Dow Elite 5400 Linear Low Density Polyethylene

Dow ELITE™ 5400 Linear Low Density Polyethylene

    • Product Name: Dow ELITE™ 5400 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 454925
    Density 0.916 g/cm³
    Meltindex 0.85 g/10 min
    Meltflowratio 8.5
    Meltingpoint 124 °C
    Vicatsofteningpoint 100 °C
    Tensilestrengthatyield 10.3 MPa
    Tensilestrengthatbreak 34.5 MPa
    Elongationatbreak 600%
    Onepercentsecantmodulus 172 MPa
    Dartimpact 250 g
    Elmendorftearmd 300 g
    Elmendorfteartd 400 g
    Haze 6%
    Gloss45 70

    As an accredited Dow ELITE™ 5400 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5400 Linear Low Density Polyethylene is packaged in 25 kg polyethylene bags, palletized for industrial shipping and storage.
    Container Loading (20′ FCL) Dow ELITE™ 5400 Linear Low Density Polyethylene is packed in 25 kg bags, palletized, and loaded into 20-foot FCL containers.
    Shipping Dow ELITE™ 5400 Linear Low Density Polyethylene is shipped as solid pellets in 25 kg bags, 1,000 kg bulk bags, or bulk trucks/railcars. It is non-hazardous; keep dry and protected from heat, moisture, and contamination. Follow local transport regulations and the SDS.
    Storage Store Dow ELITE™ 5400 Linear Low Density Polyethylene in a cool, dry, well-ventilated area away from sunlight, heat, sparks, and flames. Keep containers or packages closed to prevent moisture, dust, and contamination. Avoid strong oxidizers. Use first-in, first-out stock rotation, protect from crushing, and follow the manufacturer’s SDS and local regulations.
    Shelf Life Two years from manufacture when stored in original unopened packaging, cool, dry, and away from direct sunlight.
    Application of Dow ELITE™ 5400 Linear Low Density Polyethylene

    For the production of machine stretch film, ELITE 5400 Linear Low Density Polyethylene is processed on a high-stalk blown film line with a grooved feed extruder having an L/D of 30:1. The nominal melt flow rate of 1.0 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and the nominal density of 0.916 g/cm³ under ASTM D792 permit gauge reduction to 12–23 µm without loss of bubble stability when the die gap is set between 1.2 mm and 2.0 mm. Barrel zone temperatures are maintained from 180 °C to 210 °C, the adapter at 210 °C to 220 °C, and the die zone at 215 °C to 230 °C; these settings keep melt pressure below 350 bar in most spiral mandrel dies and reduce shear-induced melt fracture at output rates of 0.8–1.2 kg/h/mm of die diameter. A dual-lip air ring supplying air at 7 °C to 15 °C and a bubble cage controlling band movement are required when blow-up ratio exceeds 2.8:1. The high-stalk configuration with a frost line height of 8 to 10 die diameters improves machine-direction tensile at break and machine-direction Elmendorf tear, but it increases the risk of bubble breathing and gauge bands if the frost line position is not held within ±20 mm. A polymer processing aid masterbatch at 400–800 mg/kg is commonly added to reduce melt fracture on narrow die gaps, while slip and antiblock loadings are deliberately kept low because pre-stretching on powered rollers above 200% amplifies the coefficient of friction shift measured under ASTM D1894.

    Formulation tolerance in machine-wrap applications is narrow. If a tackifier masterbatch is added above 5 wt% to improve load retention on sharp pallet corners, the film may telescope on high-speed wrappers unless winding tension is held constant and edge trim removal is set to 5–10 mm per side. Dart impact is monitored under ASTM D1709/A and puncture resistance under ASTM D5748, because pre-stretched film in contact with pallet corners fails by puncture rather than by tensile yield. Cling must be balanced against blocking in warehouses where storage temperature can exceed 35 °C; a kinetic coefficient of friction below 0.20 under ASTM D1894 creates roll instability, while values above 0.35 cause inconsistent unwinding on wrappers running 20–50 packages/hour. End products are 12–23 µm machine film rolls with containment force measured according to ASTM D4649, and converter-specific additive packages dominate final performance. Published data for this specific configuration is limited because winder tension programs, hand-wrap versus machine-wrap prestretch ratios, and storage histories vary between converting plants.

