| HS Code | 268807 |
| Product Name | Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade |
| Polymer Type | Linear Low Density Polyethylene (LLDPE) |
| Density | 0.917 g/cm³ |
| Melt Index 190 C 2 16 Kg | 2.3 g/10 min |
| Melting Point | 124 °C |
| Vicat Softening Point | 100 °C |
| Tensile Strength At Yield | 9 MPa |
| Tensile Strength At Break | 30 MPa |
| Elongation At Break | 800% |
| Dart Drop Impact | 120 g |
| Elmendorf Tear Strength Md | 250 g |
| Elmendorf Tear Strength Td | 400 g |
| Haze | 2.5% |
| Gloss 45 | 90 |
| Coefficient Of Friction | 0.2 |
As an accredited Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade factory, we enforce strict quality protocols—every batch undergoes rigorous testing to ensure consistent efficacy and safety standards.
| Packing | Dow DOWLEX™ 2247A is supplied in 25 kg polyethylene bags, palletized and stretch-wrapped; 1,000 kg bulk bags are also available. |
| Container Loading (20′ FCL) | DOWLEX 2247A LLDPE Cast Film Grade: 25 kg bags, palletized; 20′ FCL typically loads 20–22 MT, subject to carrier limits. |
| Shipping | Dow DOWLEX™ 2247A is a non-hazardous polyethylene resin shipped as pellets in 25 kg moisture-resistant bags, palletized and stretch-wrapped. Typical pallets hold 55 bags (1,375 kg). Transport in clean, dry trucks or containers at ambient temperature, avoiding moisture, direct sunlight, and contamination. |
| Storage | Store DOWLEX™ 2247A in a cool, dry, well-ventilated warehouse at ambient temperature, preferably in original sealed bags or containers. Keep away from direct sunlight, heat, flames, and strong oxidizers. Prevent moisture, dust, and contamination; avoid prolonged UV exposure. Palletize off the floor, keep containers closed, and use first-in, first-out stock rotation. Follow the SDS and local regulations. |
| Shelf Life | Typically two years from date of manufacture when stored unopened in original packaging, dry, away from heat and direct sunlight. |
On cast film extrusion lines configured with a 90 mm single-screw extruder using a L/D 30:1 barrier screw and a 2,400 mm flex-lip die, DOWLEX™ 2247A is conveyed as a neat pellet feed without predrying. The resin is a low-density LLDPE cast film material with a nominal melt index of 2.0 g/10 min under ASTM D1238 and a density near 0.917 g/cm³ under ASTM D792. As-supplied polyolefin moisture uptake at 23 °C and 50 % RH remains below 0.05 %, so desiccant drying is not required unless a hygroscopic additive masterbatch above 5 wt% is introduced into the blend. Refrigerated produce over-wrap formulations on production lines typically fall within 85–95 wt% DOWLEX™ 2247A, 5–10 wt% of an LDPE with density 0.923–0.924 g/cm³ to adjust melt stiffness, and 0.5–1.5 wt% of an erucamide/oleamide slip-antiblock masterbatch. The exact additive ratio is adjusted against coefficient-of-friction data measured under ASTM D1894, with an inside-to-outside static COF target of 0.25–0.40 to accommodate automated belt infeed and vertical form-fill-seal equipment. Downstream extrusion follows a feed throat set point of 180–200 °C, mid-barrel zones of 230–250 °C, and a die body temperature of 245–265 °C. Melt curtain stability is maintained by a die gap of 0.6–1.0 mm, an air gap of 100–150 mm, and a polish chill roll temperature of 15–25 °C. At line speeds between 150 m/min and 350 m/min, the primary failure mode is edge neck-in and melt resonance; a vacuum box applied at the die-to-roll interface suppresses draw resonance, while reducing the die lip below 0.4 mm has been observed to produce uneven transverse thickness profiles. Terminal films are slit to widths of 250–600 mm and converted into flow-wrap bags, lidding film, and pallet-stabilizing over-wrap for fresh-cut produce, leafy greens, and cold-chain protein trays. Regulatory compliance for these food-contact applications requires the olefin polymer to meet 21 CFR 177.1520(c) in the United States, EU Regulation (EU) No 10/2011 with an overall migration limit of 10 mg/dm² for European food contact, and GB 4806.7-2016 for mainland China compliance when the film is sold into exported packaging lines. Additive compliance is governed by GB 9685-2016 for China and by the positive list in EU 10/2011 Annex I for slip agents such as erucamide. Operational limitations include storage of finished rolls at warehouse temperatures below 40 °C to prevent additive bloom, and corona treatment to 38–42 dyn/cm is applied only when the film is scheduled for print or lamination; untreated film is preferred for direct produce contact to limit surface-charged dust attraction on high-speed packing lines.
