Dow Dowlex 2601a Lldpe

Dow Dowlex™ 2601A LLDPE

    • Product Name: Dow Dowlex™ 2601A LLDPE
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 967042
    Polymer Type Linear Low Density Polyethylene (LLDPE)
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.85 g/10 min
    Melting Point 123 °C
    Vicat Softening Point 100 °C
    Tensile Strength At Yield 10.3 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 700%
    Flexural Modulus 241 MPa
    Dart Drop Impact 25 µm Film 120 g
    Elmendorf Tear Strength Md 25 µm Film 360 g
    Elmendorf Tear Strength Td 25 µm Film 500 g
    Haze 25 µm Film 12%
    Gloss 25 µm Film 55%

    As an accredited Dow Dowlex™ 2601A LLDPE factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow Dowlex™ 2601A LLDPE is supplied in 25 kg polyethylene-lined bags, palletized and stretch-wrapped, or 1,000 kg bulk bags.
    Container Loading (20′ FCL) 20′ FCL loaded with palletized 25 kg bags of Dow Dowlex™ 2601A LLDPE, shrink-wrapped and secured for safe ocean transport.
    Shipping Dow Dowlex™ 2601A LLDPE ships as non-hazardous solid pellets in 25 kg bags, octabins, or bulk trucks/railcars. Keep packages clean, dry, and closed; avoid excessive heat, sunlight, and moisture. Follow supplier SDS, local transport regulations, and labeling. No special DOT/IMDG/IATA hazard class.
    Storage Store Dowlex™ 2601A LLDPE resin pellets in original, closed containers in a cool, dry, well-ventilated area. Protect from direct sunlight, heat, flames, ignition sources, moisture, dust, and strong oxidizers. Avoid excessive stacking or pressure, which may cause blocking. Keep area clean, prevent contamination, inspect containers regularly, and use first-in, first-out rotation. Follow the manufacturer’s SDS and local regulations.
    Shelf Life Under cool, dry, sealed storage, Dow Dowlex™ 2601A LLDPE has no specific shelf life and remains stable indefinitely.
    Application of Dow Dowlex™ 2601A LLDPE

    At 60–80 µm thickness on vertical form-fill-seal lines running IQF vegetable and seafood packs, a monolayer blown film based on Dowlex™ 2601A LLDPE is typically modified with 2.0–2.5 wt% of a 20% silica-in-LDPE antiblock masterbatch and 0.8–1.2 wt% of a 5% erucamide slip masterbatch. The additive package lowers film-to-film coefficient of friction from an untreated value above 0.6 to 0.15–0.25 when measured under ISO 8295 after 24 h at 23 ± 2°C, preventing wicket-holder drag and jaw misfeed at line speeds of 60–100 bags/min. The film is processed on a single-screw grooved-feed extruder with 45–75 mm screw diameter and 24:1–30:1 L/D, barrier flight design, die gap 1.2–2.0 mm, blow-up ratio 2.0–2.8, melt temperature 200–225°C, and frost-line height maintained between 4 and 8 die diameters to balance haze below 8% under ASTM D1003 with dart impact above 120 g under ASTM D1709 Method A and Elmendorf tear above 15 N in machine direction under ASTM D1922.

    Food-contact compliance obligations are set by 21 CFR § 177.1520(c)3.1a and EU Regulation (EU) No 10/2011; the overall migration limit is 10 mg/dm² under EN 1186-1, and the comonomer must be listed in the regulation’s Annex I. The base resin alone does not cover non-resin components; additive masterbatches require their own food-contact approval. Extruder temperature profile must remain below 240°C because octene LLDPE begins to generate gel bodies from cross-oxidation at longer residence times, and color changes are purged with a dedicated purge compound before returning to production. Terminal products include IQF vegetable bags, frozen seafood pouches, ice cube bags, and frozen fruit sachets.

    Why Does Bubble Stability Control Sack Drop Performance More Than Resin Density?

    When the core layer of a 120–180 µm three-layer heavy-duty sack film is run at 100 wt% Dowlex™ 2601A or blended with up to 20 wt% post-industrial rework screened through a 100 µm nominal mesh melt filter, the outer skins may contain 0–10 wt% LDPE to maintain bubble stability at layflat widths above 1,200 mm. At blow-up ratio 2.2–2.6 and die gap 1.8–2.5 mm, the film reaches dart impact acceptance minima of 250 g at 120 µm and 400 g at 180 µm under ASTM D1709 Method A; Elmendorf tear is measured under ASTM D1922, with machine-direction control limits of 20–40 N for 150 µm film. Tensile yield is tested under ISO 527-3 at 500 mm/min crosshead speed. Standards applied to non-food industrial sacks include ISO 21898 for flexible intermediate bulk containers, ISO 7965-1 for drop testing, and EU Packaging Directive 94/62/EC heavy metals ceiling of 100 mg/kg combined. In UN-certified packaging lines, the liner alone does not carry the certificate; the complete sack with woven outer ply and liner is qualified under Chapter 6.5 of the UN Model Regulations for FIBCs.

