Dow Dowlex 2620 Lldpe

Dow Dowlex™ 2620 LLDPE

    • Product Name: Dow Dowlex™ 2620 LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 696160
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer 1-Octene
    Density 0.920 g/cm³
    Meltindex 2.0 g/10 min
    Meltflowratio 30
    Tensilestrengthatyield 9.7 MPa
    Tensilestrengthatbreak 24.1 MPa
    Ultimateelongation 800%
    Flexuralmodulus 240 MPa
    Vicatsofteningpoint 94 °C
    Meltingpoint 122 °C
    Crystallizationtemperature 102 °C
    Brittlenesstemperature < -70 °C
    Dartdropimpact 200 g
    Elmendorftearmd 300 g/mil
    Elmendorfteartd 500 g/mil
    Haze 10%
    Gloss45 80

    As an accredited Dow Dowlex™ 2620 LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Dowlex™ 2620 LLDPE is typically supplied in 25 kg polyethylene-lined paper bags, palletized, or 1,000 kg bulk octabins.
    Container Loading (20′ FCL) 20′ FCL container loading for Dow Dowlex™ 2620 LLDPE: 25 kg bags, palletized, approximately 20 MT net, moisture-protected.
    Shipping Dow Dowlex™ 2620 LLDPE is a non-hazardous polyethylene resin supplied as pellets in 25 kg bags, stacked on pallets and shrink-wrapped. Ship in clean, dry trucks or containers; avoid moisture, heat, and direct sunlight. No special DOT/IMO hazard classification for transport.
    Storage Store Dowlex™ 2620 LLDPE in a cool, dry, well-ventilated area, away from direct sunlight, heat, sparks, flames, and oxidizing agents. Keep containers sealed and palletized to prevent moisture and contamination. Avoid dust generation and prolonged UV exposure. Use first-in, first-out stock rotation. Maintain clean, labeled storage and follow local regulations. Protect bags from punctures; do not store near food, feed, or drinking water.
    Shelf Life Dow Dowlex™ 2620 LLDPE typically has a 24-month shelf life when stored cool, dry, in original packaging, away from sunlight.
    Application of Dow Dowlex™ 2620 LLDPE

    High-output cast stretch film lines process DOWLEX™ 2620 as an octene-comonomer linear low-density polyethylene with a nominal density of 0.926 g/cm³ (ISO 1183-1:2019) and a melt flow index of 2.0 g/10 min (ISO 1133-1:2022, 190°C/2.16 kg). The resin is plastified in a single-screw extruder with a 30:1 L/D barrier screw across a barrel profile from 190°C in the feed section to 250°C at the adapter, while the flat die is held between 245°C and 260°C to maintain melt curtain homogeneity. A die gap of 0.6–1.0 mm is paired with an air gap of 60–150 mm, and the melt curtain is pinned to a polished chill roll maintained at 15–30°C by an air knife or vacuum box. Under these conditions, the melt curtain remains stable at line speeds of 300–600 m/min, with a specific throughput of 0.8–1.8 kg/h per mm of die circumference, producing film thickness from 12 µm to 25 µm. Neck-in at the die edges typically measures 30–80 mm per side and translates to edge trim fractions of 5–15%, depending on die width and air gap setting. Draw resonance becomes the dominant failure mode when the polymer melt temperature falls below 230°C at line speeds above 450 m/min; the defect appears as periodic gauge bands across the web and is corrected by raising adapter and die temperatures or reducing the air gap. For machine wrap with a target pre-stretch ratio of 200–250%, DOWLEX 2620 is commonly run as the core layer at 60–80 wt% of the total structure, with each skin layer comprising 10–20 wt% of a higher-cling metallocene LLDPE or formulated cling masterbatch. Food-contact cast stretch film produced from DOWLEX 2620 falls within EU Regulation No 10/2011, Annex I, and FDA 21 CFR 177.1520(a)(2)(i) when the migration limits for the intended food type and contact time are met. If superficial condensation occurs after cold shipment at relative humidity above 60%, hopper drying at 60–70°C for 2–4 h is applied, but drying above 90°C is not recommended because slip and antiblock additives may degrade and alter coefficient of friction. The terminal product is a 15–23 µm machine-wrap film wound on 76 mm cores for automatic stretch-wrapping equipment.