| Jurisdiction | Regulation / Standard | Key Requirement |
|---|---|---|
| United States | 21 CFR 177.1520(c) | Olefin polymer for food contact; density and extractables within specification |
| European Union | EU 10/2011 | Overall migration limit ≤ 10 mg/dm² |
| China | GB 4806.7-2016 / GB 9685-2016 | Positive list for resin and additives |
Compounding DOWLEX™ 2247A with calcium carbonate masterbatch for breathable diaper backsheet film creates a process window centered on controlled particle debonding rather than simple melt homogeneity. On a cast line, the let-down ratio is commonly 40–50 wt% DOWLEX™ 2247A and 50–60 wt% CaCO₃ masterbatch whose filler content is 70–80 wt%; this produces a final calcium carbonate concentration of 35–45 wt% in the precursor cast film. The screw configuration must incorporate low-shear mixing elements and a grooved feed section to avoid local overheating that oxidizes the LLDPE carrier. The extrusion set profile is reduced to 210–240 °C because higher temperatures lower the melt strength needed for subsequent machine-direction orientation. Industry compliance in this segment is governed not by food-contact regulations but by REACH (EC) No 1907/2006 for the European Economic Area and, where products are marketed for infant care, by OEKO-TEX® Standard 100 testing for extractable heavy metals, formaldehyde, and targeted substances. Converters may also request ISO 10993-18 chemical characterisation if the material is used at a medical device boundary. The downstream process includes cast film production at die gap 1.2–1.5 mm to accommodate the higher viscosity of filled melts, chill roll temperature 20–30 °C, followed by an inline or off-line machine-direction orientation unit operating at 60–80 °C with draw ratios of 2:1 to 4:1. Pore formation occurs as the polymer phase orients and debonds from filler particles, yielding a porous membrane with moisture vapour transmission rate measured under ASTM E96 generally in the range of 500 g/m²·24 h to 2,000 g/m²·24 h depending on final thickness and draw ratio. Terminal product types are printed and unprinted breathable backsheet films for baby diapers, adult incontinence briefs, and feminine hygiene pads. The primary limitation is gel formation when the masterbatch contains agglomerated filler above 15 µm particle size, which can cause pinholes and machine-direction striping in films below 25 µm final caliper.
When a film converter evaluates DOWLEX™ 2247A for cast stretch film, the critical control point shifts from resin rheology to the dispersion boundary of cling and slip additives during high-output extrusion. For pallet unitization films, industrial recipes typically combine 70–80 wt% DOWLEX™ 2247A with 20–30 wt% metallocene LLDPE to raise elastic recovery and puncture resistance. Polyisobutylene cling agent is metered at 0.5–1.5 wt% in a liquid injection package, while slip components are held below 0.3 wt% to prevent loss of load retention. Extrusion is performed on a 75–150 mm single-screw extruder with a coolant-fed feed throat and die temperatures of 240–260 °C. The film is quenched on a chill roll below 20 °C and wound in line at speeds up to 600 m/min for machine-grade rolls. The critical process conflict rises at high line speeds because polyisobutylene exudation to the film surface is time-dependent; if the chill roll is run below 15 °C, additive plate-out produces haze bands across the roll and periodic cling loss. Test methods for this segment include ASTM D5748 for puncture propagation resistance, ASTM D5458 for peel cling, and ASTM D882 for machine-direction tensile, with typical pre-stretch ratios of 200–300 % on powered pre-stretch equipment. Regulatory documentation includes a signed EU REACH compliance statement and, when film is used for export packaging subject to waste reduction directives, confirmation that the product is not classified under CLP as hazardous. Finished articles include hand rolls, machine rolls, and vented pallet wrap. The operational boundary is that DOWLEX™ 2247A neat films exhibit lower cling than EVA-containing cast films, so end users relying on manual stretch with low pre-stretch should specify a higher polyisobutylene dosage within the stated range.
