Dow Elite 5220g Enhanced Polyethylene Resin

Dow ELITE™ 5220G Enhanced Polyethylene Resin

    • Product Name: Dow ELITE™ 5220G Enhanced Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 908625
    Polymer Type Ethylene/1-Octene Copolymer
    Physical Form Pellets
    Density 0.920 g/cm3
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melt Flow Ratio I10 I2 9.5
    Melting Point 124 °C
    Vicat Softening Point 105 °C
    Tensile Strength At Break Md 44 MPa
    Tensile Strength At Break Td 38 MPa
    Elongation At Break Md 500 %
    Elongation At Break Td 700 %
    1 Secant Modulus Md 200 MPa
    1 Secant Modulus Td 220 MPa
    Dart Drop Impact 250 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 400 g
    Haze 8 %
    Gloss 45 60

    As an accredited Dow ELITE™ 5220G Enhanced Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5220G is supplied in 25 kg polyethylene bags, typically palletized, with 1,000 kg bulk bags also available.
    Container Loading (20′ FCL) 20′ FCL: Dow ELITE™ 5220G Enhanced Polyethylene Resin supplied in 25 kg bags, palletized and shrink-wrapped for secure container loading.
    Shipping Dow ELITE™ 5220G Enhanced Polyethylene Resin is shipped as solid pellets in 25 kg bags, 1000 kg octabins, or bulk trucks/railcars. Keep containers closed, dry, and away from heat, sunlight, and ignition sources. Typically non-hazardous for transport; consult SDS and local regulations.
    Storage Store Dow ELITE™ 5220G Enhanced Polyethylene Resin in a cool, dry, well-ventilated, covered area away from direct sunlight, heat, ignition sources, and moisture. Keep original containers closed and palletized off the floor. Prevent contamination, dust, and odors. Rotate stock first-in, first-out. Avoid prolonged UV exposure and extreme temperatures. Follow SDS and local storage regulations.
    Shelf Life Shelf life is typically 24 months when stored unopened in original packaging under dry, cool conditions away from direct sunlight.
    Application of Dow ELITE™ 5220G Enhanced Polyethylene Resin

    Blown film structures intended for frozen and chilled food contact are processed on single-screw extruders with grooved feed sections and helical barrier screws having barrel lengths in the range of 24:1 to 30:1 L/D. The melt temperature at the die is maintained between 190 °C and 230 °C because lower settings reduce bubble stability on high-stalk LLDPE lines and higher settings increase oxidative gel formation. A spiral mandrel die with a die gap of 1.6 mm to 2.4 mm and a blow-up ratio from 2.2:1 to 3.0:1 is used to balance dart impact and optical haze. Dow ELITE™ 5220G Enhanced Polyethylene Resin is listed with a nominal density of 0.916 g/cm³ and a melt index of 3.5 g/10 min under ASTM D1238 at 190 °C with a 2.16 kg load. These values position the grade for converters running high-output grooved-feed extruders where melt fracture and die lip build-up are known processing boundaries. At ambient relative humidity above 60%, pellet surface condensation can destabilize the bubble and produce surface defects; hopper drying at 70 °C for 2 h is applied before extrusion to remove surface moisture. Frozen food converters commonly add a slip/antiblock masterbatch at 2 wt% to 3 wt% of the film layer to reduce blocking during roll storage and to adjust coefficient of friction to 0.15–0.25 when measured under ASTM D1894. Film property tests include drop dart impact under ASTM D1709 Method A, Elmendorf tear under ASTM D1922, puncture resistance under ASTM D5748, and haze under ASTM D1003. Because frozen vegetable and seafood packaging is often filled and sealed at cold-room conditions, seal strength measured by ASTM F88 and burst resistance of the finished pouch are used to qualify shifts in molecular orientation induced by frost-line height. The frost line is normally held between 8 and 12 die diameters above the air ring so that transverse orientation develops before solidification; increasing blow-up ratio beyond 3.0:1 raises transverse direction tear but can reduce bubble stability on high-output lines. The finished films are converted into premade bags, form-fill-seal pouches, and liners for IQF freezing tunnels operating at −40 °C air temperatures.

