Dow Elite 5400g Enhanced Polyethylene Resin

Dow ELITE™ 5400G Enhanced Polyethylene Resin

    • Product Name: Dow ELITE™ 5400G Enhanced Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 858979
    Density 0.917 g/cm³
    Melt Index 190 C 2 16 Kg 0.75 g/10 min
    Melt Flow Ratio I10 I2 8.0
    Melting Point 123 °C
    Vicat Softening Point 101 °C
    Tensile Strength At Yield 10.0 MPa
    Tensile Strength At Break 29.0 MPa
    Elongation At Break 600%
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 10%
    Gloss 45 70
    Coefficient Of Friction 0.2

    As an accredited Dow ELITE™ 5400G Enhanced Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE 5400G Enhanced Polyethylene Resin is supplied in 25 kg polyethylene bags, 40 bags per pallet (1,000 kg).
    Container Loading (20′ FCL) 20′ FCL container loaded with Dow ELITE™ 5400G Enhanced Polyethylene Resin in 25 kg bags, palletized, shrink-wrapped, and secured.
    Shipping Dow ELITE™ 5400G Enhanced Polyethylene Resin is shipped as free-flowing pellets in moisture-barrier bags, bulk bags, octabins, or bulk trucks and railcars. It is not classified as dangerous goods. Keep containers closed, dry, and away from direct sunlight, heat, and ignition sources during transport. Store in a cool, ventilated area.
    Storage Store Dow ELITE™ 5400G in a cool, dry, well-ventilated indoor area, away from direct sunlight, heat, moisture, and strong odors. Keep original bags sealed on pallets, preventing punctures, dust, and contamination. Avoid excessive stacking. Protect from weather and UV exposure. Use first-in, first-out rotation. Keep away from ignition sources and incompatible materials. Maintain good housekeeping and follow the supplier’s safety data sheet.
    Shelf Life Typically 24 months from manufacture when stored unopened in a cool, dry, well-ventilated area, away from direct sunlight and moisture.
    Application of Dow ELITE™ 5400G Enhanced Polyethylene Resin

    In dry bulk handling plants, heavy-duty sacks for polymer granules, cementitious materials, and bulk food ingredients are converted from blown film where puncture and tear resistance at the seal area determine filled-bag survival on concrete loading docks. Dow ELITE™ 5400G Enhanced Polyethylene Resin is qualified by melt flow rate 1.0 g/10 min per ISO 1133-1:2022 and density 0.916 g/cm³ per ASTM D792 before blending. A 150 µm monolayer or two-layer A/B structure containing 70 wt% ELITE 5400G, 20 wt% autoclave LDPE with MFI 0.3–0.5 g/10 min, and 10 wt% TiO₂ masterbatch is run on a 75 mm barrier screw extruder with 24:1 L/D and a 250 mm spiral mandrel die. Barrel profile is 180°C, 200°C, 210°C, 215°C, 215°C; die temperature is 220°C; BUR is 2.0:1; die gap is 2.0 mm; screw speed is 45 rpm. Melt pressure upstream of a 120 µm screen pack typically remains between 28 MPa and 35 MPa; excursions above 38 MPa indicate gel accumulation on the screen pack. Film qualification includes dart impact per ISO 7765-1, Elmendorf tear per ISO 6383-2, and tensile properties per ISO 527-3. The bottom impulse seal is formed at 180–200°C with jaw pressure ≤0.3 MPa and evaluated by ASTM F88 after a 1.0 s dwell. At BUR above 2.8:1, bubble instability increases; frost line height is maintained between 5 and 8 die diameters to avoid MD/TD tear anisotropy. For food ingredient sacks, resin compliance is governed by FDA 21 CFR 177.1520(c). Terminal products are 50 kg capacity heavy-duty sacks sealed by bottom impulse welding.

    What Controls Pinhole Resistance in Three-Layer Chemical Bulk Liners?

