| HS Code | 747504 |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Comonomer | 1-Octene |
| Molecular Weight Distribution | Narrow |
| Density | 0.920 g/cm³ |
| Melt Index 190 C 2 16 Kg | 0.50 g/10 min |
| Melt Flow Ratio I10 I2 | 7.5 |
| Melting Point | 124 °C |
| Vicat Softening Point | 95 °C |
| Tensile Yield Strength | 10 MPa |
| Tensile Break Strength | 25 MPa |
| Elongation At Break | 800 % |
| Flexural Modulus | 240 MPa |
| Shore D Hardness | 50 |
| Thermal Conductivity | 0.33 W/m·K |
| Haze | 10 % |
| Gloss 45 | 70 % |
| Dart Impact Strength | 120 g |
As an accredited Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | DOWLEX™ 2505 LLDPE is typically packaged in 25 kg polyethylene-lined bags, palletized, and 1,000 kg bulk bags for industrial handling. |
| Container Loading (20′ FCL) | 20′ FCL loading: DOWLEX™ 2505 narrow MW distribution LLDPE resin, 25 kg bags, palletized/floor-loaded, secured; approx. 20–22 MT net. |
| Shipping | Shipping: Dow DOWLEX™ 2505 Linear Low Density Polyethylene is a non-hazardous, solid resin supplied in bags or bulk. Transport in clean, dry, covered vehicles at ambient temperature, avoiding moisture, heat, and direct sunlight. Keep packaging sealed and comply with local regulations; no special dangerous goods classification required. |
| Storage | Store DOWLEX™ 2505 in a cool, dry, well-ventilated area away from direct sunlight, heat, flames, and oxidizing agents. Keep original packaging closed and elevated off floors to prevent moisture and contamination. Avoid prolonged UV exposure and extreme temperatures. Use first-in, first-out stock rotation. Maintain clean handling to prevent foreign matter pickup. Store in accordance with local regulations. |
| Shelf Life | Stable under normal storage conditions; indefinite shelf life when kept cool, dry, and in sealed original packaging away from sunlight. |
In three-layer heavy-duty sack coextrusion, DOWLEX™ 2505 with a nominal density of 0.935 g/cm³ and a melt flow rate of 0.5 g/10 min under ASTM D1238 at 190°C/2.16 kg is metered into the two outer skin layers at 60–80 wt%. The auxiliary resin is a high-pressure low-density polyethylene with a melt flow rate of 0.3–0.6 g/10 min and a density of 0.920–0.925 g/cm³. The core layer is charged with in-house reclaimed film scrap, metallocene-hexene LLDPE, or high-melt-strength LDPE at 20–35 wt% of total throughput. Extrusion is performed on barrier screws with L/D ratios of 30:1 to 36:1 and screw diameters between 65 mm and 90 mm. Melt temperature at the die entry is held between 215°C and 235°C. The die gap is set at 1.8–2.4 mm on a die diameter of 200–300 mm. A dual-lip air ring with chilled air at 8–15°C and an internal bubble cooling unit are operated simultaneously at a blow-up ratio of 2.5:1–3.5:1. Frost line height is maintained between 700 mm and 900 mm on a 300 mm die.
Narrow molecular weight distribution in DOWLEX™ 2505 reduces high-shear viscosity and permits faster drawdown, but the grade does not generate the strain-hardening response characteristic of high-pressure LDPE. Bubble edge weave and vertical tension oscillations are observed when LDPE content in the skin layer falls below 15 wt% at line speeds above 45 m/min. On a three-layer line fitted with a 300 mm die and internal bubble cooling, pressure differential across the collapsing frame is monitored continuously. Excursions above 0.8 kPa correlate with web wander at the winder. Gauge bands are controlled to ±3 µm on a final film thickness of 65 µm using an air ring with automatic profile control. Dart impact is measured under ASTM D1709 Method A after conditioning at 23±2°C and 50±5% RH for 40 h. Elmendorf tear resistance in machine and transverse directions is recorded under ASTM D1922. Tensile yield and elongation are evaluated at 500 mm/min according to ISO 527-3. In full-scale production trials on a three-layer line with a 250 mm die, the structure change from a butene LLDPE skin to a DOWLEX™ 2505/LDPE blend reduced gauge variation at the winder by ±1.5 µm when the outer skin contained 70 wt% DOWLEX™ 2505. Published data for other configurations is limited.
