Dow Elite 5100g Enhanced Polyethylene Resin

Dow ELITE™ 5100G Enhanced Polyethylene Resin

    • Product Name: Dow ELITE™ 5100G Enhanced Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 949254
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 102 °C
    Tensile Strength At Yield Md 9.7 MPa
    Tensile Strength At Yield Td 9.0 MPa
    Tensile Strength At Break Md 38.6 MPa
    Tensile Strength At Break Td 31.7 MPa
    Elongation At Break Md 560%
    Elongation At Break Td 780%
    Elmendorf Tear Strength Md 180 g
    Elmendorf Tear Strength Td 390 g
    Dart Drop Impact 300 g
    Haze 7.5%
    Gloss 45 75
    Coefficient Of Friction 0.2

    As an accredited Dow ELITE™ 5100G Enhanced Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow ELITE™ 5100G Enhanced Polyethylene Resin is packaged in 25 kg polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Dow ELITE™ 5100G Enhanced Polyethylene Resin, stretch-wrapped and secured for transport.
    Shipping Dow ELITE™ 5100G Enhanced Polyethylene Resin is typically shipped as non-hazardous solid pellets in moisture-resistant bags, octabins, or bulk containers. Transport in clean, dry trucks or railcars, away from heat, sunlight, and contamination. No special DOT/UN hazard classification; follow the SDS and local regulations.
    Storage Store Dow ELITE™ 5100G in a cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. Keep containers tightly closed when not in use to prevent moisture and contamination. Avoid contact with strong oxidizing agents. Maintain temperatures below the resin’s softening point, typically under 50°C (122°F), to prevent caking or blocking. Follow local regulations and SDS recommendations.
    Shelf Life Shelf Life: Typically 24 months from date of manufacture when stored in original, unopened packaging under cool, dry, well-ventilated conditions.
    Application of Dow ELITE™ 5100G Enhanced Polyethylene Resin

    Extruded on three-layer blown-film lines with 65 mm, 85 mm, and 65 mm grooved-feed extruders of 30:1 L/D, Dow ELITE™ 5100G is converted for heavy-duty shipping sacks, polymer pellet liners, and inner webs in flexible intermediate bulk containers at barrel set points of 180 °C in the feed zone, 190 °C to 205 °C in the compression zone, and 210 °C to 220 °C at the die adapter. The annular die gap is held between 1.8 mm and 2.4 mm, and the blow-up ratio is maintained at 2.2:1 to 2.6:1 to balance machine-direction tear strength against transverse-direction impact resistance. Frost-line height is set at 700 mm to 900 mm above the die face; when the frost-line drops below 600 mm, the bubble enters an unstable interlocking region and gauge bands widen beyond ±10%. In a 70 µm three-layer sack structure, the outer layer contains 95 wt% 5100G and 5 wt% silica-based antiblock masterbatch, the core contains 80 wt% 5100G and 20 wt% high-density polyethylene with a melt index of 0.05 g/10 min to 0.30 g/10 min, and the inner layer contains 98 wt% 5100G with 2 wt% slip/antiblock concentrate.

    The screw back-pressure is sensitive to reclaim addition because 5100G exhibits a narrow comonomer distribution and lower melt elasticity than C4-LLDPE. When post-industrial edge trim exceeds 15 wt%, pressure at the screen changer often rises from 280 bar to 350 bar within 6 h; sustained operation above 380 bar forces a reduction in screw speed of 5 rpm to 10 rpm to avoid pressure-limiting alarms. Melt temperature should not exceed 230 °C because gel particles can form in dead spots at the die lip and create draw marks. Finished sacks are tested for drop resistance under ISO 7965-2 and for edge tear resistance under ISO 6383-2; purchasing specifications for 50 µm heavy-duty sack film usually require dart impact above 180 g by ASTM D1709 Method A, but converters validate each lot because impact values shift with frost-line position and layer ratio.

    Regrind levels above 15 wt% also increase the coefficient of friction when the slip additive package is not replenished; converters compensate by adding 0.5 wt% of a 5% erucamide masterbatch to the outer layer and 0.3 wt% to the inner layer. If the film is intended for automatic sack-filling equipment, static decay is measured under FED-STD-101C Method 4046, and antistatic masterbatch is added at 1.0 wt% to 2.0 wt% only when surface resistivity exceeds 10^12 ohm/sq after 48 h of conditioning at 23 °C and 50% relative humidity.