    Frozen Food Seal Initiation and Low-Temperature Dart Resistance in Coextruded Structures

    In five-layer blown film for frozen vegetables, seafood, and prepared meals, ELITE 5400 is used as the sealant layer in thickness fractions of 20–30% of the total gauge, typically between 8 µm and 20 µm inside an overall 60–90 µm structure. The resin is selected for seal initiation and hot-tack strength measured according to ASTM F1921; seal initiation on form-fill-seal equipment typically requires seal bar temperatures between 105 °C and 125 °C at dwell times of 0.5 s to 1.0 s. The surrounding layers commonly include polyamide 6 or ethylene-vinyl alcohol with tie resins, so the LLDPE sealing layer must tolerate moisture vapor trapped at the polyamide-LLDPE interface; edge-curl reduction is achieved with a die temperature of 220 °C to 230 °C and a blow-up ratio of 2.0:1 to 2.5:1. Die gap is held between 1.6 mm and 2.2 mm, and frost line height is limited to 5 to 7 die diameters because excessive rapid quenching increases LLDPE crystallinity and reduces low-temperature crack resistance. If the frost line is raised above 7 die diameters, the polyamide-LLDPE interface may become unstable and visible as transverse bands under polarized light.

    Compliance for frozen food contact is governed by FDA 21 CFR 177.1520(c) and EU Regulation 10/2011 as amended. Under the EU regulation, overall migration must not exceed 10 mg/dm² using the assigned food simulant for frozen aqueous or fatty products, and the converter must verify that only permitted monomers and additives from the positive list are present. If post-consumer recyclate is blended into the core layer, the food-contact layer remains virgin ELITE 5400 at a minimum thickness of 12 µm to prevent indirect mass transfer. Low-temperature seal integrity is tested under ASTM F88/F88M-21 after conditioning at -20 °C for 24 h, with target values set by the food packer rather than the resin supplier. Antiblock masterbatch is used at 2,000–5,000 mg/kg to control sealant-side blocking in freezer storage; loadings above 8,000 mg/kg may reduce seal strength below 10 N/15 mm. End products include gusseted pillow pouches and stand-up formats for frozen shrimp, berries, and mixed vegetables.

    What Limits Gauge Variation in Form-Fill-Seal Heavy-Duty Sacks at High Bagging Rates?

    Heavy-duty form-fill-seal sacks for 50 kg fills of resin pellets, fertilizers, petrochemical granules, and construction chemicals are produced from ELITE 5400 in 80–180 µm thick three-layer A/B/A blown film. The resin is placed in the outer skins at 10–20 wt% of total structure because the central layer usually contains edge trim or post-industrial reclaim. Extrusion lines for this format commonly use a 400 mm spiral mandrel die with output of 450–600 kg/h, which demands a melt temperature controlled to 190–215 °C and a die zone at 210–225 °C. Die gap is set at 1.8–2.4 mm, blow-up ratio at 2.0:1 to 2.5:1, and frost line height at 4 to 6 die diameters. The main processing limitation is gauge variation caused by spiral mandrel back-pressure and melt-temperature differences across the die circumference; sack converters target a thickness tolerance of ±5% because a thin spot in the gusset area becomes the primary drop-impact failure point. Additive packages include a slip/antiblock masterbatch at 1,000–3,000 mg/kg, a polymer processing aid at 300–600 mg/kg, and a carbon black masterbatch at 2–5 wt% for UV-shielded outdoor storage.

