Dow Dowlex Ip 2580 Linear Low Density Polyethylene

Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene

    • Product Name: Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 280549
    Density 0.926 g/cm³
    Melt Index 190 C 2 16 Kg 0.80 g/10 min
    Melt Flow Ratio I21 I2 28
    Vicat Softening Temperature 100 °C
    Dsc Melting Temperature 124 °C
    Crystallization Temperature 108 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 30.3 MPa
    Ultimate Elongation At Break 800%
    Flexural Modulus 240 MPa
    Dart Drop Impact 250 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 8%
    Gloss 45 85%
    Coefficient Of Friction 0.2

    As an accredited Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene is supplied in 25 kg multi-wall paper bags, palletized and stretch-wrapped.
    Container Loading (20′ FCL) 20′ FCL container typically loaded with Dow DOWLEX™ IP-2580 LLDPE in 25 kg bags, totaling approximately 20 metric tons.
    Shipping Dow DOWLEX™ IP-2580 ships as non-hazardous polyethylene resin in 25 kg bags, 500–1,000 kg supersacks, or bulk truck/railcar. Store in dry, clean conditions away from direct sunlight and moisture; keep sealed to prevent contamination. Follow manufacturer SDS and local transport regulations. Handle with standard industrial practices. No special temperature control required.
    Storage Store DOWLEX™ IP-2580 resin in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original containers or packages closed, off the floor, and protected from moisture, UV, and contamination. Avoid prolonged elevated temperatures. Practice first-in, first-out rotation, and follow local regulations plus the SDS.
    Shelf Life DOWLEX IP-2580 has a shelf life of 24 months when stored unopened in a cool, dry place away from sunlight.
    Application of Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene

    On a three-layer blown-film line configured with 80 mm grooved-feed extruders for the outer skin layers and a 60 mm smooth-bore extruder for the core, DOWLEX IP-2580 is processed at melt temperatures of 215–230 °C through a 300 mm annular die with a 2.2 mm die gap. Published datasheet values place nominal density at 0.918 g/cm³ per ISO 1183-1:2019 and melt flow index at 0.8 g/10 min at 190 °C under 2.16 kg load per ISO 1133-1:2022, positioning the grade in the octene-LLDPE class used for heavy-duty shipping sacks, FIBC liners, and industrial chemical packaging. Where converter-specific published data for IP-2580 is limited, acceptance windows for equivalent octene-LLDPE industrial packaging grades are used. In converter trials on a 120 μm monolayer reference film, a formulation of 78 wt% DOWLEX IP-2580, 18 wt% LDPE with melt flow index 0.3 g/10 min, and 4 wt% of a 5% erucamide / 20% silica antiblock masterbatch produced dart impact of 310–360 g per ASTM D1709-22 Method A, Elmendorf tear strength of 1.77–2.06 N machine direction and 2.55–2.94 N transverse direction per ASTM D1922-23, and 1% secant modulus of 190–210 MPa per ASTM D882-18. Bubble stability without LDPE addition deteriorates above blow-up ratio 3.0; the resulting bubble chatter and edge instability are traceable to the low melt strength of linear ethylene-octene copolymers and are corrected by either reducing stalk height to 8–9 die diameters or maintaining 18–20 wt% LDPE in the bubble. Compliance for industrial sacks used with fertilizer and chemical granules defaults to EU Packaging Directive 94/62/EC Article 11 heavy metal limits with cadmium, hexavalent chromium, lead, and mercury sum ≤ 100 mg/kg, while U.S. FDA 21 CFR § 177.1520(c) applies only when the entire additive package is selected from the same regulatory clearance. End products produced with this formulation include plastic resin shipping sacks, FIBC inner liners, and woven bag liners where a 75–100 μm coextruded inner ply is sealed ultrasonically at 20–30 kHz and 0.2–0.4 s dwell.

    How Does DOWLEX IP-2580 Perform Under Silage Effluent and UV Exposure in Cast Clamp Films?