    Can 5100G retain puncture resistance in silage wrap after 12-month UV exposure?

    Silage bale wrap and clamp films are converted at 25 µm to 50 µm gauge with 2.5 wt% to 4.5 wt% UV masterbatch; the concentrate typically contains 20% hindered amine light stabilizer, 10% benzotriazole UV absorber, and 0.5% processing stabilizer in an LLDPE carrier. The 5100G phase is placed in the middle layer of three-layer structures at 70 wt% to 80 wt%, while outer skins use a C8-LLDPE with lower melt index to reduce cling and improve bale-wrap machine tension control. Puncture resistance is measured under ASTM D5748 at 23 °C and after 10 months or 12 months of outdoor weathering in a temperate climate; purchasing specifications frequently demand retention of 50% elongation at break after 2000 h accelerated aging per ISO 4892-2 cycle 1 with a black-standard temperature of 65 °C.

    Carbon black-loaded silage bag film uses 2.0 wt% to 3.5 wt% carbon black masterbatch; above 4.0 wt%, screen pack change intervals shorten from 8 h to 4 h because pressure rises from 320 bar to 430 bar on 90 mm extruders with 150 mesh screens. 5100G does not require desiccant drying for internal moisture absorption, but surface condensation forms when pellets stored below 10 °C are moved into a 25 °C blending mezzanine at relative humidity above 60%; this can bridge gravimetric feeders and is removed by hopper-air purging at 45 °C for 2 h. Amine-based antifog additives should be avoided in 5100G silage films when acidic silage leachate contact is expected because amine-functional surface agents can accelerate oxidative degradation at the film/effluent interface.

    Sealant-Web Formulation Windows and Hot-Tack Benchmarks in Flexible Packaging

    In three-layer pouch films, 5100G is used as the sealant web at 25 µm to 40 µm within a total laminate of 80 µm to 120 µm. The sealant layer contains 2 wt% to 3 wt% of a masterbatch with 10% synthetic silica and 5% erucamide; amide levels above 1500 ppm in the finished film can depress seal strength by 10% to 15% because surface migration blocks wetting of the seal interface. Seal initiation is measured by heat-seal curves under ASTM F88/F88M; converters set jaw temperatures 10 °C above the point at which seal strength reaches 2.0 N/15 mm, and a 0.3 s to 0.6 s dwell time at 2.8 bar jaw pressure is typical for high-speed pouching.

    Hot-tack performance is assessed under ASTM F1921 with a 0.5 s dwell and 0.2 s delay; a hot-tack force above 1.0 N/15 mm is often prescribed for vertical form-fill-seal machines running at 80 cycles/min because the seal must survive product drop before crystallization is complete. Die-lip build-up is controlled by keeping die temperature below 220 °C and by using a fluoropolymer process aid at 400 ppm to 800 ppm; higher process-aid levels are not advised because they can create plate-out on the outer die lip. The sealant web is corona-treated to 38 mN/m to 42 mN/m before lamination to solventless or solvent-based adhesives, and treatment decay below 36 mN/m can cause adhesive voids.

    Regulatory status for food-contact sealant webs is evaluated against the following matrix.

    Standard or regulationScopeTypical conditionRelevance to 5100G sealant web
    FDA 21 CFR 177.1520(c)3.2aOlefin polymers in food contactAll food types up to 100 °CSealant layer compliance
    EU 10/2011Plastic food-contact materialsOverall migration < 10 mg/dm²Finished laminate migration
    REACH 1907/2006SVHC and restrictionMonomer/oligomer < 0.1%General industrial use
    RoHS 2011/65/EUHeavy metal restrictionsPb, Hg, Cd, Cr(VI) < 1000 ppmElectrical packaging

    High-speed vertical form-fill-seal lines converting 40 µm to 60 µm monolayer films from 5100G for frozen vegetable and seafood packaging run with single-screw extruders of 25:1 L/D because the resin’s narrow comonomer distribution generates lower melt pressure than conventional C8-LLDPE at the same melt temperature. Film is conditioned at -20 °C for 4 h before low-temperature impact assessment under ISO 7765-1; acceptance criteria for freezer bags commonly require no brittle failure below -25 °C at 50 µm. Dart impact is measured by ASTM D1709 Method A at 23 °C, but the low-temperature result is the critical threshold because storage and distribution of frozen products occur below -18 °C.