    Process parameters: grooved-feed extruder 75–90 mm, 30:1 L/D, melt temperature 210–230°C, die temperature set 10–15°C lower than melt to reduce die-lip paraffin buildup, chiller-air temperature 8–15°C, and online corona treating to 38–42 mN/m for print adhesion. Rework incorporation above 20 wt% or melt filtration below 100 µm shifts dart impact variability beyond ±15% and produces transverse-direction split failures on drop tests after conditioning at -18°C for 24 h. Finished package types are heavy-duty shipping sacks for polymer granules, construction aggregate sacks, mineral box liners, and FIBC liner films.

    Three-layer greenhouse covers in 150–200 µm total thickness are produced with a Dowlex™ 2601A core at 70–85 wt% and EVA skins at 15–30 wt% of the total structure, using an EVA grade with 14–18% vinyl acetate content. The UV stabilization package, added as a masterbatch at 1.5–3.0 wt%, contains hindered amine light stabilizers and a nickel quencher; dosage is increased toward 3.0 wt% in Alpine and Mediterranean sites exceeding 120 kLy annual solar irradiation. Product conformity is assessed under EN 13206:2017 for agricultural and horticultural covering films; accelerated weathering uses ISO 4892-2, and tensile retention after ageing must remain above 60% of the original ISO 527-3 value for the intended service-life class. The film is blown on 1.8–3.2 m die diameters, die gap 1.6–2.4 mm, blow-up ratio 2.0–2.5, melt temperature 195–215°C, and internal bubble cooling above 2.0 m die size; layflat widths up to 16 m are produced. Adding more than 3.0 wt% UV masterbatch causes die-lip deposit and can reduce Elmendorf tear below 20 N in the transverse direction under ASTM D1922; under-dosing below 1.5 wt% may shorten service life below 24 months in low tunnel service. Final film products are greenhouse covering films, low tunnel films, and nursery overwrap films where the EVA skins supply thermal retention.

    An Octene-Comonomer Core Layer in 15–23 µm Pallet Wrap

    Cast stretch film for pallet load unitization uses Dowlex™ 2601A as a core-layer resin in a three-layer cast line where layer distribution is 10/80/10, with the 80 wt% core composed of 85–90 wt% Dowlex™ 2601A and 10–15 wt% metallocene polyethylene plastomer at density 0.902–0.912 g/cm³ and melt index 1.0–2.0 g/10 min to elevate tensile elongation and maintain load retention. Cling layers contain 3–7 wt% low-crystallinity tackifier masterbatch and 0.5–1.0 wt% antiblock masterbatch; tackifier above 7 wt% in the surface layers reduces unwind force and produces roll blocking in warm-warehouse storage above 35°C. Film is cast through a 0.5–1.0 mm adjustable die gap onto a 15–25°C chill roll with air knife and vacuum box; line speeds of 300–600 m/min are typical, and gauge is controlled to ±0.5 µm across 500–1,500 mm web widths. The specification references ASTM D5748 for puncture resistance, ASTM D5458 for cling force, and ISO 527-3 for tensile elongation.

    Downstream pre-stretch ratios on turntable wrappers are limited to 250–300% for this core-resin combination; higher pre-stretch above 300% produces localized neck-in and transverse-direction tear propagation at splices. The reeled output feeds downstream wrappers as hand stretch film rolls and machine-grade pallet wrap for logistics and export crating.

    In blown-film e-commerce mailer lines running 60–90 µm gauge, the monolayer or three-layer structure contains 70–85 wt% Dowlex™ 2601A, 10–20 wt% post-consumer recycled LLDPE, and 3–6 wt% black or grey masterbatch. Compliance obligations for the final mailer include EU Packaging Directive 94/62/EC heavy metals limits of 100 mg/kg combined by weight, and recyclate claims are supported by EuCertPlast or ISO 14021 verification. Extrusion conditions: melt temperature 200–220°C, die gap 1.8–2.2 mm, blow-up ratio 2.2–2.8; film is converted on side-seal or bottom-seal mailer machines at 100–250 bags/min. The converted stock is used as poly mailers in e-commerce garment and accessory fulfillment, where black masterbatch may reduce near-infrared sortability unless detectable black pigments are specified.

