Dow Dowlex 2247g Polyethylene Resin

Dow DOWLEX™ 2247G Polyethylene Resin

    • Product Name: Dow DOWLEX™ 2247G Polyethylene Resin
    • Factroy Site: Yinchuan, Ningxia, China
    • Price Inquiry: sales8@ascent-chem.com
    • Manufacturer: Ascent Petrochem Holdings Co., Limited
    • CONTACT NOW
    VTB
    Specifications
    HS Code 941540
    Polymertype Linear Low Density Polyethylene (LLDPE)
    Comonomer Octene-1
    Density 0.917 g/cm³
    Meltindex 2.3 g/10 min
    Meltingpoint 122 °C
    Vicatsofteningpoint 93 °C
    Tensilestrengthatyield 9.70 MPa
    Tensilestrengthatbreak 27.6 MPa
    Elongationatbreak 800%
    Flexuralmodulus 241 MPa
    Elmendorftearmd 280 g
    Elmendorfteartd 480 g
    Dartdropimpact 120 g
    Haze 13%
    Gloss45degree 55%

    As an accredited Dow DOWLEX™ 2247G Polyethylene Resin factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.

    Packing & Storage
    Packing Dow DOWLEX™ 2247G Polyethylene Resin is packaged in 25 kg (55 lb) polyethylene-lined industrial bags.
    Container Loading (20′ FCL) 20′ FCL container loading for Dow DOWLEX™ 2247G Polyethylene Resin: 25 kg bags, floor loaded, approximately 720 bags, 18 MT.
    Shipping Dow DOWLEX™ 2247G Polyethylene Resin is typically shipped as solid pellets in moisture-barrier bags, octabins, or bulk trucks/railcars. Transport in clean, dry, covered vehicles at ambient temperature. It is generally not classified as dangerous goods. Avoid excessive heat, moisture, and contamination. Follow the SDS and local shipping regulations.
    Storage Store DOWLEX™ 2247G Polyethylene Resin in a cool, dry, well-ventilated area, preferably indoors, in tightly closed original bags or containers. Protect from direct sunlight, heat, moisture, and contamination. Keep away from ignition sources, strong oxidizers, and incompatible materials. Avoid dust generation and prolonged outdoor exposure. Store at ambient temperatures. Follow local regulations and good industrial hygiene practices.
    Shelf Life Typically 24 months from manufacture when stored unopened in original packaging below 50°C, away from direct sunlight and moisture.
    Application of Dow DOWLEX™ 2247G Polyethylene Resin

    DOWLEX™ 2247G, an ethylene/1-octene copolymer with a density of 0.917 g/cm³ (ASTM D792) and a melt index of 2.3 g/10 min (ASTM D1238, 190°C/2.16 kg), is introduced into the core of a three-layer A/B/A cast stretch film at 65–80 wt% of total film mass. Skin layers are formulated with lower-melt-index metallocene LLDPE or polypropylene random copolymer at a combined 10–15 wt%; cling and release additives are dispersed through twin-screw masterbatches at 0.5–2.0 wt% in the skin only to avoid core contamination. The downstream converting process uses a cast film line with barrier screws at L/D 30:1 to 36:1, a melt temperature window of 240–260°C, slot die gap 0.5–0.8 mm, air gap 6–15 cm, and polished chill rolls held at 15–30°C. On production-scale lines, operators observe edge encapsulation when air-knife velocity is not matched to web speed above 450 m/min; transverse gauge bands are associated with die lip deposit formation when melt temperature exceeds 270°C and with chill roll surface pitting after prolonged use. Compliance is verified through ASTM D5748-95(2019) for stretch wrap puncture resistance and ASTM D882-18 for tensile properties of thin plastic sheeting; food-contact uses are separately controlled under FDA 21 CFR §177.1520 and EU 10/2011. Terminal finished product type is machine-grade pre-stretched and non-pre-stretched pallet-unitization stretch film for high-speed automatic wrappers operating at speeds up to 60 wraps/min.

