Dow Dowlex 2503 Linear Low Density Polyethylene Narrow Mw Distribution

Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution

    • Product Name: Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 525590
    Density 0.920 g/cm³
    Melt Index 190 C 2 16 Kg 0.75 g/10 min
    Melt Flow Ratio I10 I2 8.0
    Tensile Strength At Yield 9.65 MPa
    Tensile Strength At Break 24.1 MPa
    Elongation At Break 700%
    Flexural Modulus 1 Secant 0.241 GPa
    Vicat Softening Point 92.0 °C
    Melting Point Dsc 122 °C
    Crystallization Temperature Dsc 105 °C
    Dart Drop Impact 200 g
    Elmendorf Tear Strength Md 200 g
    Elmendorf Tear Strength Td 300 g
    Haze 10%
    Gloss 45 60%
    Coefficient Of Friction 0.20

    As an accredited Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2503 LLDPE is packaged in 25 kg polyethylene bags, with 40 bags per 1,000 kg pallet.
    Container Loading (20′ FCL) 20′ FCL: DOWLEX™ 2503 Linear Low Density Polyethylene (narrow MW distribution), 25 kg bags, palletized/floor-loaded, within payload limits.
    Shipping Dow DOWLEX™ 2503 LLDPE is shipped as solid, non-hazardous resin pellets. Typical packaging includes 25 kg polyethylene-lined bags, 500–1000 kg supersacks, or bulk trucks/railcars. Store in a cool, dry, ventilated area away from heat, moisture, and direct sunlight. No special transport classification required.
    Storage Store DOWLEX™ 2503 in a cool, dry, well-ventilated area away from direct sunlight, heat, ignition sources, and strong oxidizers. Keep containers tightly closed and palletized in original packaging to prevent moisture, dust, and contamination. Avoid prolonged high temperatures and UV exposure. Do not store near food, feed, or drinking water. Follow local regulations and the manufacturer’s SDS.
    Shelf Life Shelf life is 2 years when stored in a cool, dry place in original packaging, protected from direct sunlight and heat.
    Application of Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution

    DOWLEX™ 2503 is an ethylene-1-octene linear low density polyethylene with a nominal density of 0.925 g/cm³ under ISO 1183-1 and a nominal melt index of 0.25 g/10 min under ISO 1133-1:2022 at 190 °C/2.16 kg. The narrow molecular weight distribution shifts the melt rheology toward lower low-shear viscosity and lower melt elasticity than a broad-MWD autoclave LDPE of the same density. The resin is therefore used in converting platforms where bubble tension, seal response, and tear balance are controlled by molecular architecture rather than by long-chain branching. The scenarios below define operating conditions at production scale; where a specific published dataset for DOWLEX 2503 is unavailable, the text identifies the boundary of the transferred data instead of presenting unverified values.

    What Melt Temperature Window Prevents Bubble Instability in Heavy-Duty Liner Extrusion?

    On a 90 mm single-screw extruder with a 30:1 L/D barrier screw and a 250 mm spiral mandrel die, the melt temperature is maintained at 204–227 °C. The narrow MWD reduces melt elasticity relative to an autoclave LDPE; once the melt exceeds 232 °C, bubble oscillation becomes measurable because the extensional viscosity drops below the level required to support a 2.0:1 to 2.6:1 blow-up ratio. A dual-lip air ring delivering 8–12 m³/min and an internal bubble cooling exhaust temperature of 32–40 °C keep bubble diameter variation within ±3 mm at film thicknesses from 125 µm to 250 µm. Die gap is set at 1.8–2.3 mm, and frost line height is held at 6–8 die diameters to prevent excessive transverse direction shrinkage after winding. For 100 wt% DOWLEX 2503 liners, output is typically restricted to 180–210 kg/h; higher throughput up to 260 kg/h is achieved by dry-blending 10–20 wt% LDPE with MI 2.0 g/10 min to increase melt strength. Dart impact of the finished liner is measured per ASTM D1709-A; construction and demolition liner specifications commonly require greater than 500 g at 200 µm. Non-food hazardous waste liners are governed by ASTM D4976-12a and landfill acceptance criteria; food-contact clearance is not required for this end use. End products include asbestos abatement bags, tunnel spoil liners, and flood control tubing.

