| HS Code | 976487 |
| Density | 0.935 g/cm3 |
| Melt Index 190 C 2 16 Kg | 0.85 g/10 min |
| Melting Point Dsc | 124 °C |
| Vicat Softening Point | 108 °C |
| Tensile Yield Strength | 10.3 MPa |
| Tensile Break Strength | 25.5 MPa |
| Elongation At Break | 800% |
| Flexural Modulus | 262 MPa |
| Shore D Hardness | 50 |
| Brittleness Temperature | < -70 °C |
| Molecular Weight Distribution | Narrow |
| Comonomer | 1-Octene |
As an accredited Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Supplied in 25 kg multiwall paper bags, palletized and stretch-wrapped; bulk quantities available in 1,000 kg octabins. |
| Container Loading (20′ FCL) | Dow DOWLEX™ 2500 LLDPE, Narrow MW Distribution: 20′ FCL holds 18 pallets of 25 kg bags, 18,000 kg net. |
| Shipping | Dow DOWLEX™ 2500 LLDPE ships as non-hazardous polyethylene resin pellets. Standard packaging includes 25-kg bags, bulk bags, octabins, or bulk trucks/railcars. No DOT/IMDG/IATA dangerous goods classification applies. Keep containers closed, clean, dry, and away from heat, moisture, and UV exposure during transport. |
| Storage | Store DOWLEX™ 2500 LLDPE in a cool, dry, well-ventilated area away from direct sunlight, heat, sparks, and flames. Keep original packaging closed and protect from moisture, contamination, and physical damage. Avoid strong oxidizers. Prevent dust accumulation and follow grounding/bonding procedures if handling fine particles. Rotate stock first-in, first-out, and avoid excessive stacking. |
| Shelf Life | Indefinite under normal storage conditions; keep in cool, dry, well-ventilated area away from direct sunlight, heat, and ignition sources. |
In thin-wall injection moulding of dairy spread tubs and delicatessen containers, the melt flow path frequently exceeds a length-to-thickness ratio of 250:1, particularly in multi-cavity tools with cold sprue diameters below 3.0 mm. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is processed at melt temperatures between 210 °C and 250 °C, with mould temperatures maintained between 10 °C and 35 °C. The nominal density of 0.925 g/cm³, determined according to ISO 1183-1, and the melt flow rate of 25 g/10 min at 190 °C/2.16 kg, determined according to ISO 1133-1:2022, place the material in the high-flow LLDPE range. The narrow molecular weight distribution reduces high-shear viscosity relative to broad-MWD grades at equivalent melt index, which permits filling of wall sections from 0.35 mm to 0.60 mm without relying on excessive clamp force; machines between 1,500 kN and 3,500 kN are generally adequate for 16-cavity tools with shot weights not exceeding 150 g. When container stacking force is specified below 9.8 N per 100 cm², a slip/antiblock concentrate may be metered at 1.0 wt% to 2.0 wt%; the additive dose is confirmed by coefficient-of-friction testing according to ASTM D1894 rather than by qualitative tactile assessment.
Compliance for finished food-contact containers is evaluated under Commission Regulation (EU) No 10/2011 for plastics intended to come into contact with food, with overall migration limited to 10 mg/dm² under the standardised test conditions applicable to the intended contact time and temperature. In the United States, the base olefin polymer is covered by 21 CFR 177.1520, provided the finished article meets end-use extraction limitations for the food type. No separate resin-level certification replaces part-level migration testing, because mould release agents, colourants and regrind content affect the final extractive profile. For dimensionally critical lids, mould shrinkage determination according to ISO 294-4 typically falls within 1.2% and 1.8%; however, published data for this specific configuration is limited, so the first-article verification should derive the actual shrink allowance from a pilot tool rather than a nominal datasheet value. Terminal products include portion cups, dairy tubs, delicatessen bases and pigmented or translucent lids.
