| HS Code | 805336 |
| Density | 0.920 g/cm3 |
| Melt Index | 2.5 g/10 min |
| Melt Flow Ratio I10 I2 | 8.0 |
| Tensile Strength At Yield | 9.65 MPa |
| Tensile Strength At Break | 24.1 MPa |
| Elongation At Break | 700 % |
| Flexural Modulus | 0.241 GPa |
| Vicat Softening Point | 98.9 °C |
| Melting Point | 121 °C |
| Haze | 7.0 % |
| Gloss | 85 % |
| Dart Drop Impact | 125 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 350 g |
| Coefficient Of Friction | 0.15 |
| Film Thickness | 31.8 µm |
As an accredited Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2535 is typically supplied in 25 kg multiwall bags or 1000 kg bulk bags, palletized and stretch-wrapped for shipping. |
| Container Loading (20′ FCL) | 20′ FCL: Dow DOWLEX™ 2535 LLDPE, narrow MW distribution, 25 kg bags, palletized, stretch-wrapped, secured; approx. 18–20 MT net. |
| Shipping | Dow DOWLEX™ 2535 LLDPE is shipped as solid resin pellets in 25 kg polyethylene bags on pallets or in bulk trucks/railcars. It is not classified as dangerous goods. Keep containers closed, dry, and away from heat, moisture, and contamination during transport and storage. |
| Storage | Store Dow DOWLEX™ 2535 Linear Low Density Polyethylene in a cool, dry, well-ventilated warehouse. Keep original bags or containers sealed, palletized, and off the floor. Protect from direct sunlight, moisture, heat, and ignition sources. Avoid strong oxidizers and contamination. Maintain stable temperatures, avoid excessive stacking, and practice first-in, first-out stock rotation. Follow the manufacturer’s SDS and local regulations. |
| Shelf Life | Typically 24 months when stored in unopened original packaging, cool, dry, well-ventilated, away from direct sunlight and moisture. |
At cast film line speeds above 450 m/min, edge pinning and transverse thickness uniformity become the limiting production failure modes for octene-comonomer LLDPE in pallet unitization structures. DOWLEX™ 2535, with a melt flow rate of 2.0 g/10 min at 190 °C/2.16 kg per ISO 1133-1:2022 and a density of 0.9195 g/cm³ per ISO 1183-1:2019, is processed as a monolayer or as the core in a two-layer cast stretch film. The narrow molecular weight distribution narrows the shear-thinning transition and reduces gel streaks that otherwise cause film splits during 250–350 % machine-direction pre-stretch. A typical production configuration uses a single-screw extruder with 30:1–33:1 L/D barrier screw and screen pack of 60/80/100 mesh, feeding a flat T-slot die with lip gap 0.5–1.0 mm. Barrel temperatures are held at 190–240 °C, adapter at 240–250 °C, and die at 250–260 °C. The cast web is surface-cooled on a chrome chill roll at 15–25 °C using a vacuum box or air knife for edge pinning, and line speed is typically 300–600 m/min. Formulation practice for a machine-wrap line uses 100 wt% DOWLEX™ 2535 or 80 wt% DOWLEX™ 2535 with 20 wt% autoclave LDPE for cling and unwind force control; polyisobutylene tackifier is added at 0.5–1.5 wt%, while exceeding 1.5 wt% tackifier increases roll blocking and telescoping risk during storage above 35 °C. On production-scale runs, batch-to-batch melt-flow-rate variation outside the certified range alters die pressure and transverse gauge profile; chill-roll speed trimming is applied only if variation exceeds ±0.15 g/10 min. Edge trim from the cast line is reintroduced at up to 15 wt% into the extruder feed provided the trim is surface-cleaned and dried to below 200 ppm moisture. Finished-film mechanical verification uses ASTM D5748 for protrusion puncture resistance, ASTM D882 for tensile properties, and ASTM D5458 for peel cling. Food-contact compliance follows FDA 21 CFR 177.1520(c) and Commission Regulation (EU) No 10/2011, with finished-article migration testing required for fatty food contact. Terminal product types include machine pallet stretch wrap at 10–30 μm, hand stretch wrap, and bundling films for beverage trays and appliance corners.
