Dow Dowlex Ng 3347a Linear Low Density Polyethylene Ethylene Octene Copolymer

Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer

    • Product Name: Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 889985
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Copolymer Type Ethylene-Octene
    Density 0.934 g/cm³
    Melt Index 6.0 g/10 min (190°C/2.16 kg)
    Melt Flow Ratio 8.2
    Melting Point 124 °C
    Vicat Softening Point 108 °C
    Tensile Strength At Yield 13.8 MPa
    Tensile Strength At Break 20.7 MPa
    Elongation At Break 800%
    Flexural Modulus 448 MPa
    Hardness Shore D 50
    Environmental Stress Crack Resistance >1000 h
    Brittleness Temperature < -70 °C

    As an accredited Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Packaged in 25 kg polyethylene bags as pellets, palletized and stretch-wrapped for storage and transport.
    Container Loading (20′ FCL) 20′ FCL: 20 pallets of 25 kg bags, 1 MT each, total 20 MT; stretch-wrapped, secured, and sealed for export.
    Shipping DOWLEX™ NG 3347A is shipped as non-hazardous polyethylene pellets in 25-kg bags, octabins, or bulk trucks/railcars. No special DOT/IMDG/IATA hazardous classification applies. Keep containers closed, dry, and away from heat, sunlight, and contamination. Use clean handling equipment to prevent moisture pickup and product degradation.
    Storage Store Dow DOWLEX™ NG 3347A in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and strong oxidizers. Keep original containers or bags closed to prevent moisture and contamination. Avoid prolonged UV exposure and temperature extremes. Maintain clean, dry floors; spilled pellets are slippery. Use first-in, first-out stock rotation and follow the manufacturer’s SDS and local regulations.
    Shelf Life Shelf life is 24 months when stored in original packaging, dry, cool, away from direct sunlight and heat.
    Application of Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer

    On cast stretch lines where 90 mm single-screw extruders with 30:1 L/D barrier screws feed a coat-hanger die, DOWLEX NG 3347A is processed through melt temperatures of 230 °C to 260 °C, with die bolt zones held within ±2 °C of the target. The grade is an ethylene-octene linear low density polyethylene with a reported melt mass-flow rate of 2.3 g/10 min at 190 °C under 2.16 kg load according to ISO 1133-1:2022, and a density of 0.917 g/cm³ according to ISO 1183-1:2019. These values place the resin in the cast stretch film range that permits web thickness below 10 µm without immediate draw resonance, provided the air gap is held between 20 mm and 60 mm and the chill roll is controlled at 15 °C to 25 °C. A chill roll shift above 28 °C slows the surface quench sufficiently to create weak boundary layers during winding, and blocking on the finished roll can appear after 24 h of storage at 35 °C. Puncture resistance is measured with ASTM D5748-19 on the cast web, while pre-stretch carriages in pallet-wrapping equipment typically apply 200 % to 300 % elongation before the film contacts the load. The cling mechanism is not supplied by the base resin alone; tackifying additives such as polyisobutylene are compounded into the outer layer, and tack force is measured by ASTM D5458-95 peel force on a standard substrate. Tack values between 0.4 N and 1.0 N per 25 mm width are common for pallet wrapping, but actual set points shift with storage temperature and pre-stretch percentage. Excessive tackifying additive above 3 wt% can accelerate blocking on the roll after 24 h at 40 °C. The table below lists production parameters monitored on a cast film line for this grade.

    Line parameterControl rangeMeasurement method
    Extruder melt temperature230–260 °CIR melt probe at die inlet
    Die zone deviation±2 °CPID die bolt control
    Air gap20–60 mmLaser edge gauge
    Chill roll temperature15–25 °CClosed-loop water recirculation
    Pre-stretch ratio200–300 %Rotary encoder load cell

    Film below 8 µm produced from DOWLEX NG 3347A can exhibit machine-direction tear propagation measured by ASTM D1922-15 below 1.5 N when draw resonance is not controlled; in those cases, reducing line speed by 10 % or increasing the air gap to 35 mm restores web stability. Barrel zone temperatures below 180 °C can produce unmelted resin particles because screw torque reaches its limit before full plastication. This failure mode appears as fisheye defects in the film and is detectable by image-based gel counting when the film is run at 12 µm. For high-toughness pallet wrap, the grade is usually blended with other octene LLDPE resins in 3-layer cast structures; the outer layers carry cling and slip additives, while the core layer retains high dart impact strength measured by ASTM D1709-16a Method A.

