| HS Code | 962329 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Octene |
| Molecular Weight Distribution | Narrow |
| Density | 0.923 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.0 g/10 min |
| Melting Point | 122 °C |
| Vicat Softening Point | 99 °C |
| Tensile Strength At Yield | 10.3 MPa |
| Tensile Strength At Break | 22.1 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 241 MPa |
| Hardness Shore D | 50 |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 300 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 5% |
| Gloss 45 | 85% |
As an accredited Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2553 pellets are typically packaged in 25 kg polyethylene bags or 1,000 kg bulk bags for industrial shipment. |
| Container Loading (20′ FCL) | 20′ FCL: Dow DOWLEX™ 2553 LLDPE in 25 kg bags, palletized, floor-loaded; approx. 18–20 MT net; dry, ambient, moisture-protected. |
| Shipping | Dow DOWLEX™ 2553 LLDPE is shipped as non-hazardous, free-flowing pellets in 25-kg polyethylene bags, palletized and stretch-wrapped, or in bulk trucks/railcars. It is not regulated for transport under DOT, IMDG, or IATA. Store dry, away from heat and direct sunlight; avoid moisture and contamination. Handle according to local regulations. |
| Storage | Store DOWLEX™ 2553 in a cool, dry, well-ventilated warehouse, away from direct sunlight, heat, sparks, and open flames. Keep original bags or containers tightly closed on pallets to prevent moisture, dust, and contamination. Avoid contact with strong oxidizers. Maintain clean floors to control pellet spills and slipping. Follow local regulations and the manufacturer’s safety data sheet. |
| Shelf Life | Shelf Life: No specific expiry; stable indefinitely under normal storage. Keep cool, dry, sealed, away from heat, sunlight, and oxidizing agents. |
Pallet unitization film on high-speed cast extrusion lines is a downstream track where DOWLEX™ 2553 linear low density polyethylene, narrow molecular weight distribution, is processed into gauges from 12 μm to 35 μm under melt temperatures of 240°C to 260°C at the die exit. The resin is an ethylene-octene copolymer with a nominal density of 0.935 g/cm³ under ASTM D792 and a nominal melt index of 2.3 g/10 min under ASTM D1238 at 190°C/2.16 kg. In cast stretch film, the narrow MWD narrows the relaxation-time distribution, which reduces gauge variation during edge-pinned melt drawing and permits line speeds of 300 m/min to 600 m/min on a line equipped with a 90 mm single-screw extruder with an L/D ratio of 30:1, barrier feed section, and 80/120/80 mesh screen pack. Compliance for food-contact stretch film is anchored to FDA 21 CFR 177.1520(c) for olefin polymers and Commission Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm²; industrial machine film for non-food palletizing is specified for thickness tolerance under ASTM D2103 and puncture resistance under ASTM D5748. The formulation uses 100 parts per hundred resin DOWLEX 2553 as the base; cling performance is generated by liquid polyisobutylene injection at 0.5–2.0 wt% or a sorbitan monooleate-based cling concentrate at 0.3–0.8 wt%. Antiblock masterbatch is incorporated only at 1–3 wt% when wound-roll blocking appears in films above 23 μm, and a fluoroelastomer processing aid at 0.1–0.3 wt% is used to suppress die-lip buildup and melt fracture. The downstream production process employs a polished chill roll with surface roughness below 0.02 μm Ra and temperature of 18–28°C, with a dual-chamber vacuum box or air-knife assembly pinning the melt curtain across a 150–250 mm air gap. The die gap is held at 0.5–0.8 mm; a narrower die gap reduces transverse gauge spread but raises melt pressure ahead of the die, which on extended runs can exceed 25 MPa and trigger melt fracture if the processing aid concentration drops below 0.1 wt%. Terminal articles include hand stretch film rolls of 250–500 mm width, machine stretch film with pre-stretch ratios up to 250%, and pre-stretched films at 8–15 μm thickness. A processing boundary is high-humidity pellet storage: although polyethylene is not hygroscopic, surface condensation on cold pellets should be removed by drying at 80°C for 2 h before the feed throat to avoid steam-induced flow surging. Published data for pre-stretch ratios above 250% with this specific narrow-MWD LLDPE are limited; plant trials on a given cast line are required before sustained downgauging below 10 μm.