Because narrow-MWD LLDPE has lower melt strength than an equivalent-melt-index autoclave LDPE, air-cooled blown film lines producing frozen-food freezer bags require dual-lip air-ring control and internal bubble cooling when operating above a blow-up ratio of 2.5:1. Film structures based on DOWLEX™ 2535 are run at 70–90 wt% with 10–30 wt% of a 0.25–1.0 g/10 min LDPE to increase bubble stability. The formulation is dry-blended and processed on a single-screw extruder with 25:1–30:1 L/D, die diameter 200–350 mm, die gap 1.2–2.0 mm, and melt temperature 190–240 °C. The frost line is held at 5–8 die diameters for films of 30–80 μm; bubble flutter at the frost line leads to gauge bands and seal failure if the sizing cage is misaligned by more than 2 mm. Slip and antiblock masterbatch is added at 0.1–0.3 wt% only when the film-to-metal coefficient of friction exceeds 0.4, because higher antiblock loadings reduce clarity and seal strength. Compliance for direct food contact is evaluated under FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, with overall migration testing per EU 10/2011 Annex III and EN 1186-2 where applicable. Terminal products include frozen vegetable pouches, ice cube bags, frozen meat overwrap, and institutional freezer liners. Published comparative data for hot-tack initiation at 120–160 °C in this specific narrow-MWD configuration are limited; seal-bar temperature profiling must be established on the converting line because a ±5 °C deviation shifts seal strength from acceptable to film tearing at the jaw exit.
| Application segment | Die lip gap | Melt temperature range | Cooling condition | Line speed / haul-off |
|---|---|---|---|---|
| Cast pallet stretch film | 0.5–1.0 mm | 200–260 °C | Chrome chill roll 15–25 °C | 300–600 m/min |
| Blown frozen-food film | 1.2–2.0 mm | 190–240 °C | Dual-lip air ring, frost line 5–8 die diameters | 30–80 m/min |
| Agricultural silage wrap | 0.6–1.2 mm | 210–250 °C | Chill roll 15–20 °C | 250–500 m/min |
| Vertical form-fill-seal film | 1.0–1.5 mm | 180–230 °C | Air ring or cast roll | 50–120 m/min |
Agricultural bale wrap made from DOWLEX™ 2535 is produced on cast film lines configured for 25 μm monolayer or 20 μm three-layer structures. The narrow MWD permits high line speeds without gel-induced pinholes, but outdoor UV exposure requires a stabilizer masterbatch added at 1.0–2.0 wt% with a hindered amine light stabilizer system; color concentrates for white or green wrap are added at 2.0–4.0 wt%. The formulation may use 100 wt% DOWLEX™ 2535 or a coextruded skin of 80 wt% DOWLEX™ 2535 with 20 wt% UV-stabilized LLDPE. Production equipment includes a 30:1–33:1 L/D extruder, flat die with 0.6–1.2 mm lip gap, melt temperature 210–250 °C, and chill roll at 15–20 °C; the film is edge-trimmed and wound in 500–750 mm width rolls for round balers. During wrapping, the film is stretched 55–75 % on the baler and applied in 4–6 layers for standard round bales; higher-density grass silage bales require 6–8 layers. Mechanical verification for puncture and tear uses ASTM D5748 and ISO 6383-1, while the product standard is EN 14932:2018 for thermoplastic stretch films for wrapping bales. Terminal products include round and square bale silage wrap, haylage film, and temporary anaerobic storage covers for maize and grass silage. The operational boundary is that films without sufficient UV stabilizer lose tear propagation resistance after 12 months of outdoor exposure; wrapped bales should not be stored at ambient temperatures above 40 °C if more than 6 layers are used, because interlayer blocking reduces oxygen barrier and fermentation quality.
To prevent leaker formation at 60–120 packs/min, a sealant web based on DOWLEX™ 2535 must combine a narrow heat-seal initiation range with sufficient hot-tack strength when the filled pouch exits the jaw. The film is blown or cast at 30–70 μm and converted on vertical form-fill-seal machines with jaw temperature 120–160 °C, jaw pressure 0.3–0.6 N/mm², and dwell time 0.2–0.5 s. The downstream production process involves either a monolayer blown film with 60–80 wt% DOWLEX™ 2535 and 20–40 wt% LDPE, or a coextruded cast film with a sealant layer of 100 wt% DOWLEX™ 2535. The LDPE addition is used to reduce seal initiation temperature and to prevent blocking on the former; antiblock masterbatch is added at 0.1–0.3 wt% only when film-to-film friction exceeds the form-fill-seal machine specification. A seal width of 2–4 mm is maintained on the vertical and horizontal jaws, and hot-tack is evaluated at the jaw exit within 50 ms of opening. Compliance is based on FDA 21 CFR 177.1520 and Regulation (EU) No 10/2011, with overall migration testing required for aqueous and fatty food simulants per EU 10/2011 Annex III. Seal strength is verified under ASTM F88/F88M at the production jaw temperature. Terminal products include frozen vegetable pouches, dried soup pouches, bakery roll bags, and hygiene product overwrap. Published data for this specific grade in high-temperature retort or liquid soup pouches above 90 °C fill temperature is limited; hot-fill configurations require production-scale jaw trials and should not be qualified without seal strength retention testing.