Closure systems for beverage, cosmetic and detergent packaging must maintain removal torque and tamper-evident band integrity after warehouse temperature excursions from -20 °C to 40 °C. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is typically injection moulded in cold-runner tools with 32 to 96 cavities; melt temperature at the nozzle is held between 220 °C and 260 °C, and the mould is cooled to 15 °C to 30 °C. The narrow MWD reduces shear-induced flow orientation at the hinge region, resulting in lower residual stress and a reduced tendency for stress whitening when the tamper-evident band is stretched over the bottle finish at line speeds from 200 to 600 closures per minute. Removal torque is controlled by migration of slip additives, not by resin MWD alone; a slip concentrate containing erucamide is metered at 500 ppm to 1,500 ppm, and torque is measured after 48 h conditioning at 23 °C according to ASTM D2063 or an equivalent capping torque test specified by the bottle supplier.
Environmental stress crack resistance is relevant when closures are exposed to surfactants in laundry detergent formulations and to organic acids in food service. The polymer’s ESCR must be verified by ASTM D1693 using an Igepal CO-630 solution at 10% concentration and 50 °C; however, published data for this specific configuration is limited, because ESCR is strongly affected by closure geometry, moulded-in stress and additive package. In critical dispensing closures where child-resistant features are required, the design is tested under ASTM D3475 and must meet the protocol without brittle fracture after repeated impact. The dimensional tolerance of the closure plug or bore is commonly held to ±0.05 mm; narrow MWD reduces cavity-to-cavity variation in mass and allows process capability indices above 1.33 for mass when the mould is fully balanced. Terminal articles include tamper-evident beverage closures, cosmetic flip-top caps, detergent dosing closures and twist-lock dispensing spouts.
During twin-screw compounding of colour concentrates on a 44:1 L/D co-rotating extruder with side-fed pigment, the carrier resin must maintain low melt viscosity for pigment wetting while retaining strand melt strength for pelletizing. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is metered at 60 wt% to 80 wt% with pigment loading from 20 wt% to 40 wt%; the melt flow rate of 25 g/10 min at 190 °C/2.16 kg enables wetting of high-surface-area organic and inorganic pigments without exceeding a melt temperature of 200 °C to 220 °C at the die plate. The narrow MWD produces lower die swell than broad-MWD LLDPE carriers of similar melt index, which stabilizes strand diameter at 2.5 mm to 3.5 mm and reduces pelletizer rejects caused by stuck strands on the water slide. Screw speed is typically set between 350 min-1 and 650 min-1 for this carrier; specific energy input is machine-dependent but often falls between 0.18 kWh/kg and 0.25 kWh/kg for a 40 wt% TiO2 white masterbatch, while higher filler loadings may require a side vent to remove moisture.
The finished concentrate is let down in polyethylene blown film, cast film or injection moulding at addition ratios between 2 wt% and 8 wt%. The carrier resin is compatible with LDPE, LLDPE and HDPE matrices, so pigment agglomeration at the letdown stage is governed by dispersion quality in the concentrate and by the shear history of the final process. Colourant users must declare compositional compliance under REACH for articles placed on the EU market, and where the final package is intended for food contact, the colourant must also meet 21 CFR 178.3290 for colourants used in polymers. The carrier itself does not provide food-contact status; the complete formulation must be evaluated under the relevant migration framework. Terminal outputs include white masterbatch, single-pigment colour concentrates and additive concentrates for antioxidants, slip agents and UV stabilisers.
| Application segment | Primary standard or regulation | Critical endpoint |
|---|---|---|
| Thin-wall food packaging | EU 10/2011; 21 CFR 177.1520 | Overall migration 10 mg/dm² |
| Closures | ASTM D2063; ASTM D1693 | Torque retention; ESCR in Igepal CO-630 |
| Masterbatch | 21 CFR 178.3290; REACH | Colourant compliance; full formulation migration |
| Diagnostic consumables | USP <661.1>; ISO 10993-5; ISO 10993-10 | Extractables; in vitro cytotoxicity; irritation/sensitisation |
| Toy components | EN 71-1; EN 71-3; Directive 2009/48/EC | Mechanical safety; element migration |
Housewares such as storage totes, waste bins and consumer containers are moulded at wall thicknesses from 1.2 mm to 2.5 mm, where the flow length can exceed 800 mm in single-cavity tools. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is processed at melt temperatures between 200 °C and 240 °C, with the mould held between 15 °C and 35 °C. Because the material has a density of 0.925 g/cm³ and high melt flow, injection pressure required to fill large-area parts is lower than that of fractional-melt LDPE, but clamp force remains governed by projected area: machines from 3,500 kN to 6,000 kN are selected when projected area exceeds 1,500 cm². The hold pressure profile uses stepped decay, with initial packing pressure between 30 MPa and 50 MPa, followed by a second-stage hold at 50% of the initial value for 2 s to 5 s to reduce sink marks adjacent to ribs.