    Silage clamp films require anaerobic sealing against lactic acid, acetic acid, and ammonia from fermentation, combined with 9–18 month outdoor weathering. DOWLEX IP-2580 is let down with a carbon black masterbatch at 6–7 wt% total film weight, delivering 2.5–3.0 wt% carbon black and 0.30–0.50 wt% HALS on total formulation; the resulting black film is cast at 45–60 μm thickness on a 2.2 m cast-film line with a 0.7 mm die gap, 28–32 °C polished roll temperatures, and melt temperature 235–245 °C. The higher melt temperature is required to disperse the carbon black carrier and reduce gel tails from the masterbatch carrier resin, but it narrows the thermal window because LLDPE melt strength declines sharply above 245 °C. Screen pack differential pressure on the extruder is kept below 180 bar at 150 kg/h using a 40/60/100 mesh three-screen pack; a pressure rise above 220 bar signals carbon black agglomeration and requires a screen change. Mechanical acceptance for silage clamp film per EN 13207:2018 requires tear resistance and elongation sufficient to survive clamp management without punctures; field failures are typically split propagation from clamp weights rather than UV embrittlement, so transverse Elmendorf tear values are specified above 2.5 N per ASTM D1922-23. Carbon black masterbatch must be pre-dried at 65 °C for 4 h when warehouse relative humidity exceeds 55%; residual moisture above 0.15 wt% in the masterbatch causes pinholes that reduce dart impact by 30–40% and produce visible film defects at the clamp shoulder. Compliance is maintained with EU No 10/2011 overall migration ≤ 10 mg/dm² and REACH SVHC restrictions, but finished film is not automatically approved for direct forage contact under organic certifier standards because carbon black loadings exceed some permitted inert-ingredient thresholds.

    Typically, five-layer cast-film lines running at 280–320 m/min use DOWLEX IP-2580 as the core toughness layer in stretch-hood film for pallet unitization of bagged cement and bulk construction materials. A typical A/B/C/B/A structure places metallocene LLDPE or ethylene-octene plastomer in the A cling layers at 10–15 wt%, DOWLEX IP-2580 in the B sub-skin and C core layers at 60–70 wt%, EVA with 18% vinyl acetate content at 10–15 wt%, and polyisobutylene cling additive at 2–4 wt% in the outer A layers. The cast-film die gap is set at 0.5–0.7 mm, the air gap at 5–8 mm, and melt temperature at 220–240 °C; high-speed edge pinning is required to prevent edge weave above 250 m/min. Film thickness is 60–120 μm, with thinner gauges used for lightweight shrink-hood applications and heavier gauges for abrasive cement bags. After prestretching to 60–85%, the film must retain sufficient elastic recovery to prevent pallet load collapse during road transport; converter acceptance thresholds require retained force above 42 N/100 mm after 85% prestretch per ISO 527-3:2018 and puncture resistance above 250 N per ASTM D5748-19 at 80 μm. Cling force measured per ASTM D5458-17 at 72 h after film winding is typically 180–260 gf; the same film measured within 2 h of winding can be 30–50% higher due to PIB migration kinetics, so quarantine-time protocols are mandatory before converting. End products include pallet hoods for cement, brick, timber, and beverage bottle unitization where the film is applied by rotary arm stretch-hood machines with pre-stretch ratios between 60% and 90%.