The finished sacks are used for 25 kg and 50 kg fill weights of polymer pellets, film scrap, and mineral powders. Sack mouths are heat-sealed at 150–170°C with 1.0 s dwell time. Seal strength is checked to exceed 20 N/15 mm under ASTM F88. Because the narrow MWD grade lowers zero-shear viscosity, extruder backpressure at 220°C runs 5–10% lower than a broad-MWD butene LLDPE of equivalent melt flow rate. The structure is not recommended for sacks requiring continuous exposure to hot fill above 80°C without an HDPE-rich core layer.
A 25:75 to 40:60 blend of DOWLEX™ 2505 and a metallocene-catalysed ethylene-octene plastomer is used in cast-film production of lamination webs for frozen food and dry snack packaging. The plastomer has a nominal density of 0.902 g/cm³ and a melt flow rate of 1.0 g/10 min under ASTM D1238. Blending is performed offline by rotary drum tumblers with a batch size of 500 kg, followed by direct feed into a single-screw extruder with L/D 30:1 and a barrier melt section. The flat die has a width of 1,600 mm and a die gap of 0.6–0.8 mm. Melt temperature at the die is 230–240°C. Chill roll temperature is set to 18–22°C, and the air gap is kept below 100 mm to suppress neck-in. Line speed is maintained between 150 m/min and 220 m/min for a 30–40 µm web. The cast web is corona-treated in-line at 2.0–3.0 kW and wound with taper tension of 8–12 N per 100 mm width.
The narrow molecular weight distribution shifts the onset of the seal plateau downward. Heat-seal initiation is observed at 105–115°C on a laboratory heat sealer operating at 0.3 MPa jaw pressure and 0.5 s dwell time, compared with 115–125°C for a broad-MWD butene LLDPE of the same nominal density. Seal strength after 0.5 s dwell is evaluated under ASTM F88; seal continuity is inspected at 10× magnification. Haze is measured under ASTM D1003 after 24 h conditioning and is maintained below 5% for a 30 µm web. Gloss at 60° under ASTM D2457 is controlled above 85 GU. Due to the low melt strength of the narrow MWD grade, the web should not exceed 12 g/m² coating weight in this cast process. At higher thicknesses, draw resonance creates transverse gauge bands on chill rolls below 18°C.
Food-contact compliance for the cast lamination web is verified under FDA 21 CFR 177.1520(c) paragraph 3.2a for olefin polymers, subject to end-use temperature and food-type conditions. European Union migration testing is performed under EU Regulation No 10/2011 with simulants A, B, and D2. The following standards and test conditions apply to the final laminated structure.
| Regulation/Standard | Test condition | Limit or clause |
|---|---|---|
| FDA 21 CFR 177.1520(c) | End-use temperature ≤100°C | Olefin polymer, 3.2a |
| EU Regulation No 10/2011 | Simulant A, 10 days at 40°C | Overall migration 10 mg/dm² |
| ASTM F88 | 0.5 s dwell, 0.3 MPa | Minimum seal strength 15 N/15 mm |
| ASTM D1003 | 30 µm web | Haze 5% |
For frozen food packaging, the cast lamination web is adhesive-laminated to a metallized PET outer layer using a solventless polyurethane adhesive at 1.8–2.2 g/m². Filled pouches are drop-tested at -20°C according to ASTM D5276; cracks or seal failures are not permitted. The converted structure is run on vertical form-fill-seal machines with jaw closing force of 600–900 N and seal bar temperature of 120–135°C. Finished pouches range from 0.5 kg to 2.5 kg fill weight. Because the narrow MWD grade has lower zero-shear viscosity, extruder backpressure at 230°C is 5–10% lower than a butene LLDPE of equivalent melt flow rate.
Where a 15 L UN-certified canister must survive drop impact at -20°C, DOWLEX™ 2505 is introduced into bimodal HDPE at 20–35 wt%. The bimodal HDPE base has a density of 0.948–0.952 g/cm³ and a melt flow rate of 0.2–0.4 g/10 min. Extrusion blow moulding is performed on an accumulator-head machine with a 60 mm screw, L/D 24:1, and a die gap of 1.5–2.0 mm. Melt temperature is held at 190–205°C. The narrow MWD of DOWLEX™ 2505 lowers zero-shear viscosity and increases parison sag when the LLDPE fraction exceeds 35 wt%. Sag is quantified by optically tracking the lower parison edge over 5 s. A sag displacement above 8% of initial parison length produces wall-thickness variation above 12% in the finished canister.