Blown film for silage covers and industrial liners places a different set of constraints on DOWLEX 2553 because the bubble must remain stable while the frost line height and die gap control film gauge. The resin can be run on a 75–90 mm grooved-feed single-screw extruder with an L/D ratio of 30:1, a die gap of 1.8–2.4 mm, and a blow-up ratio of 2.0:1–2.8:1. At blow-up ratios below 1.8:1, transverse direction Elmendorf tear strength measured under ASTM D1922 degrades, while above 3.0:1 bubble instability contributes to gauge bands and poor roll conformation. Melt temperature at the die is kept in the 190–230°C band, and the frost line is positioned at 6–10 die diameters above the die face. Internal bubble cooling air is dehumidified to a dewpoint below 10°C for frost line control on lines running above 80 m/min. Formulations for outdoor silage film commonly use a three-layer structure in which DOWLEX 2553 forms the core or load-bearing layer at 60–80 wt%, a metallocene LLDPE skin contributes sealability at 10–20 wt%, and edge-trim reclaim is reintroduced at up to 10–20 wt%. Stabilization for outdoor weathering follows ISO 4892-2 exposure methodology, with a hindered amine light stabilizer masterbatch at 0.2–0.8 wt% and a benzotriazole UV absorber at 0.1–0.3 wt%. Black silage film incorporates carbon black masterbatch at 2–5 wt% to achieve opacity and ultraviolet shielding. Terminal products include bale wrap film, agricultural silage tubes, industrial liner sheeting, and FIBC inner liners. Compliance for food-contact industrial liner stock relies on FDA 21 CFR 177.1520(c), while European silage stretch film is assessed under EN 14932:2018 for mechanical and bale-wrapping performance. An operational limitation is melt temperature above 250°C during extended residence: this promotes oxidative gel formation and reduces dart impact performance under ASTM D1709. The narrow MWD reduces the population of very long relaxation-time chains, so the bubble is less likely to exhibit low-frequency diameter oscillation at high takeoff speeds, but the processor must compensate for lower shear thinning by controlling backpressure with feed-zone barrel cooling.
Extrusion lamination onto 40–80 g/m² kraft and folding boxboard places DOWLEX 2553 in a high-temperature, low-residence-time process where neck-in and draw resonance determine coating weight consistency. The resin is typically let down with 10–30 wt% high-pressure LDPE to reduce neck-in from a pure LLDPE level of 30–50 mm per side to 15–30 mm per side at a 150–300 mm air gap. Adhesion to aluminum foil or metallized film is generated by an acid copolymer or maleic anhydride-grafted polyethylene tie layer at 2–5 wt%, and a fluoroelastomer processing aid is added at 0.05–0.2 wt% to delay die-lip oxidation and edge-bead instability. The extruder is a single-screw machine with an L/D ratio of 28:1 and a barrier screw, feeding a flat die held at 280–320°C. The melt curtain is drawn down from a die gap of 0.4–0.8 mm to coating weights of 10–30 g/m² on lines running at 100–350 m/min. Nip pressure is maintained at 40–80 kN/m across the chill roll to consolidate adhesion to the fibrous substrate, and the chill roll surface finish is polished to 0.02–0.05 μm Ra. Compliance for food-contact board laminates falls under FDA 21 CFR 176.170(c) for paper and paperboard components in contact with aqueous and fatty foods, with raw-polymer clearance under FDA 21 CFR 177.1520. European laminates are assessed under Commission Regulation (EU) No 10/2011 and EC Regulation 1935/2004. Draw resonance occurs when the draw ratio exceeds a critical value at a given air gap; for DOWLEX 2553-rich formulations the instability is approached at line speeds above 300 m/min when melt temperature is below 280°C. Processors observe edge-bead oscillation as an early marker, and edge trim is adjusted from 20 mm to 40 mm per side before the melt curtain begins to oscillate. Terminal articles include aseptic board lamination, industrial multi-wall wrap, release liners for adhesive tape, and barrier laminates for dry food packaging. The low-temperature boundary is melt freeze at the die lip; below 260°C, coating weight becomes nonuniform and adhesion to kraft drops below the peel values required under ASTM F904.
