Dow Elite 5200 Linear Low Density Polyethylene

Dow ELITE™ 5200 Linear Low Density Polyethylene

    • Product Name: Dow ELITE™ 5200 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 160378
    Product Name Dow ELITE™ 5200 Linear Low Density Polyethylene
    Manufacturer Dow
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Octene
    Chemical Family Ethylene/1-Octene Copolymer
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melt Flow Ratio I21 I2 30
    Melting Point 123 °C
    Vicat Softening Point 99 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 31.0 MPa
    Ultimate Elongation 710%
    Flexural Modulus 1 Secant 241 MPa
    Dart Drop Impact 260 g
    Elmendorf Tear Strength Md 240 g/mil
    Elmendorf Tear Strength Td 380 g/mil
    Environmental Stress Crack Resistance Escr >1000 h
    Low Temperature Brittleness < -70 °C
    Hardness Shore D 50
    Haze 7%
    Gloss 45 65%
    Molecular Weight Distribution Narrow
    Cas Number 9002-88-4
    Chemical Formula (C2H4)n

    As an accredited Dow ELITE™ 5200 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5200 Linear Low Density Polyethylene typically packaged in 25 kg polyethylene bags, palletized, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) Dow ELITE™ 5200 Linear Low Density Polyethylene loaded in 20′ FCL container, palletized 25 kg bags, stowed for ocean transport.
    Shipping Dow ELITE™ 5200 Linear Low Density Polyethylene is shipped as non-hazardous, free-flowing pellets in 25 kg polyethylene bags on 1,000 kg pallets, or in bulk trucks/railcars. Keep containers sealed, store dry and cool, away from sunlight, heat, and ignition sources to prevent moisture and contamination.
    Storage Store Dow ELITE™ 5200 Linear Low Density Polyethylene in a cool, dry, well-ventilated indoor area, on pallets and away from direct sunlight, heat, flames, and strong oxidizers. Keep original packaging closed to prevent moisture, dust, and contamination. Avoid prolonged UV exposure and excessive stacking. Use clean, labelled storage with first-in, first-out rotation; follow supplier safety data sheet.
    Shelf Life Dow ELITE™ 5200 LLDPE has a typical shelf life of 24 months when stored cool, dry, and in original unopened packaging.
    Application of Dow ELITE™ 5200 Linear Low Density Polyethylene

    Blown film conversion of Dow ELITE™ 5200 for deep-freeze packaged foods typically begins with a three-layer coextrusion structure in which the resin occupies the outer layer at 30–70 wt% of total web formulation. The core layer carries 20–40 wt% post-industrial edge trim and scrap regrind derived from the same line, while the seal layer is a metallocene-catalyzed LLDPE with a seal initiation temperature below 95°C measured by heat-seal testing per ASTM F88. The resin’s nominal density of 0.920 g/cm³ (ASTM D792) and melt index of 1.0 g/10 min (ASTM D1238, 190°C/2.16 kg) place it in the lower melt strength segment of LLDPE; therefore the bubble must be supported by a chilled dual-lip air ring at 15–18°C instead of high-velocity single-lip cooling. The extruder assigned to the outer layer is normally a 55 mm single-screw unit with 30:1 L/D and a barrier screw; die diameter is 300 mm, die gap is fixed at 1.8 mm, blow-up ratio is held at 2.2:1, and melt temperature is maintained between 205°C and 215°C. The frost line height is kept between 300 mm and 400 mm to limit film gauge spread to ±5%. Food-contact status is assessed under FDA 21 CFR 177.1520(c)3.1a for the base olefin polymer, while EU conversion requires finished-article migration testing under Commission Regulation (EU) No 10/2011; the overall migration limit is 10 mg/dm² after 10-day exposure to food simulant A at 40°C per DIN EN 1186-1. The terminal film is used as frozen vegetable bags, ice cream wrap, and frozen meat liners at thicknesses of 40–80 µm; low-temperature puncture is monitored on-line via ASTM D1709 dart drop testing of conditioned samples at −20°C. Published data for this specific layer distribution is limited.

    What Limits Bubble Stability When ELITE™ 5200 Is Run at a 2.0:1 Blow-Up Ratio in Heavy-Duty Sack Extrusion?