    What Limits Bubble Stability in High-Draw Blown Film?

    In high-draw blown film conversion, the same octene-comonomer LLDPE grade is extruded through an annular die with a die gap of 1.5–2.5 mm and a blow-up ratio of 2.0–2.5:1. Stable bubble formation is governed primarily by the interaction between elongation viscosity, frost line height, and internal bubble pressure. On a monolayer line with a 300 mm die, extruder output is typically held at 0.5–1.2 kg/h per mm of die circumference, and frost line height is maintained between 6 and 10 die diameters. If the frost line height exceeds 10 die diameters, the melt film enters a low-temperature-draw regime where ethylene-octene chain segments align prematurely, producing machine-direction/transverse-direction tear imbalance and increased blocking tendency. Melt temperatures between 190°C and 220°C are standard; below 190°C, sharkskin melt fracture can appear at the die lips, particularly without polymer processing additive, and above 230°C, the bubble becomes increasingly susceptible to sag and width variation. Films of 25–75 µm are evaluated by ISO 6383-2 for Elmendorf tear strength and ASTM D1709 Method A for dart drop impact, while thickness spread across the bubble is controlled to ±5% using segmented air rings and an ultrasonic gauge scanner. Terminal uses include high-draw liners, consumer rollout bags, and clear packaging sacks where puncture resistance is required. Under EU Regulation No 10/2011, Annex I, and FDA 21 CFR 177.1520(a)(2)(i), the grade can be used for direct food contact subject to migration testing, but it is not suited for high oxygen barrier structures unless paired with EVOH or polyamide layers. Published data for this specific configuration is limited when recycled film waste streams exceed 20 wt%; gel accumulation and bubble holes are then batch-dependent and must be evaluated on the specific line.

    Heavy-Duty Sack Coextrusion Relies on Skin-Layer Strain Hardening

    Heavy-duty shipping sacks converted from a three-layer A/B/A blown film configuration use DOWLEX 2620 in the outer skins and often in the sealant side to retain puncture resistance and heat-seal integrity. Each skin layer is typically 15–25 wt% of the total structure, while the core layer is 50–70 wt% and may contain a defined fraction of post-industrial recycle or off-spec LLDPE; the skins remain virgin DOWLEX 2620 to maintain surface quality and tear propagation resistance. The die gap is set at 2.0–2.5 mm, the blow-up ratio is held near 2.0:1, and final thickness is 80–120 µm. Output rates are limited by bubble instability rather than extruder capacity; when the frost line moves beyond 10 die diameters, the sack film loses dart drop and fails drop testing more frequently. Finished sacks are subjected to drop testing according to ISO 7965 and puncture resistance measurement according to ASTM D5748, with the limiting failure mode often occurring at the gusset fold where gauge thinning reduces resistance to tear propagation. Slip and antiblock masterbatches are added to the skin layers only at let-down ratios between 50:1 and 25:1; higher levels reduce creep resistance and increase the risk of blocking in warm storage. Terminal products include granulate packaging, building material sacks, and industrial component sacks, for which REACH Regulation (EC) No 1907/2006, Annex XVII, and RoHS Directive 2011/65/EU apply to the final article. DOWLEX 2620 should not be combined with amine-based external lubricants that are not listed in the relevant food-contact positive list when the sacks are intended to hold food-grade raw materials; such combinations can also discolor the film and lower heat-seal strength.