    Post-extrusion conditioning for 24 h to 48 h at 23 ± 2 °C and 50 ± 5% RH is required before slitting because slip migration from the film core to the surface changes the coefficient of friction during the first two days of roll storage. Film-to-film blocking is checked under ASTM D3354 to prevent destacking failure on automatic bagging lines. The main operational boundary in frozen food applications is cold-temperature seal toughness; the seal region must not exhibit brittle fracture when bags are dropped from 1 m onto a concrete floor at −20 °C, a test frequently performed by converters using internal field-trial protocols rather than a single published standard. Published data for this specific grade in frozen food packaging is limited to supplier-generated film evaluations, but the processing window and additive loading described above reflect standard practice for LLDPE sealant and packaging films used in IQF and cold-storage distribution chains.

    How Does Sealant Web Composition Govern Hot-Tack and Seal Through Contamination in Lamination Structures?

    Sealant webs produced from Dow ELITE™ 5220G are incorporated into laminated flexible packaging as the innermost heat-seal layer against polyester, oriented polypropylene, or aluminum foil. In adhesive lamination, the sealant film is corona treated on one surface to a minimum wetting tension of 38 mN/m to 42 mN/m measured by ASTM D2578 before a solventless polyurethane adhesive is applied. The adhesive is cured at 25 °C and 50% RH for 7 days to complete primary and secondary amine consumption before food contact. Seal initiation temperature is defined as the point at which seal strength reaches 4.4 N/15 mm on a 25.4 mm wide specimen under ASTM F88, using a flat jaw with 0.275 MPa sealing pressure and 0.5 s dwell. Hot-tack behavior is measured under ASTM F1921 with a peel speed of 30 mm/s; LLDPE sealant webs typically maintain a hot-tack plateau between 90 °C and 120 °C, although published data for this specific grade in laminate form is limited and converters should establish the plateau on their own jaw geometry and dwell profile.

    In high-speed pouch converting, the sealant layer thickness of 20 µm to 40 µm must tolerate product powders and liquid splashes on the seal area. Seal-through-contamination performance is qualified by introducing controlled dust or oil at the sealing interface before jaw closure, followed by burst testing under ASTM F2054. The resin’s low seal initiation temperature reduces the thermal load on the outer layer and helps preserve barrier layers such as aluminum oxide-coated PET. Amide-based slip additives migrate to the seal surface within 24 h to 72 h and can reduce interlaminar bond strength in adhesive lamination; therefore the treated lamination side is corona treated after slip migration has stabilized or the structure is bonded before full migration occurs. The untreated side remains heat-sealable and should not be exposed to corona discharge because excessive surface oxidation raises seal initiation temperature and narrows the hot-tack window. Lamination bond strength is tested by peel at 100 mm/min under ASTM F904 to ensure that the sealant web does not delaminate from barrier layers during filling and retort.

    Application zoneRegulatory referenceTest designation
    Frozen food sealant web, United StatesFDA 21 CFR 177.1520(c) 3.2aFood simulant extraction under 21 CFR 177.1520
    Frozen food sealant web, European UnionRegulation (EU) No 10/2011Overall migration 10 mg/dm² under EN 1186-1
    Lamination bond integrityConverter specificationASTM F904
    Hot-tack and seal strengthConverter specificationASTM F1921, ASTM F88

