Dow Elite 5110 Linear Low Density Polyethylene

Dow ELITE™ 5110 Linear Low Density Polyethylene

    • Product Name: Dow ELITE™ 5110 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 662649
    Polymer Type Linear Low Density Polyethylene
    Comonomer 1-Octene
    Density 0.918 g/cm³
    Melt Index 0.85 g/10 min
    Melt Flow Ratio 30
    Melting Point 124 °C
    Vicat Softening Point 101 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 30.0 MPa
    Elongation At Break 700%
    Flexural Modulus 240 MPa
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 250 g
    Elmendorf Tear Strength Td 350 g
    Haze 8%
    Gloss 60 80

    As an accredited Dow ELITE™ 5110 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5110 Linear Low Density Polyethylene comes in 25 kg moisture-resistant bags, palletized, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) Dow ELITE™ 5110 Linear Low Density Polyethylene is loaded in 20′ FCL containers, 25 kg bags on pallets, securely stowed.
    Shipping Dow ELITE™ 5110 Linear Low Density Polyethylene is shipped as solid pellets in 25 kg bags, octabins, or bulk trucks/railcars. It is not classified as dangerous goods. Store in a cool, dry, ventilated area away from direct sunlight, heat, and ignition sources. Keep containers closed to prevent moisture and contamination.
    Storage Store Dow ELITE™ 5110 Linear Low Density Polyethylene in a cool, dry, clean, well-ventilated area, away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep original bags or containers closed, on pallets off the floor, to prevent moisture and contamination. Avoid excessive stacking and prolonged UV exposure. Use first-in, first-out stock rotation. Inspect containers regularly. Store at ambient temperature.
    Shelf Life Shelf life is 24 months from manufacture when stored cool, dry, and in closed original packaging under normal conditions.
    Application of Dow ELITE™ 5110 Linear Low Density Polyethylene

    Low-temperature packaging lines running vertical form-fill-seal equipment at storage temperatures below -25 °C require a blown film resin with a nominal density near 0.926 g/cm³ per ASTM D1505 and a melt index of 0.85 g/10 min per ASTM D1238 at 190 °C/2.16 kg, or per ISO 1133-1:2022, to maintain seal toughness after filling. In the European Union, the finished frozen food contact film is assessed under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; for the U.S. market, the base resin typically falls under FDA 21 CFR 177.1520 olefin polymer provisions. A monolayer starting formulation may be 100 wt% ELITE™ 5110 or a 85–90 wt% blend with LDPE, with a slip/antiblock masterbatch metered at 1.0–1.5 wt%, depending on coefficient of friction targets measured by ASTM D1894. The film is normally converted on a single- or three-layer blown film line with a 1.6–2.0 mm die gap, blow-up ratio 2.2:1–2.6:1, melt temperature 190–215 °C, and frost line height maintained between 400 mm and 600 mm above the air ring. Terminal products include frozen vegetable bags, ice cube bags, IQF seafood pouches, and frozen fruit pillow packs with a typical gauge of 40–70 µm. Operational boundary: melt temperatures above 240 °C should be avoided because gel formation increases and film optics degrade; if ambient relative humidity exceeds 60%, moisture absorbed on pelleted feedstock can generate surface defects in monolayer output, requiring hopper-air conveying dew point control below -30 °C.

    What Limits Puncture Propagation Resistance in 25 µm Silage Bale Wrap?

    Agricultural silage bale wrap produced from ELITE™ 5110 must retain tear resistance under low ambient tension after multiple wraps on a round bale. For EU animal-feed contact, the polymer is normally evaluated under Regulation (EC) No 1935/2004 and Regulation (EC) No 2023/2006 good manufacturing practice; where the film is exported to North America, FDA 21 CFR 177.1520 is commonly cited for the olefin polymer base. A production formulation for a 25 µm monolayer blown film typically comprises 92–95 wt% ELITE™ 5110, 3–5 wt% VLDPE or plastomer to increase cling, and 1.5–2.5 wt% of a polyisobutylene tackifier masterbatch containing 50% active PIB; published data specific to ELITE™ 5110 in this exact formulation is limited, and the ratio is a representative starting point. The film is blown on a three-layer IBC coextrusion line with a die diameter of 200–300 mm, die gap 1.8–2.2 mm, blow-up ratio 2.5:1–3.0:1, and melt temperature 195–220 °C. Post-annealing and edge trim are followed by winding at 500–750 mm width. The terminal product is a round bale wrap roll of 25–35 µm thickness with elongation at break measured by ASTM D882, and dart impact measured by ASTM D1709, method B. Operational boundary: excessive PIB masterbatch above 2.5 wt% may cause blocking and inconsistent unwind on bale wrappers; processing below 2:1 blow-up ratio can reduce machine-direction tear balance.