    When Silage Film Must Withstand Fermentation Acids and UV Stress

    Agricultural silage cover and bunker cover film produced from DOWLEX 2620 is typically blown in widths from 6 m to 12 m and in thicknesses from 120 µm to 200 µm. The resin forms the structural core of a three-layer agricultural film in which the outer layer contains 0.2–0.8 wt% hindered amine light stabilizer and 0.1–0.4 wt% UV absorber, the middle layer is 60–70 wt% DOWLEX 2620, and the inner layer carries an antifog package when condensation control is required. Processing temperatures are deliberately limited to 200–220°C at the die because higher temperatures accelerate the consumption of the hindered amine light stabilizer and may shorten UV protection lifetime below the required 12–24 months of field exposure. Fermentation acids from silage, typically lactic and acetic acids at pH 3.5–4.5, do not hydrolyze the polyolefin backbone, but acidic infiltrate can migrate into film wrinkles and expose stabilizer degradation products; the film is therefore evaluated after immersion in 0.1 N acetic acid for 30 days before field use. UV weathering is assessed by ISO 4892-2 xenon arc cycle testing, and tensile retention after weathering is measured by ISO 527-3. The terminal product is a bunker cover sheet, silage bag, or pre-cut cover panel with welded hems; it must withstand puncture from ensiled maize stalks and resist tear initiation at stakes and tie-down points. Published data for this specific configuration is limited when the film is produced as a monolayer with carbon black above 3.0 wt%, because carbon black loading increases melt pressure and can reduce output by 10–20% depending on the masterbatch carrier.

    Application AreaRegulation or StandardSpecific Clause or MethodTypical Requirement
    Food-contact film layers in the United StatesFDA 21 CFR 177.1520(a)(2)(i)Olefin polymers verificationCompliance with additive and monomer limits
    Food-contact articles in the European UnionEU Regulation No 10/2011Annex I, Article 17Overall migration limit 10 mg/dm²
    Heavy-duty shipping sacksISO 7965Drop test procedureNo body or seam rupture after defined drop sequence
    UV aging of agricultural filmISO 4892-2Xenon arc exposureTensile retention above 50% after 1500 h
    Heat-seal strength in pouchesASTM F1921Heat-seal test methodMinimum seal strength 12 N/25 mm

    Pressure-Sensitive Adhesive-Free Skin Peeling in Surface Protection Films

    Surface protection films for glass, pre-painted steel, and building profiles are coextruded on cast film lines using DOWLEX 2620 as the core layer at 50–70 wt% of total thickness. The skin layer that contacts the protected substrate is formulated for low peel adhesion without a pressure-sensitive adhesive; instead, adhesion is controlled by blending an ethylene-vinyl acetate copolymer or a low-crystallinity polyolefin plastomer into the skin. The DOWLEX 2620 core must provide sufficient stiffness to prevent roll blocking and sufficient extensibility to survive film stretching during manual peel. Typical film thicknesses range from 30 µm to 60 µm, and the cast line is operated at die temperatures of 240–260°C, with the chill roll held at 20–30°C. The core layer is metered into the feedblock at 60 wt%, while the skin layers are each 15–20 wt%; the remaining 0–10 wt% is used to adjust peel force via a plastomer or EVA concentrate. Peel force is measured at a 180° angle and a jaw separation speed of 300 mm/min on a universal tensile tester equipped with a 10 N load cell, with typical values for protective films on glass in the range of 0.05–0.15 N/25 mm. Published data for this specific configuration is limited when DOWLEX 2620 is used below 50 wt%, because the peel force then becomes dominated by the skin resin and may exceed the removable-range upper limit. Terminal products are roll-stock protective films with slit widths from 500 mm to 2000 mm, and they must meet the surface-quality requirements of downstream laminators without leaving residue after 6 months of outdoor exposure.