    Because the resin’s melt flow index of 1.0 g/10 min (ASTM D1238, 190°C/2.16 kg) and density of 0.920 g/cm³ (ASTM D792) reduce melt tension relative to high-pressure LDPE, inline converters commonly compound the resin at 60–80 wt% of the total polymer blend and add 20–40 wt% LDPE to the formulation to prevent bubble sag and gauge variation on 120–180 µm gusseted tubing. The extrusion line uses a 65 mm grooved-feed extruder with 30:1 L/D, a 350 mm die with dual-lip air ring, die gap 2.0 mm, blow-up ratio 2.0:1, and internal bubble cooling to extract heat from the central bubble region. The bubble stalk is intentionally shortened to 500–700 mm because the low melt strength of the resin permits faster frost line quenching than high-pressure LDPE; line speed is set between 15 m/min and 25 m/min for 150 µm final thickness. Output is maintained between 120 kg/h and 180 kg/h to avoid melt fracture at the die lip; die pressure is kept below 300 bar. Gusseted sack blanks are sealed at jaw temperatures of 160–190°C with 2.5–3.5 bar seal-bar pressure, and seal integrity is checked on a 1.2 m drop test according to ISO 7965-2. Mechanical assessment of the film is conducted by ASTM D1709 dart impact at −20°C and by ASTM D882 tensile elongation in machine and transverse directions. The terminal product is a heavy-duty polyethylene shipping sack used for polymer pellet packaging, fertilizer packaging, and pet food packaging; where the bag is not intended for food contact, compliance is still maintained under REACH 1907/2006 and relevant EU packaging waste directive 94/62/EC. Table 1 lists the regulatory and test standards applicable to this format.

    Standard/RegulationClause or Test MethodApplication Condition
    ASTM D1238Melt flow index190°C, 2.16 kg
    ASTM D792DensityResin density 0.920 g/cm³
    ASTM D1709Method ADart impact at −20°C
    ISO 7965-2Drop test1.2 m drop height on filled sack
    REACH 1907/2006Registration/Annex XVIIChemical packaging liner compliance

    In adhesive lamination of printed BOPP to metallized PET, a 15–25 µm sealant web of ELITE™ 5200 is coextruded as the innermost layer; the resin constitutes 70–100 wt% of the sealant layer when blended with a low-density metallocene plastomer at 0–30 wt% to lower seal initiation below 90°C. The web is produced on a 45 mm single-screw extruder with 28:1 L/D, die diameter 250 mm, die gap 1.5 mm, blow-up ratio 2.0:1, and internal bubble cooling; corona treatment raises surface energy to 38–42 mN/m for adhesive anchorage. Lamination adhesive is applied at 2.0–3.0 g/m² dry coat weight on the printed BOPP web, and the sealant web is nipped at 60–80°C with a pressure roll. Heat-seal strength is determined on 15 mm specimens per ASTM F88 with 0.5 s dwell time and 0.3 MPa jaw pressure. The finished laminate is used for coffee pouches, dry mix sachets, and confectionery wrappers. Food-contact compliance is evaluated through FDA 21 CFR 177.1520(c)3.1a and Commission Regulation (EU) No 10/2011, with overall migration below 10 mg/dm² after 10-day simulant contact at 40°C; external testing of the adhesive system is required because the BOPP and metallized PET layers introduce additional components outside the base resin certification.

    Stretch Hood Film Elastic Recovery and Puncture Resistance on High-Stalk Extrusion Lines

    A high-stalk blown film configuration with internal bubble cooling is used to convert ELITE™ 5200 into stretch hood film of 100–150 µm thickness; the resin is added at 50–80 wt% of the total blend, with 20–50 wt% LDPE or LLDPE regrind to stabilize the stalk below the frost line. The die diameter is 450 mm, die gap 2.2 mm, blow-up ratio is deliberately set between 1.2:1 and 1.8:1 to minimize transverse orientation, and stalk height is maintained at 1.5–2.0 m before the frost line; take-off speed runs at 25–35 m/min. Elastic recovery of the film is quantified using ISO 527-3 tensile hysteresis, with stretch ratios applied in a 0%–100% cycle, and puncture resistance is evaluated by ASTM D5748 stretch wrap energy-to-break methodology. Because the product is not intended for direct food contact, compliance is maintained under REACH 1907/2006 and EU packaging waste directive 94/62/EC. The terminal article is a stretch hood sleeve applied at 40–80% pre-stretch on high-speed palletizing lines to stabilize stacked beverage containers, paper rolls, and bagged building materials. Published data for this specific blend composition is limited, and converter-scale validation is required before full production runs.