If a three-layer lamination uses a biaxially oriented polyester or biaxially oriented polypropylene outer web and an aluminum foil or metallized barrier core, a cast sealant web of DOWLEX™ 2535 can replace the autoclave LDPE layer to reduce gel-related seal failures and improve seal-strength consistency. The cast web is produced at 20–40 μm on a flat-die cast line using 100 wt% DOWLEX™ 2535 or 80 wt% DOWLEX™ 2535 with 20 wt% metallocene LLDPE for improved seal-through-contamination performance. The downstream process involves corona treatment to 38–42 mN/m, followed by solventless adhesive lamination to the barrier web at 2.0–3.0 g/m² coat weight. The laminated web is cured for 24–48 h at 25–40 °C before slitting to 90–220 mm width for horizontal flow-wrap or pouch machines. Final seal performance is tested with seal-bar temperature 125–155 °C and pressure 0.3–0.6 N/mm². Compliance for food contact is governed by FDA 21 CFR 177.1520 and Commission Regulation (EU) No 10/2011, with EC 1935/2004 traceability documentation required for lamination adhesives. Terminal product types include dry snack pouches, salt and sugar sachets, seasoning pouches, and lidding membranes for dry-shelf bakery trays. The process boundary is that the structure is not rated for retort or high-fat frying above 100 °C; if such conditions are specified, published data for this exact sealant configuration is limited, and a different sealant resin with higher thermal resistance must be qualified separately.
Competitive Dow DOWLEX™ 2535 Linear Low Density Polyethylene, Narrow MW Distribution prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2535 Linear Low Density Polyethylene is a solution-processed linear polyethylene with a deliberately narrow molecular weight distribution. The resin is supplied as a high-flow injection moulding grade distinguished by a published density of 0.921 g/cm³ when determined according to ASTM D792-20 and a melt flow index of 25 g/10 min when measured at 190 °C under a 2.16 kg load using ASTM D1238-20, Procedure A. The narrow molecular weight distribution reduces the concentration of high-molecular-weight chains that are responsible for orientation-induced warpage and anisotropic shrinkage in thick-to-thin transition zones. The grade is formulated for injection moulding of thin-wall rigid packaging, caps and closures, housewares, and appliance components in which flow-length-to-wall-thickness ratios may exceed 150:1. Because the resin is produced in a solution polymerisation process using an ethylene-octene comonomer system, the short-chain branch distribution is more homogeneous than that of typical butene-based gas-phase LLDPE. This characteristic influences crystallisation kinetics and final dimensional stability of moulded parts.
Melt flow index is a single-point viscosity indicator, not a complete moulding specification. At shear rates typical of thin-wall injection moulding, commonly between 10³ s⁻¹ and 10⁵ s⁻¹ in gates and runners, the apparent viscosity of DOWLEX™ 2535 is lower than that of a broad-MWD LLDPE of equivalent density and lower melt index. The narrow molecular weight distribution provides a more Newtonian response at low shear rates because long-chain relaxation modes are reduced. Processors using a 120-ton hydraulic injection moulding machine with a 25 mm or 30 mm diameter single-flighted screw, a compression ratio between 2.5:1 and 3.0:1, and a general-purpose nozzle of 2.0 mm to 3.0 mm orifice diameter typically set a melt temperature between 220 °C and 250 °C. The mould temperature is maintained between 10 °C and 30 °C for unfilled parts. Under these conditions, filling of 0.8 mm to 1.2 mm wall sections requires an injection pressure of 60 MPa to 90 MPa, with holding pressure between 30 MPa and 50 MPa. Published data for this specific configuration is limited; these values represent commercial moulding practice rather than standardised material specifications.