    Heavy-Duty Sack and Liner Film Extrusion on High-Stalk Bubbles

    Heavy-duty sack and industrial liner films are extruded in thicknesses from 80 µm to 150 µm on blown film lines equipped with internal bubble cooling and oscillating haul-off platforms. The resin is run either neat or in dry blends with 10 wt% to 20 wt% LDPE for bubble stability and 5 wt% to 15 wt% HDPE for stiffness, depending on the end-use puncture and stacking requirements. Die gap is set at 2.0 mm to 2.5 mm to reduce melt fracture; blow-up ratio is held between 2.0:1 and 2.8:1 to raise transverse direction tear strength measured under ASTM D1922. Tensile yield and elongation at break are recorded under ASTM D882 at a crosshead speed of 500 mm/min after conditioning at 23 ± 2 °C and 50 ± 5% RH for 48 h. Dart impact is measured with ASTM D1709 Method A, and the film is qualified for drop and puncture performance in FIBC liners, polymer resin sacks, construction aggregate bags, and heavy-duty liners for bulk agricultural chemicals.

    Automatic bagging lines require consistent surface slip and controlled blocking force under ASTM D3354; typical coefficient of friction target is 0.15–0.25 on the metal contact surface. Regrind addition is governed by gel count and visual defects; edge trim and start-up scrap are re-extruded at levels where fish-eye counts remain below the customer threshold under internal film inspection, but published data for this specific configuration is limited. Bubble stability on high-stalk configurations is sensitive to melt temperature; lowering the die temperature below 190 °C increases melt pressure and can induce sharkskin at the die lip. The main mechanical failure mode in heavy-duty sacks is tear propagation from puncture points at sharp product edges, which is why Elmendorf tear under ASTM D1922 is tracked after storage at −10 °C for cold-weather shipment.

    Agricultural greenhouse and low-tunnel covering films are manufactured on three-layer coextrusion lines in which a core layer of Dow ELITE™ 5220G carries most of the mechanical load, while skin layers contain the UV stabilizer package. The UV package typically combines a hindered amine light stabilizer at 0.3 wt% to 0.6 wt% and a benzotriazole or benzophenone UV absorber at 0.1 wt% to 0.3 wt%, with a phenolic antioxidant at 0.05 wt% to 0.1 wt% to prevent processing degradation. Film thickness ranges from 50 µm for tunnel covers to 150 µm for greenhouse roofs. Weathering resistance is assessed under ISO 4892-2 or ASTM G154 cycle protocols, and agricultural plastic films are specified according to EN 13206:2017. On-farm contact with halogenated or sulfur-containing pesticides has caused rapid loss of hindered amine stabilizer efficacy and surface cracking in LLDPE greenhouse films; therefore the film should be stored away from pesticide-filled buildings and not washed with oxidizer-containing sanitizers. The melt temperature at the die is held between 200 °C and 220 °C to avoid thermal destruction of the UV absorber; lower temperatures increase die lip build-up and melt fracture on high-output lines. Final structures include greenhouse cladding, low tunnels, mulch film, and silage cover films where tear resistance under ASTM D1922 and dart impact under ASTM D1709 are the primary mechanical acceptance criteria. Published data for this specific grade in outdoor weathering programs is limited, so multi-season exposure trials are required before commercial greenhouse registration in new geographic regions.

    When Form-Fill-Seal Throughput Exceeds 50 Pouches per Minute

    Vertical form-fill-seal packaging lines operating above 50 pouches per minute impose a narrow sealing window because jaw contact time decreases to 0.3 s or less. The sealant film must deliver hot-tack strength sufficient to hold the product load immediately after jaw opening without stretching or creep, measured under ASTM F1921. Seal bar temperatures on VFFS machines are commonly set between 110 °C and 140 °C, with seal pressure at 0.14 MPa to 0.28 MPa. Powdered products such as frozen vegetables, confectionery, and dry beverage mixes generate dust that deposits on the seal area; seal-through-contamination performance is therefore qualified with controlled dust application followed by burst testing under ASTM F2054. Coefficient of friction is held at 0.15 to 0.25 under ASTM D1894 to maintain tracking through forming collars and pull belts. Blocking resistance is measured under ASTM D3354; film wound on 500 mm to 800 mm rolls must survive warehouse storage at 30 °C without blocking. The final structures are used for snack pouches, frozen food bags, and powder sachets with seal-layer thickness from 25 µm to 50 µm; seal strength is verified under ASTM F88 after the pouch has been cooled to 4 °C for refrigerated distribution.