    Slip and antiblock additions for frozen food films are kept lower than for dry foods because cold-seal adhesives require clean film surfaces. A typical formulation uses 800 ppm erucamide and 1200 ppm synthetic silica; erucamide levels above 1200 ppm can reduce cold-seal adhesive anchorage and cause print voids after surface printing. Coefficient of friction is measured under ASTM D1894 after 24 h conditioning at 23 °C and 50% relative humidity; automatic packaging lines usually require kinetic COF below 0.30 to avoid film misfeeds. The resin is not hygroscopic, so no desiccant drying is required; however, pellet condensation at high relative humidity can be avoided by hopper-air purging at 45 °C.

    End products are form-fill-seal freezer bags and pillow packs for frozen vegetables, seafood, and ice blocks. Compliance for direct food contact is evaluated under EU 1935/2004, and converters must confirm that the overall migration of the final printed film is below 10 mg/dm² when tested according to EN 1186-1 and the specific food simulant conditions for frozen storage.

    When 5100G replaces C8-LLDPE in machine-direction orientation for label facestock

    On blown-film MDO lines with 5:1 to 7:1 draw ratios, 5100G is blended with 10 wt% to 30 wt% high-density polyethylene for label facestock stiffness, or with 20 wt% to 40 wt% polypropylene for heat resistance during laser printing. The initial trial condition is set at 6:1 draw and 80 °C to 100 °C annealing roll temperature; higher draw ratios increase MD tensile modulus but reduce cross-direction tear, and CD tear values below 15 N/mm are considered unsuitable for pressure-sensitive label converting. Tensile properties are measured under ASTM D882, and thickness variation across the web is controlled below ±5% because non-uniform draw creates registration errors during die-cutting.

    Published data for 5100G in MDO label facestock is limited; converters should validate MD elongation at break, gloss, and secant modulus on pilot equipment before scaling to full production. The resin’s sealable nature can cause unwanted self-adhesion on annealing rolls above 100 °C, so roll temperatures are held below 95 °C and the film is cooled to 30 °C before winding. Corona treatment after MDO is applied to 40 mN/m to 44 mN/m to anchor UV flexo inks and pressure-sensitive adhesives.

    Temporary protective films for stainless steel, anodized aluminium, and glass panels are coextruded with a thin cling layer and a stiff core of 5100G at 30 µm to 60 µm total gauge. The core layer is blended with 15 wt% to 25 wt% low-density polyethylene with a melt index of 2.0 g/10 min to 4.0 g/10 min to increase scratch resistance and surface conformity. The cling layer uses an ethylene-vinyl acetate copolymer with 12% to 18% vinyl acetate at 5 wt% to 15 wt% of the total structure; high vinyl acetate content improves initial adhesion but can leave residue after 90 days of outdoor exposure. Peel adhesion is measured under ASTM D3330 Method A; a typical range of 0.3 N/25 mm to 0.8 N/25 mm is specified for flat glass and painted metal surfaces, while adhesion above 1.0 N/25 mm risks surface marking on anodized aluminium.

    Processing on cast-film lines uses a 30:1 L/D extruder with a 250 mm to 300 mm slot die and an air-gap of 80 mm to 120 mm; melt temperature is held at 220 °C to 230 °C, and the chill roll is kept at 20 °C to 30 °C to suppress haze and maintain flat lay. Edge-fold tracking is the main failure mode, and air-gap turbulence must be minimized with edge pins, particularly at line speeds above 120 m/min. The film is not crosslinked; therefore service temperature is limited to 60 °C for continuous outdoor exposure and 80 °C for short-term drying cycles.