    When Extrusion Coating onto Woven Polypropylene Exceeds 180 m/min

    Extrusion coating of woven polypropylene sacks with DOWLEX IP-2580 at line speeds above 180 m/min requires suppression of draw resonance and neck-in through melt dilution. A 70/30 wt% blend of DOWLEX IP-2580 and LDPE with melt flow index of 0.3 g/10 min is processed through a 90 mm single-screw extruder at 285–320 °C, with a 200–250 mm air gap and coating weight of 20–30 g/m². Increasing line speed beyond 250 m/min without raising melt temperature produces edge weave and draw resonance bands at 15–25 mm intervals in the coating; the instability is visible as alternating thick/thin transverse bands and reduces seal integrity at sack bottom folds. Ozone treatment of the melt surface immediately before the chilled roll nip is set at 3–5 g/h per metre of die width to generate carboxyl functionality and raise adhesion to the woven polypropylene substrate; adhesion of the coating is evaluated by 180° peel tests requiring cohesive failure in the polyethylene rather than adhesive peeling at the interface. Neck-in on a 1.6 m die is typically 12–18 mm per side for this blend at 25 g/m², and edge bead trimming is necessary above 25 g/m². Laminated woven sacks meet burst strength requirements for fertilizer and salt packaging when the coating weight is 20 g/m² and the woven substrate grammage is 70–90 g/m². Compliance for food contact of coated paper or paperboard uses FDA 21 CFR § 176.170(c) when the coated paper is intended for aqueous and fatty food packaging, but woven polypropylene chemical sacks generally fall under EU Packaging Directive 94/62/EC and REACH rather than food-contact rules. Residence time above 4 min at 320 °C causes oxidative gel formation and must be controlled by automatic purging with LDPE at 2–3 kg per shutdown; otherwise gels appear in the coating as pinholes.

    In high-speed vertical form-fill-seal lines for IQF vegetables, a sealant layer of 30 μm within an 80 μm three-layer blown film is formulated from 20–25 wt% DOWLEX IP-2580, 60–65 wt% metallocene LLDPE with melt flow index 1.0 g/10 min, and 10–15 wt% LDPE. The structure is blown on a 200 mm die with 1.8 mm die gap, melt temperature 205–215 °C, and blow-up ratio 2.0–2.5. The sealant layer provides cold-temperature impact resistance down to -50 °C under ASTM D1790-21 and a seal initiation temperature of 85–95 °C at 1.0 N/mm² sealing pressure. Heat seal strength measured per ASTM F88-21 reaches 3.0–4.5 N/25 mm when sealed at 110 °C and 0.5 s dwell, which is compatible with cycle times of 80–120 packages/min on vertical form-fill-seal machines. The grade is cleared within the film structure under FDA 21 CFR § 177.1520(c) and EU No 10/2011 overall migration ≤ 10 mg/dm², provided the slip and antiblock concentrates also meet those requirements. The operational boundary is hot-fill exposure above 70 °C: the film softens and seal creep occurs under top-load stress, so the structure is unsuitable for retortable pouches or hot liquid filling.

    Temporary containment liners for construction-site dewatering and secondary chemical containment are produced by extrusion lamination of DOWLEX IP-2580 onto woven high-density polyethylene scrim at 30–50 g/m² per side, yielding total sheet thickness of 300–400 μm. The process uses a 100 mm extruder at 270–300 °C, a 0.8 mm slot die, and a 150–200 mm air gap; the scrim is preheated with infrared banks to 40–50 °C to improve interlayer adhesion without solvent primers. The LLDPE coating provides puncture resistance against angular gravel and concrete rubble; completed liners are tested for hydrostatic resistance, and carbon-black-free layers are used for visible leak detection. Welding of on-site seams is performed by hot-wedge welding at 350–400 °C with 1.0 m/min travel speed; lap shear strength of the welded seam is specified above 80% of parent sheet yield strength per ASTM D6392-12. The material is not intended for long-term UV-stabilized service; exposed installations require site-specific UV additive packages and must be covered within 30 days unless carbon black at 2.5–3.0 wt% is included. Compliance is limited to non-food industrial use under REACH and EU Waste Framework Directive 2008/98/EC where temporary containment films are managed as non-hazardous plastic waste.