    Sealant web extrusion for polyolefin-laminated frozen-food and retort structures

    In lamination replacement structures, DOWLEX™ 2247G is blended into a blown or cast sealant web at 20–45 wt% of the sealant layer mass, with the balance composed of a lower-density ethylene copolymer or low-density polyethylene to depress seal initiation temperature and maintain hot-tack strength. The downstream process is film extrusion followed by adhesive lamination to oriented PET or BOPP; melt temperature is set at 245–275°C, die gap at 0.5–0.7 mm, and the sealant surface is corona-treated to 38–42 mN/m before lamination. A field-observed operational conflict is chill-roll sticking and sealant-layer transfer caused by migration of low-molecular-weight oligomers when DOWLEX™ 2247G exceeds 45 wt%; adding processing aid masterbatch at 0.1–0.3 wt% reduces die deposit but does not fully suppress roll-face bloom at elevated melt temperatures. Food-contact compliance is established under FDA 21 CFR §177.1520(c) paragraph 3.1a or 3.2a, EU 10/2011 with overall migration limit 10 mg/dm², and China GB 9685-2016 for food-contact additives during migration testing. Terminal finished product type is sealant web for frozen vegetable, processed meat, and retort pouch lamination, excluding aggressive high-migration simulants without a validated barrier layer.

    Heavy-duty industrial liner production uses DOWLEX™ 2247G as a toughness modifier in blown film blends with high-pressure LDPE and, in closed-loop post-industrial streams, up to 25 wt% recycled LLDPE; DOWLEX™ 2247G is commonly formulated at 30–55 wt% of the total formula. The blown film process operates with die diameters of 250–500 mm, a dual-lip air ring, blow-up ratio 2.0:1 to 2.8:1, frost line height 4–8 die diameters, and melt temperature 200–230°C. A process conflict arises when the frost line is raised above 8D to improve clarity in thicker liners: bubble resonance increases gauge variation from ±6% to ±12% on unsupported film above 80 μm, and die lip alignment must be verified after every resin changeover to prevent asymmetric gauge bands. Compliance for non-food industrial liners references ISO 527-3:2018 for tensile properties, ASTM D1709-16a for dart impact, and REACH Annex XVII for heavy metals and phthalate restrictions. Terminal finished product type is heavy-duty shipping sacks, roll-off container liners, and agricultural chemical liners with dart impact validated at 150 g for 80 μm film under ASTM D1709-16a.

    When low-temperature puncture governs silage wrap and bale stretch film selection

    For agricultural silage wrap, DOWLEX™ 2247G is compounded with UV stabilizer masterbatch at 0.5–1.2 wt%, tackifier at 0.3–0.8 wt%, and colorant at 0.2–0.5 wt%; the resin constitutes 95–98 wt% of monolayer formulas and core layers in coextruded structures. The cast film process is run at melt temperature 240–260°C, die gap 0.6–0.9 mm, chill roll 12–20°C, and winding tension tapered from 40 N to 15 N on 750 mm winders. The critical process limitation is the combination of low-temperature outdoor application and long UV exposure: without adequate stabilizer loading, elongation at break measured to ISO 527-3:2018 falls below 700% after 12 months of outdoor exposure, and cling force at 5°C measured by EN 14932:2018 declines below the 0.5 N threshold required to maintain bale wrap unwinding on round balers. Compliance is anchored to EN 14932:2018 for silage bale stretch films, ISO 4892-3:2021 for UV weathering, and REACH for stabilizer registration. Published data for this exact additive package is limited; the stated ranges represent production-level adjustment windows rather than vendor-guaranteed specifications. Terminal finished product type is high-UV bale wrap for silage and haylage preservation, including 12-month outdoor storage grades.

    Protective film substrate extrusion and adhesion build-up in low-tack masking

    Low-tack surface protection film lines use DOWLEX™ 2247G as the carrier layer at 70–90 wt% of the carrier mass, while the adhesive layer contains maleic anhydride-grafted polyethylene or ethylene-vinyl acetate copolymer at 10–30 wt% of total structure mass. The production line is a cast film configuration with melt temperature 220–250°C, die gap 0.4–0.7 mm, chilled rolls at 18–25°C, and controlled rewind hardness at 600–900 N/m to prevent telescoping. Adhesion build-up on polished stainless steel or coated glass is a known operational conflict: peel force increases from an initial 0.08–0.15 N/25 mm to 0.25–0.40 N/25 mm after 7 days at 40°C, unless release additives are compounded into the skin at 0.5–1.5 wt%. Compliance is evaluated under ASTM D3330/D3330M-04(2018) for peel adhesion, ASTM D882-18 for tensile properties of thin plastic sheeting, and REACH Annex XVII for restricted substances. Published data for long-term adhesion build-up on polycarbonate with this specific resin grade is limited; converters validate internal limits using conditioning protocols aligned to ASTM D3330. Terminal finished product type is temporary protective masking for pre-painted metal sheets, polycarbonate sheets, and appliance panels.