The high melt index of 25 g/10 min facilitates short injection times and reduces pressure loss in long flow paths. However, the low melt strength resulting from the narrow distribution and linear backbone limits use in processes that require melt extensional stability, such as blow moulding and deep-draw thermoforming. In injection moulding, the sharp solidification front is beneficial. The resin begins to crystallise over a relatively narrow temperature interval between approximately 120 °C and 90 °C during cooling, as measured by differential scanning calorimetry at a cooling rate of 10 °C/min per ISO 11357-3:2018. This narrow interval reduces the time spent in the rubbery plateau where anisotropic shrinkage develops. The practical consequence is a lower risk of sink marks, warpage, and post-mould dimensional drift in parts with variable wall thickness.
For moulders running multi-cavity tools, cavity-to-cavity fill balance is controlled by runner geometry and gate dimensions rather than by the material alone. DOWLEX™ 2535 can be run in hot-runner systems with valve gates or open nozzles. When a 16-cavity or 32-cavity closure mould is used, the resin's narrow MWD reduces the variation in flow length caused by barrel residence-time differences. The resulting part-mass standard deviation in a balanced hot-runner tool is typically below 0.5 % when the melt cushion is held constant at 3 mm to 5 mm. If the melt cushion drops below 2 mm, shot-to-shot variation increases and the screw recovery time becomes unstable. This failure mode appears as inconsistent gate vestige dimensions and occasional short shots in the cavity farthest from the sprue. The corrective action is to maintain a minimum cushion of 3 mm and to verify non-return valve function after each material or colour change.
Mechanical property differences arise primarily from comonomer type and molecular weight distribution. DOWLEX™ 2535 is an ethylene-octene linear low density polyethylene. The octene comonomer produces a higher proportion of tie molecules than ethylene-butene grades at equivalent density, which improves environmental stress crack resistance and tensile yield strength. Under ASTM D638-14 at a test speed of 50 mm/min, tensile yield strength for this density range is commonly reported between 10 MPa and 13 MPa, with elongation at break above 500 %. In contrast, high-pressure LDPE of equivalent melt index typically exhibits a tensile yield strength near 8 MPa to 10 MPa and more pronounced shear thinning due to long-chain branching. The narrow MWD of DOWLEX™ 2535 leads to lower die swell and less melt fracture than broad-MWD LLDPE at shear rates above 10⁴ s⁻¹. However, it also results in reduced melt strength. The substitution of DOWLEX™ 2535 for a broad-MWD grade in an existing mould should be accompanied by an evaluation of gate freeze-off time and part ejection temperature.
The difference in solid-state morphology is measurable by differential scanning calorimetry. The octene-based short-chain branches reduce the crystallinity to approximately 45 % to 50 %, compared with 55 % or higher for high-density polyethylene. This lower crystallinity gives the resin a lower modulus and a lower Vicat softening temperature, but improves impact toughness at low temperatures. For thin-wall packaging, the practical effect is that DOWLEX™ 2535 parts can be ejected at lower temperatures than HDPE and are less prone to warpage than polypropylene homopolymer of equivalent melt index. However, the maximum continuous service temperature is correspondingly limited. DOWLEX™ 2535 is not specified for hot-fill or sterilisation applications where sustained temperatures exceed 70 °C; the final part must be tested under the actual service temperature and load.
Mould shrinkage for DOWLEX™ 2535 is influenced by part thickness, gate type, and injection pressure. For unfilled parts with wall thickness between 1.0 mm and 2.0 mm, linear mould shrinkage measured after 24 h at 23 °C and 50 % relative humidity is typically in the range of 1.0 % to 1.4 % when evaluated according to ASTM D955-21. Shrinkage in the flow direction is generally lower than shrinkage transverse to flow because of orientation effects. The narrow MWD reduces the anisotropy ratio to approximately 1.1:1 to 1.3:1, compared with higher ratios for broad-MWD grades. Tool designers should use these values as preliminary estimates only; prototype tools must be built with steel-safe dimensions to allow for shrinkage correction. Parts with long flow lengths and high packing pressures may exhibit shrinkage below 1.0 %, while parts ejected at elevated temperatures can show post-mould shrinkage of an additional 0.2 % to 0.4 % over seven days.