    Greenhouse cover films coextruded with EVA skins use DOWLEX 2503 in the core layer at 60–80 wt% of total thickness. The surrounding skins contain EVA with 12–18 wt% vinyl acetate to raise low-temperature flex crack resistance and heat retention. Total film thickness is 180–200 µm for multi-season installations; the melt temperature is kept at 195–210 °C because EVA skins begin acetoxy degradation above 220 °C. UV stabilisation is introduced through a HALS masterbatch at 0.4–0.8 wt% and a benzotriazole UV absorber at 0.2–0.4 wt%; anti-fog concentrate at 1.0–1.5 wt% is restricted when the greenhouse film also contacts edible crops. The bubble is run at a 2.4:1 blow-up ratio with frost line height at 7 die diameters to balance haze and impact resistance. Tensile properties are tested per ISO 527-3; accelerated weathering is carried out under ISO 4892-2 cycle 1 with a target of 60% retained elongation after 3,000 h xenon-arc exposure for multi-season use. Published data for the specific grade in greenhouse film is limited; the retained elongation target is a design specification from film producers rather than a grade-specific guarantee. If the silage film contacts fermented feed, EU Regulation No 10/2011 does not apply; heavy metal documentation is typically supplied under EU Packaging Directive 94/62/EC. End products include greenhouse covers, silage bags, and low-tunnel cloche film.

    Frozen Food Sealant Web and the Onset of the Seal Plateau in 2503

    Vertical form-fill-seal conversion of three-layer frozen food pouches places a 12–25 µm sealant layer of DOWLEX 2503 against a barrier core of EVOH with tie layers. The sealant layer represents 15–30% of the total film thickness of 40–80 µm, and the pouch is sealed at jaw temperature from 115 °C to 130 °C, dwell time 0.3 s, and jaw pressure 2.5 bar. Heat seal strength is determined by ASTM F88; octene LLDPE of 0.925 g/cm³ density typically initiates a measurable seal at 88–96 °C and reaches a usable plateau at 110–125 °C. The specific seal initiation value for DOWLEX 2503 in an EVOH-containing structure is not published, so the above range is treated as an equipment-setting target rather than a grade-defined physical constant. Cold-temperature abuse resistance of the filled pouch is verified by ASTM D1922 Elmendorf tear and ASTM D1709 dart impact after conditioning at -25 °C for 24 h. Migration compliance is addressed through US FDA 21 CFR 177.1520(c) conditions 3.1a or 3.2a and EU Regulation No 10/2011 with the overall migration limit of 10 mg/dm². End products include frozen vegetable pouches, ice crystal-resistant overwrap for seafood, and deep-frozen bakery bags.

    Because high-speed form-fill-seal lines impose a shorter hot-tack window, tubular film of DOWLEX 2503 is extruded at 150–200 µm, corona-treated to 42–48 mN/m per ASTM D2578, and converted into industrial powder sacks. The FFS line seals the tube at 160–190 °C with water-cooled seal bars held at 15–20 °C; the cool time is set at 0.8–1.2 s to prevent hot-tack failure during the filling pulse. The narrow MWD requires a lower seal bar temperature than a broad-MWD LLDPE of similar density because the absence of a high-molecular-weight tail accelerates chain relaxation during sealing. Top-load compression of the filled sack is measured per ASTM D642; a typical filled sack of 25 kg must withstand 1,800–2,200 N without weld splitting. For UN-certified powder packaging, the filled sack is subjected to drop testing at -18 °C after conditioning for 24 h. Compliance for non-food industrial powders is limited to the packaging user’s internal hazard classification; REACH polymer registration and RoHS heavy metal limits for electrical equipment are not triggered for these non-electrical industrial sacks. End products include sacks for resin pellet export, mineral fillers, and open-mouth cementitious powder bags.