    When hygienic backsheet film is converted at line speeds above 150 m/min, DOWLEX™ 2247G is dry-blended with titanium dioxide masterbatch at 4–8 wt% and calcium carbonate masterbatch at 2–5 wt%, placing the base resin at 85–94 wt% of the blend. The cast film line is configured with a 45 mm single-screw extruder, barrier screw at L/D 30:1, melt temperature 240–265°C, and vacuum embossing roll at 10–18°C. A field-observed limitation is melt-pressure variability caused by inconsistent masterbatch particle-size distribution; this variability produces visible die lines and reduces water-vapour barrier measured by ASTM F1249-20, with film gauge below 15 μm possibly exceeding 5 g/m²/day at 38°C/90% RH. Compliance for non-food hygiene film is evaluated under ISO 10993-5:2009 for cytotoxicity and REACH for extractable substances; where lower odour is specified, a purge protocol of 2–4 h with high-melt-index LDPE is applied to remove volatile residuals from upstream extrusion. Published data for this exact backsheet formulation is limited; the stated composition window reflects converter line trials rather than a universal standard. Terminal finished product type is embossed breathable or non-breathable backsheet film for infant diapers and adult incontinence products.

    Free Quote

    Competitive Dow DOWLEX™ 2247G Polyethylene Resin prices that fit your budget—flexible terms and customized quotes for every order.

    For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.

    We will respond to you as soon as possible.

    Tel: +8618005193850

    Email: sales8@ascent-chem.com

    Inquiry

    Get Free Quote of Ascent Petrochem Holdings Co., Limited

    Flexible payment, competitive price, premium service - Inquire now!

    Certification & Compliance
    More Introduction

    Dow DOWLEX™ 2247G Polyethylene Resin is a linear low density polyethylene produced by solution polymerization with octene as the primary comonomer. The grade is supplied in pellet form and is intended for blown film, cast film, and coextruded film structures in which low density, moderate melt flow, and controlled short-chain branching distribution are required. The neat resin has a nominal density of 0.917 g/cm³ when determined according to ASTM D792 or ISO 1183-1:2019, and a nominal melt index of 2.3 g/10 min when measured at 190 °C/2.16 kg according to ASTM D1238 or ISO 1133-1:2022. These values place DOWLEX 2247G in the lower-density, higher-flow segment of the DOWLEX film resin portfolio. In monolayer and multilayer structures, the resin is used for packaging films, industrial liners, stretch-film layers, and agricultural films where the finished article must meet specific optical, seal, or toughness requirements. The base pellet contains no intentionally added slip or antiblock additive; surface friction and blocking behavior are adjusted by the processor through masterbatch addition or coextruded skin layers.

    What Specification Values Define DOWLEX 2247G?

    The values in the following table are typical neat resin data and are not release specifications. Because the resin is a statistical copolymer, lot-to-lot variation is assessed against the supplier certificate of analysis rather than a single fixed point. Film properties are not included in the neat resin table because they depend on gauge, die geometry, blow-up ratio, frost line height, and thermal history.

    Typical neat resin data for DOWLEX 2247G
    PropertyTypical valueTest method
    Density0.917 g/cm³ASTM D792
    Melt index2.3 g/10 minASTM D1238 at 190 °C/2.16 kg
    DSC melting peak122 °CASTM D3418

    For compliance verification, the current product data sheet and certificate of analysis should be requested from the supplier. The melt index value supports thin-gauge drawdown, but it also imposes an upper limit on melt strength. Bubble stability at low film thickness must therefore be addressed through die geometry, cooling configuration, or blending with a branched low density polyethylene.

    On cast film lines using 45 mm to 90 mm single-screw extruders with 24:1 to 30:1 L/D and barrier screws, DOWLEX 2247G is processed with a flat temperature profile from 180 °C in the feed zone to 220 °C at the die, with melt temperature held below 250 °C to avoid thermal degradation. Chill roll temperatures between 15 °C and 35 °C are applied to control crystallinity and optical haze. In blown film, the grade is typically extruded through a die gap of 1.5 mm to 2.5 mm, with a blow-up ratio of 2.0:1 to 2.5:1 and frost line height between 5 and 10 die diameters. These parameters are starting points; actual settings are tuned to cooling air temperature, die diameter, and haul-off speed. Because LLDPE has lower melt strength than high-pressure LDPE, high blow-up ratios can produce bubble instability. The addition of 10 wt% to 30 wt% LDPE or the use of internal bubble cooling stabilizes the bubble. At the die inlet, stable extrusion is indicated by melt pressure fluctuation below ±0.5 MPa. A progressive pressure increase at constant screw speed usually indicates a feed-block or screen-pack plugging issue rather than resin degradation. Before startup, the extruder should be purged with a polyolefin-based purge compound, and the system should be free of PVC, acetal, or other thermally sensitive residues. If pellets are stored in cold conditions and moved to a warm production area, surface condensation can introduce moisture. Drying is not normally required, but when condensation risk is high the pellets can be passed through a hopper dryer at 60 °C for 1 h to 2 h with an inlet air dew point below -20 °C.