Moulds for 15 L canisters require clamp force of 180–250 t, blow pressure of 0.8–1.0 MPa, and mould temperature of 10–18°C. Minimum wall thickness after trimming is 2.0 mm. Environmental stress crack resistance is tested under ASTM D1693 Condition B in 100% Igepal CO-630 at 50°C. Blends with 25–35 wt% DOWLEX™ 2505 typically exceed 1,000 h without failure. Drop impact at -20°C is evaluated according to ASTM D2463. The finished canisters are used for agricultural chemical concentrates and lubricant additives. Hydraulic pressure testing is performed at 250 kPa for 30 min. The structure is not recommended for continuous contact with concentrated amine-based additives above 40°C because stress cracking accelerates in alkaline media.
Sheet extrusion of weldable secondary-containment liners blends DOWLEX™ 2505 with medium-density polyethylene at 35–50 wt% to improve low-temperature stress crack resistance. The MDPE base resin has a density of 0.934–0.938 g/cm³ and a melt flow rate of 0.2–0.5 g/10 min. Sheet is produced on a single-screw extruder with L/D 33:1 and a 2,200 mm flat die with a die gap of 2.0–2.5 mm. The three-roll stack is set to 80–95°C, with polishing roll pressure of 0.4–0.6 MPa. Take-off speed is maintained at 3–6 m/min for a 1.5 mm sheet. The sheet is corona-treated to 44–48 mN/m prior to welding.
Weld seams are produced on automatic wedge welders with hot-air temperature of 420–450°C and welding speed of 1.5–2.5 m/min. Seam peel and shear strength are tested under ASTM D6392; welds must exceed 90% of parent sheet yield stress. Low-temperature bending is checked at -30°C according to ISO 974. Because DOWLEX™ 2505 contains no external slip package, surface coefficient of friction is controlled by texturing rolls at 70–80°C to a roughness Ra of 3–6 µm. The rough surface reduces weld contamination from dust but raises extrusion backpressure if the roll gap is below 1.8 mm.
The finished panels are welded into sump liners and bund walls for 1,000–5,000 L agricultural chemical tanks. Chemical compatibility is reviewed against DIN EN 13361 and DIN EN 13492 for geomembrane barriers. Published long-term outdoor weathering data for this specific DOWLEX™ 2505/MDPE sheet is limited. The structure is specified with a carbon black masterbatch at 2.5 wt% to meet ISO 13438 oxidation induction time requirements. The sheet is not recommended for continuous exposure to concentrated amine-based chemicals above 40°C.
Woven polypropylene tarpaulins are coated with a DOWLEX™ 2505/LDPE blend at 15–25 g/m². The blend consists of 40 wt% DOWLEX™ 2505 and 60 wt% high-pressure LDPE with a melt flow rate of 0.8–1.2 g/10 min. Extrusion lamination is performed on a T-die with a die gap of 0.6 mm, an air gap of 120–160 mm, and a chill roll at 15–20°C. Melt temperature at the die is 240–255°C. Nip pressure is set to 3–5 bar on a rubber roll of Shore A hardness 75–80. Neck-in is monitored across the die; acceptable values are below 8 mm per metre of die width. The woven PP substrate is corona-treated to 38–42 mN/m immediately before the nip.
Adhesion to the woven substrate is verified by peeling at 180° under ASTM D903. Lamination strength above 3 N/15 mm is required for flexible intermediate bulk container liners. The coated fabric is converted by hot-air welding at 350–400°C with 0.5–1.0 s dwell. Because DOWLEX™ 2505 has a narrow molecular weight distribution, the coating exhibits low heat-seal contamination and stable drawdown at 250 m/min. At coating weights above 25 g/m², draw resonance occurs unless the die gap is reduced to 0.5 mm and the air gap is shortened to 90 mm.
The laminate is used for bulk-bag outerwalls, scaffold sheeting, and intermediate bulk container liners with 1,000–1,500 kg safe working load. Tear propagation is evaluated under ASTM D5884. Hydrostatic resistance is tested under ISO 1420 at 200 kPa. Compliance with the REACH candidate list is confirmed at the lot level. Because the coating is not flame-retardant, a halogen-free phosphinate FR masterbatch is incorporated at 8–12 wt% when the tarpaulin is specified for scaffold containment; the FR masterbatch raises melt pressure by 10–15% at the same screw speed.
