Dow Dowlex 2688g Lldpe

Dow Dowlex™ 2688G LLDPE

    • Product Name: Dow Dowlex™ 2688G LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 631067
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melt Flow Ratio I21 I2 30
    High Load Melt Index 190 C 21 6 Kg 25.5 g/10 min
    Melting Point 122 °C
    Vicat Softening Point 98 °C
    Brittleness Temperature < -70 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 38 MPa
    Ultimate Elongation 800 %
    Flexural Modulus 1 Secant 240 MPa
    Dart Drop Impact 150 g
    Elmendorf Tear Strength Md 300 g
    Elmendorf Tear Strength Td 500 g
    Haze 12 %
    Gloss 45 50
    Coefficient Of Friction 0.20

    As an accredited Dow Dowlex™ 2688G LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Dowlex™ 2688G LLDPE is supplied in 25 kg moisture-resistant polyethylene bags, 55 bags per pallet (1,375 kg).
    Container Loading (20′ FCL) 20′ FCL holds 18 MT of Dow Dowlex™ 2688G LLDPE, supplied in 25 kg bags, loaded and secured for export.
    Shipping Dow Dowlex™ 2688G LLDPE is typically shipped as non-hazardous polyethylene resin pellets in 25 kg bags, octabins, or bulk trucks/railcars. Keep containers dry, sealed, and away from heat, sunlight, and contamination during transit. No special dangerous-goods placarding is required; follow local transport and storage regulations.
    Storage Store Dow Dowlex™ 2688G LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep containers tightly closed to prevent moisture and contamination. Avoid contact with strong oxidizers. Maintain stable ambient temperatures, protect from physical damage, and follow the manufacturer’s SDS and local regulations. Do not store near food or feed.
    Shelf Life Shelf life: 24 months if stored unopened in original packaging, cool, dry, ventilated, away from sunlight, heat, moisture, and contaminants.
    Application of Dow Dowlex™ 2688G LLDPE

    Flat-die sheet extrusion lines producing flexible geomembrane liners for heap leach pads, evaporation ponds, and landfill bottom barriers operate with DOWLEX 2688G as the primary carrier resin when the finished sheet must satisfy GRI-GM17 LLDPE geomembrane specifications and EPA 40 CFR Part 258, Subpart D leakage-barrier requirements. In this downstream configuration the resin is not pre-dried unless moisture exposure has exceeded 0.05 wt% water; when ambient relative humidity exceeds 60%, pre-drying at 70–80°C for 4 h in desiccant-hopper dryers is used to prevent carbon black masterbatch agglomeration and surface pitting on the polished roll stack. The extrusion formulation consists of 96.5–98.0 wt% DOWLEX 2688G, 2.0–3.5 wt% carbon black masterbatch at 40–50% carbon black concentration, and 0.2–0.5 wt% hindered amine light stabilizer-antioxidant masterbatch. The lower 2.0 wt% carbon black boundary is set by retained tensile properties after xenon-arc exposure under ISO 4892-2:2013; the upper 3.5 wt% boundary is set by loss of tensile elongation below the GRI-GM17 minimum break elongation and rising melt viscosity at elevated die temperatures. Production-scale single-screw extruders with 90–120 mm screw diameter and 30:1 L/D run barrel set points of 180–230°C, die temperature 210–225°C, and polished roll stack temperature 60–85°C at pull speeds of 3–12 m/min. Melt temperatures above 232°C increase gel formation and die-lip deposit accumulation, while melt temperatures below 195°C raise melt pressure and reduce carbon black microdispersion below the required rating under ISO 18553 Method A. Sheet thickness is 1.0–2.5 mm, width up to 8 m, with single- or double-sided texturing applied by embossing rolls. Mechanical verification uses ASTM D6693/D6693M-20 for tensile properties, ASTM D4833/D4833M-07 for puncture, ASTM D1004-13 for tear, and ASTM D1693-15 for environmental stress-crack resistance. Finished product types include 1.5 mm and 2.0 mm smooth or textured geomembrane panels fabricated into landfill caps, mining heap leach pads, and secondary containment basins.