    When Collation Shrink Requires a 15–25 wt% LDPE Blend Partner

    To raise low-shear melt memory in collation shrink film, DOWLEX 2503 is dry-blended with 15–25 wt% autoclave LDPE before double-bubble orientation. The primary tube is extruded at 180–200 µm on a 50 mm extruder with a cavity transfer mixer at 20–30 rpm; blend homogeneity is monitored by melt pressure variation below ±0.5 bar. Orientation in the second bubble is operated at 1:3.0–1:3.2 transverse draw and 1:3.0 longitudinal draw, with bubble temperature held at 105–125 °C. Below 105 °C stress whitening appears on the film surface, while bubble rupture frequency increases above 128 °C. Shrink tension at 120 °C is specified per ISO 14616 in the 0.5–1.5 N/15 mm band depending on bottle mass; the lower end of the band is selected for lightweight water bottles to avoid seal seam distortion. The final film is not normally a direct food-contact layer; where a packer requires food-contact assurance for the outer secondary packaging, EU Regulation No 10/2011 applies only at the outer surface. End products include bottled water collation shrink, canned food tray overwrap, and hygiene multipack film.

    Flexible membrane liners of 0.75–1.50 mm nominal thickness are produced by flat-die cast extrusion of DOWLEX 2503 on a 120 mm grooved-feed extruder with 38:1 L/D and a 2,000 mm coat-hanger die with lip gap 1.5–2.0 mm. Melt temperature is set at 210–230 °C; the calender roll stack is held at 60–80 °C to control surface embossing without generating transverse thickness variance. The narrow MWD allows a relatively low melt temperature during flat-die drawdown, which reduces oxidative gel formation on the die lip during long campaigns. Tensile properties are measured per ASTM D6693; puncture resistance is determined by ASTM D4833, and low-thickness tear resistance by ASTM D1004. Geomembrane specification for flexible LLDPE liners commonly follows GRI-GM17, with carbon black dispersion tested per ISO 18553 and melt flow verification per ISO 1133-1:2022. Published case data for this exact grade in geomembrane service is limited; the above conditions are standard for LLDPE geomembrane converters but should not be read as a project-specific durability guarantee. End products include pond liners, temporary landfill covers, and canal lining membranes.

    Free Quote

    Competitive Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2503 Linear Low Density Polyethylene, Narrow MW Distribution is a high-flow injection-molding grade produced from an ethylene/α-olefin copolymerization route. The resin belongs to the linear low-density polyethylene family, meaning the backbone is predominantly linear with short-chain branching introduced by comonomer insertion, rather than the long-chain branching characteristic of high-pressure LDPE. The product designation includes the phrase “Narrow MW Distribution” because the molecular architecture has been controlled to reduce the high-molecular-weight tail and to narrow the relaxation spectrum relative to conventional autoclave LLDPE. Published nominal values include a melt mass-flow rate of 75 g/10 min at 190 °C/2.16 kg under ISO 1133-1:2022 and a density of 0.930 g/cm³ under ISO 1183-1:2019. These coordinates place the grade in the high-fluidity, moderate-stiffness segment of olefin injection-molding materials. The typical application envelope therefore covers thin-walled food containers, dairy-cup lids, caps, closures, housewares, and reusable consumer articles molded in multi-cavity tools.

    Representative mechanical data reported for the grade are summarized below; values are nominal and not intended as specification limits.

    PropertyNominal valueTest method
    Melt mass-flow rate75 g/10 minISO 1133-1:2022
    Density0.930 g/cm³ISO 1183-1:2019
    Tensile stress at yield10 MPaISO 527-2:2012
    Tensile strain at break>800 %ISO 527-2:2012
    Flexural modulus, 2 mm/min260 MPaISO 178:2019
    Shore D hardness55ISO 868:2003
    Vicat softening temperature A5091 °CISO 306:2022

    Melt Rheology and Narrow-Distribution Effects on Injection Pressure

    Molecular weight distribution is conventionally expressed as the ratio of weight-average to number-average molecular weight, Mw/Mn. A narrow distribution reduces the concentration of both very short and very long chains. In semicrystalline polyethylene the short-chain fraction controls crystal perfection, while the long-chain fraction controls melt elasticity. The narrow MWD of DOWLEX 2503 therefore shifts the balance toward lower melt elasticity and more uniform crystallization. At the nominal melt mass-flow rate of 75 g/10 min, the resin occupies the high-fluidity segment of LLDPE injection-molding grades.