For outdoor storage applications, a hindered amine light stabiliser concentrate may be incorporated at 0.1 wt% to 0.3 wt% active HALS, but the formulation must be tested under ISO 4892-2 for artificial weathering if UV resistance is a specification. The resin’s narrow molecular weight distribution reduces warpage from differential shrinkage, but flatness of large panels still requires controlled ejection timing and possibly post-mould fixturing; flatness deviations above 2.5 mm over a 500 mm span are typically unrelated to MWD and are corrected by rebalancing gate positions or cooling circuits. Low-temperature drop impact of moulded articles can be evaluated by ASTM D5420 with a striker plate at -20 °C, but the resin datasheet does not provide part-level values; therefore, logistics validation on filled containers is required. Terminal products include stackable storage totes, waste containers, under-bed storage units and industrial bins.
Single-use laboratory articles, specimen transport containers and diagnostic consumables require reduced extractable profiles and consistent mass across multi-cavity tools. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is evaluated in such settings because its narrow MWD supports tight part mass repeatability, but the resin is not automatically supplied with a medical-grade regulatory file. Device manufacturers must therefore qualify the finished article under ISO 10993-5 for in vitro cytotoxicity and ISO 10993-10 for irritation or sensitisation when body contact is intended. Injection moulding of thin-wall tubes and cuvettes uses melt temperatures from 200 °C to 240 °C, mould temperatures constrained to 10 °C to 20 °C, and hold pressures between 35 MPa and 60 MPa to avoid flash at the parting line. Hot runners are limited in diagnostic disposables because internal stagnation can generate small-molecule degradation products; cold-runner tools with large sprues are preferred for extractable-critical applications.
Extractables testing is performed on the finished device according to USP <661.1> for plastic packaging systems, with acceptance thresholds determined by the intended contact phase and the analytical method, not by the polymer supplier. The resin’s polymerisation route does not employ phthalate-based catalysts, but no statement in this context replaces a supplier change notification and batch-specific certificate of analysis. Dimensionally critical parts such as cuvettes require optical path length tolerances of ±0.05 mm; narrow MWD reduces shot-to-shot mass variation to below 0.1% on electric injection moulding machines with clamp force from 1,000 kN to 2,000 kN, provided the process uses a consistent cushion of 2 mm to 4 mm. Terminal articles include specimen transport tubes, reagent reservoirs, cuvettes and pipette tip racks.
Toy components produced from olefin polymers are tested under the Toy Safety Directive 2009/48/EC and the harmonised standard EN 71-1 for mechanical and physical properties. DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution, is used for flexible toy parts where high flow improves filling of thin snap-fit features without brittle fracture at low temperatures. Melt temperatures are held between 200 °C and 240 °C, mould temperatures between 15 °C and 30 °C, and injection speeds are set high enough to maintain a flow front velocity above 100 mm/s in the thinnest section. The material’s density of 0.925 g/cm³ and high melt flow permit thin-walled parts as low as 0.5 mm to 0.8 mm to be moulded, but sharp corners below a radius of 0.25 mm are avoided to comply with EN 71-1 requirements for edges and points.