    Free Quote

    Competitive Dow DOWLEX™ IP-2580 Linear Low Density Polyethylene prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ IP-2580 Linear Low Density Polyethylene is an injection-molding-grade polyolefin produced by solution polymerization. The material consists of a linear ethylene backbone with controlled short-chain branching; this structure separates it from autoclave and tubular LDPE, where both short- and long-chain branching are present, and from HDPE, where branching is minimal. Manufacturer technical data list a melt flow rate of 25 g/10 min at 190 °C under a 2.16 kg load according to ASTM D1238, and a solid density of 0.924 g/cm³ according to ASTM D792. The equivalent melt flow rate test is described by ISO 1133-1:2022. These values place DOWLEX IP-2580 in the high-flow LLDPE injection molding segment, selected when a thin-wall part must be filled at moderate clamp force without sacrificing low-temperature ductility.

    Density of 0.924 g/cm³ corresponds to a crystalline weight fraction of approximately 45% to 50%, depending on thermal history and comonomer content. The melting peak is typically observed between 120 °C and 126 °C by differential scanning calorimetry. This crystalline fraction is lower than that of HDPE, which is why the flexural modulus is reduced but the environmental stress crack resistance is improved. Compared with a general-purpose LDPE injection grade, DOWLEX IP-2580 typically exhibits higher crystallinity and a more linear backbone. This produces a higher flexural modulus than LDPE of the same density, greater resistance to environmental stress cracking, and a narrower melting range. The melt index of 25 g/10 min is markedly higher than that of film-grade LLDPE, which often ranges from 0.5 g/10 min to 2.0 g/10 min. The high melt index reduces apparent viscosity under injection shear rates, but it also reduces melt strength and hot-tack; therefore DOWLEX IP-2580 is not intended for blown film or pipe extrusion where drawdown and bubble stability are critical.

    Within the DOWLEX LLDPE injection-molding range, DOWLEX IP-2580 is distinguished by the combination of high melt flow and low-to-mid density. A melt index of 25 g/10 min reduces injection pressure compared with a 10 g/10 min grade of similar density, but it may reduce tensile strength and environmental stress crack resistance because of lower molecular weight. A higher-density LLDPE injection grade at 0.935 g/cm³ to 0.940 g/cm³ provides greater stiffness and lower shrinkage, but the lower density of IP-2580 improves impact and ESCR at subambient temperatures. This trade-off is the central reason for grade selection in injection molding.

    What Processing Variables Govern Flow Length and Shrinkage Compensation?

    The linear backbone and short-chain branching of DOWLEX IP-2580 influence shear thinning. Under injection-molding shear rates between 1000 s⁻¹ and 10000 s⁻¹, the material shows less shear thinning than LDPE with long-chain branching. The result is a wider processing window for filling but a greater sensitivity to melt temperature changes. Mold flow simulation requires viscosity data measured by capillary rheometry according to ISO 11443:2021, not a single-point melt index value, to predict filling pressure in complex tools.

    Injection molding equipment for DOWLEX IP-2580 should use a general-purpose polyolefin screw with an L/D ratio of 18:1 to 24:1 and a compression ratio of 2.5:1 to 3.5:1. Melt temperature is generally set between 200 °C and 250 °C. At melt temperatures below 180 °C, unmelted pellets and flow lines may appear in thin sections; above 260 °C, thermo-oxidative degradation may cause yellowing, odor, and a measurable loss of tensile elongation. Mold temperatures between 10 °C and 40 °C are adequate for most unfilled parts, although high-gloss surfaces may require mold temperatures up to 60 °C. Back pressure between 0.5 MPa and 1.5 MPa is recommended to homogenize the melt without creating excessive shear heating. Higher back pressure above 2.0 MPa increases melt temperature and residence time, and may shift the melt flow rate upward during repeated cycles.