    In coextruded stand-up pouches and four-side-seal packaging, the sealant web often contains DOWLEX 2620 as the innermost layer, typically at 20–30% of total film thickness. The layer is selected for heat-seal strength, hot-tack window, and lower seal initiation relative to high-density polyethylene. Coextruded films with a total thickness of 50–80 µm are produced on blown or cast lines, with the sealant layer melt temperature between 220°C and 250°C depending on the adjacent tie layer. Heat-seal strength is measured according to ASTM F1921 on samples sealed at 110–130°C and 0.4 MPa jaw pressure for 0.5 s; hot tack is measured at a 200 mm/min peel speed. Published data for this specific configuration is limited when the sealant layer is diluted with more than 30 wt% LDPE, because seal initiation temperatures rise and the hot-tack window narrows. The outer layer may be a printable HDPE or PET-based web, and the core may contain recycled film or regrind, but the sealant layer should remain virgin DOWLEX 2620 to meet direct food-contact compliance under EU Regulation No 10/2011, Annex I, and FDA 21 CFR 177.1520(a)(2)(i). Terminal products include frozen food pouches, dry mix pouches, and liquid-containing sachets with a total bag drop test evaluated by ISO 7965 after filling.

    Free Quote

    Competitive Dow Dowlex™ 2620 LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    DOWLEX™ 2620 LLDPE is an ethylene/1-octene linear low density polyethylene resin produced by a solution polymerization process. The grade identifier 2620 denotes a nominal density of 0.935 g/cm³ when tested in accordance with ISO 1183-1:2019 and a melt mass-flow rate of 2.0 g/10 min at 190 °C under a 2.16 kg load when tested in accordance with ISO 1133-1:2022. The resin is intended primarily for rotational molding of large hollow parts in which slow crack growth resistance, sub-ambient impact toughness, and dimensional stability across wall-section transitions are the controlling performance attributes. The product is delivered as pellet or as ground powder according to the packaging and distributor configuration.

    Material identity and specification boundaries

    The resin is classified as an ethylene-octene LLDPE, not a butene-based LLDPE. The distinction is material to end-use performance because the hexyl branches derived from 1-octene participate differently in tie-molecule formation between lamellae than the ethyl branches derived from 1-butene. The following table lists typical physical property data published for the resin; these are not specification limits and do not replace the current certificate of analysis.

    PropertyTest methodTypical valueUnit
    Melt mass-flow rateISO 1133-1:20222.0g/10 min
    DensityISO 1183-1:20190.935g/cm³
    Tensile stress at yieldISO 527-2:2012, type 1B, 50 mm/min18MPa
    Tensile strain at breakISO 527-2:2012, type 1B>800%
    Flexural modulusISO 178:2019650MPa
    Vicat softening temperature A50ISO 306:2022122°C
    Environmental stress crack resistance, 100 % Igepal CO-630, F50ASTM D1693-21>1000h

    The 2.0 g/10 min melt mass-flow rate is lower than high-flow rotational molding LLDPE grades in the 4.0–6.0 g/10 min range, which increases the molecular weight fraction that contributes to environmental stress crack resistance and impact strength but may require longer oven residence time to achieve full particle coalescence in wall sections above 8 mm. The 0.935 g/cm³ density contributes stiffness and chemical resistance relative to lower-density LLDPE, while the remaining amorphous fraction provides stress relaxation during cooling to reduce warpage in large flat panels.

    For lot acceptance, the supplier’s certificate of analysis remains the controlling document. The nominal density and melt mass-flow rate are accompanied by manufacturing tolerances that are not reproduced here because they vary by production site and region. Users should not substitute nominal values for specification limits when designing tooling or setting release criteria.

    In production-scale rotational molding on a three-arm carousel machine with cast-steel molds of 10 mm nominal wall thickness, a forced-air oven set point of 300 °C, and a mold rotational ratio of 4:1, the resin has been observed to reach a peak internal air temperature of 190–200 °C at full densification. When the peak internal air temperature was limited to 175 °C, incomplete sintering at the fill-port-to-wall junction produced microporosity; instrumented puncture testing in accordance with ISO 6603-2:2023 showed a geometry-dependent reduction in puncture energy relative to the fully densified control. Published data for this specific tooling configuration is limited. The resin does not require predrying in normal closed-warehouse storage, but condensation on cold powder or mold surfaces at relative humidity above 60 % introduces surface moisture that can form pinholes during the heating cycle. In such conditions, warm-air drying at 70–80 °C for 1–2 h is applied before charging the mold.