Chemical safety for toy applications requires that finished articles intended for children under 36 months, or those likely to be mouthed, be tested under EN 71-3 for migration of antimony, arsenic, barium, cadmium, chromium, lead, mercury and selenium. The resin is not a source of heavy-metal stabilisers, but colourants and processing aids used with it must be selected accordingly and declared in the technical file. Mechanical durability is assessed by drop tests described in EN 71-1; published data for this specific configuration is limited, so article-level tests are mandatory. The uniform molecular weight distribution reduces sink marks in snap-fit bosses and gives more consistent shrinkage in multi-cavity tools. Terminal products include flexible toy components, snap-fit housings, toy hinges and non-load-bearing recreational parts.
Competitive Dow DOWLEX™ 2500 Linear Low Density Polyethylene, Narrow MW Distribution prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2500 Linear Low Density Polyethylene is a narrow molecular weight distribution resin supplied in pellet form. The product is manufactured by a solution polymerization route that yields a linear polyethylene backbone with negligible long-chain branching. The narrow MWD descriptor indicates a reduced high-molecular-weight tail relative to conventional broad-MWD LLDPE. This molecular architecture governs the product’s melt rheology, solid-state properties, and processing response. The grade is used in high-flow injection molding, thin-wall packaging, and masterbatch carrier applications where melt index, dimensional stability, and controlled shear response are primary selection criteria.
The product name differentiates the series by the narrow molecular weight distribution descriptor; this is a resin architecture rather than a filler or surface treatment. The narrow distribution is a direct consequence of the catalyst and solution process conditions and cannot be inferred from melt index alone. Processors often compare the grade with high-flow LDPE or broad-MWD LLDPE resins of the same density range, but the shear response differs in ways that affect tool design and process setup.
In capillary rheometry at 190°C and apparent shear rates from 10 s⁻¹ to 1000 s⁻¹, narrow-MWD LLDPE exhibits a flatter viscosity-shear rate relationship than a broad-MWD grade of equivalent melt index. The high-molecular-weight fraction in broad-MWD resins contributes disproportionately to non-Newtonian shear thinning; as that fraction is reduced, the resin retains a greater proportion of its low-shear viscosity at high shear rates. For DOWLEX™ 2500, the practical effect is lower melt elasticity and reduced die swell, measurable as smaller extrudate diameter after strand pelletization or capillary extrusion. The trade-off is that the resin provides less shear thinning compensation in narrow gates or long flow paths. Injection pressure demand in thin-wall tools is therefore not predicted solely from melt index; gate dimensions and runner geometry must be evaluated using pressure-drop calculations that incorporate the flatter viscosity curve.
With a melt index of 25 g/10 min under 2.16 kg load, the low-shear viscosity is already low enough for rapid cavity filling. At high injection shear rates above 10,000 s⁻¹, broad-MWD resins of the same nominal MI may show lower apparent viscosity, but DOWLEX™ 2500 may exhibit more consistent cavity-to-cavity filling because its viscosity is less sensitive to shear history. In multicavity hot-runner systems, this can reduce the influence of shear imbalance created by unequal runner lengths. However, the narrow MWD also lowers melt strength, which is not a limiting factor in injection molding but excludes the grade from blown film processes that require bubble stability under extensional deformation.
Production-scale measurements on capillary rheometers and injection-moulding machines show that narrow-MWD grades generate lower melt pressure fluctuation during screw recovery when screw speed is changed. In a single-screw extruder or injection unit with a general-purpose barrier screw, the reduced high-MW tail lowers the apparent viscosity at low shear rates near the screw root but maintains viscosity at high shear rates in the metering section. This produces a different screw torque response: torque may be more sensitive to screw speed and less sensitive to die restriction than broad-MWD grades. Machine setters should therefore not use screw torque as a direct indicator of melt viscosity when transferring a tool from a broad-MWD grade to DOWLEX™ 2500. Melt temperature measurement with an immersion probe at the nozzle is more reliable.