| Application segment | Relevant standards and codes |
|---|---|
| Cast stretch film | FDA 21 CFR 177.1520(c), Commission Regulation (EU) No 10/2011, ASTM D2103, ASTM D5748 |
| Blown silage film / industrial liners | EN 14932:2018, ASTM D1922, ASTM D1709, ISO 4892-2 |
| Extrusion lamination / coating | FDA 21 CFR 176.170(c), FDA 21 CFR 177.1520, EU No 10/2011, ASTM F904 |
| Injection molding | ISO 294-1, ISO 527-2, ASTM D638, ASTM D256, ASTM D1693 |
| Rotational molding | ASTM D1998-21, ISO 179-1, ASTM D256, NSF/ANSI 61 |
| Masterbatch compounding | EU REACH EC 1907/2006, Directive 2011/65/EU, ISO 11469 |
Thick-walled injection molding of industrial lids and large-diameter access covers pushes DOWLEX 2553 to the upper end of its melt-temperature window because thick sections require low filling resistance while the narrow MWD increases shear heating relative to a broad-MWD grade. The optimal barrel profile runs from 180°C in the feed zone to 230°C at the nozzle. Mold temperature is held between 15°C and 40°C; the lower band is used for shorter cycle times, while the upper band reduces post-molding warpage in flat lids. Injection velocity is set at 80–150 mm/s, holding pressure at 50–80 MPa for 8–15 s, and cooling time for a 3–5 mm wall section is 20–40 s. Clamp force is calculated at 0.4–0.7 tonne/cm² of projected area on hydraulic or toggle presses. Formulations include color masterbatch at 1–4 wt%, a nucleating agent at 0.05–0.2 wt% only when post-molding dimensional change exceeds 0.8% over 48 h at 23°C, and an internal mold release at 0.1–0.3 wt% to prevent sticking on untextured cores. Mechanical performance is verified using ISO 294-1 for specimen preparation, ISO 527-2 for tensile properties, ASTM D638 for tensile modulus, ASTM D256 for notched Izod impact, and ASTM D1693 for environmental stress crack resistance. Density confirmation follows ISO 1183, and food-contact parts are covered under FDA 21 CFR 177.1520(c). Terminal products include 55-gal drum lids, IBC valve covers, agricultural bins, and returnable material handling trays. The main processing conflict in this track is residence time: at barrel temperatures above 230°C or cycle interruptions longer than 10 min, the melt index shifts upward and injection pressure drops, producing sink marks and lower top-load resistance. Purging with a medium-molecular-weight HDPE after shutdown is standard practice on lines processing DOWLEX 2553.
In rotational molding of water tanks and agricultural chemical storage vessels, DOWLEX 2553 is first pulverized to a powder with a 35-mesh particle size distribution before biaxial mold rotation converts it into hollow parts with wall thicknesses from 3 mm to 6 mm. The narrow MWD reduces the interval between first melt and full densification, but this also makes peak internal air temperature control more sensitive. Oven set temperature is maintained at 260–290°C, peak internal air temperature is held at 195–215°C, and the full heating-plus-cooling cycle lasts 20–40 min depending on wall thickness and mold volume. Formulations are dry-blended before charging: hindered amine light stabilizer at 0.2–0.8 wt%, hindered phenolic antioxidant at 0.1–0.3 wt%, carbon black masterbatch at 1–3 wt% for ultraviolet shielding in outdoor service, and internal mold release at 0.05–0.15 wt%. Compliance for storage tanks is established under ASTM D1998-21 for polyethylene chemical storage tanks, impact resistance under ASTM D256 and ISO 179-1, and long-term hydrostatic strength under ISO 9080:2022 where pressure piping connections are involved. Potable water contact requires NSF/ANSI 61 certification and food-contact-grade material under FDA 21 CFR 177.1520(c). The downstream production process uses clamshell or shuttle machines with primary-axis rotation ratios of 4:1 to 6:1 and secondary-axis ratios of 1:1 to 1:5. Cooling starts with forced air for 5–10 min, then water mist until mold surface temperature falls below 70°C, followed by air cooling before demolding. Terminal articles include vertical water storage tanks from 200 L to 10,000 L, agricultural chemical tanks, toolboxes, and recreational hulls. The failure mode associated with under-curing is pinhole leakage and impact strength below 50% of the fully cured value when peak internal air temperature remains under 190°C. Over-curing above 220°C increases internal bubble formation and accelerates antioxidant depletion, which reduces long-term outdoor life under ASTM D2565 accelerated weathering.