    When ELITE™ 5200 Is Coextruded with HDPE in Industrial Liners

    Coextrusion of ELITE™ 5200 with HDPE is conducted on a three-layer blown film line where the resin is assigned to the core layer at 40–60 wt% of the liner formulation; the two outer HDPE-rich skins collectively represent 40–60 wt%, split at 20–30 wt% per skin, to provide stiffness and reduce blocking. The line uses a 70 mm single-screw extruder, 30:1 L/D, die diameter 400 mm, die gap 2.0 mm, blow-up ratio 2.5:1, and film thickness between 100 µm and 250 µm. The resulting liner web is slit and bottom-sealed at 180–220°C using a hot-knife sealer, and the finished liner is inserted into corrugated boxes, drums, or FIBCs. Mechanical properties are measured by ASTM D1709 dart impact, ASTM D1922 Elmendorf tear, and ISO 527-3 tensile elongation. For liners used in chemical packaging, compliance is maintained with REACH 1907/2006 and, where the outer packagings are tested as dangerous goods packagings, leakproofness of the inner liner is evaluated according to 49 CFR 178.604 or ADR 6.1.5.2. The terminal product is an industrial liner for free-flowing polymer granules, mineral powders, and specialty chemicals at fill weights between 10 kg and 1000 kg.

    The Resin’s Narrow Molecular Weight Distribution Alters Low-Temperature Dart Impact in Agricultural Silage Film

    Cast film conversion of ELITE™ 5200 for silage wrap is specified when a thickness tolerance below 25 µm is required; the resin is dosed at 90–94 wt% of the polymer fraction, while UV masterbatch is added at 5–8 parts per hundred resin and tackifier concentrate at 0.5–1.0 parts per hundred resin to raise cling and extend outdoor weathering. A 90 mm single-screw extruder with 33:1 L/D feeds a slot die with 2200 mm width; cast roll temperature is held at 20–25°C, and line speed is set between 150 m/min and 250 m/min to produce 500–750 mm wide bale wrap rolls. The film is tested for thickness variation per ISO 4592, tensile elongation per ISO 527-3, and dart impact per ASTM D1709 after exposure to −20°C for 24 h. Agricultural film compliance is maintained under REACH 1907/2006; food-contact regulation 10/2011 is not relevant because the film is not intended for food contact. The terminal product is a silage bale wrap used to seal fermented forage and pressed maize bales in livestock feeding operations. Published data for this specific formulation is limited, and additive supplier technical bulletins should be used to set UV masterbatch addition within the 5–8 parts per hundred resin range.

    Free Quote

    Competitive Dow ELITE™ 5200 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5200 Linear Low Density Polyethylene is a solution-processed ethylene copolymer supplied in pellet form for blown-film and cast-film conversion. The nominal density is 0.917 g/cm³ when tested in accordance with ASTM D792 or ISO 1183-1. The nominal melt flow rate is 1.0 g/10 min at 190 °C under 2.16 kg piston load using ASTM D1238 or ISO 1133-1. These values are not batch-specific specifications; a certificate of analysis should be used for shipment-level quality verification. The molecular structure differs from heterogeneous Ziegler-Natta linear low density polyethylene in that the comonomer is more uniformly distributed across the molecular weight distribution, while the controlled long-chain branch content separates it from metallocene grades with very narrow composition distributions. This architecture reduces low-molecular-weight, low-comonomer fractions that contribute to die lip build-up and to smoked or plate-out defects during extended production campaigns.