Resin characterization data are generated from injection-moulded or compression-moulded specimens according to the methods listed below. Values are nominal and should not be interpreted as product specifications unless defined in a supply agreement.
| Property | Nominal value | Test method |
|---|---|---|
| Density | 0.925 g/cm³ | ASTM D792 |
| Melt index (190°C/2.16 kg) | 25 g/10 min | ASTM D1238 |
| Tensile stress at yield | 11.0 MPa | ASTM D638 |
| Tensile strain at break | 800% | ASTM D638 |
| Flexural modulus (1% secant) | 300 MPa | ASTM D790 |
| Vicat softening temperature | 95°C | ASTM D1525 |
| DSC peak melting temperature | 122°C | Internal DSC method |
| Hardness Shore D | 53 | ASTM D2240 |
The density of 0.925 g/cm³ places the resin in the lower-density segment of the LLDPE family and supports a balance of stiffness and impact resistance. The melt index of 25 g/10 min is approximately one order of magnitude higher than extrusion-grade LLDPE resins and permits filling of thin-wall sections at lower melt temperatures than lower-MI products. Tensile yield at 11.0 MPa and flexural modulus at 300 MPa are typical for a linear polyethylene at this density; the narrow MWD reduces melt elasticity but does not produce substantial changes in short-term tensile properties relative to broad-MWD LLDPE at the same density. Long-term properties such as environmental stress crack resistance are governed by molecular weight, comonomer distribution, and cooling history, and should be evaluated on the final article rather than inferred from the melt index alone.
The Vicat softening temperature of 95°C indicates the upper service temperature for short-term contact without load. The DSC peak melting temperature of 122°C is consistent with an ethylene-octene copolymer, although comonomer type is not always disclosed in marketing literature. The narrow MWD does not significantly shift the peak melting temperature compared with broad-MWD LLDPE of the same density, but it can narrow the melting range and alter the onset of crystallisation during cooling. In injection moulding, this means the cooling time is governed primarily by part thickness and mold temperature, not by a broad melting plateau.
In reciprocating screw injection molding machines with screw L/D ratios of 20:1 to 24:1 and compression ratios between 2.5:1 and 3.5:1, barrel temperatures are typically profiled from 180°C at the feed throat to 230°C at the nozzle. Mold temperatures from 15°C to 40°C are used to accelerate crystallisation and shorten cycle time. Because the narrow MWD gives a flatter viscosity curve, screw recovery torque may remain more constant across cycle-to-cycle variations in screw speed, but injection pressure can be higher than expected from broad-MWD experience. Back pressure is usually maintained below 1.0 MPa to avoid excessive shear work and to limit melt temperature rise. Shot sizes should be selected so that the cushion remains between 3 mm and 6 mm; smaller cushions reduce residence time stability, while larger cushions increase residence time and possible degradation.
Polyethylene is not hygroscopic, and pre-drying is generally unnecessary. If pellets are stored at relative humidity above 70% or transferred from cold storage to a warm production area, surface condensation may cause splay in moulded parts. In such cases, a hopper dryer at 70°C for 2 h is sufficient. Hopper magnet and screen-pack inspection intervals should follow the plant’s polyolefin standard, because no unusual gel formation is expected under normal processing conditions. Prolonged residence above 260°C may initiate thermal oxidation; purging with a suitable polyolefin is advised when interrupting production.
Cooling and crystallisation in thin sections are rapid. At mold temperatures of 20°C to 40°C, a 1.5 mm wall can reach ejection temperature in 5–10 s depending on coolant flow. This narrow window makes cycle time sensitive to mold cooling design. Conformal cooling channels are beneficial because the resin’s high flow permits filling at lower melt temperature, reducing the temperature differential and thermal stress. Uneven cooling can produce differential shrinkage and warpage in flat parts, which the narrow MWD cannot fully compensate.
Thin-wall injection moulding of caps, overcaps, and small containers places the resin under high shear and rapid cooling. The reduced melt elasticity of DOWLEX™ 2500 lowers frozen-in orientation and can reduce out-of-plane deformation in flat lids with wall thickness below 1.5 mm. In multicavity valve-gated hot-runner tools, the flatter viscosity curve reduces the tendency for shear-induced viscosity differences between gates to amplify fill imbalance. However, because the resin has less shear thinning than broad-MWD LLDPE, gate diameters below 0.8 mm may require higher injection velocity or higher melt temperature to maintain complete filling. Gate freeze time is controlled by the melt temperature and mold temperature; with a mold temperature of 20°C and melt temperature of 220°C, gate freeze is governed by the thermal diffusivity of the resin and part thickness. Published data for this specific configuration is limited, but the processing trend is consistent with capillary rheometry and injection-moulding flow simulation using a cross-WLF viscosity model fitted to narrow-MWD LLDPE data.