Coextruded surface protection films place an unusual demand on DOWLEX™ 2247A because the material must simultaneously act as a stiff support layer and a controlled modulus base for a lower-crystallinity adhesive skin. A three-layer A/B/C die is used, where the core is 70–80 wt% DOWLEX™ 2247A, the adhesive tie skin is 15–25 wt% of a low-crystallinity ethylene-vinyl acetate or ULDPE, and the release skin is 5–10 wt% of an LDPE-rich blend to reduce blocking during storage. The die body runs at 230–250 °C, chill roll finishing is either super-polish for optical sheet or matte for painted metal and aluminum composite panel protection, and roll winds are stored at 20–30 °C to avoid adhesive creep. Peel adhesion is measured under ASTM D3330 Method A using a 180° peel angle and 300 mm/min pull speed. For glossy PMMA and polycarbonate sheet, the target is between 0.5 N/25 mm and 1.5 N/25 mm after ageing for 24 h at 23 °C. Below 0.3 N/25 mm, film edges lift during CNC cutting; above 2.0 N/25 mm, adhesive residue becomes likely after outdoor weathering beyond 30 days. Compliance for this application is driven by RoHS Directive 2011/65/EU for lead, cadmium, mercury, chromium VI, PBB and PBDE, supported by IEC 62321 test procedures, and by EU REACH SVHC screening of the adhesive skin. Chinese GB/T 2792 can be requested for peel adhesion in mainland China. Terminal products are masking films for architectural polycarbonate sheet, PMMA glazing, pre-coated steel and aluminium coil, and appliance panels. Published data for long-term outdoor clean removal of polyisobutylene-based adhesives with this exact resin is limited beyond 90 days, so converters must validate weathering for exterior applications.
Narrowly defined, the cast-film sealant layer in medical device packaging converts DOWLEX™ 2247A into lamination webs that seal against uncoated Tyvek and medical paper without splitting under ethylene oxide or radiation sterilization. A cast sealant web for medical pouches typically uses 90–100 wt% DOWLEX™ 2247A and 0–10 wt% LDPE to shift seal initiation temperature downward. The film is extruded at 20–40 µm and tested on a laboratory heat sealer at 115–135 °C, 0.5 MPa seal pressure, and 0.5–1.0 s dwell. The governing standards are ISO 11607-1:2019 for packaging for terminally sterilised medical devices, EN 868-5 for paper and plastic pouch materials, and chemical characterisation under ISO 10993-18 to support toxicological risk assessment when the sealant is part of a device packaging system. The downstream process replaces high-slip food-grade additives with cleanroom-compatible packages; corona treatment is not applied because it may create low-molecular-weight oxidised species detectable in extractables. Terminal articles include form-fill-seal pouches, header bags, and vented lidding for surgical kits. The principal boundary is that DOWLEX™ 2247A is not supplied with a certified medical-grade designation, so a device manufacturer must demonstrate extractables and leachables appropriate to the intended shelf life and sterilization dose.
Competitive Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade prices that fit your budget—flexible terms and customized quotes for every order.
For samples, pricing, or more information, please contact us at +8618005193850 or mail to sales8@ascent-chem.com.