    Unsupported Tubular Film Die Gap Adjustments for 50 kg FFS Sacks

    Heavy-duty form-fill-seal sacks for dry bulk chemicals are converted from unsupported tubular film that must survive 1–2 m drop tests after filling. Compliance for non-food industrial packaging is commonly anchored to ISO 21898:2004 for terminology and, where the sacks are used for UN-regulated solid materials, UN 21.1.1 or UN 21.2.1 performance requirements under the UN Model Regulations. A three-layer line may use a core layer of 60–70 wt% ELITE™ 5110, 20–30 wt% HDPE for modulus, and 5–10 wt% LDPE for bubble stability, with a fluoropolymer process aid at 200–400 ppm. The film is produced on a high-stalk tubular blown film die with 2.0–2.5 mm die gap, blow-up ratio 2.0:1–2.3:1, melt temperature 210–240 °C, and output per die circumference controlled between 0.8 kg/h/mm and 1.4 kg/h/mm. Downstream FFS equipment typically fills 25–50 kg sacks at 1,200–1,600 bag/h using heat-seal bars set to 140–170 °C and a dwell time of 300–700 ms. Terminal product types include valve sacks for cementitious materials, block-bottom sacks for mineral fillers, and gusseted bags for resin pellets. Operational boundary: blends containing more than 30 wt% HDPE may reduce interlayer weld strength and increase minimum sealing temperature; die gaps below 1.8 mm can increase melt fracture in the high-stalk configuration.

    When a Lamination Sealant Web Must Maintain Heat-Seal Integrity Below 105 °C

    Lamination sealant films destined for flexible packaging are produced as thin, surface-treated substrates that are subsequently adhesive-laminated to PET, BOPP, or aluminum foil. In the EU, the finished laminate must comply with Regulation (EU) No 10/2011, including specific migration limits for additives; U.S. structures often rely on FDA 21 CFR 177.1520 for the sealant resin. A sealant web formulation may contain 90–100 wt% ELITE™ 5110 with the balance being a metallocene VLDPE, while a slip/antiblock package is limited to 0.5–1.2 wt% to avoid reducing lamination bond strength. The film is blown at a gauge of 20–40 µm, die gap 1.5–2.0 mm, blow-up ratio 2.0:1–2.5:1, and melt temperature 185–215 °C. Corona treatment to 38–42 mN/m is applied in-line before winding, and the film is laminated within 24 h to prevent surface energy decay below 36 mN/m. Heat-seal strength is evaluated by ASTM F88 after sealing at 105–130 °C and 0.5 s dwell; published data specific to ELITE™ 5110 in this lamination configuration is limited. Terminal product structures include stand-up pouches for dry foods, pillow pouches for coffee, and lidding film laminates for dairy cups. Operational boundary: additive packages containing amide-based slip agents should be kept below 1.0 wt% because excess migration can reduce adhesive laydown and lower bond strength under ASTM F904 testing; corona discharge above 42 mN/m can create surface oxidation that interferes with polyurethane adhesive cure.

    Compliance and test method matrix for ELITE™ 5110 downstream film applications
    Application segmentFood-contact or industrial standardKey physical test methodTypical gauge
    Frozen food VFFSFDA 21 CFR 177.1520, EU No 10/2011ASTM D1709, ASTM D88240–70 µm
    Silage bale wrapRegulation (EC) No 1935/2004, FDA 21 CFR 177.1520ASTM D5748, ASTM D192225–35 µm
    FFS heavy-duty sacksISO 21898, UN Model RegulationsASTM D882, ASTM D1709120–200 µm
    Lamination sealant webEU No 10/2011, FDA 21 CFR 177.1520ASTM F88, ASTM F90420–40 µm
    Drum liners / bag-in-boxEU No 10/2011, FDA 21 CFR 177.1520ASTM F392, ASTM D574880–200 µm
    Pallet stretch hoodREACH, ISO 527-3ASTM D5748, ISO 527-380–120 µm