    The viscosity curve is less shear-thinned than that of a broad-MWD LLDPE of identical MFR. The narrower relaxation-time spectrum arises from the reduced concentration of very long chains, and the practical consequence in a reciprocating-screw injection machine with an 18:1–22:1 L/D general-purpose screw is a more uniform melt delivery across the barrel residence-time distribution. Mold-filling simulations using a Cross-WLF viscosity model are generally sufficient for gate and runner balancing in thin-wall tools. For injection-molding simulation, the high MFR reduces injection pressure sensitivity to fill time in the shear-rate range from 103 s−1 to 104 s−1, which are characteristic of thin-wall gates. Die swell at the gate is lower than for broad-MWD LLDPE of the same nominal density, which reduces gate-vestige variation in stackable articles.

    Because the backbone is linear without long-chain branching, the resin does not exhibit the strain-hardening response observed in LDPE. Blown film, blow molding, and other processes requiring melt strength are therefore outside the recommended processing envelope; where these are required, a broad-MWD autoclave LLDPE or an LDPE-rich blend is normally specified instead. Published data for this specific configuration is limited, and tool trials are required for restrictive sub-runner or valve-gated systems.

    In cold-runner multi-cavity tooling used for dairy-cup lids and thin-walled food containers, nozzle melt temperature is normally maintained between 190 °C and 230 °C, while mold temperature is controlled from 10 °C to 40 °C using chilled-water circuits with turbulent flow. Injection velocity is set to fill the cavity in 0.2–0.6 s; holding pressure is then applied until gate freeze. The narrow MWD allows a shorter plastication residence time than a broad-MWD grade of equivalent density because the absence of a high-molecular-weight tail reduces unmelted-particle persistence.

    Moisture-related defects are uncommon because polyethylene absorbs less than 0.01 % water at 23 °C; however, pellet surface condensation must be removed when bins have been stored outdoors at sub-zero temperatures. Regrind from sprues and runners is generally incorporated at addition levels up to 20 % by weight, provided that screens remove fines and that regrind is not contaminated with polypropylene or paper label residue. Accumulator-head and continuous extrusion processes are not recommended because the grade lacks the melt strength necessary for parison stability and drawn-melt processing. The same limitation applies to microcellular foaming, where the narrow MWD reduces cell stabilization at low pressure.

    When Dimensional Stability in Stackable Articles Encodes Cooling-Rate Heterogeneity

    Shrinkage in a semicrystalline LLDPE is a function of crystalline fraction and cooling-rate distribution across the part. At a nominal density of 0.930 g/cm³, the resin has a higher crystalline fraction than a 0.915 g/cm³ film-grade LLDPE but a lower crystalline fraction than an MDPE or HDPE injection grade. The narrow MWD narrows the distribution of crystallizable chain lengths, which in turn reduces the breadth of spherulite sizes and lowers the differential shrinkage measured between the gate area and the distal wall. On stackable containers, this behavior reduces the incidence of out-of-round lids when mold-temperature asymmetry is held within ±5 °C.

    Differential scanning calorimetry of linear polyethylenes with this density typically shows a primary melting endotherm between 120 °C and 126 °C; the onset of crystallization during cooling is shifted to higher temperature by the narrow MWD because the chain-length distribution is more uniform. This narrows the transition from melt to solid and reduces the interval in which differential shrinkage develops. The practical specification is therefore to maintain turbulent flow in chilled-water circuits and to avoid coolant temperature differences greater than 5 °C between core and cavity.

    Cooling time is governed by the Vicat softening temperature of 91 °C under ISO 306:2022; demolding below this temperature is necessary to avoid distortion. Production trials on thin-wall tubs with wall stock below 1.0 mm have indicated that the high MFR permits shorter hold-pressure decay and earlier gate freeze than medium-flow LLDPE grades, but published data for this specific configuration is limited. Secondary crystallization during the first 24 h after demolding contributes an additional 0.1–0.3 % shrinkage in olefin parts. Metrology should therefore be delayed until conditioning at 23 °C and 50 % RH for at least 48 h, unless accelerated conditioning is specified in the internal control plan.