    Mechanical acceptance is based on dart impact under ASTM D1709/A, Elmendorf tear under ASTM D1922, and drop testing of filled sacks under ISO 7965-2. The end product must survive a 1.2 m drop on the vertical face and a 0.8 m drop on the gusset seam without leaking; therefore the skin-layer ELITE 5400 loadings and core-layer reclaim content are limited to 30 wt% maximum post-industrial reclaim. Higher reclaim concentrations reduce dart impact and increase gusset crease splitting at low warehouse temperatures. Film blocking on the filling spout is another operational boundary: if slip migratory additives are overdosed above 3,000 mg/kg, the film will print and seal poorly, while underdosing below 1,000 mg/kg creates blocking rings at roll edges after storage at 40 °C.

    Application downstreamMelt temperature rangeBlow-up ratioDie gapOutput per die diameterPrimary control limit
    Machine stretch film200–230 °C2.8:1–3.2:11.2–2.0 mm0.8–1.2 kg/h/mmFrost line ±20 mm; COF range 0.20–0.35
    Frozen food coextrusion210–230 °C2.0:1–2.5:11.6–2.2 mm0.7–1.0 kg/h/mmEdge curl; sealant thickness > 12 µm with recycled core
    Heavy-duty FFS sacks190–215 °C2.0:1–2.5:11.8–2.4 mm0.9–1.3 kg/h/mmGauge ±5%; reclaim ≤ 30 wt%
    Sealant web for lamination200–225 °C2.0:1–2.5:11.6–2.0 mm0.7–0.9 kg/h/mmThickness band ±5%; corona ≥ 38 dyn/cm

    Ensiling wrap produced from ELITE 5400 is typically converted on a cast stretch-film line with three or more layers, although blown film lines are also used where oxygen permeability must be reduced by orientation balance. Gauge is held between 25 µm and 35 µm, width at 500 mm to 750 mm, and roll length at 1,500 m to 2,000 m. The extruder melt temperature in cast processing is maintained at 240–260 °C, the chill roll temperature at 18–25 °C, and the line speed at 300–600 m/min. A tackifier masterbatch is added at 5–10 wt%, a UV stabilizer masterbatch containing hindered amine light stabilizers at 0.5–1.5 wt%, and a white or green color masterbatch at 1–3 wt% to reduce light transmission. The finished film must meet the requirements of EN 13206 for wrapping round bales, including cling, puncture resistance, and elongation recovery after stretch on a baler. Puncture resistance is verified under ASTM D5748, cling force under ASTM D5458, and tensile properties under ISO 527-3. Operational boundaries include storage roll tension below 0.15 N/mm² to prevent permanent deformation at the core, and application temperature above 5 °C because tackifier migration slows sharply at lower field temperatures and can reduce cling below the level needed for bale sealing.

    In practice the resin is selected for consistent stretch on round balers that pre-stretch film by 55–70% before wrapping. Excessive gel content in regrind layers must be avoided because gels create pinholes at the bale surface and accelerate oxygen ingress, leading to silage spoilage. Oxygen permeability measured under ASTM D3985 becomes the limiting barrier indicator when gauge is reduced below 25 µm; under such conditions, ensiling fermentation may shift toward acetic acid formation and dry matter loss increases. Converters therefore specify thickness control of ±3% across the web and monitor gel count per 10 m² by visual inspection. The end product is a multi-season bale wrap for grass, maize, and lucerne silage, with converted rolls suitable for both table and round baler systems operating at high speed.

    When Sealant-Web Thickness Falls Below 25 µm in Solventless Lamination

    The use of ELITE 5400 as a sealant web in solventless lamination is constrained by the thickness control of the blown sealant film and the flatness of the heat-seal jaw. The sealant web is corona-treated to 38–42 dyn/cm before lamination to biaxially oriented polyester, biaxially oriented polypropylene, or aluminum foil; adhesive coat weight is held at 1.5–2.5 g/m², nip temperature at 45–55 °C, and cure time at 24–48 h at 35–45 °C. The laminator targets sealant thickness of 25–35 µm; when thickness falls below 25 µm, gauge variation from the blown film process and uneven jaw pressure create channel leakers at the package side seals. Heat-seal settings for the LLDPE sealant layer are generally 115–140 °C, dwell time 0.3–0.5 s, and jaw pressure 0.3–0.5 MPa. Hot-tack performance is measured under ASTM F1921, and seal strength after aging is measured under ASTM F88/F88M-21.