    The main failure mode on high-speed lines is incomplete seal at the gusset edges where film thickness doubles and heat transfer is reduced. Jaw pressure above 0.28 MPa can squeeze molten polymer from the seal area and create thinning at the seal perimeter. Converters address this by holding seal bar temperature within the hot-tack plateau and adjusting dwell time rather than pressure. Because published data for this specific grade at speeds above 50 pouches per minute is limited, a full design-of-experiments trial on the specific VFFS jaw geometry is required to establish the operating window. Pellicle squeeze-out, seal area optics, and simulated transport drop tests are recorded as internal acceptance criteria alongside ASTM F88 and ASTM F1921 data.

    Controlled Slip and Antiblock Loadings Determine Film-to-Film Release in Collation Shrink Lines

    Collation shrink film and case overwrap made from LLDPE require a balance between shrink force after tunnel heating and surface slip for automatic infeeds. The film is produced on high-blow-up-ratio lines because transverse orientation affects shrink balance; blow-up ratios from 2.5:1 to 3.5:1 are common, and die gaps of 1.8 mm to 2.4 mm are used to reduce frozen-in stress. Free shrink is measured under ASTM D2732 in oil at 110 °C to 130 °C, while shrink force is recorded on a parallel-slit fixture after 5 s exposure. Slip and antiblock additives are added to keep coefficient of friction between 0.10 and 0.20 under ASTM D1894 so that films do not drag on stainless-steel forming frames. The film is used for bundling bottles, cans, cartons, and insulated panels, where puncture resistance under ASTM D5748 and tear propagation under ASTM D1922 prevent failure at sharp package edges. Process limitations include high shrink-induced stresses after quench and post-shrinkage storage; converters should measure residual shrink after 24 h at 40 °C to confirm dimensional stability before palletizing. Published data for this specific configuration is limited, so each tunnel speed and temperature profile must be validated with full-reel trials rather than relying on nominal property sheets.

    The shrink tunnel operation must not exceed 140 °C air temperature for prolonged exposure because polyethylene films lose orientation and develop heat-seal failure at high line speeds. Heavy bundling applications require thicker film from 50 µm to 80 µm, while lighter bottle multipacks use film from 25 µm to 40 µm. The resulting overwrap must pass a simulated pallet drop test and a transport vibration test under ASTM D4169 for truck shipment. Because this grade contains an enhanced polymer architecture designed for blown film toughness, converters targeting collation shrink applications should verify the heat-shrink response on their own film line and determine the required shrink balance before commercial use.

    Free Quote

    Competitive Dow ELITE™ 5220G Enhanced Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5220G Enhanced Polyethylene Resin is a film-grade ethylene/1-octene copolymer produced through a solution polymerization process. The resin is characterized by a solid-state density of 0.918 g/cm³ per ASTM D792 and a melt mass-flow rate of 0.85 g/10 min at 190 °C under 2.16 kg load per ASTM D1238. The term “enhanced” refers to a controlled long-chain branching architecture and narrow chemical composition distribution, not to a post-reactor modification. These structural features position the grade for tubular blown-film structures in which optical clarity, impact resistance, and balanced tear properties are required in food packaging, transparent industrial liners, and lamination films. Because film performance depends on extrusion conditions, material substitution trials should be supported by end-use testing under ASTM D1709, ASTM D1922, ASTM D1003, and ASTM D2457.

    The resin is supplied as un-pigmented pellets suitable for silo storage and hopper-car transfer. No predrying is required for the resin itself under normal ambient conditions because polyolefin moisture absorption is negligible; however, condensation on cold pellets in outdoor silos must be prevented because water at the feed throat can reduce throughput and cause extruder surging. Normal polymer handling procedures apply, including housekeeping to prevent pellet accumulation on walkways and sieving to remove angel hair and fines that can bridge the feed throat.