    What Causes Tear Resistance to Fail After 60 % Pre-Stretch on Round Baler Wrapping Arms?

    The round bale wrapping sequence applies film at pre-stretch ratios between 55 % and 70 %; after wrapping, the outer layers must survive UV exposure and mechanical abrasion against stored bales. DOWLEX NG 3347A film at 25 µm is tested for tensile elongation to ASTM D882-18 and trouser tear to ASTM D1938-19. The octene short-chain branching reduces crystallinity compared with butene LLDPE of equivalent density, which raises dart impact measured by ASTM D1709-16a Method A while retaining machine-direction stretch. In silage film, oxygen transmission rate measured by ASTM D3985-17 at 23 °C and 0 % RH is the primary barrier indicator. LLDPE film of 25 µm typically shows oxygen transmission above 2,000 cm³/(m²·day·bar), so layer overlap and film thickness control fermentation quality more than intrinsic permeability. Published data for this exact grade in ensiling trials is limited; converters using octene LLDPE of density 0.917 g/cm³ report edge tear failures when film thickness drops below 18 µm or when pre-stretch exceeds 70 % on worn baler rollers with surface roughness above 0.8 µm Ra. UV stabilization requires addition of hindered amine stabilizers at 0.3–0.6 wt%, but additive packages containing high levels of unsaturated carrier resins can reduce tack and allow oxygen ingress at overlap edges. Compliance with EN 13207:2018 for thermoplastic silage films requires reporting UV resistance after artificial weathering; the unmodified base resin without a UV package does not provide a 12-month outdoor classification because the olefin backbone is inherently susceptible to photo-oxidative chain scission under prolonged sunlight exposure.

    Because dusty mineral and polymer granulate packaging exerts abrasion and puncture stress during filling and stacking, heavy-duty form-fill-seal sacks are routinely produced from DOWLEX NG 3347A at wall thicknesses of 150–200 µm. The film is qualified by dart impact to ASTM D1709-16a Method A and seal strength to ASTM F88/F88M-21. On a vertical FFS line filling 20–50 kg sacks, the seal bar temperature is controlled at 130 °C to 160 °C with dwell times of 0.8–1.5 s. Failure at the lower end occurs because the octene-rich amorphous regions have not fully flowed into the contaminated seal area. When seal strength falls below 12 N/15 mm, the failure mode converts from cohesive film tear to interfacial peel, especially when product dust is present in the seal zone. The broader hot-tack window of octene LLDPE compared with butene LLDPE is measured by ASTM F1921-12 as maximum seal force after 0.1 s cool time over a seal bar temperature range of 100 °C to 150 °C. Processing on heavy-duty FFS equipment typically uses a 2.2:1 blow-up ratio and frost line height of 8–12 die diameters when the grade is run on a 3-layer blown film line with a die gap of 1.8–2.2 mm. Ink adhesion requires corona treatment to 38–42 mN/m, measured by contact angle according to ASTM D2578-17. Without surface oxidation, printing inks delaminate from the sack surface after barrel tumbling or pallet compression.

    Heat-Seal Initiation and Extractives Control in Multi-Layer Sealant Webs

    A 15 µm sealant web based on DOWLEX NG 3347A is paired with biaxially oriented PET or polypropylene in flexible food packaging. The target heat-seal initiation temperature, defined as the minimum seal bar temperature producing 4 N/15 mm seal strength to ASTM F88/F88M-21, falls in the 90–110 °C range for this grade; the actual value depends on layer thickness, corona treatment level, and additive package. Hot tack force measured by ASTM F1921-12 at 110 °C and 0.2 s dwell is relevant for vertical packaging machines where product weight pulls the seal before cooling. Because the polymer is an olefin resin, it is suitable for food-contact use under FDA 21 CFR 177.1520 conditions of use A through H, subject to extractable limits. In European applications, the final laminate must comply with EU Regulation No 10/2011 overall migration limit of 10 mg/dm² when tested by EN 1186-1:2002 and EN 1186-14:2002 using simulant D1 for fatty foods. Actual migration values depend on the tie layer, printing ink, and outer web. A compliance checklist appears below.