    What Limits Dart Impact Retention in Heavy-Duty Sack Film Containing 10–20 wt% Post-Industrial Recyclate?

    Blown film lines converting DOWLEX 2688G into heavy-duty industrial sacks for fertilizers, polymer pellets, and construction chemicals absorb post-industrial LLDPE recyclate at 10–20 wt% without failing 49 CFR Part 178 drop-impact requirements only when the recyclate melt index remains within ±0.2 g/10 min of the virgin resin and dust content remains below 500 ppm. Formulation practice for 80–120 µm film uses 75–85 wt% DOWLEX 2688G, 10–20 wt% dried post-industrial LLDPE reclaim, 5–10 wt% low-density polyethylene for bubble stability, and 1.5–2.5 wt% processing aid masterbatch containing fluoroelastomer at 2–3% active content. The processing aid is critical at die gap 1.2–1.8 mm because high-output 250–400 mm spiral mandrel dies exhibit melt fracture when the blend viscosity mismatch exceeds 15%. Compliance is verified by ASTM D1709-16a dart impact, which should remain above 200 g for 80 µm film, by ASTM D4272/D4272M for retained impact after recyclate addition, by ASTM D638-14 for tensile properties, and by ASTM D1790-21 for low-temperature brittleness at -30°C. Three-layer coextrusion lines with 50–70 mm screw diameters and 30:1 L/D operate at blow-up ratio 2.2–2.8:1, frost line height 600–900 mm, die temperature 190–210°C, and winding tension 5–10 N/100 mm of film width. Finished product types include gusseted heavy-duty sacks, valve bags, hazardous material inner liners, and FIBC liner films.

    Silage preservation systems requiring oxygen transmission rate below 4,500 cm³/(m²·day·atm) at 23°C and 0% RH use DOWLEX 2688G in coextruded multi-layer covers and bale wrap skins where the film must resist puncture from corn stover and withstand UV exposure for 12–24 months. The formulation for pit covers contains 92.0–95.0 wt% DOWLEX 2688G, 3.0–5.0 wt% UV-stabilized white masterbatch, 1.0–2.0 wt% carbon black masterbatch, and 1.0–2.0 wt% slip-antistatic masterbatch; bale wrap skin layers omit carbon black and reserve the tackifier for the cling layer at 4.0–6.0 wt% polyisobutylene-based masterbatch, not in the DOWLEX 2688G outer layer. Compliance is verified by EN 13206:2017 for agricultural thermoplastic films, ISO 527-3:2018 for tensile properties, ASTM D3985-17 for oxygen transmission, and ASTM D1004-13 for tear resistance. Five-layer blown film lines with 50–70 mm extruder screw diameters, 250–400 mm die diameters, blow-up ratio 2.0–2.5:1, melt temperature 200–220°C, and frost line height 700–900 mm produce thicknesses of 25–45 µm for bale wrap and 150–250 µm for pit covers. At thickness below 25 µm, field puncture failure under corn-stubble contact becomes the limiting boundary; converters therefore shift to cast cling-wrap constructions or increase outer-layer thickness rather than adding antiblock masterbatch to the DOWLEX 2688G skin layer. Finished product types include black-white pit cover sheet, silage bag film, and 750 mm wide bale wrap rolls in 1,500 m lengths.

    Extrusion Coating of Helical-Seam Spiral Steel Pipe with Electrostatic Epoxy Primer