High-pressure LDPE has traditionally been used in closures and overcaps where toughness and torque retention are required. DOWLEX™ 2535 offers a narrower molecular weight distribution and a higher melt flow index, making it suitable for closures with fine-pitch threads and thin annular walls. The higher stiffness of LLDPE relative to LDPE at equivalent density allows wall thickness reductions of 10 % to 15 % without reducing dimensional stability. The replacement requires a reduction in melt temperature. High-pressure LDPE is often processed at 180 °C to 220 °C; DOWLEX™ 2535 requires 220 °C to 250 °C to maintain flow, because its linear backbone has a higher viscosity at equivalent melt index than branched LDPE at low shear rates. The higher melt temperature increases cooling time unless mould cooling is improved. In thick closures with wall sections above 2.5 mm, the cycle time penalty may outweigh the mechanical property benefit. The grade is therefore most competitive in thin-wall closures with wall thickness of 0.8 mm to 1.5 mm, where the high melt flow index enables filling without excessive melt temperature and the narrow MWD keeps warpage low.
At melt temperatures below 210 °C, the viscosity of DOWLEX™ 2535 rises sufficiently to produce injection pressure spikes above 100 MPa in thin-wall tools. This condition may exceed the clamping force of a 120-ton machine and cause flash at the parting line. At melt temperatures above 260 °C, the resin may generate volatile degradation products that appear as splay or silver streaks on the part surface, especially when the residence time exceeds 10 minutes. The practical melt-temperature window for this grade is therefore 220 °C to 250 °C. Screw recovery speed should be set so that the screw rotation completes within 1.5 s to 3.0 s before the cooling time ends. A back pressure of 5 MPa to 10 MPa is sufficient for colour dispersion when using a single-flight screw with a mixing section; higher back pressure increases melt temperature and reduces cycle time.
DOWLEX™ 2535 in natural form does not generally require desiccant drying before injection moulding when stored in closed packaging at ambient relative humidity below 60 %. When the resin is blended with hygroscopic color masterbatch or mineral-filled masterbatch, moisture uptake at the pellet surface can generate splay and surface defects. In these systems, drying for 2 h to 4 h at 60 °C to 70 °C in a desiccant dryer with a dew point below -20 °C is recommended when the ambient relative humidity exceeds 60 %. Prolonged drying above 80 °C should be avoided to prevent pellet surface softening and bridging in the hopper. The resin is thermally stable at standard injection moulding temperatures up to 250 °C; residence time at melt temperature should be kept below 10 minutes. At melt temperatures above 280 °C, the onset of chain degradation produces low-molecular-weight species and can reduce notched impact performance. If a production interruption exceeds 15 minutes, the barrel temperature should be reduced to 160 °C or the screw should be purged with a low-MI polyethylene.
The narrow molecular weight distribution reduces the amount of low-molecular-weight extractable species that migrate to the surface during long residence times. This is relevant to organoleptic performance in food packaging and to paint adhesion in decorated parts. In a 24-hour continuous moulding trial on a 16-cavity closure mould using a 2 wt% polypropylene-based color masterbatch, the accumulation of deposit on the core side was visually lower than that observed with a broad-MWD butene LLDPE of equivalent density and melt flow. The observation is not a substitute for standardised extractables testing; total migration into food simulants must be determined according to EN 1186 and specific migration limits per EU Regulation (EU) No 10/2011.
When DOWLEX™ 2535 is used in multi-component moulding with polypropylene or HDPE, the shrinkage differential must be considered in the tooling design. The linear chain architecture of DOWLEX™ 2535 creates a lower surface energy than polypropylene and a higher coefficient of linear thermal expansion than HDPE. In sequential overmoulding, adhesion is mechanical rather than chemical; mechanical interlocks or through-holes are required. The resin is not recommended for co-extrusion with polar barrier polymers without an adhesive tie layer because the non-polar ethylene-octene backbone does not form polar bonds to EVOH or polyamide. Published data for this specific configuration is limited.
For food-contact applications, DOWLEX™ 2535 is designed to meet the compositional requirements of FDA 21 CFR 177.1520 for olefin polymers and the relevant monomer restrictions in EU Regulation (EU) No 10/2011. Compliance is not a property of the resin alone; the finished article must be tested under its intended conditions of use, including temperature, time, and food simulant categories. Migration testing is conducted according to EN 1186 series methods or FDA migration protocols. Processors must also verify that any added masterbatch, lubricant, or processing aid meets the same regulatory status. The resin is not intended for medical implant use and is not classified as hazardous under CLP Regulation (EC) No 1272/2008. Consult the manufacturer's safety data sheet for specific handling and disposal guidance.