    RequirementStandard or regulationControl limit
    US olefin polymer food contact21 CFR 177.1520Conditions of use A–H
    EU overall migrationEN 1186-1:200210 mg/dm²
    EU specific migration of octeneEU 10/2011Specific migration limit applies to final article
    Seal strengthASTM F88/F88M-21≥4 N/15 mm
    Hot tackASTM F1921-12Force at 0.2 s cool time

    Extractives from the polyethylene layer are controlled by limiting low-molecular-weight fractions during polymerization; the narrow molecular weight distribution of DOWLEX NG 3347A reduces migration of oligomers into fatty simulants. Converters still verify lot-to-lot extractives because masterbatch additives can raise hexane extractable values above 2.0 % when the final film is tested by FDA 21 CFR 177.1520 extraction methods. For a 15 µm layer, seal bar temperature above 120 °C can cause film distortion and shrink-back at the seal edge unless the outer web has sufficient heat resistance. This interaction is measured as seal strength decline and visual failure during ASTM F2029-16 heat-seal testing. A stable sealant web must also withstand 40 °C storage without coefficient of friction changes above 0.2 units when measured to ASTM D1894-14, because multi-layer laminates are often fed through high-speed packing machines with film-to-metal contact surfaces.

    When Pallet Loads Require Vertical Containment, Recoverable Stretch and Mandrel Tear Resistance Become Interdependent

    Stretch hood machinery draws polyethylene hoods from a gusseted tubular roll and expands them over a load, then releases the film to recover and lock the pallet. DOWLEX NG 3347A at thicknesses from 80 µm to 150 µm is evaluated for recoverable stretch after 100 % elongation and for Elmendorf tear by ASTM D1922-15 in both machine and transverse directions. The critical failure mode on the hooding mandrel is a machine-direction tear that initiates at the lower pallet edge. Mandrel corners with radius below 5 mm or rough edges above 0.5 µm Ra increase the tear initiation rate. Because octene LLDPE has higher elongation at break than butene LLDPE, hoods made from DOWLEX NG 3347A can often withstand mandrel expansion up to 1.5:1 stretch ratio without localized stress whitening. Load retention is measured by wrapping a pallet and recording film force after 24 h at 23 °C; values below 3 N/10 mm indicate excessive relaxation. Coextruded hoods with a tacky inner layer may require slip and antiblock additives to control unwinding tension; this grade without slip can exhibit blocking after 7 days at 40 °C if the roll is stored under high tension. Published data for this specific grade in stretch hood applications is limited to converter trials; the film processor should set the extrusion draw ratio below 10:1 to preserve transverse tear strength. Blending with metallocene LLDPE at 20–30 wt% can further raise dart impact by ASTM D1709-16a Method A and reduce film fracture at the pallet corners.

    Where intermediate bulk container liners are heat-sealed from heavy-gauge sheet, flex-crack resistance after 1,000 Gelbo flex cycles measured by ASTM F392-93 determines whether the liner remains dust-tight during transport. DOWLEX NG 3347A at 150 µm sheet is fabricated with heated seal bars at 150 °C to 170 °C and 1.0–2.0 s dwell to create leak-free side seams. The seal mode is inspected under ASTM F88/F88M-21; a minimum seal strength of 15 N/15 mm is required for liners carrying 1,500 kg of polyethylene pellets. Because liner film must withstand repeated fork tine impacts, puncture resistance by ASTM D5748-19 and slow-puncture resistance by ASTM F1306-19 are used to screen lots. On production-scale blown film lines, the grade is run with a 2.5:1 blow-up ratio and 2.0 mm die gap. Excessive melt temperature above 260 °C can cause polymer degradation and pinhole formation. Peel tests at overlap seams should produce cohesive film tears, not adhesive delamination, after 48 h of creep at 60 °C. If no slip or antiblock additive is included, converters handling high-speed bag insertion must add 1,000–2,000 ppm silica or erucamide masterbatch to prevent blocking and static charge buildup during liner inflation.