We will respond to you as soon as possible.
Tel: +8618005193850
Email: sales8@ascent-chem.com
Flexible payment, competitive price, premium service - Inquire now!
Dow DOWLEX™ 2247A Linear Low Density Polyethylene, Cast Film Grade is an ethylene-octene copolymer produced by solution polymerization and supplied as pellets for flat-die cast film conversion. Nominal resin properties reported by the manufacturer include a density of 0.917 g/cm³ when determined by ASTM D792 and a melt mass-flow rate of 2.3 g/10 min under ASTM D1238 at 190 °C and 2.16 kg. Differential scanning calorimetry places the peak melting temperature near 123 °C, and the Vicat softening temperature is approximately 94 °C per ASTM D1525. This melt-flow rate positions the grade for cast film rather than blown film; cast film lines rely on chill-roll quenching and a short melt draw-down distance.
The C8 comonomer distribution differentiates the product from butene-based LLDPE cast film grades. Hexyl branches disrupt crystallizable ethylene sequences more effectively at a given density than ethyl branches, shifting the balance between lamellar thickness and tie-chain concentration. The significance is not simply density reduction; it is the placement of short-chain branches along the chain that governs low-temperature fracture and seal behavior in converter films. The grade’s narrow molecular weight distribution, typical of solution LLDPE, reduces the high-gel population that can form in some gas-phase polymerization processes and contributes to optical uniformity after cast quenching.
Because the base resin is not formulated as a high-cling or high-slip system, surface additives such as erucamide and silica antiblock must be introduced at the converter level when coefficient of friction control is required. The grade is supplied with an antioxidant package intended for melt stability during cast film processing; it is not a retortable film grade unless the finished structure is qualified for retort use.
In monolayer cast film, the octene-derived branch distribution expresses itself in ASTM D1922 Elmendorf tear and ASTM D1709 Method A dart impact, but the measured values are not resin constants. Quench rate, die gap, melt draw ratio, and chill-roll temperature alter crystalline orientation and amorphous tie-chain orientation. Film produced at 25 µm total gauge on a 0.7 mm die gap and a chill roll set at 20 °C typically develops machine-direction orientation; transverse-direction tear is consequently lower than machine-direction tear. Converter measurements on octene LLDPE of this density class often show MD/TD tear anisotropy of 1.5:1 to 2.0:1. Grade-specific values for 2247A must be generated on the actual line because additive masterbatches and edge trim recycle affect tear propagation.
Tie-chain formation in linear polyethylene is a consequence of melt draw and quench under high stress. When 2247A is drawn from a 0.7 mm die gap to 25 µm film, extensional stress orients chains. Rapid quenching by a 20 °C chill roll traps a fraction of oriented chains and reduces lamellar thickness; a slower quench permits relaxation and thicker lamellae with lower toughness. The same pellet can therefore yield different tear values across a 5 °C roll temperature shift. The processing window for consistent physical properties is narrow, and chill roll temperature is normally held within ±3 °C to avoid large mechanical property changes.
Seal initiation is evaluated using ASTM F88 or ASTM F2029. Octene comonomer depresses the crystalline melting onset and allows seal formation at temperatures 10–20 °C below butene LLDPE grades of the same density class. However, the precise seal initiation temperature of 2247A depends on film thickness, sealing dwell time, jaw temperature uniformity, and chill-roll-induced surface crystallinity. Published heat-seal curves specific to 2247A below 25 µm are limited; converter trials should replace supplier typical values for commercial release decisions.