    What distinguishes Dowlex 2620 from conventional butene-based LLDPE?

    Conventional butene-based LLDPE of similar density and melt index contains ethyl branches derived from 1-butene. Ethyl branches are less effective than the hexyl branches derived from 1-octene at increasing the concentration of load-bearing tie molecules between adjacent lamellar crystals. Under slow crack growth testing in accordance with ASTM D1693-21, DOWLEX™ 2620 LLDPE typically exhibits a longer F50 failure time than a butene-based resin of comparable 0.935 g/cm³ density and 2.0 g/10 min melt mass-flow rate. Under instrumented puncture loading in accordance with ISO 6603-2:2023, the octene-based microstructure generally shifts the ductile-to-brittle transition to a lower temperature; the magnitude of the shift is dependent on specimen geometry and processing history.

    The difference in slow crack growth resistance between octene-based and butene-based LLDPE is not simply a function of comonomer length. The distribution of comonomer units along the polymer backbone determines the thickness of the interfacial amorphous layer and the probability that a chain participates in more than one lamella. Octene-based solution LLDPE resins generally exhibit a broader distribution of lamellar thicknesses and enhanced tie-molecule density at equivalent density. This effect is measurable as a higher F50 value in ASTM D1693-21 and as a lower ductile-to-brittle transition temperature in ISO 6603-2:2023 instrumented puncture tests.

    The solution polymerization route also yields a narrower molecular weight distribution and lower catalyst residue than typical gas-phase butene LLDPE, which reduces gel counts and improves surface consistency on large rotomolded panels. Compared with metallocene-catalyzed LLDPE of similar density, the product may show a slightly broader comonomer distribution and therefore a different balance of dart impact and ESCR retention after multiple thermal cycles. Published data for this specific comparison is limited; comparative evaluations should use the same specimen geometry, conditioning protocol, and test standard.

    In capillary rheometry, the resin displays the shear-thinning behavior expected for a linear polyolefin. Melt flow ratio is not a primary release specification for rotomolding; cycle development is controlled instead by powder particle size distribution, oven temperature, mold rotational ratio, and peak internal air temperature.

    Peak internal air temperature and the ±5 °C densification window

    The practical rotomolding window for this resin is commonly described by processors as a ±5 °C band around the mold-specific optimum peak internal air temperature. The lower boundary is set by incomplete sintering of powder particle boundaries and residual porosity; the upper boundary is set by the onset of thermo-oxidative chain scission, surface discoloration, and loss of slow crack growth resistance. In large spherical tank tooling with a 6 mm nominal wall, the optimum peak internal air temperature typically falls between 190 °C and 195 °C when the oven set point is 290–300 °C and the rotational ratio is 4:1. At 185 °C, the inner surface may retain powder texture and show reduced low-temperature puncture energy under ISO 6603-2:2023; at 200 °C or above, discoloration and a reduction in ASTM D1693-21 F50 ESCR may occur before visible outer-surface deformation. Published data for this specific resin and tooling geometry is limited; the exact band must be established with an internal air thermocouple and molded panel testing for density, impact, and ESCR after each cycle change.

    The narrow window is partly attributable to the 0.935 g/cm³ density, which increases the crystalline fraction relative to lower-density LLDPE rotomolding grades. Under-sintering at the lower limit leaves voids at the melt-crystallization front; overshooting accelerates oxidation at the inner air-polymer interface, which is continuously exposed to hot air. The oven temperature must be selected so that the polymer melt reaches the target peak internal air temperature without exceeding the oxidative induction time of the stabilized powder. If the oven is operated above 315 °C, the outer mold surface temperature may rise rapidly and cause the inner air temperature to overshoot before the thermocouple responds; this can degrade the inner surface even when the average cycle time is unchanged. Conversely, if the oven set point is below 260 °C, the melting plateau may extend past the point at which the powder at the mold surface begins to oxidize, because the total cycle time increases. These boundaries are general for LLDPE rotational molding and should be validated for the specific mold mass and wall thickness.

