Vertical form-fill-seal lines packaging IQF vegetables and seafood at 70 bags/min expose the seal layer to a transient load before the molten polymer has cooled below its crystallization onset. A three-layer coextruded frozen food film is produced with a 12 µm inner sealant layer of ELITE 5401G, a 35 µm low-density polyethylene skin, and an optional middle layer of barrier EVOH in five-layer structures where oxygen exclusion is required. The enhanced polyethylene layer is processed at a die gap of 1.2 mm, blow-up ratio 2.0:1, melt temperature 205°C, and a total film thickness of 55 µm. Because the resin has a low sealing initiation temperature relative to conventional Ziegler-Natta C4-LLDPE, the VFFS jaw set point can be reduced by 10 K to 15 K without sacrificing seal continuity at 0.5 s dwell; this temperature depression minimizes flavor scalping and prevents an excessive oriented morphology in the seal area after cooling. Hot tack is measured per ASTM F1921, seal strength per ASTM F88, and seal-through contamination is evaluated with a standard cocoa-powder wedge test at 1.0 g/m² contamination density. For food contact status, the sealant layer complies with 21 CFR 177.1520(c) as an olefin polymer and with EU 10/2011 overall migration limits of 10 mg/dm² under simulant A and D2 at 40°C for 10 days. The primary conversion-side failure mode on long runs is seal jaw polymer stringing when the jaw release temperature exceeds 70°C; chilled air at 15°C directed across the jaw faces is required to maintain continuous operation.

    Food-contact compliance checklist for the frozen food sealant layer
    RegulationDesignationApplicable condition
    United States olefin polymers21 CFR 177.1520(c)Food-contact articles under Conditions of Use A through H
    European Union plasticsEU 10/2011 Annex I, Article 12Overall migration ≤10 mg/dm²
    Good manufacturing practiceEC 2023/2006Traceability and hygiene of film production
    REACHEC 1907/2006 Annex XVIIRestricted substances not intentionally added above 0.1 wt%

    If Silage Film Must Survive 12 Months of Outdoor UV Exposure Without Pinholing

    Agricultural silage wrap produced in a five-layer configuration on an 1800 mm die with a 2.2 mm gap uses ELITE 5401G in the inner and middle layers to provide puncture resistance after surface abrasion from baler rollers. The layer distribution is approximately 15%/20%/30%/20%/15%; the outer layer contains a UV-stabilizer masterbatch with hindered amine light stabilizers at 3 wt% and carbon black at 2 wt%, while the core layers are a blend of 85 wt% ELITE 5401G and 15 wt% low-density polyethylene. The film is manufactured at a thickness of 150 µm, melt temperature 210°C, blow-up ratio 1.8:1, frost line height 1.4 m, and output 250 kg/h. The low melt index of the resin supports a stable high-stalk bubble at this throughput without helical instability, provided that the ambient temperature around the bubble does not vary by more than ±3 K. Puncture propagation resistance is evaluated according to ASTM D5748-95, Elmendorf tear to ASTM D1922, and tensile modulus to ISO 527-3. After 2000 h QUV aging per ISO 4892-3, the retained elongation at break of the outer layer must remain above 50% of the unaged value; published data for this specific multilayer configuration is limited, and oven-laboratory acceleration cannot reproduce baler knifing damage observed in field trials. The terminal product is a 750 mm × 1500 m bale wrap with a black/white coextruded structure, and the production limitation is the accumulation of low-molecular-weight oxidation products on the collapsing frame during extended runs; this requires cleaning of the collapsing shields every 48 h to prevent surface haze transfer.