    Crosshead annular die extrusion lines for three-layer polyethylene coatings on spiral-welded steel pipe use DOWLEX 2688G in the outer topcoat layer because its low-temperature flexibility allows pipe bending after coating without cracking at -40°C when the total coating thickness is 1.8–4.0 mm. The coating system consists of an epoxy primer layer applied at 40–80 µm, an adhesive copolymer tie layer at 150–250 µm, and a DOWLEX 2688G topcoat at 1.5–3.8 mm; the topcoat formulation is 96.0–98.0 wt% DOWLEX 2688G and 2.0–4.0 wt% carbon black-UV stabilizer masterbatch, while the tie layer is an ethylene-butyl acrylate or maleic anhydride-grafted polyethylene distinct from the topcoat compound. Coated pipe complies with DIN 30670:2012, ISO 21809-1:2018, and NACE SP0394-2019; peel-strength and cathodic disbondment performance are evaluated by the relevant ISO 21809-1 procedures. Steel pipe is blast-cleaned to Sa 2½ near-white per ISO 8501-1, preheated to 170–220°C, epoxy primer sprayed electrostatically, and the DOWLEX 2688G topcoat applied via sheet wrap from a 90 mm single-screw extruder with 30:1 L/D at melt temperature 210–230°C, pressure-roll pressure 0.4–0.8 MPa, and water quench at 20–35°C; line speeds range from 1.5 to 4.0 m/min depending on wall thickness. Operating boundaries are defined by maximum service temperature 60°C; above this threshold topcoat softening reduces peel adhesion and cathodic disbondment performance. Finished product types include anti-corrosion-coated line pipe for oil and gas transmission, water transmission, and offtake piping in diameters of 508–1,220 mm.

    When Canal Liner Flat-Die Extrusion Requires Ambient Cast Film Quenching for Irrigation Infrastructure

    Thin-gauge canal liner sheet for irrigation water conveyance uses DOWLEX 2688G when the finished liner must withstand puncture from gravel embedment and remain installable at temperatures below 0°C; in this process, ambient cast film quenching at 20–30°C is used instead of heated chill rolls to lower crystallinity and improve tear propagation resistance. The formulation contains 96.5–98.0 wt% DOWLEX 2688G, 2.0–3.0 wt% carbon black masterbatch, and 0.5 wt% antioxidant-processing stabilizer masterbatch; no post-consumer recyclate is added in this specification because canal liner fusion seams must retain long-term weld strength under ASTM D6392/D6392M. Compliance is verified by GRI-GM17, ASTM D4833/D4833M-07 for puncture, ASTM D1004-13 for tear, and ASTM D5884/D5884M for tear propagation resistance. Flat-die extrusion lines with 2,000–3,500 mm die widths, 0.8–2.0 mm die gaps, roll stack temperatures 50–70°C, air knife pressure 0.2–0.5 MPa, and line speeds 10–30 m/min produce sheet at 0.5–1.5 mm thickness. Ambient quenching at 20–30°C is the critical control point; when quench air temperature exceeds 30°C, cooling rate decreases, crystallinity increases, and edge curl becomes measurable on 1.0 mm sheet, causing fusion seam insertion failures during panel installation. Finished product types include prefabricated canal liner panels in 1.0 mm and 1.5 mm thickness, reservoir covers, modular water storage lining systems, and transition mats for irrigation structures.

    Free Quote

    Competitive Dow Dowlex™ 2688G LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2688G LLDPE is a solution-polymerised ethylene–octene linear low-density polyethylene supplied as pelletised feed for injection moulding and compounding operations. Trade literature characterises the grade by a nominal density of 0.941 g/cm³ when tested according to ISO 1183-1:2019 and a nominal melt flow rate of 7.5 g/10 min at 190 °C/2.16 kg when tested according to ISO 1133-1:2022. These figures are typical values rather than contractual release limits; batch-level certificates of analysis remain the controlling specification. The combination of density above conventional film-grade LLDPE and a melt flow rate above conventional extrusion grades places DOWLEX™ 2688G in a processing class where flow length, mould filling, and solid-state toughness must be evaluated together. As an ethylene–octene copolymer, the resin carries short-chain branching that disrupts crystallinity relative to HDPE while retaining a predominantly linear backbone. This architecture reduces long-chain branching effects seen in high-pressure LDPE and supports narrower melt-temperature control during injection processing.

    What Distinguishes DOWLEX™ 2688G from Film-Grade LLDPE and High-Density Polyethylene Injection Resins?