    In cast-film conversion, the grade is extruded through a flat die with a die gap of 0.4–0.8 mm onto a chilled roll maintained at 15–30 °C. The lower melt strength relative to low-density polyethylene requires a shorter draw distance between die exit and the chill roll to prevent neck-in and edge instability. Line speeds for 20–30 µm film can exceed 150 m/min on modern cast-film lines, but the exact limit is determined by melt temperature, chill roll diameter, and vacuum box design. Cast film produced from the 5200 grade generally displays lower haze than blown film of the same gauge because the orientation state is uniaxial rather than biaxial; this makes it suitable for applications where optical clarity and gauge uniformity are more important than tear resistance. Published data for this specific configuration is limited.

    Which Extrusion Parameters Govern Bubble Stability in Blown Film Lines?

    On production-scale monolayer blown-film lines equipped with 30:1 to 36:1 L/D barrier screws and annular die gaps of 1.2–1.6 mm, the grade is generally processed with barrel profiles from 170–190 °C in the feed zone, 190–220 °C in the compression and metering zones, and 210–240 °C at the adapter and die. Blow-up ratios of 2.0:1 to 3.0:1 provide a useful compromise between machine-direction and transverse-direction mechanical properties; blow-up ratios above 3.5:1 may cause low-frequency bubble oscillation if the air ring cannot maintain a stable air velocity profile across the film circumference. Frost line height is commonly held at 2–4 die diameters above the air ring. Melt pressure at the die entry typically falls between 200 bar and 350 bar depending on extruder diameter and output rate; a pressure fluctuation greater than ±1.5% of the mean value under constant screw speed is generally treated as an indication of feed variation, screw wear, or insufficient melt homogeneity. Because the melt index is 1.0 g/10 min, the motor load is higher than would be expected for a 2.0 g/10 min grade, but lower than for a 0.5 g/10 min high-toughness film resin. On lines with internal bubble cooling, the additional cooling air has been observed to reduce frost line variability and improve gauge uniformity; however, internal bubble cooling must be sized for the wet-bulb temperature and line speed rather than imposed as a universal retrofit. Barrier screws with 24:1 to 30:1 L/D and Maddock mixing sections are typically used; grooved feed throats with 5–8 mm groove depth improve solids conveying. Screen packs of 60/80/100 mesh may be used to remove particulate contamination, but fine mesh increases back pressure and should be compensated with melt temperature adjustment.

    At a film thickness of 25 µm, the grade typically falls within the performance envelope for LLDPE film resins of 0.917 g/cm³ density when tested by ISO 7765-1 or ASTM D1709 Method A; published data for this specific configuration is limited, but dart impact values above 350 g are common in this density and melt-index class. Elmendorf tear in the machine direction is frequently reported between 4.0 N and 8.0 N, and transverse-direction tear between 5.0 N and 9.0 N, with the balance controlled by blow-up ratio and frost line height. Tensile stress at yield is generally in the 9–11 MPa range when measured under ISO 527-3 or ASTM D882, with elongation at break above 500%. Secant modulus at 1% strain is typically 180–220 MPa in the machine direction and 200–240 MPa in the transverse direction, depending on orientation. The anisotropy in tear strength is a direct consequence of molecular orientation during tubular film stretching; raising blow-up ratio above 2.5:1 usually increases transverse-direction tear while reducing machine-direction tear. These representative ranges must be confirmed on the intended extruder because die gap, melt temperature, output rate, and cooling air temperature each shift the residence time and orientation state of the solidified film.

    Comparative Property Matrix Against Conventional Ziegler-Natta and Metallocene LLDPE

    The product can be differentiated from conventional Ziegler-Natta LLDPE by three process-linked characteristics: lower gel count in thin film, later onset of sharkskin surface melt fracture, and improved retention of dart impact after down-gaugeing. The solution process used for the 5200 grade minimizes high-molecular-weight fractions that contain little or no comonomer; such fractions are a primary source of optical gel defects in conventional LLDPE film. In laboratory capillary rheometry, linear low density grades of 1.0 g/10 min melt index typically exhibit sharkskin melt fracture at wall shear rates of 50–200 s⁻¹; the 5200 grade usually remains processable at the higher end of this range before surface roughness becomes visible. Relative to metallocene LLDPE of equal density, the product often shows slightly broader molecular weight distribution. That broader distribution improves bubble stability on air-quenched lines by increasing melt elasticity, but it may reduce ultimate optical clarity when compared with a very narrow metallocene grade. The ranking of these differences is equipment-specific; published data for this specific configuration is limited, and side-by-side runs on the target blown-film line are necessary to establish a commercial performance offset.