    For 200 L drum liners and flexible liquid packaging inserts, a low-melt-index LLDPE grade with a nominal density of 0.926 g/cm³ must resist puncture after side-weld folding and bottom gusset creasing. Food-contact liquid liners sold in the EU are assessed under Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; in the U.S., the olefin polymer base is typically covered by FDA 21 CFR 177.1520. A monolayer or two-layer structure may use 85–95 wt% ELITE™ 5110 and 5–15 wt% LDPE to improve melt strength, with a stabilizer masterbatch at 0.5–1.0 wt%. The film is produced on a low-BUR blown film line with 2.2–2.8 mm die gap, blow-up ratio 1.8:1–2.2:1, melt temperature 200–225 °C, and a gusseted collapsing frame. Terminal products include round-bottom drum liners for 200 L steel drums, boxed liquid liners for 3–20 L bag-in-box systems, and anticorrosive liners for viscous industrial fluids. Operational boundary: film gauge below 80 µm may fail crease-flex testing after bottom-weld folding under ASTM F392; excessive LDPE above 15 wt% lowers the softening point and may increase permeation, while melt temperatures above 235 °C can generate oxidation-related surface gel specks.

    Pallet stretch hood film lines running on automatic stretch hood machines impose cyclic cold-stretch at 5–15% elongation without tearing at gusset edges. Industrial packaging of this type is governed less by food-contact rules and more by performance standards such as ISO 527-3 for tensile properties of films and ASTM D5748 for puncture resistance; for export structures, REACH Regulation (EC) No 1907/2006 applies to the resin and additives. A three-layer formulation for a 80–120 µm film may use 70–80 wt% ELITE™ 5110 in the core and skin layers, 10–20 wt% VLDPE for stretch recovery, and 5–10 wt% LDPE for process stability, with a slip/antiblock package at 0.5–1.0 wt%. The film is fabricated on a three-layer high-output blown film line with 2.0–2.5 mm die gap, blow-up ratio 2.0:1–2.5:1, melt temperature 210–230 °C, and a collapsing frame with rotating air ring. Terminal products are pallet hoods for chemical drums, bagged agricultural products, and building material bundles. Operational boundary: film gauge below 70 µm may show excessive stretching at the top corner of the pallet; VLDPE content above 20 wt% can reduce stiffness and cause film slipping on the hooding machine.

    Free Quote

    Competitive Dow ELITE™ 5110 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction
    Dow ELITE™ 5110 Linear Low Density Polyethylene is a single-site catalyzed ethylene/α-olefin copolymer supplied as pellets for blown film extrusion. The nominal density of 0.9255 g/cm³ determined by ASTM D792 places the grade in the upper-middle density range of linear low density polyethylene film resins, where stiffness, puncture resistance, and seal performance are balanced. The melt index of 0.85 g/10 min measured by ASTM D1238 at 190 °C under a 2.16 kg load provides sufficient melt viscosity for bubble stability on high-stalk blown film lines while retaining drawdown capability. The resin is produced by a solution polymerization process using a constrained geometry catalyst system. Unlike high-pressure autoclave low density polyethylene, the polymer backbone carries short-chain branches from the α-olefin comonomer plus a controlled population of long-chain branches introduced by the catalyst. This architecture reduces the haze penalty that can appear when high melt strength is generated through autoclave branching.
    Table 1. Nominal base resin properties for Dow ELITE™ 5110.
    PropertyNominal ValueTest Method
    Density0.9255 g/cm³ASTM D792 / ISO 1183-1
    Melt index0.85 g/10 minASTM D1238 / ISO 1133-1:2022
    Melting point123 °CDow internal DSC method
    Vicat softening temperature102 °CASTM D1525

    What Distinguishes a Constrained-Geometry Solution LLDPE from Autoclave LDPE?

    The principal structural difference is the distribution of branching and molecular architecture. Autoclave high-pressure LDPE carries a broad distribution of long-chain branches and short-chain branches that creates high melt strength and low melt tension, but also increases optical haze and reduces tensile elongation. Constrained-geometry solution LLDPE contains a narrower short-chain branching distribution and a lower long-chain branch density. At a comparable density of 0.925 g/cm³, the LLDPE grade requires higher motor torque and generates higher die pressure on the same extruder than LDPE. Film produced at 25 µm thickness with a 2.5:1 blow-up ratio is evaluated for tear resistance by ASTM D1922 and for dart impact by ASTM D1709-16a; the linear structure generally yields higher elongation at break than autoclave LDPE of equivalent thickness, but the comparative values depend on die gap, frost line height, and orientation balance. Unlike LDPE, the reduced long-chain branching of this grade decreases neck-in and promotes machine direction orientation, which affects shrinkage symmetry and dart impact.