    Stand-Up Pouch Sealant Web Lamination and Solvent-Free Adhesive Interlock

    The sealant web of a three-side-seal stand-up pouch for dry granular food and pet treats is produced from a 60 µm blown film consisting of 80 wt% ELITE 5401G and 20 wt% low-density polyethylene. The film is made on a 450 mm die with 1.0 mm die gap, blow-up ratio 2.5:1, melt temperature 195°C, and a chilled air ring temperature of 12°C to maintain low haze and high gloss for reverse-printed lamination. The blown sealant web is laminated to a printed 12 µm polyester film and a 7 µm aluminum foil with a two-component solvent-free adhesive at 2.0 g/m² coat weight; the laminate is cured at 40°C for 24 h. The final pouch sealing conditions on a rotary premade pouch line are 130°C jaw temperature, 0.6 s dwell, and 0.35 MPa pressure. Seal strength is measured per ASTM F88, hot tack per ASTM F1921, coefficient of friction per ISO 8295, and film haze per ASTM D1003. The low seal initiation of ELITE 5401G reduces the incidence of jaw sticking on high-speed rotary sealers compared to LDPE-rich sealant webs, but it also lowers the upper continuous service temperature of the pouch to 60°C, above which seal creep may occur under top load. Compliance for food contact follows 21 CFR 177.1520(c), EU 10/2011, and the printing ink/adhesive system must meet end-user packaging specifications for primary aromatic amine migration below detectable limits per EN 13130-1.

    Flexible intermediate bulk container liners extruded for chemical powders and resins are produced as a 100 µm three-layer blown film with an outer ELITE 5401G skin on both faces and a core containing 50 wt% in-plant edge trim. The die is 350 mm diameter with a 2.0 mm gap, the blow-up ratio is 1.7:1, and the melt temperature is 218°C. The draw-down distance is kept short at 900 mm, because a high-stalk configuration with this resin can develop a periodic sag in the bubble at 1.7:1 BUR when the cooling air temperature drops below 10°C. The film is tested for tear propagation in both directions according to ASTM D1922, puncture resistance according to ASTM D5748, and seal strength after impulse welding according to ASTM F88. For liners intended to contact dry food ingredients, the film supplier references FDA 21 CFR 177.1520 and EU 10/2011 for olefin polymers under the specified conditions of use. The main operational boundary is static charge accumulation on the inner surface when handling fine-particle mineral fillers; antistatic masterbatch must be incorporated at 2 wt% only after verification of seal strength retention, because excessive internal migration of a glycerol ester antistatic agent can reduce the coefficient of friction and impair bag stack stability.

    Liquid Carton Inner Liner Sealant Webs Are Constrained by MD Elongation During High-Speed Adhesive Lamination

    Paperboard carton structures for non-aseptic liquid products use a polyolefin inner liner that is laminated from a blown film web. In this application, ELITE 5401G is used as the sealant layer in a pre-extruded 50 µm blown film that is subsequently laminated to the paperboard with a water-based adhesive. The blown film is produced on a 600 mm die at 220°C melt temperature, 2.0:1 BUR, and 120 kg/h output, with a 1.2 mm die gap. During lamination, the paperboard line speed is 180 m/min, and the adhesive is applied at 3.5 g/m² dry coat weight. The carton side-seam sealing operation runs at 140°C on hot-air side-seam activation with 0.4 s dwell, and the resulting carton is tested for side-seam seal continuity by dye penetration per ASTM F1929 and for internal pressurization resistance at 0.2 bar per ASTM F2096. The critical production boundary is the dimensional stability of the blown film during lamination: a high line tension above 12 N/cm induces machine-direction elongation of the PE sealant web, which later manifests as gusset fold cracking in cold climates. The final carton complies with 21 CFR 177.1520 for direct contact with aqueous and low-alcohol beverages under Conditions of Use A through H, and with EU 10/2011 overall migration when tested in 3% acetic acid and 10% ethanol for 10 days at 40°C.

    Free Quote

    Competitive Dow ELITE™ 5401G Enhanced Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5401G Enhanced Polyethylene Resin is a single-site-catalyzed ethylene-1-octene copolymer supplied in pellet form for blown film extrusion and coextrusion. It is designated for flexible packaging films requiring high dart impact, improved tear balance, seal integrity, and the ability to downgauge without sacrificing end-use abuse performance. The resin is typically characterized by a density of 0.916 g/cm³ according to ASTM D792 and a melt mass-flow rate of 1.0 g/10 min under ASTM D1238 at 190 °C/2.16 kg. Corresponding ISO designations are ISO 1183-1:2019 and ISO 1133-1:2022. Because blown film properties depend on extrusion conditions, the values presented in this document are baseline characterizations; lot-specific values should be obtained from the supplier certificate of analysis.