    Flexible liners for liquid agrochemicals, fatty acids, and petroleum-based lubricants in corrugated boxes or steel drums require a balance of flex-crack resistance and seal integrity at creases. A 200 µm three-layer A/B/A film with skins of 30 wt% ELITE 5400G and 70 wt% autoclave LDPE, and a core of bimodal HDPE, is produced with a 2.5 mm die gap, BUR 2.5:1, and die temperature 215–225°C. The core extruder is 90 mm with 30:1 L/D; the skin extruders are 60 mm with 24:1 L/D. Flex-crack resistance is screened per ASTM F392 Gelbo flex test at 24°C and −20°C, with pinhole count after 100 cycles specified by the converter's drum-liner specification. Seal strength at side creases is tested by ASTM F88 after a 1.0 s dwell at 180°C and 0.3 MPa jaw pressure; the target is peel mode rather than film elongation mode at the seal edge. Chemical compatibility is screened by immersion in the specific fill fluid at 40°C for 30 days with mass change below the customer's threshold. The terminal products are pressure-sensitive valve liners for 200 L steel drums and 1000 L intermediate bulk container liners in corrugated outer boxes.

    On vertical form-fill-seal (VFFS) lines for frozen vegetables, par-fried potato products, and individually quick-frozen seafood, film temperatures reach −20°C during filling, which shifts failure to jaw seal corners. A 70 µm two-layer blown film containing 80 wt% ELITE 5400G, 20 wt% LDPE, 2 wt% silica antiblock masterbatch, and 1 wt% slip masterbatch is used where seal initiation in the 95–105°C range is required; the actual window is established by ASTM F88 over dwell times of 300–800 ms at 0.3 MPa jaw pressure. Hot tack is measured by ASTM F1921 at 0.2 s dwell to verify seal integrity before the product load stresses the closing jaw. Coefficient of friction is measured per ASTM D1894 after 7 days at 40°C to avoid tracking drift on formers. Haze is determined by ASTM D1003 on 70 µm film conditioned per ASTM D618. Direct food contact compliance is governed by FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 with overall migration ≤10 mg/dm² per EN 1186-1. Terminal packages include 1 kg frozen vegetable pouches and 2.5 kg IQF seafood bags.

    Greenhouse Cover Film Weathering and the Role of 5400G in Three-Layer Structures

    Three-layer greenhouse cover film for 12–18 month service in Mediterranean and subtropical climates is coextruded with a UV-absorber/HALS skin at 30 wt%, a core layer at 40 wt% ELITE 5400G, and an antifog/dust-suppressing skin at 30 wt%. Total thickness is 180 µm; die gap is 2.5 mm; BUR is 2.1:1; output on a 300 mm die is limited to 75 m/min because UV-stabilized melt increases die-lip buildup. Puncture resistance at installation is screened by ASTM D5748, and tensile elongation at break by ISO 527-3. After 2500 h of accelerated weathering per ASTM G155 Cycle 1, elongation retention is specified by the agronomic service contract; published data for this specific formulation are limited, so converter validation is mandatory. In tropical high-humidity conditions above 80% RH, pellets stored in unheated silos must be brought above the dew point of the plant air before extrusion to prevent surface moisture from generating bubble defects. The terminal product is a 180 µm greenhouse cover film with service life governed by UV stabilizer consumption and not by polymer thermal stability.

    When Solventless Lamination Replaces Wax-Coated Sealant Webs

    For dry food pouches of nuts, powdered beverages, and dehydrated fruit, a sealant web is required that bonds through solventless polyurethane adhesives to metallized PET or BOPP barrier layers without curtaining. A cast film line with a 90 mm extruder running 100 wt% ELITE 5400G at 30–40 µm gauge uses a chilled roll temperature of 18–22°C and 42 dyn/cm corona treatment on the seal side prior to lamination. Adhesive coat weight is 1.2–1.8 g/m²; lamination bond strength after 24 h cure is evaluated by ASTM F904 at 23±2°C and 50% RH. Seal strength on the finished pouch after 0.4 s dwell at 130°C must be validated by ASTM F88 because the metallized PET layer changes heat transfer at the jaw. Direct food contact compliance is governed by FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 overall migration ≤10 mg/dm²; the solventless adhesive must comply with 21 CFR 175.105 and primary aromatic amines from the adhesive must be below 0.01 mg/kg in the finished laminate. Terminal products include stand-up pouches and three-side-seal flat pouches for 250 g to 1 kg dry food portions.