Common processing defects observed on production lines include splay from surface moisture, gate blush from excessively high injection velocity, and warpage from nonuniform mold cooling. Reducing injection velocity to keep gate shear rate below 100,000 s⁻¹ can reduce gate blush without causing short shots, but thin-wall parts may require higher velocity. The appropriate velocity is determined by a cavity pressure study; short-shot weight should be stable within ±1.5% before production start.
As a masterbatch carrier, the high melt index and narrow MWD provide a predictable viscosity base for dispersing pigments and additives in co-rotating twin-screw extruders with L/D ratios of 40:1 or greater. The resin’s low melt temperature demand permits compounding at barrel set points from 160°C to 200°C, limiting thermal degradation of heat-sensitive organic pigments. Specific energy input can be maintained between 0.15 kWh/kg and 0.25 kWh/kg depending on pigment loading and screw design. The narrow MWD reduces viscosity variation across the screw profile, which improves pressure stability at screen changers and strand die plates. Let-down ratios in downstream polyolefin moulding are generally between 2 wt% and 5 wt%. Avoid formulations containing amine-based additives that can react with certain pigments or generate discoloration under prolonged heat history.
Carrier resin requirements for masterbatch include melt index, viscosity stability, and thermal stability. The narrow MWD reduces viscosity fluctuations caused by shear history differences across the screw profile, which improves pigment wetting on high-shear mixing elements. When compounding with 40 wt% carbon black, the high MI allows lower melt temperature and reduces oxidative degradation. However, high filler loadings above 50 wt% may require a higher-MI or broad-MWD carrier to maintain strand integrity because the narrow-MWD melt has less extensional strain hardening. Published data for this specific configuration is limited.
Relative to autoclave LDPE of equivalent melt index, DOWLEX™ 2500 has a linear backbone with negligible long-chain branching, which lowers extensional strain hardening and bubble stability. This makes the grade unsuitable for blown film and extrusion coating where neck-in and bubble instability are controlled by melt strength. In injection moulding, the linear structure and 0.925 g/cm³ density provide higher tensile yield and better puncture resistance than LDPE at equivalent stiffness. Compared with broad-MWD LLDPE of the same nominal melt index, the narrow-MWD product exhibits lower die swell, reduced post-filling screw recovery variation, and improved part weight consistency. The trade-off appears in high-shear flow: broad-MWD LLDPE may display lower apparent viscosity at shear rates above 1000 s⁻¹, which can reduce injection pressure in extremely thin-wall parts with long flow lengths. Selection between the two architectures should be based on a flow simulation or molding trial that captures the shear-rate range of the specific tool.
Compared to metallocene-catalysed LLDPE with narrow MWD, DOWLEX™ 2500 may have a broader comonomer distribution depending on catalyst system; the term “narrow MW distribution” does not imply narrow chemical composition distribution. This is critical in sealing applications, because the sealing initiation temperature is governed by comonomer distribution and surface properties, not solely by MWD. The grade is not optimised as a sealant resin; processors requiring low seal initiation temperature should evaluate a specialised mLLDPE grade.
For food-contact articles, the resin is typically referenced under FDA 21 CFR 177.1520(c)3.2a for olefin polymers, subject to extraction limits and end-use conditions. The product is not recommended for continuous contact with strong oxidizing agents, aromatic hydrocarbons, or chlorinated solvents, which can swell the polyethylene and reduce mechanical integrity. Processing above 260°C or excessive residence time may generate oxidative degradation products; adequate nitrogen blanketing or purging during extended shutdowns is advised. The absence of long-chain branching also means that melt strength is too low for rotomoulding or blown film operations where sagging, bubble instability, or thinning under gravity is expected.