    The principal difference is the density–melt flow rate balance. Film-grade LLDPE resins are commonly supplied at density 0.918–0.922 g/cm³ and melt flow rate 0.5–2.0 g/10 min, favouring bubble stability, dart impact, and tear resistance in blown-film lines. Injection-grade HDPE resins, by contrast, are typically supplied at density 0.950–0.965 g/cm³ with melt flow rates from 5 g/10 min upward. DOWLEX™ 2688G occupies an intermediate density position at 0.941 g/cm³ while offering a mould-filling melt flow rate of 7.5 g/10 min. The practical consequence is that thin-section moulding operations obtain lower injection pressure than with film-grade LLDPE, while the finished article retains higher low-temperature ductility than many HDPE grades of comparable flow.

    Tensile and flexural data illustrate the trade-off. Published typical values for DOWLEX™ 2688G include tensile stress at yield of 23 MPa when tested per ISO 527-2:2012 and flexural modulus of 1,030 MPa when tested per ISO 178:2019. Film-grade LLDPE often exhibits tensile yield stress nearer 10–15 MPa and flexural modulus below 600 MPa, reflecting lower crystalline content. HDPE injection grades may reach tensile yield stress above 25 MPa and flexural modulus above 1,200 MPa, but environmental stress-crack resistance under constant strain can decline as density rises. DOWLEX™ 2688G therefore offers a mid-range stiffness profile while preserving sufficient chain mobility for stress relaxation in slow-loading applications.

    Typical property values for DOWLEX™ 2688G LLDPE and comparative resin classes
    PropertyDOWLEX™ 2688GFilm-grade LLDPEInjection-grade HDPE
    Density (ISO 1183-1:2019)0.941 g/cm³0.918–0.922 g/cm³0.950–0.965 g/cm³
    Melt flow rate (ISO 1133-1:2022)7.5 g/10 min0.5–2.0 g/10 min5–20 g/10 min
    Tensile stress at yield (ISO 527-2:2012)23 MPa10–15 MPa24–31 MPa
    Flexural modulus (ISO 178:2019)1,030 MPa300–600 MPa1,100–1,500 MPa
    Vicat softening temperature (ISO 306:2022)122 °C95–110 °C125–130 °C

    Environmental stress-crack resistance is typically assessed by ASTM D1693-15. Published data for DOWLEX™ 2688G across all test conditions is limited, so comparative ranking should be generated on the actual moulded wall thickness and surface condition of interest rather than inferred solely from density.

    On a general-purpose single-screw injection unit with an L/D ratio of 24:1, a practical starting barrel profile is 190–220 °C from feed throat to nozzle, with mould temperature held between 15 °C and 40 °C. Screw back pressure in the range of 0.5–1.5 MPa is sufficient to homogenise melt temperature without excessive shear heating. The melt temperature should not exceed 270 °C; above this limit, oxidative chain scission can shift melt flow rate upward, produce surface splay, and increase odour generation. Screw speeds of 50–120 min⁻¹ are typical for unfilled LLDPE, but the actual value should be matched to shot size and plastication time. Because the material has no hydrolysable backbone, predrying is not mandatory in normal closed storage. However, when pellets are stored at relative humidity above 60% and transferred into a warm hopper, surface condensation can introduce moisture-related surface defects. In that case, dehumidified hopper drying at 60 °C for 1 hour is generally adequate.

    Additive compatibility follows standard polyolefin practice. Colour concentrates based on polyethylene carriers disperse readily, but carrier melt flow rate should be within ±30% of the base-resin value to avoid localised viscosity mismatch and flow marks. Peroxide masterbatches intended for vis-breaking should not be added without controlled pilot-scale verification, because uncontrolled peroxide decomposition in an already high-flow LLDPE can exceed the upper melt flow rate specification and create gel clusters on the mould surface.

    When Thin Sections and Short Cycle Times Demand a High-Flow Ethylene–Octene Matrix

    DOWLEX™ 2688G is suited to injection-moulded articles where wall thickness is below 2 mm and cycle time is controlled by filling pressure rather than by cooling only. The 7.5 g/10 min melt flow rate allows lower injection pressure at a given flow length compared with a 1.0 g/10 min film-grade LLDPE. In practice, this becomes visible in cavity-pressure traces as a reduced pressure peak and shorter fill time when the same tool is run at constant barrel temperature. Specific flow-length spiral data for DOWLEX™ 2688G is not reproduced here because published data for this specific configuration is limited; spiral-flow evaluation should be conducted on the production tool using the actual gate design and flow-channel thickness.