    ApplicationRegulation/standardTest methodRequirement
    Frozen VFFS webFDA 21 CFR 177.1520(c)Extractables per 21 CFR 177.1520Olefin polymer conforming
    Frozen VFFS webEU Regulation 10/2011EN 1186-1Overall migration ≤10 mg/dm²
    Dry food lamination sealant webFDA 21 CFR 177.1520(c)Extractables per 21 CFR 177.1520Olefin polymer conforming
    Solventless adhesive21 CFR 175.105FDA adhesive complianceConforming as adhesive
    Dry food laminationEU Regulation 10/2011LC-MS/MSPrimary aromatic amines below 0.01 mg/kg

    Pallet load containment films for glass containers and heavy construction products are converted on high-output blown film lines where MD tear resistance and puncture propagation determine load stability during transit. A three-layer structure containing 65 wt% ELITE 5400G in the core and 17.5 wt% softer butene LLDPE in each skin is run with a die gap of 2.0 mm, BUR 3.0:1, and frost line height 6 die diameters. The film is oriented in the machine direction by setting haul-off speed 15–20 m/min above winder speed to produce a stretch hood profile. Puncture propagation is measured by ASTM D5748; Elmendorf tear by ISO 6383-2; MD tensile elongation by ISO 527-3 after conditioning per ASTM D618. Because the films are non-food and used in industrial sites, only REACH EC 1907/2006 restrictions apply; no specific food contact migration testing is required. Terminal products are stretch hoods applied by automatic stretch hood machines on pallets of hollow glass weighing up to 1200 kg.

    Free Quote

    Competitive Dow ELITE™ 5400G Enhanced Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5400G Enhanced Polyethylene Resin is a solution-process ethylene–1-octene copolymer supplied as pellets for blown-film and cast-film conversion. The nominal density is 0.916 g/cm³ when measured in accordance with ASTM D1505 or ISO 1183-1, and the nominal melt flow index is 1.0 g/10 min at 190 °C under 2.16 kg load following ASTM D1238 and ISO 1133-1. These values place the material in the linear low-density polyethylene range but with a comonomer architecture distinct from traditional butene-based Ziegler–Natta LLDPE. Typical conversion uses include heavy-duty bulk shipping sacks, agricultural films requiring puncture resistance, and sealant layers in multilayer flexible packaging. Film thicknesses range from 15 µm sealant plies in coextruded structures to 200 µm monolithic heavy-duty sacks. Converters running monolayer and multilayer lines typically process the resin on single-screw extruders with 24:1 to 30:1 L/D ratios, spiral mandrel dies of 200 mm to 400 mm diameter, and dual-lip air rings; the material’s rheological response under shear requires a wider die gap than LDPE homopolymer to mitigate melt-fracture onset at commercial output rates.

    What Distinguishes a Solution-Process 1-Octene Copolymer from Butene-Based LLDPE

    At equivalent nominal density and melt index, the 1-octene comonomer in 5400G produces a more uniform short-chain branch distribution than 1-butene copolymers produced by conventional Ziegler–Natta catalysis. This uniformity has direct consequences for film failure. The onset of dart impact failure under ASTM D1709 shifts to higher values for film of 25 µm gauge when compared with butene-based LLDPE of similar density; published supplier data indicate the increase is large but strongly dependent on blow-up ratio, frost-line height, and die gap. The heat-seal initiation temperature measured by ASTM F88 is typically lower because the octene branches expand the amorphous phase without creating the low-molecular-weight extractable fractions to the same extent as heterogeneous butenes. The trade-off appears in flexural secant modulus and tensile yield stress: films from 5400G are less stiff than high-density polyethylene and slightly less stiff than some butene LLDPE grades of equivalent density, a result consistent with the disruptive effect of short-chain branches on crystalline lamellae thickness.

    The resin’s optical profile measured by ASTM D1003 haze and ASTM D2457 60° gloss is generally lower haze and higher gloss than butene-copolymer LLDPE, because the narrow composition distribution reduces large crystalline aggregates that scatter light. Direct comparison requires identical film processing; blow-up ratios outside 2.5:1 to 3.2:1 or frost-line heights below 3 die diameters can erase optical advantages. Gel permeation chromatography of similar solution-process octene copolymers shows a polydispersity index below 3.0, whereas conventional butene Ziegler–Natta LLDPE often has a polydispersity index above 4.0. The lower high-molecular-weight tail reduces visible gel counts but also reduces melt strength under elongational flow.