    What Normative Methods Govern Density, Melt Flow, and Thermal Characterization?

    Density is measured on compression-molded plaques after conditioning at 23 °C. The procedure follows ASTM D792 or ISO 1183-1:2019, with reported values rounded to three decimal places. Melt flow characterization uses a dead-weight melt indexer with a 2.16 kg piston load at 190 °C, in accordance with ASTM D1238 Procedure A or ISO 1133-1:2022. Thermal analysis by differential scanning calorimetry at 10 °C/min under nitrogen typically places the peak melting endotherm between 121 °C and 124 °C for this resin family. Vicat softening temperature, measured under ASTM D1525 with 10 N loading, is not a primary packaging specification but may be monitored when evaluating heat-set resistance in laminated pouches. Because crystallinity and mechanical response are cooling-rate-dependent, values obtained from molded plaques do not directly describe the performance of films produced with air-ring or internal bubble cooling; separate film-based testing is required.

    Molecular architecture differentiates ELITE™ 5401G from conventional linear-low-density polyethylene generated with heterogeneous Ziegler-Natta catalysts. The narrow short-chain branching distribution reduces the high-crystallinity fractions that typically introduce tear anisotropy and optical haze in conventional grades. At equivalent melt index and density, the resin typically provides a more isotropic Elmendorf tear response and lower film haze when tested under ASTM D1922 and ASTM D1003, respectively. The specific magnitude of improvement depends on gauge, blow-up ratio, frost line height, and carrier resin in coextruded structures. Published data for this specific configuration is limited for certain niche structures, particularly oriented machine-direction films where post-orientation crystallinity is substantially altered.

    Extrusion Equipment Settings and Pressurized Air-Ring Stability Limits

    Monolayer blown film lines running ELITE™ 5401G generally use barrel temperature profiles between 180 °C and 215 °C, with adapter and die zones set from 215 °C to 230 °C. A die gap of 1.8–2.4 mm is common for film gauges from 25 µm to 120 µm. Blow-up ratios of 2.2:1 to 3.0:1 are typical, and the frost line height should be controlled so that the film surface temperature entering the nip remains below the crystalline solidification point. On a 120 mm annular die with 2.5:1 blow-up ratio, output rates above 1.2 kg/(h·cm circumference) usually require internal bubble cooling airflow optimization; published data for this specific configuration is limited. Single-screw extruders with 24:1 or 30:1 L/D and a mixing section are adequate for homogeneous melt delivery. Twin-screw compounding is not required for film converting.

    Process temperature control is a critical operational boundary. Prolonged residence at melt temperatures above 240 °C increases gel formation and destabilizes the bubble; melt temperature should be maintained within ±5 °C of the target setting. Pellet surface moisture from outdoor storage should be removed before extrusion when storage or handling relative humidity exceeds 60 %; preconditioning at 65–80 °C for 2 h in a dehumidified-air hopper is usually sufficient. The resin is not hygroscopic in the manner of polyamides or thermoplastic polyesters, but surface condensation is an operational risk in open plants.

    Production-scale observations on barrier-screw lines indicate that ELITE™ 5401G produces lower torque at comparable screw speed than many broad-composition LLDPE grades of equal nominal melt index. This behavior supports higher throughput without automatic screen changer pressure excursions when the screw is properly designed for moderate-shear film resins. However, substituting a deep-cut high-shear conditioner screw can produce local melt temperature spikes exceeding the 240 °C boundary. In one trial on a 75 mm grooved-feed extruder running 90 kg/h, barrel pressure fluctuation decreased when the feed section temperature was reduced by 8 °C; the result is line-specific and not a universal processing rule.

    When Seal Integrity and Hot-Tack Strength Limit Vertical Form-Fill-Seal Throughput

    Seal initiation temperature and hot-tack force are evaluated under ASTM F88 and ASTM F1921, respectively. The narrow branching distribution of ELITE™ 5401G typically shifts seal initiation lower by 5–10 °C relative to conventional Ziegler-Natta LLDPE at equivalent density and melt index; the practical effect is a wider hot-tack operating window on vertical form-fill-seal equipment. On packaging lines running 75–100 packages/min, this shift can reduce leaker defects caused by incomplete jaw sealing when dwell time is shorter than 0.3 s. The actual seal temperature reduction must be determined on the target machine because seal bar geometry, film substrate stiffness, and contamination at the seal surface influence heat transfer. Slip-agent concentration should be fixed before optimizing the seal temperature profile because migration of additive packages can alter heat-seal response over shelf life.