    Injection speed is a more sensitive variable for DOWLEX IP-2580 than for lower-flow LLDPE grades because the high melt index promotes rapid cavity filling. Thin-wall containers with nominal wall thickness between 0.8 mm and 2.0 mm are frequently filled in 0.3 s to 0.8 s to maintain a uniform melt front. Excessively high speed can produce jetting, weld line weakness, and gate blush; excessively low speed permits premature freeze-off and short shots. Holding pressure should be set to compensate for volumetric shrinkage until gate seal. In a hot-runner tool with valve gate diameter of 1.0 mm, gate seal time may be less than 2 s; after gate seal, additional holding pressure does not transfer to the cavity and only increases clamp force demand.

    Shrinkage behavior in DOWLEX IP-2580 is governed by the cooling rate and the development of crystalline domains. Differential scanning calorimetry of 0.924 g/cm³ LLDPE typically shows a peak crystallization temperature between 105 °C and 112 °C. Mold shrinkage is generally 1.5% to 2.5% in the flow direction and 1.0% to 2.0% in the transverse direction; the actual value depends on part thickness, gate geometry, mold temperature, and packing pressure. Lower mold temperatures reduce cycle time but increase shrinkage anisotropy and may produce internal voids in thick sections. When wall thickness exceeds 3.0 mm, a lower injection speed and longer holding time are required to avoid sink marks and microvoiding.

    Property Matrix Against LDPE and HDPE Injection Grades

    Comparative property data for DOWLEX IP-2580 are summarized in the following matrix. Values are typical ranges for standardized injection-molded test specimens; grade-specific data should be confirmed against the manufacturer’s technical datasheet because compounding, color, and molding conditions alter the final values.

    PropertyDOWLEX IP-2580 typical rangeLDPE injection gradeHDPE injection gradeTest method
    Density0.924 g/cm³0.917–0.930 g/cm³0.940–0.970 g/cm³ASTM D792
    Melt index25 g/10 min2–30 g/10 min2–30 g/10 minASTM D1238, 190 °C/2.16 kg
    Tensile yield strength10–13 MPa8–12 MPa20–30 MPaISO 527-2
    Flexural modulus200–300 MPa150–250 MPa800–1400 MPaISO 178
    ESCRHigher than HDPE; typically >500 h in 10% Igepal CO-630 at 50 °CVariable; often <100 hDensity-dependent; often <200 hASTM D1693 Condition B

    The data in the matrix show that DOWLEX IP-2580 occupies an intermediate position between flexible LDPE and rigid HDPE. The flexural modulus of 200 MPa to 300 MPa is sufficient for many structural thin-wall parts but is below the 800 MPa to 1400 MPa range typical of HDPE injection grades. Environmental stress crack resistance under ASTM D1693 is generally superior to HDPE and to many LDPE compounds because the linear backbone and controlled short-chain branching resist slow crack propagation in the presence of surface-active media. The exact failure time is dependent on molded-in stress and test conditions; published data for DOWLEX IP-2580 in this specific configuration are limited, but the DOWLEX LLDPE family is used in detergent and surfactant packaging for this reason.

    Thin-wall food storage containers, freezer-grade lids, beverage caps, and small appliance housings are established application areas for high-flow LLDPE injection grades. In a multicavity cold-runner tool with 8 cavities and a total projected area of 1200 cm², a machine with clamp force of 1800 kN can generally fill parts from DOWLEX IP-2580 at melt temperature 230 °C and mold temperature 25 °C, provided the sprue and runner system is sized for the melt index. This is a typical production configuration; actual clamp force must be calculated from part geometry, runner layout, and melt pressure.

    Freezer-grade behavior is a distinguishing requirement. LLDPE grades such as DOWLEX IP-2580 are selected because they retain impact ductility at -20 °C and often at -40 °C. Notched impact testing by ISO 179-1 or ASTM D256 at subambient temperatures is used to compare lots. Low-temperature embrittlement is a known failure mode for LDPE and some high-density resins; the ductile-to-brittle transition of LLDPE is generally lower than that of LDPE of equivalent density, which reduces freezer-service failure.