    Comparison axisTest methodObserved direction for 5400G relative to butene-based LLDPE of equivalent density and melt index
    Dart impact filmASTM D1709-16aHigher; magnitude depends on gauge, blow-up ratio, frost line
    Elmendorf tearASTM D1922-15Higher machine-direction and transverse-direction tear at similar thickness
    Heat-seal initiationASTM F88/F88M-15Lower seal initiation temperature
    HazeASTM D1003-13Lower haze due to narrower composition distribution
    1% secant modulusASTM D882-18Comparable to lower; not a stiffness replacement for HDPE

    On blown-film lines, the primary process limit is thermo-oxidative degradation. For Dow ELITE™ 5400G, barrel setpoints from 160 °C to 190 °C in the feed and compression zones and a die setpoint from 200 °C to 220 °C are common starting conditions on single-screw lines; melt temperature measured at the adapter should remain below 240 °C to avoid chain scission. Unlike LDPE, the resin does not exhibit high melt strength under elongational flow; bubble stability is therefore maintained by running the frost-line height at 3 to 6 die diameters and blending 10 wt% to 20 wt% LDPE when high stalk heights or low gauge below 30 µm are required. Extruder screw designs with a barrier section and a Maddock mixing element improve melt homogeneity and gel dispersion at screw speeds above 90 rpm, but excessive shear heating can raise melt temperature beyond the setpoint and reduce tear strength in the machine direction.

    The apparent viscosity at 190 °C and 100 s⁻¹ for a 1.0 g/10 min linear low-density polyethylene is typically in the range of 600 Pa·s to 900 Pa·s by capillary rheometry; direct measurement on the actual lot is required because catalyst residue and additive package affect the flow curve. The wall shear stress at which sharkskin melt fracture appears is commonly in the range of 0.14 MPa to 0.30 MPa for narrow molecular weight distribution LLDPE, which is why the die gap should be set at 1.0 mm to 2.0 mm rather than the 0.6 mm to 0.8 mm typical of LDPE. Output on a 90 mm extruder with a 300 mm spiral mandrel die can reach 150 kg/h to 220 kg/h, but the die pressure may exceed 35 MPa if melt temperature drops below 190 °C; this pressure limit is controlled by screen changer design and clamp rating. Melt flow ratio measured as I10/I2 under ASTM D1238 is commonly in the range of 7.5 to 8.0 for solution-process octene LLDPE. This parameter is a practical indicator of shear thinning; lower ratios relative to LDPE indicate less shear thinning, which increases die pressure but improves gauge uniformity in high-output cast film. In blown film, the higher viscosity at low shear supports bubble formation, but the limited elongational hardening means that a dual-lip air ring with lower air volume than LDPE is often required to prevent vibration.

    Converters using fluoropolymer-based processing aid masterbatches at 200 ppm to 500 ppm by weight can delay sharkskin onset and reduce die pressure. The processing aid should be added to the feed throat, not to the hot melt, to ensure dispersion. This resin generally accepts silica-based antiblock up to 5000 ppm, with haze increase governed by particle size under ASTM D1003. Lot-to-lot control for melt flow index is typically maintained within ±0.1 g/10 min and density within ±0.001 g/cm³; these limits are relevant for converters running automatic gauge control because density variation shifts the frost-line height and roll diameter at constant take-off speed. Solution-process production lines can exhibit lower gel counts than high-pressure autoclave LDPE, but transfer between bulk railcar and feed hopper should include magnetic and screen filtration at 200 µm to 500 µm mesh to protect narrow spiral channels from occasional carbon or metal contamination.

    Moisture uptake is not a bulk property concern; the pellets are non-hygroscopic under standard storage, but condensation formed when cold silo pellets enter a warm humid blending room can create surface moisture that causes bubble instability and surface splay. Feedstock should be kept at or above the dew point. Sustained contact with strongly oxidizing acids, halogens, or unsaturated aromatic solvents at elevated temperature is outside recommended use; swelling agents such as toluene can plasticize the amorphous phase and reduce crystallization temperature. Storage below 50 °C and away from direct sunlight is recommended for unopened packaging.