Industrial cast film lines running DOWLEX 2247A are typically configured with single-screw extruders having L/D ≥ 30:1, barrier screws, and screen packs of 60/80/100 mesh. A gear pump downstream of the extruder is used to damp pressure oscillations. The adapter and die zones are maintained at 240–260 °C; die temperatures above 270 °C accelerate oxidative gel formation if melt hold-up exceeds 10–15 min. A flat die gap of 0.5–0.8 mm is a suitable starting point for thin-gauge cast film. If sharkskin appears above 150 m/min, the corrective sequence is to widen the die gap to 0.8–1.0 mm, raise melt temperature within the specified ceiling, and add a fluoropolymer processing aid masterbatch at 200–800 mg/kg. The air gap between die exit and chill roll is normally 25–40 mm; longer air gaps increase neck-in and reduce melt curtain stability. Draw resonance, visible as sinusoidal gauge variation along the machine direction, may initiate when the draw ratio exceeds 4:1 to 6:1. Short air gap, reduced melt temperature, and lower line acceleration are the standard responses.
| Parameter | Typical starting range | Equipment or measurement basis |
|---|---|---|
| Melt temperature at die | 240–260 °C | Melt thermocouple at adapter |
| Flat die lip gap | 0.5–0.8 mm | Flexible-lip flat die |
| Chill roll temperature | 15–25 °C | Spiral baffle chill roll |
| Air gap | 25–40 mm | Die-to-roll gap |
| Line speed | 100–300 m/min | Nip section encoder |
| Extruder L/D | ≥30:1 | Barrier single-screw |
| Screen pack | 60/80/100 mesh | Stainless steel screens |
The chill roll is not a passive heat exchanger. Roll temperatures above 30 °C slow quench, increase spherulite size, and raise haze measured per ASTM D1003. At constant throughput, increasing chill roll temperature from 15 °C to 35 °C can reduce dart impact and lower film toughness in this density class; the magnitude is matrix-dependent and not a linear function of roll setpoint. Film gloss measured by ASTM D2457 at 45° is similarly coupled to quench and die-lip cleanliness. Cast film converters therefore control roll temperature, water flow rate, and roll surface roughness as primary variables, not secondary settings.
Capillary rheometry at 190 °C may be used to compare lot-to-lot process consistency. Linear low-density polyethylenes of 2.3 g/10 min melt index typically exhibit apparent viscosity in the range of 150–1,000 Pa·s between 1,000 s⁻¹ and 100 s⁻¹. A rise in die pressure greater than 15–20 % at constant throughput suggests gel accumulation, screen blockage, or contamination from incompatible recycle. These threshold values guide shift operators more reliably than visual observation alone; grade-specific capillary data for 2247A should be collected from the user’s own lot with a standardized instrument and known die length-to-diameter ratio.
Edge trim from cast film is typically returned to the extruder at 10–20 % of the screw feed in industrial practice. If trim has been corona-treated, the oxidized surface can generate gel upon re-melting; a blend cap of 20 % by weight is commonly applied to limit gel accumulation. Consecutive batches of 2247A may show melt index variation of ±0.2 g/10 min; operators use a ±3 % throughput adjustment to compensate for viscosity shifts. Film defect detection on the line uses optical inspection and thickness scanning systems; gauge variation above ±2 % over 1 m of film indicates draw resonance or die lip fouling.
Melt fracture and sharkskin are distinct defects. Sharkskin appears as fine surface roughness at the die lip and is related to high shear stress at the polymer/metal interface; a fluoropolymer processing aid migrates to the die surface and lowers interfacial stress. Die drool, if observed, may be reduced by raising die temperature or using a fluoropolymer processing aid; the melt temperature should not exceed 270 °C for routine operation.
Direct substitution of DOWLEX 2247A into structures designed for high-pressure LDPE alters melt elasticity. High-pressure LDPE contains long-chain branches that stabilize the melt curtain and reduce die-to-web neck-in; DOWLEX 2247A is linear and lower in melt strength at equivalent melt index. A 2.0 g/10 min LDPE typically has enough melt elasticity to permit air gaps above 40 mm; 2247A may develop edge bead and gauge variability under the same conditions. Therefore, the air gap is reduced toward 25 mm and edge pinning is used. Blending 10–30 % by weight of high-pressure LDPE into the 2247A layer reduces melt curtain instability while preserving much of the low-temperature toughness. The blend ratio is not fixed; a die lip set at 0.6 mm and a line speed of 150 m/min may require less LDPE than a line running 250 m/min.