    Compliance for the final laminated structure includes FDA 21 CFR 177.1520(c) for the polyethylene component and EU Regulation 10/2011 for overall migration of 10 mg/dm², with testing carried out in the intended food simulant. If the pouch is packed with hot-filled products above 80 °C, the sealant web must maintain seal strength at the fill temperature; this usually requires a thicker sealant layer and a high-seal-strength tie layer rather than a simple monolayer sealant. For dry snacks and frozen contents, a 20 µm sealant web is technically feasible, but the heat-seal window narrows to ±5 °C and the pouch maker must verify seal bar deflection on high-speed rotary machines. End products include stand-up pouches, flat-bottom pouches, and four-corner seal sachets for snacks, frozen fruit, and portion packs.

    Regulatory or test domainReference standard or regulationKey threshold or condition
    U.S. food contactFDA 21 CFR 177.1520(c)Olefin polymer compliant; final article conditions of use apply
    EU food contactEU Regulation 10/2011Overall migration ≤ 10 mg/dm²; positive list only
    U.S. food-contact sealsASTM F88/F88M-21Seal strength targets set per packer after -20 °C conditioning
    Hot tackASTM F1921Seal window 115–140 °C; dwell 0.3–0.5 s
    Heavy-duty sack dropISO 7965-21.2 m vertical face drop; 0.8 m gusset seam drop
    Silage bale wrapEN 13206Puncture, cling, elongation recovery on round balers
    REACH SVHCRegulation EC 1907/2006Candidate list substance ≤ 0.1% w/w
    RoHSDirective 2011/65/EUPb, Hg, Cd, Cr(VI) limits per homogeneous material; Cd ≤ 0.01% w/w

    Industrial Stretch Hood Tear Propagation at -20 °C

    Stretch hood film produced from ELITE 5400 is blown or cast into heavy-gauge tubular film, often 100–160 µm, for pallet containment of insulation boards, cement bags, and household appliances. The film is folded into gussets and sealed into hoods that are stretched by 50–100% and released over the pallet. Tear propagation at subzero temperatures is the critical mechanical risk because a small puncture caused by a sharp corner can propagate along the machine-direction orientation if the film has been over-stretched. Elmendorf tear testing is conducted under ASTM D1922 after conditioning at -20 °C for 24 h, and tensile elongation at break is measured under ASTM D882. The extrusion processing window uses a die gap of 2.2–2.6 mm, blow-up ratio of 2.0:1 to 2.5:1, and melt temperature of 195–215 °C. Additives typically include an antistatic masterbatch at 1–2 wt% for packaging wood-composite products, and a slip/antiblock package at 1,000–2,000 mg/kg to prevent film-to-film blocking during roll storage. The end product is a pre-formed stretch hood supplied on reels for automatic stretch hood machines operating on pallet conveyors at 40–80 pallets/hour; film thickness is matched to pallet weight and load sharpness, with thicker hoods used above 800 kg pallet mass.

    Free Quote

    Competitive Dow ELITE™ 5400 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5400 Linear Low Density Polyethylene is a solution-polymerised ethylene/α-olefin copolymer classified for blown and cast film structures requiring a low seal initiation temperature, high tear resistance, and controlled optical haze. The resin is characterised by a nominal density of 0.916 g/cm³ when tested under ASTM D792-20 and a nominal melt index of 1.0 g/10 min under ASTM D1238-13 at 190 °C and 2.16 kg. The grade is supplied with antioxidant stabilisation and without intentionally added slip or antiblock. As a result, coefficient of friction and blocking behaviour must be controlled by masterbatch addition or by coextrusion with a formulated skin layer. In comparison with conventional Ziegler-Natta butene-1 LLDPE, ELITE™ 5400 is differentiated by its octene-1 comonomer, its narrow molecular weight distribution, and a low level of long-chain branching that provides melt strength closer to high-pressure LDPE while retaining linear low density polyethylene toughness. The designation “5400” identifies the base resin within the Dow ELITE™ series; published data for suffix-modified additive packages is limited and should be confirmed against the supplier certificate of analysis before use in food-contact constructions.