    When Heavy-Duty Sack Applications Require Low-Temperature Puncture Resistance

    Industrial heavy-duty sacks used for polymer pellets, fertilizer granules, or mineral powders are converted with film thicknesses from 100 µm to 200 µm. In this range, the puncture resistance of Dow ELITE™ 5400G is governed by the rate of plastic deformation in the amorphous tie-chain network; the octene-derived branch length permits load distribution across multiple lamellae before yield. Production-scale lines with 1.8 m layflat and 250 kg/h output have reported stable bubble geometry when the frost line is maintained at 4 to 5 die diameters. Low-temperature storage at -20 °C does not produce the ductile-to-brittle transition observed in propylene-rich copolymers; however, the resin is not a substitute for ultra-high-molecular-weight polyethylene in abrasion-intensive slurry pipe liners or for polyamide in high-temperature barrier sacks. Continuous use at or above 65 °C can lead to creep deformation under constant load.

    In multilayer structures, the resin is used in the sealant ply or as a toughness layer in laminated heavy-duty packaging. Seal strength under ASTM F88 is typically evaluated after dwell times of 0.5 s to 2.0 s and sealing pressures of 0.3 MPa to 0.6 MPa; the seal initiation temperature is lower than butene-based LLDPE and is influenced by hot-tack performance under ASTM F1921. Converters targeting high-speed form-fill-seal operations should evaluate hot-tack strength at 50 m/min to 80 m/min line speeds, as the narrow molecular architecture can react differently to cooling-rate changes after sealing.

    Compliance Matrix and Handling Boundaries for Dow ELITE™ 5400G

    The resin is typically covered by manufacturer statements for olefin polymers used in contact with food under U.S. FDA 21 CFR 177.1520(c), with end-use limitations determined by migration testing under 21 CFR 176.170(c) for fatty and aqueous foods. For European applications, compliance with Regulation (EU) No 10/2011 requires an overall migration limit not exceeding 10 mg/dm² under prescribed simulants and time–temperature conditions; users performing multilayer structures must confirm the functional barrier assumptions in Annex IV. REACH registration under Regulation (EC) No 1907/2006 and absence of substances listed in Annex XIV or Annex XVII restrictions should be confirmed by the Safety Data Sheet. The polymer does not contain intentionally added heavy metals, but RoHS compliance under Directive 2011/65/EU is a finished-article obligation after conversion.

    Regulatory or compliance areaReference designationVerification status
    U.S. FDA food contact21 CFR 177.1520(c)Supplier statement; conditions of use apply
    EU plastics food contactRegulation (EU) No 10/2011Overall migration limit 10 mg/dm²
    REACHRegulation (EC) No 1907/2006Check SDS for registration and SVHC status
    RoHSDirective 2011/65/EUFinished-article obligation; no intentional Pb, Cd, Hg, Cr(VI), PBB, PBDE

    Blending Dow ELITE™ 5400G with low-density polyethylene in a ratio of 80:20 by weight is used on blown-film towers that require higher melt strength and deeper frost lines. The addition of LDPE lowers the zero-shear viscosity and increases elongational stress at bubble freeze, but reduces dart impact and tear resistance compared with the neat resin. For converters evaluating 5400G against a metallocene-catalyzed broad molecular weight distribution high-density polyethylene, the selection depends on required stiffness: the high-density material will show a 1% secant modulus above 600 MPa under ASTM D882, while 5400G typically sits below that threshold but provides higher puncture and tear. Published data for this specific configuration is limited when process conditions deviate from supplier-recommended ranges.

    Because the resin is supplied without a universal UV stabilizer package, outdoor service requires carbon black or hindered amine light stabilizer incorporation; unstabilized films exposed to direct sunlight can lose more than 50% of tensile elongation within several months, depending on climate and thickness. This is a general property of polyethylene and not a grade-specific specification, but it defines the boundary for agricultural and construction films. The absence of polar groups also limits adhesion strength unless the surface is treated by corona discharge or ozone treatment to raise surface energy above 38 mN/m for lamination and printing.