    Gate freeze is influenced by the solidification rate of the semicrystalline structure. The nominal density of 0.941 g/cm³ gives a crystalline fraction high enough to accelerate gate freeze relative to lower-density LLDPE, so gate diameter and holding-pressure duration must be set to avoid premature gate seal before volumetric shrinkage is fully compensated. Mould shrinkage is typically within the range accepted for moderate-density polyethylene, but published absolute values for DOWLEX™ 2688G vary with injection speed, packing pressure, and wall thickness. A conservative tool-design assumption for isotropic shrinkage is 1.5–2.5%, with verification on a prototype cavity before final tool steel is cut.

    Melt Rheology, Gate Freeze, and Mould Shrinkage in Unfilled LLDPE

    The melt rheology of DOWLEX™ 2688G shows the shear-thinning behaviour common to linear low-density polyethylene. Compared with LDPE of similar melt flow rate, the grade exhibits lower melt strength and lower extrudate swell, which can reduce die drool in hot-runner injection systems but can also limit parison stability if the material is improperly substituted into continuous blow moulding. The lower melt strength is a direct structural consequence of the absence of long-chain branching. In injection moulding, the same characteristic improves shear transmission through gates and reduces melt fracture at high shear rates. In extrusion coating or blow moulding, however, the material is not a direct drop-in replacement for LDPE where melt tension is a processing requirement.

    Because neat LLDPE is unpolar and electrically insulating, surface preparation for printing, bonding, or painting generally requires corona discharge or flame treatment. The treatment window and dyne level should be specified for the final application; 38–42 mN/m is a commonly cited target for adhesion, but the required level depends on the ink or adhesive system. The grade is not inherently antistatic, and static charge dissipation in dry conveying lines may require external ionisation bars.

    For injection moulding of thin-walled containers and industrial packaging, the combination of high flow and intermediate density reduces cycle time relative to film-grade LLDPE but increases stiffness relative to lower-density LLDPE. Published data for specific impact performance at sub-zero temperatures is limited; instrumented puncture testing per ISO 6603-2:2023 is recommended when the part is expected to survive drop impact below −20 °C.

    Regulatory status for food-contact use is not inferred from the resin type alone. DOWLEX™ 2688G is typically positioned as an olefin polymer falling under FDA 21 CFR 177.1520 in the United States, provided the final article is used under the conditions of use described in 21 CFR 176.170(c). For the European Union, compliance with Regulation (EU) No 10/2011 and its subsequent amendments must be verified against the specific migration limits applicable to the final food simulant and contact condition. REACH obligations arise under Regulation (EC) No 1907/2006, and RoHS applicability is assessed under Directive 2011/65/EU. These standards are regulatory frameworks, not product certifications; a supplier-issued compliance certificate for the specific lot and grade is required before use in regulated food-contact or electrical and electronic applications.

    Lower Melt Strength than LDPE, Higher Environmental Stress-Crack Resistance than HDPE

    The operational boundaries of DOWLEX™ 2688G follow from its molecular architecture. The material should not be processed above 270 °C for extended residence times, and residence time at melt temperature should be kept below 10 minutes when interruptions occur. Purge with a general-purpose HDPE or LDPE before shutdown and after colour changes avoids cross-contamination in hot-runner systems. Storage should be in closed, dry conditions away from direct ultraviolet exposure. If bags are opened and exposed to outdoor storage for prolonged periods, oxidative embrittlement can occur before the resin is melted, and the melt flow rate may drift outside the declared range. The resin is not specifically formulated for long-term hot-water pressure pipe service, and published data for this specific configuration is limited. For applications involving continuous exposure to aggressive surfactants, organic media, or sustained flexural strain, end-use testing under the actual chemical environment is required rather than extrapolation from standard ESCR specimens.

    Top