    Free Quote

    Competitive Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ NG 3347A Linear Low Density Polyethylene, Ethylene-Octene Copolymer is a pelletized, solution-polymerized ethylene/1-octene copolymer classified as linear low density polyethylene within the density range of 0.915 g/cm³ to 0.940 g/cm³. The manufacturer assigns a nominal density of 0.917 g/cm³ under ASTM D792 and a melt index of 2.3 g/10 min at 190 °C under a 2.16 kg load using ASTM D1238. The octene-derived C6 pendant branch distinguishes the polymer from butene-based LLDPE, which introduces only a C2 ethyl branch, and from hexene-based LLDPE, which introduces a C4 butyl branch. The material is not a high-pressure long-chain branched LDPE and does not rely on 1-butene as a short-chain branching agent. The CAS Registry Number for polyethylene is 9002-88-4. The product is supplied as free-flowing pellets and is typically evaluated for blown film, cast film, and sealant layers in flexible packaging and industrial film where puncture resistance, tear resistance, and optical clarity are specified. Published data for specific end-use configurations is limited; final film properties require converter-scale verification.

    What Are the Main Extrusion Boundaries for This Resin on Grooved-Feed Blown Film Equipment?

    On mono-layer blown film lines using a grooved feed throat, a 30:1 to 33:1 L/D barrier screw, and a spiral mandrel die of 200 mm to 300 mm diameter, melt temperature is commonly maintained between 190 °C and 210 °C at the die. Above 230 °C, oxidative chain scission and crosslinking can generate gel particles that cause bubble breaks; below 175 °C, high molecular weight fractions can produce melt fracture and haze. A die gap of 1.2 mm to 2.0 mm, blow-up ratio of 2.0 to 3.0, and frost-line height of 0.8 to 1.2 die diameters are typical starting points. Because the resin lacks the long-chain branching of LDPE, melt strength and shear thinning are lower; bubble stability often requires internal bubble cooling or a high-stalk configuration. On a 75 mm extruder, narrow spiral channel dies can be pressure-limited before torque-limited. These are starting conditions, not a universal processing window, and the final regime must be set against die pressure, motor load, and ambient air temperature.

    Comparative Comonomer Architecture, Tear, and Impact Response

    In comparison to butene-based LLDPE of equivalent density and melt index, the octene comonomer in DOWLEX NG 3347A introduces a longer C6 branch that is less readily incorporated into the polyethylene crystal lattice. The resulting crystallites are thinner and more numerous, lowering the crystalline melting point while increasing interlamellar tie-chain probability. Under ASTM D1922, Elmendorf tear values in the machine direction for octene-based films are frequently higher than those of butene-based films at equal thickness, though the improvement is nonlinear and can range from low single digits to more than 40% depending on blow-up ratio, frost-line height, and film gauge. Dart drop impact under ASTM D1709 shows similar dependence on orientation and thermal history. These trends do not automatically transfer to coextruded structures; tie layers, skin layers, slip/antiblock additive packages, and corona treatment modify the film surface and load-bearing cross-section. Tensile properties should be measured per ASTM D882 on actual film samples rather than predicted from pellet data.

    Substitution of DOWLEX NG 3347A for a butene grade should not be based solely on nominal density and melt index. The octene-derived branch structure shifts heat seal initiation and hot tack response. In packaging operations where sealing speed exceeds 25 m/min, the seal-bar set point may require adjustment relative to butene-based LLDPE. Seal strength should be measured according to ASTM F88, and hot tack according to ASTM F1921, with dwell time, jaw pressure, and cooling time recorded. Although the grade is supplied with a melt index suitable for film production, low-temperature seal performance depends on the coextruded substrate, sealant-layer thickness, and thermal history of the film. Published data for this specific configuration is limited.