    Film extrusion processing of ELITE™ 5400 is constrained primarily by melt temperature and residence time rather than by screw torque. On single-screw extruders with 24:1 to 30:1 L/D barrier screws, the melt temperature is typically maintained between 190 °C and 230 °C. The lower bound is set by incomplete plastication and surface roughness; the upper bound is set by gel formation, odour development, and oxidation. Die gaps from 1.4 mm to 2.5 mm and blow-up ratios from 2.0:1 to 3.0:1 are reported in processing guides for solution LLDPE blown film. Frost line height is held between 5 and 8 die diameters, with higher frost lines improving bubble stability but increasing haze and lower frost lines improving optics but raising orientation stress. The melt index of 1.0 g/10 min produces lower head pressure than fractional-melt grades, but the molecular architecture supplies sufficient melt strength for stable high-stalk operation. Because the melt flow ratio under 190 °C/10 kg is not specified in public data sheets, melt index alone is insufficient to predict shear thinning; capillary rheometry is required for die design. On production-scale lines, melt temperature excursions above 240 °C have been associated with gel counts and odour changes; excursions below 185 °C increase motor load and die-lip build-up. Prolonged idle at 230 °C should be limited to 10 min without purge or temperature setback. No pre-drying is required for the virgin resin stored below 60% relative humidity; if condensation forms on cold pellets, a 60 °C to 70 °C desiccant dryer residence of 1–2 h is sufficient. Published data for specific extruder sizes and die diameters is limited, and processors should establish the temperature window on the target line.

    What Distinguishes ELITE™ 5400 from Conventional Ziegler-Natta LLDPE and High-Pressure LDPE Film Grades?

    The principal difference arises from the catalyst and polymerisation platform. Conventional Ziegler-Natta butene-1 LLDPE has a broad intermolecular comonomer distribution; low-molecular-weight chains carry proportionally more comonomer, which raises hexane extractables and can shift seal initiation upward. ELITE™ 5400 is produced on a solution platform with single-site catalysis and octene-1 as the predominant α-olefin. The resulting short-chain branching distribution is narrower, allowing the 0.916 g/cm³ density to be achieved with lower extractable content and reduced surface tack. High-pressure LDPE remains the reference material for melt strength and drawdown, but it exhibits lower tear resistance and tensile strength than ELITE™ 5400 at equivalent gauge. The following comparative matrix is based on typical classes reported in polymer producer technical bulletins; the entries are not film specifications.

    ParameterELITE™ 5400Ziegler-Natta butene LLDPE film gradeHigh-pressure LDPE film grade
    Density class0.916 g/cm³0.918–0.922 g/cm³0.922–0.924 g/cm³
    Melt index at 190 °C/2.16 kg1.0 g/10 min0.8–1.2 g/10 min0.8–2.0 g/10 min
    Comonomeroctene-1butene-1none
    Molecular architecturenarrow MWD, low level of long-chain branchingbroad MWD, linearhighly branched
    Melt strengthintermediatelowhigh
    Seal initiation temperaturelowerhighermoderate
    Elmendorf tear in machine directionhigherlowermoderate