    Molecular Architecture and Grade Positioning

    The solution process used for DOWLEX 2247G produces an ethylene-octene copolymer with a more homogeneous short-chain branching distribution than conventional gas-phase butene-based LLDPE. At equivalent density, the octene comonomer is incorporated more efficiently at disrupting crystalline lamellae and promoting tie-molecule formation. This molecular difference is observed on film lines as a lower tendency for brittle failure in high-speed dart impact testing and more balanced machine-direction/transverse-direction Elmendorf tear. In comparison with high-pressure LDPE, DOWLEX 2247G has a narrower melting range, higher potential drawdown, and lower melt elasticity; it therefore requires tighter control of die gap and bubble geometry. Within the DOWLEX portfolio, 2247G is positioned as a lower-density, higher-flow product relative to grades such as DOWLEX 2045G. The higher melt index favors screw throughput and thin-gauge drawdown, while the lower density reduces secant modulus and heat-seal initiation temperature. The principal trade-off is lower stiffness and reduced melt strength compared with higher-density DOWLEX grades or bimodal film resins. Processors transferring from a butene-based LLDPE should evaluate film tear, optics, and seal strength under their own extrusion conditions; a direct drop-in without adjustment of die gap, melt temperature, or cooling rate may not reproduce the expected balance.

    When Thin-Gauge Drawdown, Clarity, or Food-Contact Compliance Are Required

    Thin-gauge cast film is a demanding application for DOWLEX 2247G. On chill-roll cast lines, the resin can be drawn to gauges below 15 µm when melt temperature is kept between 210 °C and 240 °C, and when the air gap and vacuum box are adjusted to prevent edge neck-in. Optical haze is measured according to ASTM D1003 and is minimized by maintaining a high melt temperature, a small die gap, and a controlled frost line height; the homogeneous comonomer distribution reduces light-scattering crystallites in thin films. In blown food packaging, the grade is often placed in the sealant layer of a coextruded structure; a low-density sealant layer from DOWLEX 2247G can reduce heat-seal initiation temperature relative to higher-density LLDPE. Heat-seal strength is measured according to ASTM F88/F88M or ISO 527-3 on specimens sealed at controlled temperature and dwell. For food-contact, the finished film must satisfy 21 CFR 177.1520 for olefin polymers or European Union Regulation (EU) No 10/2011, including an overall migration limit of 10 mg/dm² for the final article. DOWLEX 2247G is not a UV-stabilized weathering grade; agricultural film requires the addition of carbon black or hindered amine light stabilizer masterbatch to meet service-life requirements. The low density of the resin also lowers stiffness; if a film requires load-bearing modulus, blending with a higher-density LLDPE or an HDPE component may be necessary.

    Typical standards and regulatory anchors for DOWLEX 2247G
    FunctionStandard or regulationMeasured or assessed parameter
    Melt mass-flow rateASTM D1238 / ISO 1133-1:20222.3 g/10 min at 190 °C/2.16 kg
    DensityASTM D792 / ISO 1183-1:20190.917 g/cm³
    Food-contact olefin polymer21 CFR 177.1520End-use extractives and migration limits
    EU plastic food-contact(EU) No 10/2011Overall migration 10 mg/dm²
    Film hazeASTM D1003Percentage light scattering
    Seal strengthASTM F88/F88MForce per width

    In stretch-film structures, DOWLEX 2247G is used as a cling-layer component when blended with ultralow-density ethylene-octene copolymers or polyisobutylene-based cling additives. The cling force of the film is quantified by a 180° peel test according to ASTM D5458, while elongation and puncture resistance are evaluated under ASTM D882 and ASTM D5748. The grade supports low-gauge stretch film production on cast extrusion lines with high line speeds, provided that the extruder screw design delivers sufficient plasticating capacity and the chill roll surface finish is matched to the desired cling release behavior. Published data for specific formulations of DOWLEX 2247G with cling additives is limited; processors should validate the additive loading and roll winder tension on pilot equipment before production.

    Top