The use of DOWLEX 2553 as the carrier resin in high-filler masterbatch production is concentrated in co-rotating twin-screw extrusion, where the narrow MWD provides a stable viscosity profile under high filler loadings and reduces pellet-to-pellet let-down variation. A typical masterbatch formulation contains 30–50 wt% DOWLEX 2553 carrier, 50–70 wt% surface-treated calcium carbonate or talc, 2–6 wt% polyethylene wax dispersant, and 0.5–1.5 wt% calcium stearate acid scavenger. A fluoroelastomer processing aid at 0.1–0.3 wt% is added when die pressure exceeds 8 MPa. Compounding is carried out on a co-rotating twin-screw extruder with an L/D ratio of 40:1, screw speed of 400–600 rpm, barrel set temperatures of 180–250°C, and side stuffing of filler into barrel zones 5–7. Vacuum devolatilization is maintained at -0.08 MPa to remove moisture and low-molecular-weight volatiles before the strand die. Compliance is governed by EU REACH Regulation EC 1907/2006 for chemical safety and Directive 2011/65/EU RoHS for restriction of heavy metals in masterbatch used in electrical and electronic enclosures. ISO 11469 marking is applied to molded articles containing the masterbatch at the specified let-down ratio. The terminal product is masterbatch pellets designed for let-down into film, sheet, injection molding, and blow molding at 2–8 wt% addition, but the narrow MWD carrier is not recommended for high-clarity film masterbatches because the density of DOWLEX 2553 contributes haze above the levels accepted for optical film applications. Filler loadings above 70 wt% raise specific energy demand beyond 0.25 kWh/kg and torque toward the extruder safety limit; this operational boundary defines the upper practical filler concentration.
Competitive Dow DOWLEX™ 2553 Linear Low Density Polyethylene, Narrow MW Distribution prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2553 Linear Low Density Polyethylene is a rotational moulding and profile extrusion grade characterised by a narrow molecular weight distribution and a density of 0.935 g/cm³ measured according to ASTM D792. The melt index is 2.3 g/10 min at 190 °C/2.16 kg using ASTM D1238. The resin is produced via a solution polymerisation route using an ethylene-octene comonomer system, which yields a controlled short-chain branching distribution and a reduced low-molecular-weight tail compared with broad-molecular-weight-distribution linear low density polyethylene. In rotational moulding, these architectural features translate into higher environmental stress-crack resistance, more uniform anisotropic shrinkage, and fewer pin-hole defects in large tanks.
| Property | Test method | Typical value |
|---|---|---|
| Density | ASTM D792 | 0.935 g/cm³ |
| Melt index | ASTM D1238 | 2.3 g/10 min |
| Tensile yield strength | ASTM D638 | 18 MPa |
| Elongation at break | ASTM D638 | 800% |
| Flexural modulus | ASTM D790 | 550 MPa |
| Environmental stress-crack resistance | ASTM D1693 | 1000 h F50 in 100% Igepal |
| Vicat softening point | ASTM D1525 | 119 °C |
| Shore D hardness | ASTM D2240 | 55 |
The property values are typical laboratory values and are not intended as specification limits. Batch-to-batch variation is controlled by the narrow molecular weight distribution; however, on a carousel rotational moulding line with oven gas temperature uniformity of ±5 °C, wall thickness variations in parts exceeding 6 mm nominal wall are more sensitive to cooling rate than to melt flow variation.
The molecular architecture of DOWLEX 2553 is based on a linear ethylene backbone with short-chain branching introduced by 1-octene. Unlike conventional Ziegler-Natta linear low density polyethylene, the narrow molecular weight distribution reduces the concentration of very low molecular weight chains while also limiting the highest molecular weight fraction. The short-chain branching distribution is more homogeneous, which lowers the tendency for low-density fractions to melt prematurely and for high-density fractions to crystallise early during cooling.
At low shear rates, narrow-molecular-weight-distribution resins exhibit less shear thinning than broad-distribution grades of the same melt index. For rotational moulding, this rheological response is acceptable because the process operates at very low shear rates during powder densification and bubble removal. The melt index of 2.3 g/10 min measured at 190 °C/2.16 kg provides sufficient flow to fill complex mould features without requiring the higher melt index values that reduce tensile strength and environmental stress-crack resistance.