    Free Quote

    Competitive Dow Dowlex™ 2601A LLDPE prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow Dowlex™ 2601A LLDPE is a solution-process linear low-density polyethylene resin supplied in pellet form for blown-film extrusion. The product is an ethylene–octene copolymer with a nominal density of 0.926 g/cm³ and a nominal melt index of 1.0 g/10 min measured at 190 °C under a 2.16 kg load per ISO 1133-1:2022 and ASTM D1238-20. The octene comonomer introduces short-chain branching that is longer than the butene branch of conventional gas-phase commodity LLDPE; this alters the chain-fold and tie-molecule distribution during crystallization and shifts the balance between stiffness, tear resistance, and low-temperature puncture resistance. The grade is specified for heavy-duty shipping sacks, industrial liners, freezer packaging, and agricultural films in which down-gauging and abuse resistance are controlled by standards such as ASTM D1709-15 and ASTM D1922-21. The primary conversion route is blown-film extrusion; some cast-film lines process the grade when high tear strength and gauge uniformity are required.

    What separates octene-based DOWLEX 2601A from butene LLDPE and metallocene film resins?

    At equal nominal density and melt index, an ethylene–octene solution LLDPE generally yields higher Elmendorf tear and dart impact than a gas-phase butene LLDPE. The longer comonomer branch is less efficient at disrupting crystallinity, so the density is maintained with a higher tie-molecule concentration between lamellae. This manifests in film as improved slow-crack-growth resistance and less notch sensitivity. In comparison with butene LLDPE, the processing penalty is a higher low-shear viscosity and a higher melt temperature requirement at the die; the advantage is the ability to operate at lower gauge under the same abuse-resistance specification. The precise gauge-reduction window is influenced by blow-up ratio, frost-line height, die gap, and output; published data for this specific grade's gauge-reduction window are limited.

    Compared with LDPE, DOWLEX 2601A has lower melt strength and a lower first normal stress difference at the die exit, so die swell and bubble stability cannot be managed using LDPE settings. The die gap is typically widened and the air ring is run with higher internal bubble pressure to stabilize the stalk. Compared with metallocene LLDPE, the solution Ziegler-Natta architecture gives a broader molecular weight distribution, which reduces extruder backpressure and improves bubble stability on older single-lip air rings but generally produces poorer clarity and higher extractables. Optical properties are not grade constants; haze must be measured per ISO 14782:2021 or ASTM D1003-21 at the intended film gauge and orientation.

    Within the Dowlex solution LLDPE family, DOWLEX 2601A differs from lower-density grades such as DOWLEX 2045G primarily by its higher nominal density. The 0.926 g/cm³ density of 2601A raises secant modulus and yield stress but lowers the maximum attainable dart impact and Elmendorf tear at equal film gauge. Converter selection between the two grades is governed by the relative priority of stiffness under load against extreme puncture resistance. For a shipping sack where creep under stacking load must be minimized, the higher-density grade is favoured; for a heavy-duty freezer bag requiring extreme low-temperature abuse resistance, the lower-density octene grade may be preferred. Published data for direct converter comparisons are limited; the choice is normally confirmed by pilot-scale extrusion on the target line.

    On a 75 mm single-screw blown-film line with a 30:1 L/D barrier screw, a 250 mm die, and a dual-lip air ring, the melt-temperature window is normally between 190 °C and 220 °C at the adapter inlet. The die gap is set between 1.5 mm and 2.3 mm. A blow-up ratio between 2.0:1 and 2.5:1 is used when balanced machine-direction and transverse-direction tear are required. Frost-line height is maintained at 1.0 to 2.0 die diameters; higher frost lines increase machine-direction orientation and may shift tear balance. Extruder torque is typically 10% to 20% higher than an LDPE of equal melt index, so motor current is not a direct indicator of throughput. On smooth-bore extruders, the feed throat should be kept below 50 °C to prevent pellet bridging; grooved-feed sections are used on lines exceeding 200 kg/h. The melt is kept below 240 °C at all points to avoid oxidative gel formation. These are starting-point conversion parameters; converter qualification should confirm the values on the actual line because published data for this specific equipment configuration are limited.

    In capillary rheometry, the material exhibits shear-thinning typical of a 1.0 g/10 min linear polyethylene. The low-shear viscosity is higher than a branched LDPE of comparable melt index but lower than a narrow-MWD metallocene LLDPE, which is why the grade is less likely to overload the screen pack and die than an mLLDPE. The absence of long-chain branching means the extensional viscosity does not show the strain hardening that stabilizes LDPE bubbles; high-stalk operation therefore requires careful control of the internal bubble pressure and air-ring velocity. On spiral mandrel dies, flow marks can appear if the melt temperature drops below 190 °C or if the output rate exceeds the die's flow-channel capacity. A breaker plate with screen pack 40/60/80 mesh is a common starting point, but the final mesh selection is governed by the contamination level of the recycling stream and the target gel count.