    Free Quote

    Competitive Dow ELITE™ 5100G Enhanced Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow ELITE™ 5100G Enhanced Polyethylene Resin is an ethylene-octene copolymer produced on a solution polymerization platform and supplied as a granular, pelletized blown-film extrusion grade. Published product data identify a nominal density of 0.920 g/cm³ and a melt index of 0.85 g/10 min at 190°C under 2.16 kg. The octene comonomer introduces short-chain branches that are distributed along the polyethylene backbone with greater uniformity than is typical of conventional Ziegler-Natta butene LLDPE. The molecular design also includes controlled long-chain branching, which modifies shear-thinning behaviour and melt relaxation without suppressing the crystallinity required for film stiffness. These structural features differentiate the grade from generic butene LLDPE, LDPE-rich blends, and older metallocene LLDPE products in tear resistance, dart impact, seal initiation, and bubble stability. The resin is used in heavy-duty sacks, industrial liners, form-fill-seal packaging, agricultural film, and coextruded structures where puncture resistance and downgauging are processing and performance priorities.

    Physical Property Profile for the 0.920 g/cm³ Ethylene-Octene Resin

    Melt index is determined in accordance with ISO 1133-1:2022 or ASTM D1238-20, Procedure A, using a 2.16 kg weight at 190°C. Density is measured after compression moulding and conditioning following ISO 1183-1:2019 or ASTM D792-20. Differential scanning calorimetry per ISO 11357-3:2018 typically places the main melting endotherm near 122°C, with a secondary low-temperature endotherm associated with the low-crystallinity fraction that contributes to seal performance. Vicat softening temperature is commonly reported in the range of 100°C to 105°C under ASTM D1525-17e1. Because film tensile strength, elongation, Elmendorf tear, and dart impact depend on gauge, blow-up ratio, die gap, frost line height, and cooling air conditions, published typical values are configuration-specific. Direct transfer of a film property set from one blown-film line to another without revalidation is not appropriate. Melt rheology data are not fully published for all shear-rate windows; users requiring viscosity curves for screw design or flow simulation should request capillary rheometry data from the supplier rather than extrapolate from melt index alone.

    On production-scale monolayer blown-film lines using grooved-feed single-screw extruders with 25:1 to 30:1 L/D and spiral mandrel dies, the resin is typically processed at melt temperatures from 190°C to 230°C. Die gaps from 1.2 mm to 2.0 mm and blow-up ratios of 2.0:1 to 3.0:1 are common starting conditions. Increasing melt temperature above 240°C can promote oxidative chain scission, gel formation, and die lip deposits, while operation below 180°C may raise die pressure and reduce melt fracture resistance. The pressure drop across a 250 mm spiral mandrel die is machine-specific and should be monitored against extruder amperage and specific energy input rather than against a single universal value. Pre-drying is not normally required because polyethylene contains negligible polar moisture uptake, but pellets stored in environments with high relative humidity or cyclic condensation should be protected from surface moisture and reintroduced only after adequate venting. Batch-to-batch variance is controlled by supplier specification, but the converter should still verify melt index and density on incoming lots when film gauge and seal windows are tightly specified.

    When 5100G Is Run in High-Gauge Heavy-Duty Sack Applications

    In heavy-duty sack production, film layers from 100 µm to 200 µm are formed on high-output lines. The resin is often blended with 10–30 wt% LLDPE or LDPE to adjust stiffness and bubble stability, but the enhanced architecture permits a higher proportion of 5100G in the core layer without complete loss of bubble collapse resistance. On high-output lines, maintaining a frost line height of 5 to 8 die diameters improves gauge uniformity and reduces directional tear imbalance. The octene-based short-chain branching increases tie-molecule concentration relative to a butene LLDPE of the same 0.920 g/cm³ density, which is expected to improve Elmendorf tear and dart drop measurements. Dart impact is measured by ASTM D1709-16 Method A or ISO 7765-1, and Elmendorf tear is measured by ASTM D1922-15 or ISO 6383-2. The exact improvement ratio depends on the reference resin and film fabrication conditions; published data for direct comparisons with specific Ziegler-Natta grades should be obtained from the manufacturer’s technical data package. Tensile elongation at break is assessed according to ASTM D882-18 or ISO 527-3, and the ratio of machine-direction to transverse-direction elongation is used as an indicator of orientation balance.