    Blown Film Melt Temperature, Die Gap, and Bubble Cooling

    On single-screw extruders with screw diameters between 45 mm and 90 mm and L/D ratios from 24:1 to 30:1, a barrel temperature profile of 180–210 °C in the feed and compression zones and an adapter/die temperature of 210–230 °C are commonly used. The melt temperature should be maintained below 250 °C to avoid oxidative chain scission and gel formation; operation below 180 °C may produce melt fracture at high screw speeds. A die gap of 2.0–2.5 mm is appropriate for this melt index. Narrower gaps below 1.6 mm increase shear stress at the die lip and can reduce dart impact, while gaps above 3.0 mm reduce transverse orientation and may lower bubble stability. Blow-up ratios from 2.0:1 to 2.8:1 provide balanced orientation for general-purpose film. A frost line height of 2–4 die diameters is typically maintained to control crystallinity and film blocking. Pre-drying is not required at ambient relative humidity below 60%; pellets exposed to condensation should be dried at 60–70 °C for 2–4 hours in a desiccant dryer before extrusion. In monolayer heavy-duty shipping sacks, the resin is processed at 25 µm thickness with a 2.5:1 blow-up ratio. The resulting film is evaluated for tear resistance by ASTM D1922 and puncture resistance by ASTM D1709. Operators on high-stalk blown film lines report fewer bubble collapses than with conventional Ziegler-Natta LLDPE of equivalent density and melt index when the die gap is maintained at 2.0 mm or greater; however, published production-scale case data for this specific configuration is limited. The grade is also used in coextruded sealant webs where a seal initiation temperature below that of high-pressure LDPE is required. Hot tack and seal strength are measured according to ASTM F1921 and ASTM F88/F88M-21, with results dependent on seal bar pressure, dwell time, and substrate thickness.

    When ELITE™ 5110 Replaces Conventional Ziegler-Natta LLDPE in Sealant Layers

    Direct substitution on a coextrusion line often requires adjustment of the extruder temperature profile because the single-site resin has a narrower melting curve and undergoes a more abrupt viscosity change as melt temperature decreases at the die. The processing window is most sensitive at melt temperatures below 190 °C, where surface haze and melt fracture may appear. The grade’s optical properties, measured as haze by ASTM D1003 and gloss at 45° by ASTM D2457, derive from a narrow comonomer distribution and reduced high-molecular-weight tail. This allows evaluation of sealant layer downgauging from 20 µm to 15 µm in some structures without loss of seal strength. The heat-seal temperature range should be validated by ASTM F1921 hot-tack testing across the specific coextruded substrate because hot-tack performance is influenced by substrate crystallinity and seal bar contour.
    Table 2. Regulatory compliance matrix applicable to Dow ELITE™ 5110 as a base olefin polymer.
    Regulatory ReferenceApplicable Condition or Limit
    FDA 21 CFR 177.1520(c) 3.2aOlefin polymers permitted for food contact under conditions of use A–H
    EU Regulation 10/2011Overall migration limit 10 mg/dm²; compliance verified under intended food contact conditions
    RoHS 2011/65/EULead 0.1% w/w, cadmium 0.01% w/w, mercury 0.1% w/w, hexavalent chromium 0.1% w/w, PBB and PBDE 0.1% w/w
    REACH 1907/2006Substances of very high concern not intentionally added above 0.1% w/w per candidate list

    Regulatory Status Under FDA 21 CFR 177.1520 and EU Regulation 10/2011

    The base resin is designed for food packaging applications where olefin polymer clearance is required. United States food contact compliance is based on FDA 21 CFR 177.1520(c) 3.2a, which covers olefin polymers produced from specified monomers and permits use under the regulatory conditions of use defined in 21 CFR 176.170(c). European Union compliance is assessed under EU Regulation 10/2011, with an overall migration limit of 10 mg/dm² for food contact materials. The resin contains no intentionally added lead, cadmium, mercury, hexavalent chromium, polybrominated biphenyls, or polybrominated diphenyl ethers above the maximum concentration values set by RoHS 2011/65/EU. For REACH compliance, substances of very high concern on the candidate list are not intentionally added above 0.1% w/w. Users must verify that the finished article meets the relevant migration limits under actual time, temperature, and food simulant conditions. The resin is incompatible with strong oxidizing agents and should not be stored at temperatures above 50 °C for extended periods. Pellets exposed to airborne fines or dust accumulation on a production floor can carry surface defects into the melt; a dedicated resin handling system with 0.5–1.0 mm screen filtration is typical. Addition of reclaim from mixed-film waste reduces Elmendorf tear and dart impact; the reduction is measurable after 10 wt% incorporation, and the specific magnitude depends on the contamination level and thermal history of the recycled content. In coextruded structures, contamination with polypropylene or high-pressure LDPE can reduce interlayer adhesion and tear strength; the effect should be evaluated by ASTM D1922 before full-scale conversion.
    Top