Compared with broad-molecular-weight-distribution linear low density polyethylene of the same density and melt index, DOWLEX 2553 displays reduced die swell in profile extrusion and decreased elastic memory. This lowers extrusion-direction orientation and post-mould shrinkage anisotropy. In melt flow testing, the narrow distribution produces a more Newtonian viscosity profile at low rates; however, published capillary rheometry data for this specific grade is limited, and processors should generate a melt flow curve on production equipment when tight dimensional tolerances require exact viscosity control.
Rotational moulding of DOWLEX 2553 is performed on carousel-type machines with independently controlled heating, cooling, and service stations. The resin is typically pulverised to pass 35 mesh (500 µm) because finer powders accelerate densification while coarser particles can leave internal voids. Oven temperature set points of 260 °C to 315 °C are used in production, with the peak internal air temperature target usually between 200 °C and 230 °C. If the peak internal air temperature remains below 190 °C, microvoids and non-coalesced powder remain on the inner wall surface. If it exceeds 260 °C, thermo-oxidative degradation accelerates and visible discoloration plus tensile property loss occur.
Cooling rate in the mould is controlled through forced air, water mist, or water spray. Cooling rates above 8 °C/min in the recrystallisation zone may reduce total crystallinity but can increase warpage in flat panels. Cooling rates below 4 °C/min extend cycle time without proportional improvement in dimensional stability. Symmetrical parts are generally moulded at a rotation ratio of 4:1; complex parts may require 10:1. On production-scale machines with arm indexing, demoulding above 60 °C is avoided because it creates residual thermal stresses and wall distortion.
Pulverisation behaviour is also influenced by melt flow. The melt index of 2.3 g/10 min permits high-speed attrition milling, but frictional heat in the mill can soften the resin. Mill outlet temperatures above 70 °C are associated with particle agglomeration and screen blinding. Water-jacketed pulverisers are therefore used on production lines where throughput exceeds 500 kg/h.
Tensile yield strength of 18 MPa and flexural modulus of 550 MPa position the grade above lower-density linear low density polyethylene for load-bearing tanks while maintaining elongation at break of 800%. Environmental stress-crack resistance exceeds 1000 h in 100% Igepal, which is relevant for detergent and agricultural chemical containers. The Shore D hardness of 55 is typical for a 0.935 g/cm³ density polyethylene and supports scratch resistance in industrial containment parts.
Broad-molecular-weight-distribution linear low density polyethylene provides greater shear thinning and higher melt strength, but it also contains a larger low-molecular-weight fraction that can reduce environmental stress-crack resistance, increase extractables, and contribute to plate-out during processing. In rotational moulding, broad-distribution grades may require lower oven temperatures but often display greater part-to-part warpage variation because the broad distribution broadens the recrystallisation temperature range.
Autoclave low density polyethylene has high long-chain branching, which gives high melt strength and excellent bubble stability in extrusion coating, but its stiffness is lower than DOWLEX 2553 because autoclave grades commonly have densities near 0.923 g/cm³. Tensile yield strength and environmental stress-crack resistance are also lower. The high branching of autoclave low density polyethylene produces a broader melting range and more dimensional variability in thick rotational moulded sections.
DOWLEX 2553 is not a high-melt-strength grade for deep-draw thermoforming or foamed sheet. Where high zero-shear viscosity or high melt tension is required, a broad-distribution LLDPE or low density polyethylene grade should be selected instead. The principal differentiation of DOWLEX 2553 is the combination of 0.935 g/cm³ density, 2.3 g/10 min melt index, and controlled narrow molecular weight distribution, which balances stiffness, stress-crack resistance, and low-shear processability.
Regulatory status for food contact should be verified against FDA 21 CFR 177.1520 and EU Regulation 10/2011 for the specific additive package and end-use conditions. Potable water applications may require NSF/ANSI 61 certification. The resin is not inherently UV stabilised; outdoor exposure requires a carbon black concentration of 2.0–2.5 wt% or a suitable hindered amine light stabiliser formulation. Continuous service above 70 °C under mechanical stress may require oxidation-resistant packaging. Contact with strong oxidising acids, aromatic hydrocarbons, and chlorinated solvents at elevated temperature should be avoided because polyethylene swells and stress cracks.
Polyethylene is non-hygroscopic; pre-drying is not normally required below 60% RH. If pellets are stored below dew point, surface condensation must be removed by drying at 80 °C for 2 h before processing to prevent surface voids. Demoulding is performed below 60 °C to avoid asymmetric post-mould shrinkage; ejection above this threshold is associated with warpage in flat panel production.