    When the 5200 Grade Is Coextruded with Low-Density Polyethylene in Sealable Web Formats

    In coextruded films, the 5200 grade is often used as a core or outer layer adjacent to sealant resins such as ethylene-vinyl acetate or ionomer. Addition of 3–20 wt% low-density polyethylene (LDPE) increases melt elasticity and shear thinning, which supports stable bubble formation at output rates above 3 kg/h per cm of die circumference on conventional single-screw lines. The resin itself is not formulated as a sealant; seal initiation temperature depends on the chemistry and thickness of the seal layer. In heavy-duty sack constructions of 100–150 µm, the 5200 layer contributes to puncture resistance and creep resistance under load, while the outer layer may be modified for slip and antiblocking. The as-supplied stabilizer package is intended for typical film extrusion and pellet storage, not for prolonged ultraviolet exposure in outdoor structures. Finished articles requiring extended weathering must be compounded with an appropriate UV stabilizer masterbatch at the extruder, and the addition level should be verified by accelerated weathering under ISO 4892-2 or ASTM G154.

    Frozen-Environment Film Structures Require a Different Balance of Tear and Puncture

    Low-temperature toughness in polyethylene is governed by the beta-relaxation process in the amorphous phase and by the concentration of intercrystalline tie-molecules. The 0.917 g/cm³ density of the 5200 grade provides a relatively low crystallinity that helps retain puncture resistance at temperatures below −20 °C, but the failure mode in frozen-food packaging is not uniform across formats. In a 30–40 µm frozen vegetable bag, machine-direction tear may be the limiting property after initial perforation; in a bone-in frozen meat pouch, blunt puncture failure can dominate. Standard puncture and dart tests performed at 23 °C do not capture this temperature-dependent shift. Finished packages should be tested at the intended storage and distribution temperature using ASTM D1709, ISO 7765-1, or a filled-bag drop test that reproduces the specific handling damage. Published data for this specific configuration is limited; converters should confirm performance through abuse testing on filled packages.

    For food-contact applications in the United States and European Union, the resin may be used in articles that comply with 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011. Compliance is not a property of the resin alone; the finished article manufacturer must verify overall migration and specific migration of additives under the intended food type, contact time, and temperature. The overall migration limit of 10 mg/dm² specified in EU 10/2011 applies to the final article. The resin contains no intentionally added per- and polyfluoroalkyl substances and is subject to registration under REACH (EC) No 1907/2006. It is not classified as hazardous under CLP (EC) No 1272/2008. The table below summarizes the applicable frameworks; certification for a specific lot must be obtained from the resin supplier.

    Framework Standard or Regulation Relevant Scope
    United States food contact 21 CFR 177.1520 Olefin polymers; end-use limitations apply
    EU food contact Commission Regulation (EU) No 10/2011 Plastic materials and articles; overall migration 10 mg/dm²
    Chemical safety REACH (EC) No 1907/2006 Registration, evaluation, authorization of substances
    Hazard communication CLP (EC) No 1272/2008 Classification, labelling and packaging
    RoHS Directive 2011/65/EU Restriction of hazardous substances in electrical and electronic equipment

    Processability boundaries are defined by melt temperature and residence time. Degradation may begin if melt temperature exceeds 280 °C or if the melt is held for an extended period in an injection-molding accumulator; blown-film and cast-film extruders normally remain below this threshold. Polyolefins are not hygroscopic, but condensation on cold pellets can introduce surface moisture that causes voids and streak defects. If pellet surface moisture is present after storage under high relative humidity or thermal cycling, drying at 70–80 °C for 2–3 hours in a desiccant dryer should be carried out before extrusion. The product should not be compounded with amine-based antistatic additives unless their compatibility with the stabilizer package has been confirmed by a thermal-oxidative stability test. Melt temperature, screw speed, and output rate should be logged continuously to detect process drift before film defects appear.

    Top