Competitive Dow DOWLEX™ 2505 Linear Low Density Polyethylene, Narrow MW Distribution prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2505 Linear Low Density Polyethylene is a narrow molecular weight distribution ethylene-octene copolymer produced by solution polymerization and supplied as pelletized resin. The grade is specified with a melt index of 2.0 g/10 min at 190 °C/2.16 kg per ASTM D1238 and a nominal density of 0.932 g/cm³ per ASTM D1505. The narrow distribution corresponds to a reduced concentration of very high-molecular-weight chains and a lower low-molecular-weight tail than conventional broad-distribution Ziegler copolymers, which lowers melt elasticity, reduces die swell, and changes the shear-thinning transition. Long-chain branching is intentionally low, so extensional strain hardening is lower than autoclave LDPE. These properties place the grade in high-drawdown cast film, extrusion coating, and lamination processes rather than in blown-film applications that depend primarily on melt strength for bubble stability.
Molecular structure also influences sealing, opticals, and extractables. A narrow distribution decreases the low-molecular-weight fraction that can migrate into packaged contents, but it may also raise the seal initiation temperature relative to LDPE-rich formulations. Equipment runnability is affected by the more abrupt viscosity curve: pressure fluctuations in a starved feed zone are less damped by high-molecular-weight chain entanglement, which increases the importance of melt pump stability on high-speed cast lines. Batch-to-batch density variation should be monitored because a shift of 0.002 g/cm³ in this LLDPE class can change flexural modulus by approximately 30–50 MPa.
On production-scale cast lines using 75–90 mm, 30:1 L/D single-screw extruders with barrier screw geometry and Maddock mixing sections, the resin is typically processed with a rising temperature profile from 200 °C in the feed zone to 270 °C at the metering zone and a melt temperature of 260–290 °C at the die. Screw speeds are line-rate dependent; for a 75 mm extruder running at 80–120 min⁻¹, output rates of 120–180 kg/h are common when die width and chill-roll speed are matched to produce 20–50 μm film. The use of a melt pump between extruder and die reduces surging and improves gauge uniformity because the resin’s narrow molecular weight distribution gives a more abrupt viscosity transition and can amplify pressure fluctuations when the extruder is operated below its stable pumping range.
Cast film dies are set at 0.5–1.0 mm gap; the wider gap is required for thicker film above 40 μm or for extrusion coating with an air gap above 15 cm. Chill-roll temperatures are maintained at 18–25 °C to control crystallization rate. Lower temperatures in this band increase quench-driven orientation and can improve optical clarity, whereas higher temperatures reduce blocking by allowing relaxation before winding. For extrusion coating onto paperboard or aluminum foil, line speeds up to 250 m/min have been reported in industrial practice with 300–350 mm slot dies and air gaps of 10–15 cm; neck-in and draw resonance are the two limiting defects. Published data for this specific configuration is limited, and these ranges represent industrial practice rather than guaranteed operating limits.
Representative published resin properties for DOWLEX 2505 are listed below. They are typical values obtained from controlled specimens, not batch-release specifications. Converters should verify the purchased lot against the certificate of analysis and the equivalent ISO 1133-1:2022 and ISO 1183-1:2019 methods where required.
| Property | Test method | Typical value |
|---|---|---|
| Melt index | ASTM D1238 | 2.0 g/10 min |
| Density | ASTM D1505 | 0.932 g/cm³ |
| Tensile strength at yield | ASTM D638 | 16 MPa |
| Elongation at break | ASTM D638 | 800 % |
| Flexural modulus, 1% secant | ASTM D790 | 550 MPa |
| Vicat softening point | ASTM D1525 | 121 °C |
| Low-temperature brittleness | ASTM D746 | < -75 °C |
The 121 °C Vicat softening point and < -75 °C low-temperature brittleness place the grade between conventional low-density polyethylene and medium-density polyethylene in thermal resistance while preserving deformation resistance under cold-chain conditions. These values are density-dependent, and incoming lot density should therefore be monitored when the resin is used in thin-gauge structures where stiffness controls the end-use performance.
For cast film structures below 30 μm total thickness, the grade’s narrow distribution reduces gauge variation but also lowers the melt extensional stress that resists draw resonance. In coextruded structures with a low-melt-index sealant skin, processors often blend 5–10 wt% autoclave LDPE into the core layer to restore web stability; this addition typically reduces line-speed fluctuation without eliminating the increased stiffness and dart impact contributed by the LLDPE fraction. On blown-film lines, the same low melt strength requires a blow-up ratio below 2.2:1, a reduced frost line height, and a high-density-neck air ring; without such adjustments, bubble instabilities appear as a consequence of limited strain hardening. The resin is therefore used preferentially in cast film and extrusion coating rather than blown film. When downgauging to 15 μm cast film, gel counts and surface roughness become more sensitive to screw condition, barrel temperature overshoot, and filter pack cleanliness than broad-MWD resin because low-mobility chains are less available to mask localized melt defects.