    Property, standard, and compliance matrix

    Table 1: Nominal characteristics of Dow Dowlex™ 2601A LLDPE
    CharacteristicTest methodNominal value/status
    Melt flow rateISO 1133-1:2022, 190 °C, 2.16 kg1.0 g/10 min
    DensityISO 1183-1:2019, ASTM D792-200.926 g/cm³
    ComonomerManufacturer solution-process documentationOctene; linear low-density polyethylene
    Conversion routeManufacturer processing guideBlown-film extrusion; limited cast-film use
    Food-contact regulatory statusFDA 21 CFR §177.1520; EU Regulation (EU) No 10/2011Conforms when the finished article meets migration limits
    REACH/RoHS statusEU Regulation (EC) No 1907/2006; Directive 2011/65/EUCompliance declared on the safety data sheet; no SVHC above 0.1% w/w

    The listed values are nominal resin data and not specification limits. Lot-specific certificates of analysis should be reviewed against the converting specification; mechanical and optical film values must be measured on the production film at the intended gauge because orientation balance changes the result.

    If the grade is specified for food-contact packaging, what must be verified on the finished article?

    Resin compliance does not clear the package. Under EU Regulation (EU) No 10/2011, the finished plastic article must meet an overall migration limit of not more than 10 mg/dm² of food-contact surface area, or 60 mg/kg for food simulants for infants and young children, using the appropriate Annex III simulant. For fatty food simulant, 95% ethanol or iso-octane is selected depending on the technical feasibility; olive oil may be required for certain food categories. In the United States, FDA 21 CFR §177.1520 applies to olefin polymers, but the end-use conditions, additive package, coatings, and printing inks are evaluated on the final film. If the grade is supplied without slip and antiblock additives, converters frequently add slip and antiblock masterbatch; those additives must separately comply and be included in migration testing. Corona treatment and lamination adhesives also enter the compliance assessment.

    Pellets are non-hygroscopic and do not require drying in normal warehouse conditions. If sacks are transferred from cold storage to a warm production area, surface condensation can form; film defects such as bubbles or die-lip drool may then occur. In that case, drying at 70 °C to 80 °C for 1 to 2 hours in a desiccant-hot-air dryer with a dew point below -20 °C is sufficient. Storage below 50 °C and away from ultraviolet light preserves the antioxidant package. The base resin does not contain a high level of UV stabilizer; agricultural films require a UV masterbatch selected for the intended exposure period and climatic zone. Contact with strong oxidizing acids, chlorinated solvents, or aromatic hydrocarbons should be avoided in packaging service because polyethylene can swell or undergo environmental stress-cracking in certain liquid media.

    At melt temperatures above 240 °C, thermo-oxidative degradation of linear polyethylene can generate peroxides that lead to crosslinking; this may appear as gels that cannot be re-melted and that block screen packs. The condition is more likely at the die lip when a high output rate is combined with a high blow-up ratio and low quench air velocity. The use of a screen changer with oversize filtration area reduces pressure-drop sensitivity to gel loading. If gel counts increase during a shift, the first corrective action is to reduce the barrel temperature profile, not to increase backpressure or raise screw speed.

    Converted-film qualification uses a matrix of orientation-dependent tests. Tensile yield and break are measured per ISO 527-3 or ASTM D882-18 on specimens cut in the machine and transverse directions. Elmendorf tear is measured per ISO 6383-2:2015 or ASTM D1922-21. Dart impact is measured per ISO 7765-1:2017 or ASTM D1709-15, with Method A or Method B selected according to gauge and expected impact level. Haze is measured per ISO 14782:2021 or ASTM D1003-21. Surface tension after corona treatment is monitored to 38 to 42 dyn/cm per ASTM D2578-23 before printing because LLDPE film can lose treatment with time. Heat-seal strength is measured per ASTM F88/F88M-21 on the target packaging line, since seal-through-contamination behavior and hot-tack performance depend on film surface treatment and masterbatch loading.

    In heavy-duty sack production at 100 µm to 150 µm, the final gauge is not set by resin density alone. The sack is tested after conditioning at 23 °C and 50% relative humidity for at least 24 h; dart impact per ASTM D1709-15 Method A and Elmendorf tear per ASTM D1922-21 are common release criteria. A film that meets lot certification may still fail a bag drop test if the sealing jaw temperature creates localized thinning at the seal edge; the sealing jaw temperature must be optimized on the specific packaging machine because hot-tack performance and seal-through-contamination behavior vary with film surface treatment and masterbatch loading.

    Top