    For sealant layers in coextruded films and lamination structures, the grade’s low sealing initiation temperature is exploited to increase packaging line speed. Heat seal testing is typically conducted on laboratory tack sealers with controlled dwell time and pressure, following ASTM F2029-16 or equivalent. The exact seal initiation temperature is a function of sealing pressure, dwell time, and film thickness; published data for this specific configuration are limited, and converter trials are required to establish the seal window. In coextrusion, the resin is placed in the sealant skin with a backing layer of HDPE or PP, and the differential melting behaviour must be considered to avoid interfacial distortion. The resin’s low-density fraction can migrate to the seal surface after annealing, altering hot-tack strength. Hot tack is evaluated using a hot tack tester per ASTM F1921-12. The balance between seal initiation and heat-seal strength is often adjusted by blending with lower-density or higher-melt-index polyethylenes; such blending should be validated with full-scale packaging trials because laboratory hot-tack data do not always predict form-fill-seal machine performance.

    What Distinguishes 5100G From Butene-Based LLDPE in Tear and Impact Response?

    The primary molecular difference is comonomer type and distribution. Butene-based LLDPE of similar density and melt index introduces shorter branches with a heterogeneous distribution when produced on conventional Ziegler-Natta catalysts. The octene comonomer in 5100G produces longer short-chain branches, and the catalyst system reduces the low-molecular-weight, high-density fraction that can crystallise rapidly and form tie-molecule-poor regions. During film stretching, tie-molecule density governs deformation resistance; a higher tie-molecule population delays craze coalescence and increases tear resistance. The difference is detected by Elmendorf tear measured according to ASTM D1922-15 and dart impact measured according to ASTM D1709-16. Comparative blown-film evaluations generally show an advantage for 5100G over conventional butene LLDPE at equal gauge, but the magnitude is influenced by blow-up ratio, die gap, frost line height, and film cooling rate. The grade also differs from LDPE-rich blends because its higher melting point and narrower melting range reduce bubble instability at high output, although LDPE remains the preferred additive when high melt elasticity and bubble collapse resistance are required.

    Regulatory status is use-specific. For food-contact applications in the United States, the grade may be used subject to compliance with FDA 21 CFR 177.1520 when the finished article meets the extraction and specification requirements of that section. In the European Union, compliance with Regulation (EU) No 10/2011 on plastic materials and articles intended to come into contact with food must be evaluated for the specific migration limits of the final article. REACH registration under Regulation (EC) No 1907/2006 applies to monomer and polymer import or manufacturing obligations within the supply chain. The RoHS directive 2011/65/EU restrictions on lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE are typically not relevant to neat polyethylene, but converted articles may require verification if pigments, masterbatch, or additives are introduced. The resin should not be combined with strong oxidising agents or processing aids that generate free radicals at high temperature, as uncontrolled chain scission or crosslinking can alter melt index and film gel count. Storage should be in a dry environment at ambient temperature below 40°C to avoid pellet agglomeration and oxidative degradation. Opened containers should be resealed to limit dust and moisture ingress.

    Compliance AreaStandard or Regulation
    US food contactFDA 21 CFR 177.1520
    EU food contactRegulation (EU) No 10/2011
    REACHRegulation (EC) No 1907/2006
    RoHSDirective 2011/65/EU

    Downgauging trials on heavy-duty sacks often replace a conventional butene LLDPE film of 125 µm with a 5100G-based film of 100 µm to 110 µm. The decision to downgauge is validated through dart drop per ASTM D1709-16, Elmendorf tear per ASTM D1922-15, tensile elongation per ASTM D882-18, and creep resistance under constant load. The enhanced resin’s lower melt index relative to a generic 1.0 g/10 min LLDPE may increase extruder torque at high screw speeds; barrel cooling and die pressure should be monitored. On coextruded lines, layer distribution adjustment is often required because the viscosity of 5100G is higher than that of high-MFR skin materials, leading to interfacial instability if the layer ratio is not optimised. Published data for this specific configuration are limited, and full-scale validation is necessary to confirm the target gauge reduction without sacrificing seal integrity or tear resistance. Laboratory film samples produced on small chill-roll cast lines are not sufficient to predict blown-film bubble stability or orientation-induced tear anisotropy on production equipment.

    Top