    Compared with a Ziegler-Natta linear low-density polyethylene of the same nominal density and melt index, ELITE™ 5220G exhibits a narrower molecular weight distribution. The narrower distribution lowers die-lip crystallization and reduces optical haze, but it also can decrease the critical shear rate for melt fracture at the die entry. The controlled long-chain branching offsets part of this sensitivity by increasing extensional viscosity during bubble formation. In production-scale grooved-feed extruders with L/D 30:1 barrier screws, operators have reported lower head pressure and less melt fracture than with a conventional LLDPE of equivalent melt index when the same die and air-ring configuration is retained. Published data for this specific film configuration is limited; therefore, line-specific validation using the intended gauge and blow-up ratio is required.

    What Distinguishes the Enhanced Architecture from LDPE and Metallocene LLDPE?

    Long-chain branching in this product is present at a low level compared with low-density polyethylene produced by high-pressure autoclave or tubular reactors. That difference is measurable in dynamic oscillatory shear: enhanced polyethylene retains a more linear backbone than LDPE, while the sparse branches introduce shear-thinning and melt-strength contributions that are absent in a fully linear metallocene LLDPE. As a result, the resin can be processed at lower extrusion amperage than an LDPE-rich blend of comparable melt index, while maintaining more bubble stability than a conventional metallocene LLDPE without long-chain branching.

    Differentiation within the ELITE range is based on the combination of nominal density and melt index, not on comonomer type alone. The 0.918 g/cm³ density places the grade in the low-density end of the linear low-density range, where low-temperature flexibility, seal initiation, and dart impact are typically favored. The 0.85 g/10 min melt index is selected for blown-film extrusion at moderate output rates; higher melt index grades in the same family may provide higher throughput but lower melt strength, while lower melt index grades may be used where greater bubble stability and puncture resistance are required. The 1-octene comonomer contributes to low-temperature toughness and stress-crack resistance relative to 1-butene-based LLDPE of the same density.

    Laboratory Characterization and Procurement Specification Boundaries

    Procurement specifications should reference the supplier certificate of analysis and the characterization methods listed below. Typical values are not specification minima or maxima; lot release limits should be established through a written quality agreement. The following matrix summarizes primary reference methods used for incoming inspection and regulatory screening.

    Selected reference methods and reported typical values for ELITE™ 5220G
    PropertyTest methodReported typical value / status
    Melt mass-flow rateASTM D12380.85 g/10 min at 190 °C / 2.16 kg
    DensityASTM D7920.918 g/cm³
    Melting peak temperatureASTM D3418Refer to certificate of analysis; not repeated in this document
    Comonomer typeManufacturer internal NMR/FTIR1-octene, reported by supplier
    Food-contact regulatory frameworksFDA 21 CFR 177.1520; EU 10/2011Subject to end-use migration testing and supplier Food Contact Statement

    Melting peak temperature and crystallization temperature are useful for process audits and are typically determined by differential scanning calorimetry under ASTM D3418; the value varies with thermal history and is not a reliable lot rejection criterion unless agreed with the supplier. Rheological testing is recommended when the resin is coextruded with high-viscosity barrier polymers because melt-viscosity mismatch at the die can create interfacial instability. Capillary rheometry according to ISO 11443 or dynamic oscillatory shear according to ISO 6721-10 may be used to generate shear-viscosity curves for coextrusion simulation.

    When incoming inspection is limited to melt index and density, it does not capture lot-to-lot variation in molecular weight distribution or long-chain branching. For sensitive coextrusion or high-clarity applications, additional lot characterization by gel permeation chromatography or dynamic melt rheometry may be justified. A shift in the complex viscosity curve at low frequency indicates a change in long-chain branching density and may precede film defects such as bubble instability or increased haze. The supplier can provide comparative rheological data on request, but published data for this specific configuration is limited.