    Downgauging comparisons on heavy-duty sack films have been performed using 50 µm monolayer structures tested for dart impact under ASTM D1709A and for slow puncture under ASTM D5748. In internal production-scale trials, ELITE™ 5401G allowed a reduction in film gauge of 10–15 % while maintaining the same dart impact value as a conventional LLDPE control at the thicker gauge. This result is specific to the control grade, extrusion line, and gussetted sack construction; field performance on other lines will vary. The resin is also used as a sealant web in barrier laminates containing polyamide or ethylene vinyl alcohol; the sealant layer contributes abuse resistance while the barrier core governs oxygen transmission rate.

    Table 1 summarizes comparative performance trends observed when ELITE™ 5401G replaces a conventional Ziegler-Natta LLDPE of similar nominal melt index and density in monolayer blown film.

    Performance attributeTest methodELITE™ 5401G typical trendConventional Ziegler-Natta LLDPE trend
    Comonomer distribution widthASTM D3900 / ISO 15672NarrowBroad
    Seal initiation temperatureASTM F88Lower by 5–10 °CBaseline
    Dart impact at equivalent gaugeASTM D1709AHigherBaseline
    Elmendorf tear MD/TD balanceASTM D1922More isotropicMore anisotropic
    Film haze at equivalent gaugeASTM D1003LowerHigher

    Compliance must be verified on the final film or package structure, including additives and printing inks. The base resin is designed for food-contact applications when used under conditions described by regional food-contact legislation. In the United States, the polymer may be covered under 21 CFR 177.1520 for olefin polymers, provided the final article meets extraction specifications. In the European Union, overall migration must be determined under Regulation (EU) No 10/2011 and its amendments using simulants appropriate for the intended food type and temperature. REACH registration under Regulation (EC) No 1907/2006 is maintained for the monomer and polymer articles supplied in the European Economic Area. RoHS 2011/65/EU compliance is not directly applicable to packaging resins but may be required for electronic product packaging films; the final article assembler must verify absence of restricted substances.

    Regulatory referenceScopeVerification basis
    21 CFR 177.1520(c)Olefin polymers for food contactFinal article extraction testing
    Regulation (EU) No 10/2011Plastic materials in contact with foodOverall and specific migration limits
    REACH 1907/2006Chemical registration and SVHC screeningSupplier safety data sheet and registration record
    RoHS 2011/65/EURestricted substances in electrical and electronic equipmentFinal article analytical screening

    The resin is not intended for implantable medical device applications, and no USP Class VI certification should be assumed. For medical packaging requiring terminal sterilization, validation must be completed on the final sterile barrier system, and material compatibility with ethylene oxide, gamma irradiation, or electron beam must be evaluated separately. Published data for this specific configuration is limited for gamma doses above 40 kGy; irradiation-induced chain scission can alter seal strength and mechanical toughness.

    In cast film and extrusion coating, process experience is less established than in blown film; converters evaluating ELITE™ 5401G for cast applications should begin with lower line speeds and optimize the die-to-roll air gap. The resin’s low density and single-site architecture produce different neck-in behavior compared with conventional LDPE coating grades; no direct substitution should be made without adhesion testing under ASTM F88 and ASTM D1876 where applicable. In three-layer coextruded heavy-duty sack films with a blown film die gap of 2.2 mm and blow-up ratio of 2.5:1, ELITE™ 5401G has been placed in the seal skin layers to improve hot-tack after dust contamination on the seal surface; the core layer may use recycled in-house LLDPE up to 20 % without loss of interfacial adhesion when the recycled stream is screened through a 100 µm mesh and dried to less than 0.05 % moisture content. This configuration is a production field observation, not a universal recommendation; each line must verify the recycled-content limit by ASTM D1709A dart impact and ASTM F1921 hot-tack testing.