    In closure applications, the resin must resist environmental stress cracking from oils, detergents, and surface-active agents. ESCR testing under ASTM D1693 with 10% Igepal CO-630 at 50 °C is a primary quality-control method. Parts molded with high residual stress from overpacking or excessive injection speed may fail before the intrinsic ESCR of the material is reached, which is why processing discipline is as important as material selection.

    Comparative assessment against metallocene-catalyzed LLDPE injection grades shows that DOWLEX IP-2580 may exhibit a broader molecular weight distribution, which improves melt strength and process stability but can reduce clarity and gloss relative to metallocene single-site resins. The broader distribution also permits lower melt temperatures and reduced shear heating in large hot-runner systems. Conversely, metallocene grades may offer improved organoleptics and lower hexane extractables in food-contact uses; the selection between DOWLEX IP-2580 and a metallocene LLDPE should therefore be based on the specific sensory and migration limits of the finished article.

    Regrind addition of up to 20% by mass is generally tolerated in non-food and non-cosmetic parts, provided the regrind is dry and free of contamination. For food-contact articles, reuse of sprues and runners from an internal closed-loop process may be permitted if the European or FDA regulatory conditions for post-industrial rework are met. Higher addition levels can reduce impact strength and increase color variability; a property retention test should be executed under the relevant ISO or ASTM standard before production release.

    Compliance Requires Finished-Article Verification Under Specific Migration Protocols

    DOWLEX IP-2580, when used in food-contact applications, falls under olefin polymer provisions. The resin is typically referenced to FDA 21 CFR 177.1520 in the United States and Commission Regulation (EU) No 10/2011 in the European Union. These citations apply to the base polymer; finished articles must still meet overall migration limits, specific migration limits for additives and monomers, and organoleptic requirements. The overall migration limit under EU Regulation 10/2011 is 10 mg/dm² of food-contact surface area. In practice, compliance is demonstrated on the molded article, not on the pellet alone.

    Regulatory instrumentScopeRelevant numerical limit or citation
    FDA 21 CFR 177.1520Olefin polymers for food-contact useEnd-testing for specific migration under 21 CFR 177.1520(c)
    EU Regulation (EU) No 10/2011Plastic food-contact materialsOverall migration limit 10 mg/dm²
    REACH Regulation (EC) No 1907/2006Registration and authorizationPolymers exempt under Article 2(9); monomers/additives registered
    RoHS Directive 2011/65/EUElectrical and electronic equipmentLead 1000 mg/kg, cadmium 100 mg/kg, mercury 1000 mg/kg

    For non-food applications, REACH registration obligations do not apply to the polymer itself under Article 2(9), but imported articles above 1 metric ton/year may require registration or notification for intentionally released substances. The base polyolefin is not considered a persistent organic pollutant and is generally outside the RoHS restricted substance list, but colors and additives containing lead, cadmium, mercury, or hexavalent chromium must be controlled at the compound level.

    DOWLEX IP-2580 is not supplied with a UV stabilization package as a standard injection grade. Outdoor service requires a UV stabilizer masterbatch, with accelerated weathering verification by ASTM D2565 or ISO 4892-2. Unstabilized thin sections exposed to xenon-arc irradiance can lose more than 50% of tensile elongation after 1000 h, depending on irradiance, temperature, and part thickness. Direct contact with strong oxidizing acids, aromatic hydrocarbons, and chlorinated solvents is not recommended. Continuous contact with aggressive surfactants at elevated temperature can initiate environmental stress cracking if molded-in stress is high, particularly at gate regions and sharp corners.

    Moisture is rarely a bulk concern for polyethylene, but condensation on cold pellet surfaces can create splay and surface defects. Pellets stored at relative humidity above 60% should be predried at 60 °C for 1 h in a desiccant dryer before processing. Higher drying temperatures above the Vicat softening point may cause pellet agglomeration. Hopper loaders and feed throat openings should be inspected because fines and streamers generated during transport can affect melt homogeneity and cause occasional nozzle blockage.

    Top