    What Distinguishes DOWLEX 2503 from Broad-MWD Autoclave LLDPE and LDPE?

    The primary comparative distinction is the molecular weight distribution. Autoclave LLDPE grades typically combine a low-density fraction with a high-molecular-weight tail to impart melt strength and bubble stability in film extrusion; the high-molecular-weight tail raises shear viscosity at low shear rates and broadens the relaxation spectrum. DOWLEX 2503 is positioned for injection molding, not for blown film or cast film. The narrow MWD removes much of the high-molecular-weight tail, yielding a low-viscosity melt that fills thin sections at fast injection velocities, but it also lowers zero-shear viscosity and strain hardening.

    Compared with LDPE of similar density, the resin lacks long-chain branching. This reduces extrudate swell and improves tensile toughness and environmental stress-cracking resistance, but the linear structure cannot support the same melt strength in extrusion coating or blown film. Compared with a low-flow LLDPE injection-molding grade, the 75 g/10 min MFR allows substantial reduction in injection pressure and cycle time; the trade-off is a lower notched impact strength because of the lower average molecular weight. These differences are therefore process- and end-use-specific rather than absolute.

    For replacement of an LDPE grade in an existing tool, the higher melt index usually permits a reduction in melt temperature of 10–20 °C or a reduction in injection pressure; however, the linear backbone increases shear heating at the gate. Process engineers should map the pressure-limited region before shortening cycle time because the narrow MWD reduces the forgiveness to gate-freeze deviations.

    Three terminal use boundaries are relevant during design review. First, continuous service at temperatures above 70 °C is not recommended for load-bearing articles because the Vicat softening point is 91 °C and creep resistance declines steeply near the crystalline onset. Second, the resin should not be exposed to strong oxidizing acids, chlorinated solvents, or sustained UV radiation without carbon black or stabilizer packages; LLDPE is susceptible to environmental stress cracking in contact with polar detergents under high hoop stress. Third, because the narrow MWD reduces melt strength, processing in foamed or drawn-melt processes is limited. A clear distinction from higher-density injection grades is the moderately low flexural modulus of 260 MPa under ISO 178:2019. Where stack load or snap-fit retention demands a modulus above 600 MPa, an HDPE or PP grade is normally substituted. Conversely, where low-temperature impact below −40 °C is required, this LLDPE retains ductile behavior more effectively than many PP homopolymers.

    In a thin-wall container with a snap-fit undercut, the lower molecular weight of DOWLEX 2503 relative to medium-flow LLDPE may reduce resistance to slow crack growth under continuous strain. The part designer should evaluate environmental stress-cracking resistance according to ASTM D1693 or an equivalent notched constant-strain test if the part contacts stress-cracking fluids.

    Regulatory Extraction Limits and Food-Contact Status

    Unmodified polyethylene resins of this class are generally evaluated under U.S. FDA 21 CFR 177.1520(c) for olefin polymers and under EU Regulation 10/2011, Article 12 for plastic food-contact materials when the grade is listed by the supplier. Compliance is valid only for the base resin without non-conforming additives and only when the end article meets overall migration limits of 10 mg/dm² or 60 mg/kg under EU 10/2011 for the applicable food simulant. The manufacturer’s product stewardship bulletin should be consulted before use in medical packaging or pharmaceutical closures.

    REACH registration under EC 1907/2006, Article 33 applies to the monomer and polymer as marketed, and the resin contains no intentionally added substances of very high concern above 0.1 % w/w. RoHS recast 2011/65/EU, Annex II limits for lead, mercury, cadmium, hexavalent chromium, PBB, and PBDE are met in the unfilled natural product, but black colorants or recycled content must be independently verified.

    Regulatory frameworkDesignationCondition or limit
    U.S. FDA olefin polymers21 CFR 177.1520(c)Base resin compliance; end-use extraction testing required
    EU food contactEU 10/2011, Article 12Overall migration limit 10 mg/dm² or 60 mg/kg
    REACHEC 1907/2006, Article 33SVHC content below 0.1 % w/w
    RoHS recast2011/65/EU, Annex IIPb, Hg, Cd, Cr(VI), PBB, PBDE restrictions
    Top