Compared with butene LLDPE of the same melt index class, DOWLEX 2247A has a lower seal initiation onset and higher puncture resistance, as measured by ASTM F88 and ASTM F1306. This is an inherent consequence of the octene short-chain branch length and distribution. Compared with metallocene ethylene-octene grades, 2247A may show lower dart impact and lower gloss but often provides broader processing latitude due to its molecular weight distribution. Published side-by-side comparative data across supplier grades are limited; the appropriate comparison is made on the converter’s own cast line using film at the target gauge and with the same additive masterbatch.
Sealant layers in coextruded cast film are a primary use case. In a 3-layer A/B/A construction, 2247A may occupy the sealant layer while high-pressure LDPE skins provide melt curtain stability. Corona treatment to 38–42 mN/m wetting tension, measured by ASTM D2578, is applied before lamination or printing. Solventless polyurethane adhesives bond the treated 2247A surface to biaxially oriented PET or BOPP; adhesion is evaluated by ASTM D1876. For produce overwrap, anti-fog masterbatch is added at the converter level; the base resin does not provide anti-fog function.
In hygiene backsheet and industrial lamination, the film is often compounded with calcium carbonate masterbatch or coextruded with filled layers. Tensile targets are set according to ASTM D882, and tear targets according to ASTM D1922 on the final laminated or filled structure, not on monolayer resin samples. Slip and antiblock additives are required for high-speed packaging operations; erucamide at 500–1,000 ppm and silica antiblock at 1,000–3,000 ppm are typical starting concentrations. These additives influence the coefficient of friction measured by ASTM D1894 and reduce seal strength at levels above the target range; over-addition increases haze and may affect lamination adhesion.
Cast film structures that include EVOH or polyamide barrier layers require an approved tie resin because 2247A is not inherently compatible with high-polarity polymers. The grade also is not formulated as a cling layer for stretch film; where cling performance is required, polyisobutylene tackifier or a coextruded cling layer must be incorporated. Pre-stretch ratios above 200 % require converter validation on the specific stretch film line and die configuration.
Compliance is a property of the finished article, not the resin alone. In the United States, this polymer type may be used in food-contact films when the finished film satisfies 21 CFR 177.1520(c); the converter must verify extractives and end-use restrictions for the specific application. For Europe, the finished film must meet Regulation (EU) No 10/2011 overall migration and specific migration requirements under the relevant food simulants. REACH registration under Regulation (EC) No 1907/2006 is maintained by the manufacturer or importer; the safety data sheet should be checked for the resin batch. DOWLEX 2247A is not intentionally formulated with phthalates or bisphenol A, but logistical contamination from shared silos or transfer lines should be assessed before medical or sensitive-application claims are made.
| Compliance condition | Framework | Converter verification |
|---|---|---|
| Olefin polymer food-contact use | 21 CFR 177.1520(c) | Finished film extractives and end-use restrictions |
| Plastic food-contact migration | EU 10/2011 | Overall and specific migration by food simulant |
| Chemical registration and SVHC screening | Regulation (EC) No 1907/2006 | Safety data sheet and SVHC list |
| Heavy metal restrictions | RoHS Directive 2011/65/EU | Supplier certificate and material screening |
Processing constraints are as important as regulatory boundary conditions. Melt temperature should not remain above 280 °C for extended hold-up. Outdoor storage that permits surface condensation above 70 % relative humidity can introduce moisture into the feed throat; drying at 60–70 °C for 2 hours is used when condensation is observed. Blending with ionomers without tie-layer design can produce delamination and unstable melt curtains. Long melt hold-up in transfer lines above 260 °C can result in oxidized gel, yellowing, and a shift in melt flow index; purge with LDPE before shutdown is standard practice. These boundaries are operational rules for stable cast film production, not post-conversion performance claims.