Comparative cast film data generated at 25 μm thickness under ASTM D882 testing indicate that DOWLEX 2505 delivers tensile elongation values above 800%, while dart drop impact measured by ASTM D1709 Method A commonly falls in the 110–140 g range. LDPE of similar melt index typically yields dart drop values of 60–80 g and lower puncture resistance, but LDPE retains higher neck-in resistance and better melt strength during extrusion coating. Against broad-MWD Ziegler LLDPE of equivalent 0.932 g/cm³ density, the narrow distribution reduces die lip buildup and improves high-shear drawdown, while low-shear melt viscosity is lower. The consequence is a narrower operating band in slow-forming processes and a lower tolerance for wide air gaps. Under ASTM D1003 haze testing on 50 μm cast film, the narrow-MWD resin typically yields values below 8%, but the result is strongly influenced by chill-roll surface finish and cooling water temperature.
Extensional rheometry of narrow-MWD LLDPE shows a later onset of strain hardening relative to LDPE. At Hencky strain rates of 1.0 s⁻¹ and 150 °C, the transient extensional viscosity remains closer to the linear viscoelastic envelope than autoclave LDPE, which rises sharply due to long-chain branching. The practical result is lower resistance to air-gap sag but more uniform drawdown once contact with the chill roll is established. Die lip buildup on cast lines is often tied to low-molecular-weight fractions migrating to the die surface; the lower low-end tail of DOWLEX 2505 slows the formation of oxidized deposits on the die lip during extended runs at constant output.
Regrind addition beyond 30 wt% in edge-trim recycle has been associated with increased gel count, optical haze, and odor in cast film, particularly when the regrind has undergone repeated extrusion above 280 °C. The narrow molecular weight distribution provides less low-molecular-weight material to wet and homogenize oxidized trim fragments; as a result, gels and fish eyes are not readily masked. Processors running closed-loop trim recycle on 90 mm cast lines report that the use of a 100 μm melt filter pack and a melt temperature cap of 290 °C maintains gel counts below acceptable film-processing thresholds when regrind is kept under 25 wt%. Above that level, gel-related extrusion coating voids may appear at coat weights below 15 g/m².
The resin should be stored at temperatures below 50 °C and protected from ultraviolet exposure during extended warehouse storage. Moisture uptake is not typically a processing issue for virgin pellets, but wet regrind should be dried at 70–80 °C for 2 h before blending. During transitions from LDPE to this grade, barrel temperatures should be raised to 240 °C before startup, and a fracture-resistant LDPE or commercial purging compound should be used. Extended shutdown at temperatures above 180 °C in the die can degrade the narrow-distribution chains, leading to black specks and a melt index increase.
Applications documented for this resin class include high-drawdown cast stretch film core layers, lamination base films for printed packaging, and extrusion coating for moisture-resistant paper and board. In lamination, adhesion to substrates is typically promoted by corona treatment to a surface energy of 38–40 mN/m measured per ASTM D2578. Heat seal performance is evaluated by ASTM F88 and hot tack by ASTM F1921; the narrow distribution reduces low-molecular-weight seal-initiation aids, so the seal initiation temperature is slightly higher than for an LDPE-rich formulation of equivalent density. Compared with metallocene LLDPE film grades of similar density and melt index, DOWLEX 2505 may exhibit lower clarity at 50 μm cast thickness but is more tolerant of extrusion temperature fluctuations and less prone to melt fracture.
Regulatory inquiries are lot-specific. The standards commonly applied to this resin class are listed below. Verification against the lot-specific statement of composition remains mandatory because additives and catalyst residues influence migration and odor.
| Regulation or standard | Relevance |
|---|---|
| FDA 21 CFR 177.1520(c)(3.2a) | Olefin polymers for food-contact articles |
| EU Regulation 10/2011 | Specific migration limits and overall migration testing for food-contact plastics |
| REACH 1907/2006 | Registration, evaluation, authorization, and restriction of substances |
| RoHS 2011/65/EU | Restricted substances in electrical and electronic equipment components |