    Seal initiation temperature is measured with ASTM F88/F88M-21 using 25.4 mm wide specimens, a dwell time of 0.5 s, and an applied pressure of 0.28 MPa. Hot-tack strength is evaluated under ASTM F1921-18 at the same jaw geometry. A common acceptance threshold is 10 N/25 mm for seal strength; the temperature at which this threshold is reached is not a fixed resin property because it depends on film thickness, coextruded skin layers, seal bar geometry, and dwell time. ELITE™ 5400 is reported in supplier technical bulletins to offer a lower seal initiation temperature than Ziegler-Natta butene-1 LLDPE of equivalent density and melt index when both materials are compared under identical test conditions. The narrower composition distribution reduces the population of low-melting chains that remain tacky after the seal bar opens, which widens the hot-tack window on vertical form-fill-seal packaging. For food-contact packages, hexane extractable content can be determined by ASTM D5227-21 as part of end-use compliance under FDA 21 CFR 177.1520(c); lower extractables are expected for the solution-grade resin because of the octene-1 distribution, but actual values must be generated on the finished film.

    Dart Impact Resistance and Optical Properties in Heavy-Duty Sack Film Structures

    In heavy-duty sack and collation shrink film structures, ELITE™ 5400 is often coextruded with high-pressure LDPE skins to balance mechanical strength and bubble stability. Dart impact resistance is assessed using ASTM D1709-16a; because the measured value is dependent on film gauge, blow-up ratio, frost line height, and extender masterbatch content, the supplier does not specify a single dart value for the resin. Tear propagation resistance is evaluated by ASTM D1922-15, and the octene-1 comonomer distribution increases the energy required for tear propagation relative to butene-1 LLDPE of similar density. Haze is measured under ASTM D1003-21; gloss is measured under ASTM D2457-21. Minimum haze is obtained with chilled air rings and high blow-up ratios, but these settings reduce bubble stability and output; the processing compromise must be defined on the target line. In cast film, the resin can be drawn to 25 μm when melt temperature is maintained between 190 °C and 230 °C; lower temperatures produce melt fracture, and higher temperatures increase gel formation. Published data for this specific configuration is limited, so converters should qualify each film construction against the end-use performance specification.

    When Post-Consumer Recyclate Content Is Blended at 20–30 wt%

    Blending ELITE™ 5400 with post-consumer recyclate at 20–30 wt% reduces optical clarity and melt strength because the recyclate stream contains polypropylene, polyethylene terephthalate, adhesives, and inorganic residues. Production-scale handling requires a 60 mm to 90 mm single-screw extruder with 30:1 L/D and continuous melt filtration at 80–120 mesh to remove particles above 180 μm. Surface moisture on the PCR fraction must be removed with a desiccant dryer at 60 °C to 70 °C for 1–2 h when condensation is visible; the virgin ELITE™ 5400 component does not require pre-drying below 60% relative humidity. The processing window narrows because recyclate promotes melt fracture and die-lip deposits; melt temperature is usually reduced by 5 °C to 10 °C relative to virgin operation to limit odour while retaining bubble stability. The blend should not be used for direct food-contact applications unless the PCR fraction meets FDA 21 CFR 177.1520(c) and EU Regulation No 10/2011 for the intended food simulant and contact conditions. Published data for this specific configuration is limited, and the converter is responsible for migration testing and odour evaluation.

    Regulatory compliance of ELITE™ 5400 is established through the standards listed in the matrix below. The resin is not specifically certified for ionising radiation sterilisation above 25 kGy; published data for this specific configuration is limited. End-use food-contact compliance is not granted by resin selection alone; the finished package must be tested for overall migration and specific migration under the applicable simulant conditions.

    Regulatory domainStandard or regulationCondition
    US food contactFDA 21 CFR 177.1520(c)Olefin polymers; intended use subject to end-test requirements
    EU food contactEU Regulation No 10/2011Overall migration limit 10 mg/dm²; specific migration limits apply per food simulant
    EU chemicals managementREACH Regulation (EC) No 1907/2006Substance registration; SVHC candidate list declaration required
    RoHSDirective 2011/65/EUNo intentional addition of Pb, Cd, Hg, Cr(VI), PBB or PBDE
    DensityASTM D792-20 / ISO 1183-1:20190.916 g/cm³ nominal
    Melt mass-flow rateASTM D1238-13 / ISO 1133-1:20221.0 g/10 min at 190 °C/2.16 kg
    Top