    When the Sealant Layer Is Coextruded Against EVOH, Nylon, or Aluminium Foil

    In flexible packaging, the resin is evaluated as a sealant layer laminated or coextruded to biaxially oriented polypropylene, aluminium foil, or metallized polyethylene terephthalate. The low density and homogeneous comonomer distribution support low-temperature sealing, but the final food-contact status is determined by the finished article. U.S. FDA compliance falls under 21 CFR §177.1520 for olefin polymers when end-use extraction testing under 21 CFR §177.1520(c) is completed. European Union food-contact obligations are governed by Regulation (EU) No 10/2011, including overall migration limits of 10 mg/dm² and specific migration limits for additives and catalyst residues. REACH registration under Regulation (EC) No 1907/2006 applies to imported monomers and additives but not to the polymer itself. The base resin is not a medical-grade material and has no USP Class VI designation in the standard product data. No migration statement should be transferred from pellet lot to finished laminate without fixed extraction time, temperature, and food simulant data.

    Normative referenceScopeApplicable condition
    ASTM D792Density0.917 g/cm³ nominal
    ASTM D1238Melt index2.3 g/10 min at 190 °C/2.16 kg
    ASTM D1922Film tear resistanceMachine-direction and transverse-direction samples conditioned at 23 °C, 50% RH
    ASTM D1709Dart drop impactMethod A or B depending on film gauge
    ASTM F88Seal strengthRecord dwell, jaw pressure, and specimen width
    ASTM F1921Hot tackTemperature-dependent seal peel force

    Blending with LDPE is often evaluated when the resin is used in extrusion coating. In a flat-die process, the absence of long-chain branching increases neck-in and reduces draw-down performance relative to high-pressure LDPE. A blend containing 10% to 30% by weight LDPE is a common starting point to restore neck-in while retaining octene-LLDPE toughness. The die lip gap is typically set between 0.4 mm and 0.6 mm, and the chill roll temperature is maintained below 25 °C to control crystallization. The specific blend ratio must be optimized on the target line because published data for this configuration is limited.

    Moisture absorption of this polyolefin is negligible; pre-drying is usually unnecessary if pellets are stored indoors at relative humidity below 60%. However, condensation on cold pellets from outdoor storage or bulk handling can introduce surface water that turns to steam during extrusion. When surface water is suspected, a desiccant dryer operating at 60 °C to 80 °C for 4 h to 6 h can be used, but prolonged heating above 100 °C may cause pellet agglomeration. The resin should not be combined with amine-based antifog additives without verifying thermal stability, because amine additives can promote oxidative discoloration in some olefin systems.

    Metallocene-catalyzed ethylene-octene plastomers with density below 0.910 g/cm³ exhibit lower modulus, lower melting point, and higher impact than DOWLEX NG 3347A, but they often require lower extruder temperatures and may cause pellet handling blockage in warm feed zones. The 0.917 g/cm³ density of this grade maintains a distinct crystalline network, making it more suited to medium-stiffness film and sealant structures than ultra-low density plastomers. Melting behavior under differential scanning calorimetry at 10 °C/min heating shows a primary endotherm in the 120 °C to 125 °C range for solution-process octene LLDPE. Grade-specific melting point should be confirmed by the manufacturer’s certificate of analysis.

    Regulatory referenceAreaCondition or limit
    21 CFR §177.1520U.S. food contactFinished article extraction testing required
    Regulation (EU) No 10/2011EU food contactOverall migration limit 10 mg/dm²
    Regulation (EC) No 1907/2006REACHPolymer exempt, monomers/additives registered
    Directive 2011/65/EURoHSPb, Hg, Cd, Cr(VI), PBB, PBDE limits apply to electrical/electronic articles; base polyolefin commonly below limits
    ISO 15270Plastics recoveryIdentifies recoverable polyolefin stream

    Post-industrial edge trim and film scrap can be reclaimed on a reprocessing line equipped with an 80 mesh or finer melt filter. The addition of reclaim above 15% may increase gel counts and reduce film clarity; the exact limit depends on film gauge and final quality specification. No published data establishes a universal maximum reclaim level for this specific grade.

    Top