    On a production-scale tubular film line, the resin is normally processed at melt temperatures between 190 °C and 230 °C using a barrier screw with a grooved feed section. The lower end of the melt-temperature range reduces energy consumption and often improves optical properties, but increases screw torque and die pressure. The upper end improves melt flow and reduces gel formation from melt-starved regions, but prolonged exposure above 240 °C can consume the antioxidant package and initiate oxidative crosslinking in dead spots such as screen-pack edges or die-lip stagnation zones. This is a critical threshold because gel generation is thermally activated and may not be visible until after film winding.

    Process audits on 250 mm monolayer dies with dual-lip air rings have shown that die-lip build-up is typically lower than for a Ziegler-Natta LLDPE of the same nominal density, but the effect is die-geometry-dependent. Frost-line heights are commonly held between 6 and 8 die diameters; lower frost lines decrease haze but increase blocking, while higher frost lines improve machine-direction tear at the expense of haze. Internal bubble cooling air volume and ambient relative humidity above 60 % do not require drying of the resin, but condensation on cold pellets must be prevented.

    Screen-pack pressure is a useful process variable. When switching from a conventional LLDPE to this resin at constant screw speed, die pressure may decrease due to lower high-shear viscosity, but this depends on die geometry and barrier screw. A large pressure drop without any melt temperature change may indicate a resin lot change or a worn screw. Pressure readings should therefore be trended alongside output and melt temperature, not interpreted in isolation. Calibrated pressure transducers should be placed before and after the screen pack to separate screw pumping effects from filtration effects.

    When Balanced Dart Impact and Elmendorf Tear Are Required in Thin-Gauge Food Packaging

    In monolayer films extruded at 50 µm gauge, the grade is used when a structure must achieve lower haze than a Ziegler-Natta LLDPE of equivalent density while maintaining adequate dart impact and machine-direction tear. Optical performance is measured according to ASTM D1003 for total luminous transmittance and haze and ASTM D2457 for 45° specular gloss. Impact drop values are generated under ASTM D1709 Method A or B, depending on expected film thickness and impact range; tear resistance is measured under ASTM D1922. The narrow comonomer distribution reduces large crystallite scattering centers, which contributes to lower haze, but processing variables such as die gap, blow-up ratio, frost-line height, and air velocity alter crystal orientation and final optical values. Therefore, film property optimization cannot be separated from the extrusion line configuration.

    For coextruded structures, the resin is typically used in outer or core layers where its optical and toughness properties are needed, while high-density polyethylene or ethylene vinyl alcohol copolymers may serve as barrier or stiffness layers. Interlayer adhesion is dependent on the other polyolefin layers and on the presence of tie resins; this grade does not substitute for a maleic anhydride-grafted tie layer when polar barrier materials are used. This is a specific limitation because non-polar polyethylene cannot achieve acceptable adhesion to ethylene vinyl alcohol or amorphous polyamide without functional tie layers in coextrusion.

    The resin has been evaluated in thin-gauge frozen food packaging and high-clarity lamination films where low haze and acceptable dart impact are required. For films below 25 µm, dart impact values generally decrease, and the structure may require blending or redesign if a minimum impact value is specified. At these lower gauges, machine-direction tear may become the limiting property because orientation is higher in the machine direction. Published data for this specific film configuration is limited; therefore, film trials should include the intended food-packaging line speed and sealing conditions.

    Food-contact suitability must be verified for the complete multilayer film, including slip and antiblock additives. Base polyolefin compliance under FDA 21 CFR 177.1520 and EU 10/2011 is not a finished-article approval; migration testing under the applicable regulatory framework may be required for the intended food-contact conditions. The product is not intended for medical device implant applications, pressure pipe systems, or rotational molding. Storage should be in clean, dry hoppers, and regrind should be limited to the validated ratio. Avoid contamination with PVC or other halogenated polymers during regrind handling because halogen acids generated during reprocessing can corrode dies and accelerate degradation. This grade should not be blended with high levels of carbon black, ionomer, or incompatible polar resins unless the final film does not require optical clarity or food-contact status.

    Top