    Differential scanning calorimetry in accordance with ISO 11357-3:2018 can track crystalline melting behavior, and oxidation induction time testing in accordance with ISO 11357-6:2018 can detect thermal history effects in regrind and reworked material. A statistically significant reduction in oxidation induction time relative to virgin powder indicates excessive thermal history and requires a reduction in oven temperature or cycle time.

    Powder particle size distribution is a further control on the window. Excessive fines melt prematurely at the mold surface and trap air; coarse particles may remain partially unmelted at the inner surface. Rotational molding powders are commonly controlled by sieve analysis to 35 mesh (500 µm) with fines below 200 mesh (75 µm) controlled to avoid dusting. Published data for DOWLEX™ 2620 LLDPE powder from a specific distributor is limited; the grinding specification should be obtained from the supplier. Regrind addition above 20 wt% can shift the densification window and reduce impact properties; regrind must be validated by ISO 6603-2:2023 puncture testing and ASTM D1693-21 ESCR testing before production use.

    On a mold with a 12 mm thick flat panel adjacent to a 3 mm thin sidewall, the difference in cooling rate creates differential shrinkage. A controlled cooling curve in which the internal air temperature is reduced at 2–4 °C/min through the crystallization range of 120 °C to 90 °C is used in tooling development to limit panel distortion. The crystallization temperature range can be measured by ISO 11357-3:2018; the cooling-rate target is tooling-dependent and published data for this specific configuration is limited.

    When storage tanks require ESCR classification under ASTM D1998

    Rotationally molded polyethylene storage tanks designed for chemical service are often evaluated under ASTM D1998-21. In these applications, the ASTM D1693-21 F50 environmental stress crack resistance of DOWLEX™ 2620 LLDPE, typically above 1000 h in 100 % Igepal CO-630, provides a margin against slow crack growth in the presence of polar liquids, detergents, and mild acids. The design standard, however, requires the engineer to apply a specific design factor to the hydrostatic design basis and to account for chemical resistance factors for each stored fluid. The resin supplier’s chemical resistance chart must be consulted before specification for a particular chemical.

    The 0.935 g/cm³ density provides higher stiffness and lower permeation than LLDPE grades below 0.920 g/cm³, but it also reduces the elastic strain to yield. Section changes, sharp radii, and inserts in a storage tank can concentrate stress; the designer must avoid undercuts and use generous radii to prevent localized environmental stress cracking. For applications requiring continuous exposure to polar fluids at temperatures above 40 °C, accelerated chemical resistance testing is required because the F50 ESCR value measured at ambient temperature does not directly predict elevated-temperature performance.

    The material is not recommended for strong oxidizing acids, chlorinated solvents, or aromatic hydrocarbons that plasticize the amorphous phase and reduce long-term ESCR below the neat-resin value. For outdoor service, ultraviolet stabilization is mandatory. The base resin contains only processing stabilizers; it does not contain a sufficient hindered amine light stabilizer or carbon black loading to prevent chalking and embrittlement after extended exposure. Weathering tests under ASTM D2565-21 or ISO 4892-2:2013 should be conducted on the actual pigmented or stabilized compound, not on natural resin.

    Regulatory status is limited to the specific formulation and manufacturing site. Polyethylene grades of this type are generally considered compliant with FDA 21 CFR 177.1520 for olefin polymers in food contact when used under the intended conditions of use, and with EU Regulation (EU) No 10/2011 for plastic materials intended to come into contact with food. These statements do not apply to all service temperatures, food simulants, or regional requirements, and the current regulatory data sheet for the exact grade and lot must be consulted.

    Top